다성분계 산화물의 요업재료 제조를 위한 석유 증발 건조 방법 (Hot Petroleum Drying Method to the Preparation of Multicomponent Oxide Ceramic Material)

  • 변수일
    • 한국세라믹학회지
    • /
    • 제14권3호
    • /
    • pp.163-168
    • /
    • 1977
  • As a wet chemical drying process "hot petroleum drying method" was applied and developed for preparing uniformly fine oxide powder with high purity and sinterreactivity. Using this method solution of sulfates was dried in hot petroleum bath (~17$0^{\circ}C$) to sulfate powder from which corresponding mullite doped by Fe3+ ion was formed. Particle size, shape, decomposition by heat, and phase identification of sulfate andoxide powders determined by DTA, TGA, X-ray diffraction, analysis and electron microscopy: sulfate powder prepared by this drying method is an intimate mixture of the amorphous form of uniformly and finely distributed spherical particles (0.05-0.1$\mu$). Mullitization with the sulfate powder occurs at 110$0^{\circ}C$ in air. The morphology of mullite particle made by firing the sulfate powder at 135$0^{\circ}C$ in oxygen atmosphere is granular of 0.1-0.3$\mu$ in size. This drying process proved to be a very effective method for preparing fine, homogeneous, and highly sinterreactive multicomponent oxide powder without conventional ceramic process of mixing, milling, and granulating. This process can be also applied for preparing electronic ceramic materials which are requisite for high purity and homogeneity.mogeneity.

  • PDF

규석 분말의 교반형 볼 밀 분쇄효율에 미치는 열처리의 영향 (Effect of Heating Treatment of Silica Powder on Stirred Ball Milling Efficiency)

  • 김병곤;박종력;최상근;이재장
    • 한국세라믹학회지
    • /
    • 제40권7호
    • /
    • pp.696-701
    • /
    • 2003
  • 교반형 볼 밀에서 실리카 분말의 열처리에 따른 분쇄효율을 분쇄에 따른 에너지 소비량을 측정함으로써 조사하였다. 열처리를 행한 것과 행하지 않은 시료를 비교해 보면, 600~90$0^{\circ}C$에서 열처리 후 실온에서 냉각된 시료를 건식 분쇄하였을 경우 약 40~50% 정도, 열처리 후 물속에서 급속 냉각한 경우 약 52~62% 정도의 에너지의 감소 효과가 있었다. 또한 열처리한 실리카 분말을 습식 분쇄를 할 경우 건식 분쇄에 비하여 약 40% 정도의 분쇄에너지가 적게 소모되고 있음을 알 수 있었다. 또한 실리카 분말을 열처리 한 후, 급속 냉각할 경우 발생하는 열충격은 입도에 대한 영향을 거의 받지 않으며 분쇄효과를 향상시킴을 알 수 있었다.

음향주파수 분석에 의한 엔드밀의 마모상태 추정에 관한 연구 (A Study on the Wear Estimation of End Mill Using Sound Frequency Analysis)

  • 이창희;조택동
    • 대한기계학회논문집A
    • /
    • 제27권8호
    • /
    • pp.1287-1294
    • /
    • 2003
  • The wear process of end mill is so complicated process that a more reliable technique is required for the monitoring and controlling the tool life and its performance. This research presents a new tool wear monitoring method based on the sound signal generated on the machining. The experiment carried out continuous-side-milling for 4 cases using the high-speed-steel end mill under wet condition. The sound pressure was measured at 0.5m from the cutting zone by a dynamic microphone, and was analyzed at frequency domain. As the cutter impacts the workpiece surface, a situation of farced vibration arises in which the dominant forcing frequency is equal to the tooth passing frequency of the cutter. The tooth passing frequency appears as a harmonics form, and end mill flank wear is related with the first harmonic. It is possible to detect end . mill flank wear. This paper proposed the new method of the end mill wear detection.

