Evaluations of Microstructure and Electrochemical Anodic Polarization of AISI 304L and AISI 316L Stainless Steel Weld Metals with Creq/Nieq Ratio (Creq/Nieq비에 따른 AISI 304L 및 AISI 316L 스테인리스강 용접부의 미세조직 및 전기화학적 양극분극 평가)

  • Kim, Yeon Hee;Jang, Ah Young;Kang, Dong Hoon;Ko, Dae Eun;Shin, Yong Taek;Lee, Hae Woo
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.12
    • /
    • pp.1090-1096
    • /
    • 2010
  • This pitting corrosion study of welded joints of austenitic stainless steels (AISI 304L and 316L) has addressed the differentiating solidification mode using three newly introduced filler wires with a flux-cored arc welding process (FCAW). The delta ferrite (${\delta}$-ferrite) content in the welded metals increased with an increasing equivalent weight ratio of chromium/nickel ($Cr_{eq}/Ni_{eq}$). Ductility dip cracking (DDC) was observed in the welded metal containing ferrite with none of AISI 304L and 0.1% of AISI 316L. The potentiodynamic anodic polarization results revealed that the $Cr_{eq}/Ni_{eq}$ ratio in a 3.5% NaCl solution didn't much affect the pitting potential ($E_{pit}$). The AISI 316L welded metals with ${\ddot{a}}$-ferrite content of over 10% had a superior $E_{pit}$ value. Though the AISI 316L welded metal with 0.1% ferrite had larger molybdenum contents than AISI 304L specimens, it showed a similar $E_{pit}$ value because the concentration of chloride ions and the corrosion product induced severe damage near the DDC.

Microstructure Evolution of UFG Steel Weld by Hybrid and Laser Welding (하이브리드 용접과 레이저 용접에 의한 세립강 용접부의 미세조직변화에 관한 연구)

  • Dong, H.W.;Lee, M.Y.;Ahn, Y.S.
    • Journal of Power System Engineering
    • /
    • v.14 no.3
    • /
    • pp.58-63
    • /
    • 2010
  • A laser beam welding and an electric arc welding were combined, and the positive points of each welding method are drawn such as high speed, low thermal load, deep penetration, and high productivity. The fiber laser-MIG conjugated welding. namely the hybrid welding has been studied mainly for the automation industry of a pipeline welding. In this study, the MIG welding was combined with a fiber laser welding to make up the hybrid welding. The weld shapes, microstructures and mechanical properties for weld zones after the hybrid welding or only fiber laser welding were investigated on the 700 MPa grade Ultra Fine Grained(UFG) high strength steel. The amount of acicular ferrite in weld metals and HAZ(heat affected zone) was observed larger after hybrid welding compared with after only laser welding. The Vickers hardness of the top area of the fusion zone after fiber laser welding was higher compared with after hybrid welding.

A Study on the Characteristic of Weld Joint and Tensile Fracture of SUS304 and Cu High-Speed Dissimilar Lap Welds by Single Mode Fiber Laser (싱글모드 파이버 레이저를 이용한 SUS304와 Cu의 고속 겹치기 용접에서 접합부 및 인장시험 파단부의 특성에 관한 연구)

  • Lee, Su-Jin;Kim, Jong-Do;Katayama, Seiji
    • Journal of Welding and Joining
    • /
    • v.32 no.6
    • /
    • pp.56-63
    • /
    • 2014
  • To develop and understand dissimilar metals joining of Stainless steel and Copper, ultra-high speed laser lap welding was studied using single mode fiber laser in this study. SUS304 and Cu have large differences in materials properties, and Cu and Fe have no intermetallic compounds by typical binary phase of Cu and Fe system. In this study, ultra-high speed lap welds of SUS304 and Cu dissimilar metals using single-mode fiber laser was generated, and weldability of the weld fusion zone was evaluated using a tensile shear test. To understand the phenomenon of tensile shear load, weld fusion zone of interface weld area and fracture parts after tensile shear test were observed using scanning electron microscopy (SEM) and energy dispersive X-ray spectroscopy (EDX) analysis system. And it was confirmed that Cu was easily melting and penetrating in the grain boundaries of SUS304 because of low melting temperature. And high thermal conductivity of copper occurred dissipate heat energy rapidly. These properties cause the solidification cracking in weld zone.

