• 제목/요약/키워드: wood discoloration

검색결과 62건 처리시간 0.02초

목재(木材)의 오염(汚染)에 의한 변색(變色) (2) - 한국산(韓國産) 활엽수재(闊葉樹材)의 화학적(化學的) 변색(變色) - (Discoloration of Woods (2) - 36 Commercial Hardwoods Grown in Korea -)

  • 안경모;공영토;조재명
    • Journal of the Korean Wood Science and Technology
    • /
    • 제14권1호
    • /
    • pp.55-60
    • /
    • 1986
  • Discoloration sensitivities of woods grown in this country haven't reported yet. Therefore we examined discoloration sensitivities of domestic wood specimens to iron (0.1 %, $FeCl_3.6H_2O$), alkali (pH 12.0, NaOH). acid (pH 1.0, $C_2H_2O_4$) and exposing to sunlight (40 hrs), Thirty-six hardwood species were collected and examined. All specimens were prepared from heartwoods of the collected species. But the specimens of 4 Betula species were divided into sapwoods and heartwoods. By iron stain, the color differences (${\Delta}E$) of 21 wood specimens including one Betula sapwood showed above 12.0, which means strong discoloration sensitivities, and of 3 specimens including one Betula sapwood showed below 2.5, which means weak discolorations. The most strong iron discoloration species was Jungkukgulpi-namu (Pterocarya stenoptera). By alkali stain, the color differences (${\Delta}E$) of 3 wood specimens showed above 9.0, which means strong discoloration sensitivities, and of 18 wood specimens including 4 Berula sapwoods showed below 2.5, which means weak discolorations. By acid stain, the color differences (${\Delta}E$) of 6 wood specimens showed above 10.0 which means strong discoloration sensitivities, and of 12 wood specimens including one Betula sapwoods showed below 2.5, which means weak discolorations. By exposing to sunlight, the color differences (${\Delta}E$) of 31 wood specimens including one Betula sapwoods showed below 6.5, which means, strong discoloration sensitivities, and of only one specimens showed below 2.5, which means weak discoloration. The most strong discoloration species by exposing to sunlight was Guirung-namu (Prunus padus). In general, it was shown that hardwoods grown in Korea were most subject to change of color by exposing to sunlight and next were by iron stain. Domestic hardwoods showed some differences in discoloration sensitivities from domestic softwoods previously reported.

  • PDF

Furfurylation Effects on Discoloration and Physical-Mechanical Properties of Wood from Tropical Plantation Forests

  • HADI, Yusuf Sudo;HERLIYANA, Elis Nina;PARI, Gustan;PARI, Rohmah;ABDILLAH, Imam Busyra
    • Journal of the Korean Wood Science and Technology
    • /
    • 제50권1호
    • /
    • pp.46-58
    • /
    • 2022
  • Wood from tropical plantation forests has lower physical and mechanical properties than mature wood. Furfuryl alcohol (FA) impregnation into the wood could help to enhance hydrophobic properties, dimensional stability, and structural strength. Furfurylation was applied to specimens of the following four fast-growing tropical wood species: jabon (Anthocephalus cadamba), sengon (Falcataria moluccana), mangium (Acacia mangium), and pine (Pinus merkusii). The discoloration and physical and mechanical properties were subsequently measured, and the results showed that furfurylated wood had a darker color and better physical and mechanical properties than untreated wood. Specifically, the furfurylated wood had higher density, modulus of elasticity, and hardness and lower moisture content, water absorption, swelling, and shrinkage. The furfurylation significantly enhanced physical and mechanical properties.