Verneuil법에 의한 $SiO_2$를 첨가한 Sapphire 단결정 성장 (SiO2 Doped Sapphire single Crystal Growth by Verneuil Method)

  • 조현;오근호;최종건;박한수
    • 한국세라믹학회지
    • /
    • 제29권10호
    • /
    • pp.822-826
    • /
    • 1992
  • SiO2 doped sapphire single crystals were grown by Verneuil method using feed material which prepared by adding SiO2 in Al2O3. Crystal growing were attempted with varing doping amount of SiO2 from 0.01 to 1.0 wt% and when the doping amount of SiO2 were 0.01~0.04 wt%, single crystals could be attained. Starting materials for feed powder were 99.99% purity alumina and extra pure SiO2 powder. Mixing these two materials by wet milling for 24 hours and drying the mixture and then was calcined at 900~110$0^{\circ}C$ for 2~4 hours. The grown crystals had yellowish color and were somewhat transparent. During growing process the flow range of oxygen was 5~7.5ι/min and of hydrogen was 13~25ι/min, the average growth rate was 7.0~11 mm/hr. The pressure of gases were fixed at 5psi. The color of crystal was appeared and mechanical property of sapphire was developed by doping of SiO2.

  • PDF

CeO2의 첨가량 변화에 따른 세리아 안정화 지르코니아 세라믹스의 기계적 특성 관찰 (Mechanical Properties Observation of Ce-TZP Ceramics by Quantity Change of CeO2)

  • 강종봉
    • 한국세라믹학회지
    • /
    • 제47권5호
    • /
    • pp.439-444
    • /
    • 2010
  • The usual ceramic process of mixing and milling in state of oxide of $ZrO_2$ and $CeO_2$ was adopted in wet process to manufacture Ce-TZP in this study. The maximum dispersion point of every slurry manufactured with mixture of $ZrO_2$ and $CeO_2$ was neat at pH10. The stable slurry in average particle size of 90 nm can be manufactured when it is dispersed with use of ammonia water and polycarboxylic acid ammonium. The sintered Ce-TZP ceramics manufactured with addition of $CeO_2$ less than 10 mol% was progressed to the fracture of specimen due to the monoclinic phase existence more than 30% at the room temperature. More than 99% of tetragonal phase was created for the sintered body with addition of $CeO_2$ beyond 18 mol%, but the mechanical property degrade on the entire specimen was brought due to the $CeO_2$ existing above 3%. Consequently, the optimal Ce-TZP combined in oxide state was identified in 16 mol% of $CeO_2$ contents.

플라즈마 이온질화에 의한 Fe 나노분말소결체의 표면경화 가능성 연구 (A Feasibility Study on the Surface Hardening of Sintered Iron Nanopowder by Plasma Ion Nitriding)

  • 윤준철;이재성
    • 한국분말재료학회지
    • /
    • 제19권1호
    • /
    • pp.13-18
    • /
    • 2012
  • This study has been performed on the full density sintering of Fe nanopowder and the surface hardening by plasma ion nitriding. The Fe sintered part was fabricated by pressureless sintering of the Fe nanopowder at $700^{\circ}C$ in which the nanopowder agglomerates were controlled to have 0.5-5 ${\mu}m$ sized agglomerates with 150 nm Fe nanopowders. The green compact with 46% theoretical density(T.D.) showed a homogeneous microstructure with fine pores below 1 ${\mu}m$. After sintering, the powder compact underwent full densification process with above 98%T.D. and uniform nanoscale microstructure. This enhanced sintering is thought to be basically due to the homogeneous microstructure in the green compact in which the large pores are removed by wet-milling. Plasma ion nitriding of the sintered part resulted in the formation of ${\gamma}$'-$Fe_4N$ equilibrium phase with about 12 ${\mu}m$ thickness, leading to the surface hardening of the sintered Fe part. The surface hardness was remarkably increased from 176 $H_v$ for the matrix to 365 $H_v$.

