Evaluation of Weathering Durability of Waterborne Preservative Treated Wood by Accelerated Weathering (수용성 방부처리재의 기상열화 저항성 평가)

  • Lee, Myung-Jae;Lee, Dong-Heub;Kim, Gyu-Hyeok
    • Journal of the Korean Wood Science and Technology
    • /
    • v.31 no.4
    • /
    • pp.44-49
    • /
    • 2003
  • This study was carried out to evaluate the weathering durability of waterborne preservative (AAC, ACQ, CCA, CuAz) treated Japanese red pine (Pinus densiflora S. et Z.) sapwood samples by accelerated weathering, and to find out the factor of stability. When considered the color changes, weight losses, surface degradation, and microstructure changes due to weathering, ACQ-, CCA-, and CuAz-treated samples were durable against weathering; the weathering durability of AAC-treated samples was poor and similar to untreated controls. The lignin content in aqueous extracts collected from ACQ-, CCA-, and CuAz-treated samples during weathering was lower than that from untreated and AAC-treated ones. From these findings, we might concluded that weathering durability of ACQ-, CCA-, and CuAz-treated samples was enhanced by the fixation of preservative component(s) onto the lignin structure, which is very susceptible to weathering.

Effects of salt crystallization on stone durability (염분의 결정화 현상이 석재 내구성에 끼치는 영향)

  • 김성수
    • Economic and Environmental Geology
    • /
    • v.32 no.2
    • /
    • pp.203-208
    • /
    • 1999
  • The main objective of this study is to suggest a new assessment method of the influence of weathering due to salt crystallization on the engineering property of rock. For this purpose, various sources of salt and salt crystallization were investigated, and artificially accelerated weathering tests were carried out. In natural envionment, weathering rate is very slow and weathering process involves complex mechanisms. Therefore artificial weathering test is essential for systematic analysis. Arificial weathering test is defined as test which controls weathering rate and agents by controlling arificial environmental condition. In this study, salt crystallization test was selected among various artificial weathering test methods, for its important role in weathering. Change of various stone properties were detexted. The change of physical properties by salt crystallization were observed as follows : 72% in Brazilian tensile strength and 72% in Slake durability. These results explain the importance of salt crystallization in the mechanical behaviour and properties of stone.

  • PDF

Weathering durability of biopolymerized shales and glacial tills

  • Amelian, Soroosh;Song, Chung R.;Kim, Yongrak;Lindemann, Mark;Bitar, Layal
    • Geomechanics and Engineering
    • /
    • v.28 no.4
    • /
    • pp.375-384
    • /
    • 2022
  • The glacial tills and shales in Midwestern states of the USA often show strength degradation after construction. They are often in need of applying soil modification techniques to remediate their strength degradation with weathering process. This study investigated the weathering durability of these natural soils and biopolymer treated soils by comparing direct shear test results for wet-dry and wet-freeze-thaw-dry cycled specimens. The tests showed that untreated glacial tills maintained only 62% and 50% initial shear strength after eight wet-dry cycles and eight wet-freeze-thaw-dry cycles, respectively. These untreated soils could not withstand by themselves after 16 weathering cycles. The same soils treated with 1.5% (by dry weight) food-grade Xanthan gum maintained 140% and 88% initial shear strength of untreated soils after 16 weathering cycles for wet-dry cycles and wet-freeze-thaw-dry cycles, respectively. The same soils treated with 1.5% (by dry weight) Gellan gum maintained 82% and 60% initial shear strength of untreated ones after 16 weathering cycles, respectively. Similar results were obtained for crushed shales, manifesting that the biopolymerization method may be adopted as a new eco-friendly method to enhance the weathering durability of these problematic soils of glacial tills and shales.

Physical and Chemical Weathering Indices for Biotite Granite and Granitic Weathered Soil in Gyeongju

  • Ban, Jae-Doo;Moon, Seong-Woo;Lee, Seong-Won;Lee, Joo-Gong;Seo, Yong-Seok
    • The Journal of Engineering Geology
    • /
    • v.27 no.4
    • /
    • pp.451-462
    • /
    • 2017
  • Physical weathering caused by external forces and chemical weathering caused by the decomposition or alteration of constituent materials are the two factors that dominate the mechanical properties of rocks. In this study, a field investigation was undertaken to identify the physical and chemical weathering characteristics of the biotite granite and granitic weathered soils in Gyeongju, South Korea. Samples were collected according to their grade of weathering and subjected to modal analysis, XRD analysis, XRF analysis, physical property tests, particle size distribution tests, and slake durability tests. Modal and XRD analysis identified these rocks as biotite granite; secondary alteration minerals were not observed. Physical property tests and particle size distribution analyses indicate an average porosity of 41.28% and a sand content of > 90 wt.%. These values are somewhat higher than those of granites in general. The results of the slake durability test and XRF analyses show that the physical and chemical weathering indices of the samples vary with the degree of weathering.