은행나무 목재의 가공적 성질 (Processing Properties of Ginkgo Wood)

  • 김규혁;김재진;조재성
    • 한국가구학회지
    • /
    • 제11권2호
    • /
    • pp.37-43
    • /
    • 2000
  • Ginkgo trees have long been planted in Korea as roadside trees and ornamental trees, but the wood was seldom used except some utilization f3r small artifacts. Soaring prices of imported wood and future uncertainty about long-term supply of foreign woods have stimulated research on value-added utilization of less-utilized domestic wood resources such as Ginkgo wood. The processing properties of Ginkgo wood were investigated to determine its utilization potential in this study, and the results of treatability, drying characteristics, gluability, paintability, bending properties, chemical discoloration characteristics were presented.

  • PDF

Peracetic Acid Treatment as an Effective Method to Protect Wood Discoloration by UV Light

  • PARK, Kyoung-Chan;KIM, Byeongho;PARK, Hanna;PARK, Se-Yeong
    • Journal of the Korean Wood Science and Technology
    • /
    • 제50권4호
    • /
    • pp.283-298
    • /
    • 2022
  • Wood has always been used for various day-to-day applications such as interior or exterior construction materials, and household products. However, it can undergo photodegradation and discoloration by environmental factors including ultraviolet (UV) light, and thus has shortened its service life. Bleaching or delignification of wood surfaces is a suitable solution to stabilize wood against weathering by UV because these techniques can alter or remove the chromophores in lignin, which is a main factor of wood discoloration. To improve the color stability of wood surface according to the lifespan, surface delignification was conducted using peracetic acid (PAA) and hydrogen peroxide (HP) on the woods of Larix kaempferi and Quercus mongolica. After the PAA treatment, L* increased considerably from 60-70 to 90-95. Furthermore, wood surface color did not change significantly after UV exposure. The color differences (𝜟E*) between before and after PPA treatment of wood showed the 4.8-12.2 of L. kaempferi, and 1.7-3.7 of Q. mongolica, respectively. The lignin-related peaks in Fourier transform infrared spectroscopy (FT-IR) spectra disappeared with increased duration of PAA treatment. These results confirmed that the lignin component was partially or completely removed after the PAA treatment; the color differences (𝜟E*) clearly showed that there was a reduction in redness (a*) and yellowness (b*), and an increase in lightness (L*) owing to the removal of lignin. Based on these results, this study demonstrated that the partial removal of lignin from wood surfaces is a fundamental method for resolving photo-degradation.

Stain Fungi and Discoloration Control on Rubberwood (Hevea brasiliensis Muell. Arg.) by Vacuum-Pressure Treatment with Catechin from Gambir (Uncaria gambir Roxb.)

  • Dodi NANDIKA;Elis Nina HERLIYANA;Arinana ARINANA;Yusuf Sudo HADI;Mohamad Miftah RAHMAN
    • Journal of the Korean Wood Science and Technology
    • /
    • 제51권3호
    • /
    • pp.183-196
    • /
    • 2023
  • Recently, the morphological and molecular features of five stain fungi infecting rubberwood (Hevea brasiliensis), namely Paecilomyces maximus, Paecilomyces formosus, Penicillium crustosum, Paecilomyces lecythidis and Aspergillus chevalieri, have been studied. Prior to this study, the authors revealed that catechin from gambir (Uncaria gambir) could inhibit the growth of the white-rot fungus Schizophyllum commune, and it was important to determine the bioactivity of the aforementioned agent against A. chevalieri. The efficacy of the biocidal agent was examined using a laboratory wooden block test. Rubberwood blocks, 8 mm in thickness, 20 mm in width, and 30 mm in length, were impregnated with catechin solution at concentrations of 6%, 9%, 12%, and 15% (w/v) using the vacuum-pressure method, and their bioactivity was monitored over three weeks through visual and scanning electron microscope assessment of fungal growth as well as the discoloration intensity of the wood samples. The results showed that catechin treatment increased the resistance of wood samples to A. chevalieri. Overall, the higher the catechin concentration, the lower the fungal growth. The lowest fungal growth was observed in the wood samples treated with 12% and 15% catechin (score of 0), demonstrating no discoloration. In contrast, the fungal growth score of the untreated wood samples reached 4, indicating severe discoloration. Catechins appear to be adequate biofungicides against stain fungi in rubberwood.