X-ray 회절의 반치전폭(FWHM)을 이용한 Y-TZP세라믹스에서 반복 열응력에 의한 입계크기 분석 (Grain Size Analysis by Hot-Cooling Cycle Thermal Stress at Y-TZP Ceramics using Full Width at Half Maximum(FWHM) of X-ray Diffraction)

  • 최진삼;박규열;공영민
    • 한국재료학회지
    • /
    • 제29권4호
    • /
    • pp.264-270
    • /
    • 2019
  • As a case study on aspect ratio behavior, Kaolin, zeolite, $TiO_2$, pozzolan and diatomaceous earth minerals are investigated using wet milling with 0.3 pai media. The grinding process using small media of 0.3 pai is suitable for current work processing applications. Primary particles with average particle size distribution D50, ${\sim}6{\mu}m$ are shifted to submicron size, D50 ${\sim}0.6{\mu}m$, after grinding. Grinding of particles is characterized by various size parameters such as sphericity as geometric shape, equivalent diameter, and average particle size distribution. Herein, we systematically provide an overview of factors affecting the primary particle size reduction. Energy consumption for grinding is determined using classical grinding laws, including Rittinger's and Kick's laws. Submicron size is obtained at maximum frictional shear stress. Alterations in properties of wettability, heat resistance, thermal conductivity, and adhesion increase with increasing particle surface area. In the comparison of the aspect ratio of the submicron powder, the air heat conductivity and the total heat release amount increase 68 % and 2 times, respectively.

Annealing 수침처리에 따른 습식제분 쌀가루의 전분 특성 (Properties of Starch Isolated from Wet-milled Rice after Steeping at Elevated Temperatures for Annealing Effect)

  • 이영택;유문식;이보람;박종현;장학길
    • 한국식품과학회지
    • /
    • 제36권3호
    • /
    • pp.393-397
    • /
    • 2004
  • $40,\;50,\;60^{\circ}C$의 실온 이상의 상승된 온도에서 쌀을 수침처리한 후 습식제분한 쌀가루로부터 분리한 전분의 특성을 조사하였다. 수침처리하지 않은 대조구 쌀 전분에 비해 수침처리한 쌀 전분의 명도는 약간 감소하였으며 전분의 평균 입자크기는 다소 감소하였다. 전분의 팽윤력과 용해성은 대조구보다 전반적으로 높았으며 특히 $40^{\circ}C$에서 수침처리한 쌀 전분에서 가장 높았지만 그 이상의 처리온도에서는 다소 감소하는 경향이었다. DSC 호화개시온도, 호화정점온도는 $40^{\circ}C$$50^{\circ}C$ 수침처리한 쌀 전분에서 감소하였고 호화엔탈피는 증가하였으나 $60^{\circ}C$ 수침처리에서는 호화개시온도와 호화정점온도가 증가하였고 호화온도범위가 감소하여 전분의 annealing 현상이 나타남을 제시해 주었다. $40^{\circ}C$에서 수침처리한 쌀 전분은 Rapid Visco-Analyzer(RVA) 최고점도가 증가한 반면, $50^{\circ}C$$60^{\circ}C$에서는 최고점도가 감소하였고 breakdown이 감소하였으며 최종점도는 증가하여 setback이 높게 나타났다.

국산 압축벤토나이트 완충재의 첨가제 혼합을 통한 열전도도 향상 (Increasing of Thermal Conductivity from Mixing of Additive on a Domestic Compacted Bentonite Buffer)

  • 이종표;최희주;최종원;이민수
    • 방사성폐기물학회지
    • /
    • 제11권1호
    • /
    • pp.11-21
    • /
    • 2013
  • 현재 고준위 방사성 폐기물 심층 처분 시스템에서 기본 완충재 물질로서 건조밀도 1.6 g/$cm^3$의 경주산 칼슘 벤토나이트를 사용하고 있으나, 열전도도가 낮은 단점이 있다. 따라서 본 연구에서는 기준 완충재의 열전도율을 0.8 W/mK에서 1.0 W/mK로 향상시키기 위한 목적으로 다양한 첨가제를 다양한 혼합 방법을 통해 배합하고 열전도도를 측정하였다. 첨가제는 CNT(Cabon Nano Tube), Graphite, Alumina, CuO 및 $Fe_2O_3$ 등을 사용하였다. 혼합 방법의 경우, 핸드 믹서기를 통한 건식혼합, 습식 Milling 혼합, 건식 Ball Mill 혼합 등을 실시하였다. Ball Mill 혼합의 경우가 가장 균일하게 혼합되었기 때문에, 값의 편차가 가장 적었고 열전도도 증가율이 가장 좋았다. 지금까지 수행된 시험에서 소량의 고열전도 물질의 첨가로 경주산 칼슘 벤토나이트의 열전도도를 1.0 W/mK 수준으로 용이하게 증가시킬 수 있음을 실험적으로 확인할 수 있었다. 결론적으로, 본 연구에서 제시된 열전도 향상 방법은, 첨가제 혼합이 벤토나이트의 기본 성질인 팽윤압과 수리전도도에 미치는 영향까지 제시된다면, 국내 고준위폐기물 처분장의 개념 설계에 유용하게 활용될 수 있을 것으로 기대된다.