Quantitative Evaluation for Effectiveness of Consolidation Treatment by Using the Chemical of Ethyl Silicate Series for the Sandstone in Yeongyang (영양 사암을 대상으로 한 에틸실리케이트 계열 처리제의 강화효과 평가)

  • Lee, Jang-Jon;Han, Min-Su;Song, Chi-Young;Jun, Byung-Kyu;Do, Min-Hwan
    • 보존과학연구
    • /
    • s.30
    • /
    • pp.125-136
    • /
    • 2009
  • Stone cultural heritages in Korea have a severe damages from chemical and biological weathering because most of them have been situated in outdoors without any suitable protection systems, and this in turn causes deformation and structural damage. To counteract these problems and increase durability, various kinds of conservation materials are used in the conservation and restoration treatments. However until now there are not many practical and technological experiments on this subject. This paper attempts quantitative evaluation of effectiveness about chemical of ethylsilicate based resin for sandstone in Yeongyang-gun. It takes a long time to evaluate durability and side effect after conservation materials treatment. So we use artificial weathering through freezing§ thawing experimental method. As a result of this experiment, porosity and absorptance increased, and elastic wave speed, elastic modules, unconfined compression strength and tensile strength decreased more than before. This study plans to make a scientific method study about weathering factor and mechanism, and to deduce correlation between artificial weathering and natural weathering.

  • PDF

A Study on the Change of Conservation Materials Properties Using Artificial Weathering Test (인공풍화 실험을 이용한 보존처리제의 물성 변화 연구)

  • Do, Min-Hwan;Han, Min-Su;Lee, Jang-Jon;Jun, Byung-Kyu;Song, Chi-Young
    • 보존과학연구
    • /
    • s.29
    • /
    • pp.149-162
    • /
    • 2008
  • Because stone cultural heritages in Korea are mostly situated outdoors without any notable protection, there are severe damages from physical, chemical and biological weathering. And this in turn causes deformation and structural damage. To counteract this problem and increase durability, various kinds of conservation materials are used in the conservation and restoration treatment. However, there are not many practical and technological experiments on this subject. Accordingly this research is for analysis of effect for treatment to make use a resin of the ethyl silicate for the granite in Mt. Nam of Gyeongju. It takes a long time to confirm the test result regarding durability and side effects of the conservatives after treatment. So we built up an artificial environment through freezing and melting test, and evaluated the conservation materials. As a result of this experiment, porosity and absorptivity was increased in accordance with processing of freezing and melting test. But other things such as elastic wave speed, elastic modulus, uniaxial compressive strength and tensile strength was decreased. It will make a plan to form a method of research systematically for mechanism and element of weathering and to elicit a correlation among experiment of artificial weathering and practical natural weathering from next research.

  • PDF

The change of rock properties by artificial weathering tests and its implications for durability of building stones

  • Min Kyoung-Won;Park Jin-Dong
    • 한국지구물리탐사학회:학술대회논문집
    • /
    • 2003.11a
    • /
    • pp.557-560
    • /
    • 2003
  • Some well-known artificial weathering tests such as freezing-thawing, acid immersion, and salt crystallization are adopted to examine the change of rock properties during the processes of artificial weathering. Granites and other rock types of limestone, marble and basalt collected from different quarries in south Korea were sampled for this study. All tests were performed up to 30 cycles and physical properties were measured after experiencing every ten cycles of artificial weathering tests. During the tests, the variation trends of rock properties were too variable to draw generalized variation patterns but it can be concluded that weathering agents have different effect on rock properties depending on weathering circumstance and time. Even in short terms of salt crystallization tests, some rocks were severely deformed and then burst, and in the early stages of salt weathering, recrystallized salts filling pores and cracks in rocks could be a important factor affecting rock properties.

