• Title/Summary/Keyword: wetting test

Search Result 201, Processing Time 0.019 seconds

Thermal-Hydro-Mechanical Behaviors in the Engineered Barrier of a HLW Repository: Engineering-scale Validation Test (고준위폐기물처분장 공학적방벽의 열-수리-역학적 거동 연구: 엔지니어링 규모의 실증실험)

  • Lee, Jae-Owan;Cho, Won-Jin
    • Tunnel and Underground Space
    • /
    • v.17 no.6
    • /
    • pp.464-474
    • /
    • 2007
  • An enhancement in the performance and safety of a high-level waste repository requires a validation of its engineered barrier. An engineering-scale test (named "KENTEX") has been conducted to investigate the thermal-hydro-mechanical behaviors in the engineered barrier of the Korean reference disposal system The validation test started on May 31, 2005 and is still under operation. The experimental data obtained allowed a preliminary and qualitative interpretation of the thermal-hydro-mechanical behaviors in the bentonite blocks. The temperature was higher as it became closer to the heater, while it became lower as it was farther away from the heater. The water content had a higher value in the part close to the hydration surface than that in the heater part. The relative humidity data suggested that a hydration of the bentonite blocks might occur by different drying-wetting processes, depending on their position. The total pressure was continuously increased by the evolution of the saturation front in the bentonite blocks and thereby the swelling pressure. Near the heater region, there was also a significant contribution of the thermal expansion of bentonite and the vapor pressure in the pores of the bentonite blocks.

Corrosion Protection Method of Reinforcing Steel in Concrete by Using Corrosion Inhibitors

  • Bae Su-Ho;Chung Young-Soo;Kim Dae-Ho
    • KCI Concrete Journal
    • /
    • v.14 no.4
    • /
    • pp.145-150
    • /
    • 2002
  • Reinforced concrete is inherently a durable composite material. When properly designed for the environment to be exposed and carefully constructed, reinforced concrete is capable of giving maintenance-free performance. However, unintentionally using improper materials such as non-washed sea sand having much salt together with poor controlled quality, or the concrete are placed in highly severe environment such as marine atmosphere, the corrosion of reinforcing steel in concrete becomes one of the most significant concerns of concrete. The purpose of this experimental research is to evaluate the performance of corrosion inhibitors for normal strength and high strength concrete, and to propose desirable measures for controlling corrosion of reinforcing steel in concrete. Test specimens in normal strength and high strength concrete were made with and without corrosion inhibitors. The accelerated corrosion test for reinforcing steel in concrete was adopted in accordance with JCI-SC3, which required the periodic 20 cycles for 140 days. One cycle includes 3 days for the wetting condition of $65^{\circ}C$ and $90\%$ RH, and 4 days for the drying condition of $15^{\circ}C\;and\;60\%$ RH. It was observed from the test that corrosion inhibitors in normal strength concrete and high strength concrete showed excellent corrosion resistance for reinforcing steel in concrete, but the silica fume in high strength concrete was found to have a negligible corrosion resistance if not used with corrosion inhibitors, since the chloride corrosion threshold limit in concrete containing silica fume without corrosion inhibitor was found to be considerably smaller than that of the case with corrosion inhibitor.

  • PDF

Studies for ENIG surface behavior of FCBGA through the time by using water dip test method

  • Shin, An-Seob;Kim, Jeom-Sik;Ok, Dae-Yool;Jeong, Gi-Ho;Park, Chang-Sik;Heo, Cheol-Ho;Lee, Kum-Ro
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.412-412
    • /
    • 2008
  • ENIG(Electroless Nickel Immersion Gold)is a surface treatment method that is used most widely at fine pitch's SMT and BGA packaging process. ENIG has good diffusion barrier of Ni against solder and good wettability due to Au finish. But when the discoloration occurred on the Au finish of ENIG, some key characteristics related to the quality and reliability of PCB such as bondability, solderability and electrical flowing of packaging process could be deteriorated. In this paper, we have performed the water dip test ($88^{\circ}C$ purified water) which accelerates the galvanic corrosion of Ni diffused from the Ni-P layer. That is, the excessive oxidation of the Ni layer could result in non-wetting of the solder because the flux may not be able to remove excessive oxides. Though Au discoloration have been reported to be caused by Ni oxides in many literature, it is still open to verify and discuss The microstructures and chemical compositions have been investigated using FE-SEM, TEM, FIB, EDS and XPS. As a result, authors have found that the Au discoloration in ENIG type is severely caused by the oxidation of the Ni and the mechanism of Au discoloration can be confirmed through the experiment result of water dip test.