국내산 밀의 제면 적성에 관한 연구 (Noodle- Making Properties of Domestic Wheats Cultivars)

  • 남재경;한영숙;현영희;오지영
    • 한국식품조리과학회지
    • /
    • 제16권6호
    • /
    • pp.593-601
    • /
    • 2000
  • 국내산 밀로 수원 261, 수원 265, 은파, 고분, 알찬, 올그루, 금강밀 및 표준밀 ASW(Australian Standard White Wheat)의 제면 적성에 대하여 평가하였다. 국내산 밀의 원맥과 밀가루의 회분함량은 표준밀 ASW보다 0.1-0.3%정도 높게 나와 제분시 회분의 조절이 더 요구되었다. 단백질 함량은 밀가루의 가공공정을 좌우하는 것으로 국내산 밀 품종 중 수원 261, 수원 265, 금강밀이 각각 10.32, 11.3, 9.57%로 제면용으로 적합하였다. Farinograph의 valorimeter value(v.v.)는 은파, 올그루, 금강밀이 각각 68, 67, 61 v.v.로 표준밀인 ASW의 70v.v.와 비슷한 값을 나타내어 중력분에 속함을 알 수 있었다. Extensograph의 형상계수가 적을수록 박력분인데, 본 결과에서는 국내산 밀의 형상계수가 표준밀 보다 낮게 나타났다. 전분의 호화특성을 측정하는 amylograph에서 최고점도가 500-800 BU가 제면용으로 적합한데 국내산 밀 중 은파밀, 올그루밀, 금강밀이 이에 속하였다. 국내산 밀과 표준밀의 건면, 습면의 조리특성은 무게증가, 부피증가, 탁도로 나타내었는데 단백질 함량이 낮아 수분 침투가 많았던 올그루밀의 무게 , 부피증가가 높았다. 탁도는 무게, 부피의 증가와 비례하는 경향을 보이지는 않았으나 수원 265밀과 은파밀을 제외한 국내산 밀 품종은 표준밀 ASW와 비슷한 값을 보였다. 국수의 기계적 조직감을 습면, 건면으로 제조한 후 조리 전, 후로 나누어 TPA test를 측정하였다. 습면의 경우 조리에 의해 탄력성과 응집성을 증가시키며 국내산 밀이 표준밀 ASW보다 높은 값을 보여주었다. 건면의 경우 탄력성, 응집성은 조리 전, 후 품질간 뚜렷한 경향을 보이지 않았고 검성, 씹힘성, 견고성의 경우 전반적으로 국내산 밀 품종이 표준밀보다 높은 값을 보였다 인장력의 경우 습면은 시료간 차이가 없었으나 건면의 경우 국내산 밀이 표준밀보다 높은 인장력을 보였고, 표준밀은 습면의 인장력과 비슷한 값을 보였으나, 국내산 밀의 경우는 습면과 비교시 2-3g force전도 인장력이 상승되었다. 국내산 밀 품종과 표준밀 ASW의 색도는 밀가루와 반죽은 큰 차이를 보이지 않았으나 표준밀이 적색도가 낮았고, 습면의 경우 밀가루보다 백색도와 적색도가 크게 감소하였다. 건면의 경우도 시료간 차이를 보이지 않았으나 표준밀 ASW가 국내산 밀보다 역시 적색도가 낮았으며 습면과 비교시 백색도는 비슷하였고 적색도와 황색도는 증가되었다. 관능검사 항목은 습면과 건면으로 나누어 측정하였으며 습면, 건면 모두에서 금강밀이 전체적인 기호도에서 우수한 것으로 나타나 금강밀이 제면용으로 적합함을 알 수 있었다.

  • PDF