Biocontrol of Blue Stain in Pine Wood with Lyophilized Mycelium of Ophiostoma quercus Albino Strain

  • Cho, Byung-Ju;Kim, Nam-Kyu;Cho, Nam-Seok;Lee, Jong-Kyu
    • The Plant Pathology Journal
    • /
    • 제24권3호
    • /
    • pp.309-316
    • /
    • 2008
  • Mycelium of Ophiostoma quercus albino strain cultured in liquid culture media was harvested, lyophilized, and stored for examining biocontrol efficacy against wood discoloration by staining fungi in the laboratory and field conditions. Dry weight of mycelium grown in brown sugar yeast extract broth(BYB) showed 3.8 times higher than that grown in potato dextrose broth(PDB). The optimum culture period in BYB was 4 weeks. In vitality test of the albino strain, the lyophilized mycelium stored in liquid nitrogen($-196^{\circ}C$) or in a refrigerator($4^{\circ}C$) kept the vitality until 13 months after storage; however, the mycelium stored at room temperature lost the vitality completely after 13 months. The mycelium stored in liquid nitrogen or in a refrigerator protected wood chips from the discoloration by pretreating mycelial suspension on pine wood chips. The mycelium stored at room temperature for 7 months also showed complete protection. These results suggest that the lyophilized mycelium have a biocontrol efficacy only if it keeps the least vitality. In the field conditions, both albino strain and $Woodguard^{(R)}$(commercial chemical protectant) showed significant differences(p=0.05) in discoloration rate as compared to the non-treated control when these were treated on the wood logs of Pinus rigida. The albino strain showed better protection than $Woodguard^{(R)}$. Isolation frequency of blue stain fungi from the chips of wood logs treated with the albino strain was 0% at three months after treatment, while that treated with $Woodguard^{(R)}$ was 76.7%. In another experiment, pre-treatment of mycelial suspension on the cut surface of wood logs also showed significant protection from wood discoloration. Spraying of both albino strain on the cut surface and insecticides on the bark also showed relatively good control effects as compared to insecticide alone on the bark or nontreated control.

Surface Discoloration of Ultraviolet (UV)-Irradiated Phyllostachys bambusoides Bamboo

  • Hyoung-Woo LEE;Eun-Ju LEE;Yoon-Jung SHIN;Ha-Yeong JO;Dae-Yeon SONG
    • Journal of the Korean Wood Science and Technology
    • /
    • 제51권3호
    • /
    • pp.173-182
    • /
    • 2023
  • Color is an attribute of visual perception and can be an important factor that affects the preference of customers toward bamboo and wood products. Solar radiation can discolor bamboo surfaces and initiate cracking. The purpose of this study is to investigate the effects of an ultraviolet (UV)-protective coating on the photodiscoloration of untreated and heat-treated Phyllostachys bambusoides bamboo surfaces. Artificial UVA radiators are set at a UVA irradiance of 2,000 W/m2 to accelerate the aging of the outer surfaces of hot-air-dried and heat-treated bamboo samples. Half of the samples are coated with transparent UV-protective paint. As the UVA radiation progresses, the discoloration prevention efficiency (DPE) of the UV-protective coating on all samples decreases gradually. The DPEs of the hot-air-dried samples are estimated to be 31.4% and 18.8% after 21 and 72 hours of artificial UVA radiation, respectively. The heat-treated samples exhibit similar trends (29.0% after 21 hours and 10.3% after 72 hours). Recoating the UV-protective paint periodically every six months is expected to minimize the discoloration of the bamboo's outer surface.