The Study about Characteristics of Welding Consumable and Weld Metal for EGW (EGW 용접재료 및 용접부 특성에 관한 연구)

  • Lee, Jeong-Soo;Yun, Jin-Oh;Jeong, Sang-Hoon;Park, Chul-Gyu;An, Young-Ho
    • Journal of Welding and Joining
    • /
    • v.28 no.2
    • /
    • pp.79-83
    • /
    • 2010
  • In this study, newly developed welding consumables for EGW were welded in EH 36 TM steel plates and their welded joints were evaluated in point of mechanical properties and microstructures compared with imported consumables. Newly developed welding consumables were evaluated as good arc stability and slag fluidity, substantially the same with imported products. The tensile strength of all welded joints were sufficient to meet the requirements specified in a ship’s classification(490~640MPa) and all areas of fracture were heat affected zone(HAZ). Charpy absorbed energy values of all EG welded metals were sufficient to meet the requirements of classification(min. 34J) and those of newly developed wires were evaluated to be better than those of imported wires. As a result observing microstructures of single and tandem EG welded metals through optical and scanning electron microscope (OM&SEM), no grain boundary ferrite(PF(G)) were created in a prior austenite grain boundary and a volume fraction of a fine acicular ferrite were observed very high.

Characteristics of Friction Welding of Bulk Metallic Glass Rods and Tubes (벌크 비정질 금속 봉재 및 튜브재의 마찰접합 특성)

  • Shin, Hyung-Seop;Park, Jung-Soo;Jung, Yoon-Chul
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.33 no.7
    • /
    • pp.687-692
    • /
    • 2009
  • The friction welding of Zr-based bulk metallic glass (BMG) rods and tubes to similar BMGs, and to crystalline metals were performed. An infrared thermal imager (FLIR-Thermal Cam SC-2000) was used to measure the temperature distribution at joining interface of the specimens during friction welding. All BMGs adopted in this study showed a successful friction joining to similar BMG. The shape of the protrusion formed at the weld interface were examined. In order to characterize the friction weld interface, the micrographic observation and the X-ray diffraction analysis on the weld cross-section were carried out. The obtained results were discussed based on the temperature distribution measured at the weld interface A successful joining of the BMGs to crystalline metals could be obtained for certain pairs of the material combination through the precise control of the friction condition. The residual strength after dissimilar friction welding of BMG was evaluated by the four-point bending test and compared with the cases of friction welding to similar materials.

A Case of Metal Fume Fever Associated with Copper Fume in a Welder (용접공에서 발생한 구리흄에 의한 금속열 1례)

  • Lim, Hyun-Sul;Cheong, Hae-Kwan
    • Journal of Preventive Medicine and Public Health
    • /
    • v.31 no.3 s.62
    • /
    • pp.414-423
    • /
    • 1998
  • Metal fume fever has been known as an occupational disease is induced by intense inhalation of fresh metal fume with a particle size smaller than $0.5{\mu}m\;to\;1{\mu}m$. The fumes originate from heating metals beyond their boiling point, as happens, for example, in welding operations. Oxidation usually accompanies this process. In most cases, this syndrome is due to exposure to zinc oxide fumes; however, other metals like copper, magnesium, cadmium, manganese, and antimony are also reported to produce such reactions. Authors report a case of metal fume fever suspected to be associated with copper fume inhalation. The patient was a 42-year-old male and was a smoker. He conducted inert gas tungsten arc welding on copper-coated materials without safety precautions such as a protective mask and adequate ventilation. Immediately after work, he felt metallic taste in his mouth. A few hours after welding, he developed headache, chilling sensation, and chest discomfort. He also complained of myalgia, arthralgia, feverish sensation, thirst, and general weakness. Symptoms worsened after repeated copper welding on the next day and subsided gradually following two weeks. Laboratory examination showed a transient increase of neutrophil count, eosinophilia, elevated erythrocyte sedimentation rate, and positive C-reactive proteinemia. Blood and urine copper level was also increased compared to his wife. Before this episode, he experienced above complaints several times after welding with copper materials but welding of other metals did not produce any symptoms. It was suggested that copper fume would have induced metal fume fever in this case. Further investigations are needed to clarify their pathogenic mechanisms.

  • PDF

A Study on Factors Affecting Airborne Fume Composition and Concentration in Welding Process (용접공정에서 발생된 공기중 흄의 조성과 농도에 영향을 미치는 요인에 관한 연구)