  • PDF

A Study on the Dust Control Effect of PM10 Dust Inhibitor by Polysaccharides and its Effect on Water Quality and Soil Environment (Polysaccharides를 이용한 PM10 먼지억제제의 먼지제어 효과와 수질 및 토양 환경에 미치는 영향에 대한 연구)

  • Lee, Han Seob;Choi, Sung Boo;Hwang, Su Jin;Hwang, Hyun Seok
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.39 no.2
    • /
    • pp.59-65
    • /
    • 2017
  • In this study, A dust inhibitor for $PM_{10}$ was prepared by using molecular structure, molecular weight, viscosity, hydrophilicity, swelling and wetting / moisturizing properties of natural polysaccharide which is widely used as food and cosmetic materials. Various dust control effects were confirmed and superior results were obtained than simple water spraying and synthetic PVA as a control. In addition, the comparison of water evaporation, pot test of cabbage seed germination, effects on fish and aquatic plants, and effects on herb plant growth were studied and the safety of soil and water quality was studied. The availability of the dust inhibitor was confirmed.

Digital Image Analysis (DIA) for Estimating the Degree of Saturation of The Soil-Water Characteristic Curves (SWCC) (SWCC의 포화도를 구하기 위한 DIA 적용)

  • Min, Tuk-Ki;Huy, Phan Thieu
    • Journal of the Korean Geotechnical Society
    • /
    • v.24 no.3
    • /
    • pp.53-63
    • /
    • 2008
  • The aim of this study was to validate the suitability of an digital image analysis (DIA) method to measure the degree of saturation in the unsaturated conditions. This study was carried out on the Joo-Mun-Jin standard sand. A one-dimensional sand column test was used in the constant water level condition to get the correlation equation between the color number ($C_n$) and the measured degree of saturation (5). In addition, the hanging wale. column technique to determine the soil-water charactenstic curve (SWCC) was performed in a Buchner funnel. The average degree of saturation ($S_{ave}$) in the SWCC could be obtained by substituting average color number at each suction head value with the $C_n\;-\;S$ correlation equation. Comparisons were made between the measured results by the hanging water column test and those obtained from DIA method. Results showed that the DIA method tested here provided fairly good saturation distribution values in the drying and wetting processes.

The Application of Surfactants to the Suppression of Fugitive Dust Generated from the Scrap Metal Loading Field in Inchon Port and Preliminary Evaluation on Their Wetting Capability (인천항 고철 하역 작업시 발생하는 비산분진 억제를 위한 계면활성제의 적용 및 기초 성능 평가)

  • Lee, Bo-Young;Yoo, Yong-Ho;Jung, Yong-Won;Kim, Jin
    • Journal of Korean Society for Atmospheric Environment
    • /
    • v.17 no.1
    • /
    • pp.85-96
    • /
    • 2001
  • The objective of this study is to develop the water spraying which can effectively by applied to the control or suppression of the fugitive dust generated from the scrap metal handling area at the Port of Inchon. As a first step toward this goal, we carried out some preliminary analyses on the chemical composition, physical shape, and particle size distribution of the sample dust. Next, to quantitatively investigate the effect of adding surfactants to the spraying water on the wettability of the sample dust, the Standard Sink Test was carried out for four different surfactants and at six different concentrations using the surfactants considered in this study. Results of from the preliminary analysis indicated that the main chemical component consisting of the sample dust is Goethite(FeO(OH)) and that the particles smaller than 10 ${\mu}{\textrm}{m}$ in geometric diameter occupy about 36% of the sample dust in mass. This result implies that the fugitive dust generated from the scrap metal handling area at the Port of Inchon should affect the environment nearby more than we have expected. This is because of relatively large mass percentage of the small metal particles less than 10${\mu}{\textrm}{m}$ in geometric diameter, what we may call respirable particles. As for the results of the Standard Sink Test, higher surfactant concentration tends to result in the higher wettability of the sample dust for the surfactants considered in this study, which in turn ensures the high particle collection efficiency of the droplets generated from the water spraying system. Based upon this preliminary results, studies to develop more sophisticated scaled model for dynamic test in underway and the effort to find the best surfactants as well as the optimum operating conditions are being made at the same time.

  • PDF

The flexural strength Changes by the Low Temperature Degradation of Uncolored zirconia Ceramic for All Ceramic Restoration (전부도재 수복을 위한 무색지르코니아 세라믹의 저온열화에 따른 굴곡강도 변화)