색채 목가구 개발을 위한 천연염료의 이용에 관한 연구(제3보) - 천연염색 밤나무 목재의 변색 방지 - (Application of Natural Dyes for Developing Colored Wood Furniture (III) - Prevention of Discoloration of Chestnut Wood by Natural Dyes -)

  • 문선옥;김철환;김경윤;정호경;신태기;김종갑;박종열
    • Journal of the Korean Wood Science and Technology
    • /
    • 제35권3호
    • /
    • pp.79-87
    • /
    • 2007
  • 추출에 의해 얻어진 천연염료로 염색한 착색 밤나무재의 변색방지를 위하여 래커 마감도장시편는 500 lux의 실내광 및 50,000~70,000 lux의 실외광 수준의 광변색, 내산성, 내알칼리성, 내열성 영향을 시편의 색차로 측정하였다. 모든 변색실험에서 래커 마감처리 한 시편이 빛, 산, 알칼리, 온도 등에 기인한 변색방지에 효과를 나타내는 것을 알 수 있었다. 또한 염액의 pH가 알칼리로 짙어질수록 천연염색 가구재의 광변색을 경감시키는데 효과적인 것으로 나타났다.

표백에 의한 라디에타소나무의 청변 제거 (Removing Sapstain of Radiata Pine by Bleaching)

  • 김규혁;김형준;나종범;김재진
    • Journal of the Korean Wood Science and Technology
    • /
    • 제31권1호
    • /
    • pp.46-51
    • /
    • 2003
  • 본 연구는 라디에타소나무 제재목의 균 변색을 제거하기 위한 표백처리의 사용 가능성을 조사하기 위하여 수행하였다. 염소계 표백제인 아염소산나트륨과 차아염소산나트륨은 표백조건(약제농도, 처리온도, 처리시간)의 조절에 따라 만족할만한 변색제거 효과를 얻을 수 있었다. 비염소계 표백제인 과산화수소는 표백조건의 조절만으로는 변색제거가 불가능하였으나 규산나트륨과 수산화나트륨을 활성제로 첨가하는 경우에는 염소계 표백제보다 탁월한 변색제거 효과를 나타내었다. 그러나 활성제 첨가에 따라 재색의 녹색화 문제가 발생하였는데, 앞으로 이러한 문제점을 해결하기 위한 연구가 진행되어야 할 것이다. 또한, 앞으로 본 연구를 통해 개발된 변색제거 방법의 현장 적용을 위한 후속 연구도 필요하다고 본다.

Identification of Sapstain Fungi on Weathered Wooden Surfaces of Buildings at Jangheung and Jeju Island

  • YUN, Jeonghee;SHIN, Hee Chang;HWANG, Won Joung;YOON, Sae-Min;KIM, Yeong-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • 제49권6호
    • /
    • pp.591-601
    • /
    • 2021
  • Recently it is trend to increase wood use as carbon neutral materials, there is recognized to need necessarily durability improvement of wooden building. It is very rare to report existing on the identification of isolates causing discoloration in domestic weathered wooden building used for long period. The objective of this study was identification of fungi that cause discoloration on the exteriors of weathered domestic wooden buildings in the southern part of South Korea. Our findings can be helpful to establish protection technology for weather deterioration of domestic wooden buildings. Wood chip samples presumed to be contaminated with sapstain fungi were collected from the surface of wooden members used in wooden buildings at Jangheung, Jeollanam-do (two locations, #13 and #14), and Jeju Island (two locations, #31 and #33). The growth of microorganisms was confirmed by performing culture tests for the collected samples, and fungi were isolated, purified, and identified. The results indicated that the fungal strains isolated from wooden buildings #13 and #14 at Jangheung, Jeollanam-do, were 99.83% and 100% homologous to Aureobasidium melanogenum, respectively. For wooden building #31 at Jeju Island (two locations), the fungal strain isolated was 100% homologous to A. melanogenum, which is the same species isolated from the wooden buildings at Jangheung. The fungal strain isolated from wooden building #33 (Jeju Island) had 99.83% homology with A. pullulans, which is commonly found in wood degraded by weather or ultraviolet rays. Our findings can be utilized as a basis for establishing protection technology in domestic wooden buildings.