  • Shin, Yong Chul;Yi, Gwang Yong;Park, Seung Hyun;Lee, Na Roo;Jeong, Jee Yeon;Park, Jung Keun;Oh, Se Min;Moon, Young Hahn
    • Journal of Korean Society of Occupational and Environmental Hygiene
    • /
    • v.7 no.2
    • /
    • pp.181-195
    • /
    • 1997
  • The purpose of this study was to investigate factors affecting the composition and concentrations of fumes generated from various types of welding processes. The results are as follows. 1. Iron(Fe), zinc(Zn) and manganese(Mn) were predominant in Welding fumes. The Fe content in total fumes was 25.5% in coated electrode and 28.2% in $CO_2$ are welding, and the Zn content was 4.5% and 9.1%, respectively, and the Mn was 3.6% and 7.8%, respectively. 2. It was found that the important factors determining composition and concentration of fumes were type of industries, type of welding processes, type and composition of electrodes, composition of base metals, confinement of workplaces or condition of ventilation, work intensity, coated metals such as lead and Zn in paint. 3. The Mn content in airborne fumes was highly correlated with that of electrode(r=0.77, p<0.01) and was about 4 times higher than that in electrodes or base metals. The results lindicate that Mn is well evaporated into air during welding. The higher vapor pressure of Mn may explain this phenomenon. 4. the airborne total fume concentrations were significantly different among types of industries(p<0.001). The airborne total fume concentration was higher in order of sleel-structure manufacturing($GM=15.1mg/m^3$), shipbuilding($GM=13.2mg/m^3$), automobile-component manufacturing ($GM=7.8mg/m^3$) and automobile assembling industry($GM=3.0mg/m^3$) 5. The airbone total fume concentration was 6 times higher in $CO_2$ welding than in coated electrode welding, and approximately 3 times higher in confined area than in open area, in steel-structure manufacturing industry. 6. The concentration of welding fume outside welding helmet was about 2 times higher than that inside it. It is recommened that air sampling be done inside helmet to evaulate worker's exposure accurately, for it has an outstanding effect on reducing worker exposure to fumes and other contaminants.

  • PDF

Study on The Status of Welded Parts According to The Types of Shielding Gas in TIG Welding (TIG용접에서 실드가스 종류의 변화에 따른 용접부의 변화상태 고찰)

  • Kim, Jin-Su;Kim, Bub-Hun;Lee, Chil-Soon;Kim, Yohng-jo;Park, Yong-Hwan
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.14 no.2
    • /
    • pp.38-43
    • /
    • 2015
  • Tungsten inert gas (TIG) welding is commonly used in industries that require airtightness, watertightness, oiltightness, and precision. It is a non-consumable welding method that is commonly used for the welding of non-ferrous metals, but it can be used to weld most metals. The methods of TIG welding can be divided into three types. The first, manual welding is done directly on the metal by a welder with a torch. The second, semi-automatic welding, gets help from a material supplying machine, but it is conducted by a welder. Lastly, automated welding is conducted fully by a machine during its process and operation. Depending on the selection of electrode, the amount of heat that is applied to the base material and the electrode rod changes and makes the shape of welded parts different. A direct-current positive electrode was used for this study. Through the change of shielding gas type on a structural steel (SS-400) that is commonly used in industry, the composition and shape changes in welded parts were detected after welding. The heat-affected area, hardness value, and tensile strength were also identified through hardness testing and tensile testing. In this study, it was found that the higher hardness value of the heat-affected is, the weaker the tensile strength becomes.

Microstructure and Tensile Properties of SS400 Carbon Steel and SUS430 Stainless Steel Butt Joint by Gas Metal Arc Welding

  • Poonnayom, Pramote;Chantasri, Sakchai;Kaewwichit, Jesada;Roybang, Waraporn;Kimapong, Kittipong
    • International Journal of Advanced Culture Technology
    • /
    • v.3 no.1
    • /
    • pp.61-67
    • /
    • 2015
  • The application of SS400 carbon steel and AISI430 ferritic stainless steel joint has been increased in industries because of the advantage of both metals was able to increase the service lifetime of the important structures. Therefore, a fusion welding process that could produce a sound weld and good joint properties should be optimized. This research is aimed to weld a butt joint of SS400 carbon steel and AISI430 ferritic stainless steel using Gas Metal Arc Welding (GMAW) welding process and to study the effects of welding parameters on joint properties. The experimental results were concluded as follows. The optimized welding parameter that produced the tensile strength of 448 MPa was the welding current of 110A, the welding speed of 400 mm/min and the mixed gas of $80%Ar+20%CO_2$. Increase of the welding current affected to increase and decrease the tensile strength of the joint, respectively. Lower welding current produced the incomplete bonding of the metals and indicated the low tensile strength. Microstructure investigation of the welded joint showed a columnar grain in the weld metal and a coarse grain in the heat affected zone (HAZ). The unknown hard precipitated phases were also found at the grain boundaries of the weld metal and HAZ. The hardness profile did not show the difference of the hardness on the joint that was welded by various welding currents but the hardness of the weld metal was higher than that of the other location.