  • Kim, Jung-Sook
    • Journal of Technologic Dentistry
    • /
    • v.31 no.2
    • /
    • pp.39-44
    • /
    • 2009
  • In the orthopedic field which firstly used zirconia as artificial joints, researchers had studied the reasons for collapsing zirconia used as restorative material by accumulated inner cracks in several years and they found out Low Temperature Degradation is one of the reasons. In the dentistry field, it has not been too long since they used zirconia as the cores of all-ceramic restoration; however, the study is needed as prophylactic measure against Low Temperature Degradation which can be caused by saliva wetting the mouth all the time and frictional forces such as bite pressure and masticatory pressure. Artificial aging by autoclaving is used because there are difficulties of testing in the patient's mouth. To study the changes in the material properties, the flexural strength of dental zirconia ceramic is measured before and after the test. The following are the result of the test. 1) The zirconia blocks in the autoclaves at $130^{\circ}C$ and $200^{\circ}C$ are phase-shifted tetragonal to monoclinic by Low Temperature Degradation. 2)The non-autoclaved specimens have the average fractural strength of 1346.4MPa, the specimens autoclaved at $130^{\circ}C$ have 1226.4Mpa and the specimens autoclaved at $200^{\circ}C$ have 1024.1MPa. The tests show that as the temperature increases, the flexural strength tend to decrease and the differences are noticeable(p<0.001). 3)Through the Duncan's post-hoc test, the differences in flexural strength of the 3 groups were listed in order of strength like normal temperature>at $130^{\circ}C$ autoclave low temperature degradation> at $200^{\circ}C$ autoclave low temperature degradation.

  • PDF

A Study on the Basic and Compression Characteristics of Lightweight Waste for Use as Fill Materials (성토재 적용을 위한 경량폐기물의 기본물성 및 압축특성 연구)

  • Lee, Sung-Jin;Kim, Yun-Ki;Koh, Tae-Hoon;Lee, Su-Hyung;Shin, Min-Ho
    • Journal of the Korean Geotechnical Society
    • /
    • v.27 no.5
    • /
    • pp.61-74
    • /
    • 2011
  • This is a fundamental research on use as fill material of lightweight waste such as bottom ash and tire shred. We carried out the test for particle size distribution, specific gravity, density, shear strength, permeability and vertical compression settlement, considering water content change and temperature effect of several waste materials. Bottom ash, which is lighter than soils, has similar permeability and particle size distribution to those of weathered soils. But permeability may differ depending on the particle size distribution. The shear strength aspect of bottom ash and tire shred mixed materials are similar to that of natural fill materials. In the 1-D vertical compression settlement test, we could be assured that bottom ash and tire shred mixed materials showed similar compression settlement to that of sand under actual vertical stress. Furthermore, materials including bottom ash showed smaller compression settlement than that of weathered soils in the long-term settlement test under wetting and freezing-thawing condition.

Study on the Soldering of Off-eutectic Pb-Sn Solders in Partial Melting State

  • Park, Jae-Yong;Ha, Jun-Seok;Kang, Choon-Sik;Shin, Kyu-Sik;Kim, Moon-Il;Jung, Jae-Pil
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.7 no.2
    • /
    • pp.63-68
    • /
    • 2000
  • This paper introduces the partial melting process for solder application and characterization of its possibility using off-eutectic Pb-Sn alloy. In order to show that the liquid phase in the semi-liquid state maintains the wettability as the single-phase liquid, the wetting balance test are conducted with varying temperatures and compositions. The results are then compared with the surface tension of liquid, both measured and calculated, to examine the correlation. The results from this investigation indicate that the partial melting can yield satisfactory solder joints as long as the liquid phase acquires sufficient chemical activity. At a condition where the partial melting is effective, a direct correlation between the wettability and the surface tension is found to exist. All alloys are found to show a reasonable wettability in semi-liquid state.

  • PDF

Strength and durability characteristics of biopolymer-treated desert sand

  • Qureshi, Mohsin U.;Chang, Ilhan;Al-Sadarani, Khaloud
    • Geomechanics and Engineering
    • /
    • v.12 no.5
    • /
    • pp.785-801
    • /
    • 2017
  • Biopolymer treatment of geomaterials to develop sustainable geotechnical systems is an important step towards the reduction of global warming. The cutting edge technology of biopolymer treatment is not only environment friendly but also has widespread application. This paper presents the strength and slake durability characteristics of biopolymer-treated sand sampled from Al-Sharqia Desert in Oman. The specimens were prepared by mixing sand at various proportions by weight of xanthan gum biopolymer. To make a comparison with conventional methods of ground improvement, cement treated sand specimens were also prepared. To demonstrate the effects of wetting and drying, standard slake durability tests were also conducted on the specimens. According to the results of strength tests, xanthan gum treatment increased the unconfined strength of sand, similar to the strengthening effect of mixing cement in sand. The slake durability test results indicated that the resistance of biopolymer-treated sand to disintegration upon interaction with water is stronger than that of cement treated sand. The percentage of xanthan gum to treat sand is proposed as 2-3% for optimal performance in terms of strength and durability. SEM analysis of biopolymer-treated sand specimens also confirms that the sand particles are linked through the biopolymer, which has increased shear resistance and durability. Results of this study imply xanthan gum biopolymer treatment as an eco-friendly technique to improve the mechanical properties of desert sand. However, the strengthening effect due to the biopolymer treatment of sand can be weakened upon interaction with water.