  • PDF

Physical Weathering Characteristics of Mica-Schist in Sinbuk Area, Chuncheon, Korea (춘천시 신북지역에 분포하는 운모편암의 물리적 풍화특성)

  • Woo, Ik;Han, Byeong-Hyeon
    • Economic and Environmental Geology
    • /
    • v.40 no.6
    • /
    • pp.771-784
    • /
    • 2007
  • This study shows the weathering characteristics of mica-schist affected by faulting and metamorphism through laboratory tests. Frozen-thaw test, which simulate the physical-chemical weathering processes in the laboratory, shows the important influence of foliation developed in mica-schist, resulting in $20{\sim}40%$ reduction of UCS according to weathering grade of rock. Slaking durability test was carried out for different weathering grade rock specimens and indicated that the specimens from fault area had a low durability index compared to other relatively fresh samples. XRD analysis allowed to estimate the dynamic evolution of mineral composition through wet-dry cycle in which the chlorite was the most important mineral leached out during slaking test. The creep test indicated that the main deformation produced along the foliation plane. The compacted clay minerals between discontinuity planes influence on the discontinuity shearing properties and result in a big difference between peak shear strength and residual strength. The results of laboratory tests on mica-schist show the possibility of a important deformation along the foliation plane or discontinuity.

A Study of Engineering Properties and Deformation Behavior of Weathered Rock Mass (풍화 암반의 공학적 특성 및 변형거동에 관한 연구)

  • 강추원;박현식;김수로
    • Explosives and Blasting
    • /
    • v.22 no.2
    • /
    • pp.33-43
    • /
    • 2004
  • The six grades weathering system is normally used in weathered rock classification. In this study. fresh and weathered rock block of grade I to V were sampled in Jang-soo ana but samples of the grade VI was omitted from this study. The variation quantities of chemical weathering indices with weathering degree are smaller than those of physical and mechanical properties. Increase of Weathering degree is well indicated by physical and mechanical properties such as strength, hardness, ultrasonic velocity and slake durability result. Especially, absorption and porosity ratio is a good indicator. As weathering proceeds. a number of the cracks affect the rock deformation. Therefore, stress-strain curves of weathered rocks in unconfined state are quite different from ones of fresh rocks.

Evaluation of Exterior Durability of Domestic Plywood for Temporary Construction (국산(國産) 가설재용(假說材用) 합판(合板)의 옥외(屋外) 내구성(耐久性) 평가(評價))

  • Kim, Gyu-Hyeok;Jo, Jae-Sung;Song, Ki-Young
    • Journal of the Korean Wood Science and Technology
    • /
    • v.22 no.1
    • /
    • pp.20-27
    • /
    • 1994
  • Water repellent preservative (WRP) treated and untreated, small-sized specimens prepared from semiwater resistant, water resistant, and tegofilm-overlaid plywood were exposed to outdoor weathering for one year. Exterior durability of specimens was evaluated on the basis of changes in dynamic modulus of elasticity, degree of delamination, modulus of elasticity, modulus of rupture, and glueline shear strength. Among untreated specimens, tegofilm-overlaid plywood showed the best outdoor durability, and durability between semiwater resistant and water resistant plywood was similar. Although WRP treatment increased the durability of all types of plywoods, the effect of treatment on the increase in durability for semi water resistant plywood was not distinct. Accordingly, it can be concluded that semi water resistant plywood, which is used for temporary construction such as concrete formwork in our country, can not be inadequate for exterior use, regardless of WRP treatment. The bending strength and glueline shear strength of untreated water resistant plywood measured after weathering for one year did not exceed the minimum value specified by Korean Standard (KS), thereby the outdoor use of water resistant plywood was not desirable without WRP treatment. Exterior durability between treated water resistant plywood and untreated tegofilm-overlaid plywood was very similar. This result suggests that if an exposed plywood surface is treated with WRP regularly water resistant plywood can be used for temporary construction. This suggestion, however, needs to be investigated. In summary, semiwater resistant plywood cannot be used for temporay construction regardless of WRP treatment. Water resistant plywood can be used only with WRP treatment. Comparing the cost of tegofilm-overlaid plywood to costs of water resistant plywood and WRP treatment, however, it can be concluded that use of tegofilm-overlaid plywood for temporay constrution is strongly suggested from the point of view of both outdoor durability and costs.