순도를 달리한 알루미나 세라믹스의 마멸과정 및 이의 기구에 관한 연구 (A Study on The Wear Process and Wear Mechanism of the Alumina Ceramics with Different Alumina Purity)

  • 전태옥;진동규
    • 대한기계학회논문집
    • /
    • 제18권12호
    • /
    • pp.3404-3412
    • /
    • 1994
  • The present study was undertaken to investigate the dry wear process and wear mechanism of the alumina ceramics in the purity variation which are used for the mechanical seal, roll, liner and dies. The wear test was carried out under different experimental condition using the wear testing device and in which the annular surface rubbed on dry sliding condition various sliding speed, contact pressure and sliding distance. In case of alumina purity 95%, there was speed range which wear loss increased rapidly owing to enlargement of heat impact force and temperature rise of wear surface. According as the alumina purity increased, wear loss decreased but alumina purity 85% with much void and defect had the most wear loss than any other alumina purity. The friction coefficient of sliding initial stage of wear curves has a large value but according to increase of sliding distance, it decreased owing to drop of the shear strength of wear surfaces.

첨단복합방식재를 이용한 각종 선박구조물의 마찰마모손상의 최소화 (Minimization of Friction and Wear Damage of Marine Structures by Using the Advanced Anti-corrosive Composite Materials)

  • 김윤해;김진우
    • 해양환경안전학회지
    • /
    • 제5권2호
    • /
    • pp.15-26
    • /
    • 1999
  • The marine structures with sea water cooling system always expose to the oceanic atmosphere. Therefore, the protection of the equipments is very important. To investigate the effectiveness of advanced composite materials for the application in offshore environments, the tensile test, hardness test, undercutting property test, permeance test and the friction and wear test were carried out by using various applicable coating materials. The main results obtained can be summarized as follows; 1. The micro-hardness of the Archcoat 502B showed the highest value. 2. The coefficient of friction of the Rigspray coating at the speed of 2.21m/sec showed the lowest value, and that of the Archcoat 502B coating at 1.08m/sec and 0.18m/sec indicated the lowest values. 3. The wear mass at the speed of 0.18m/sec and 1.08m/sec in dry condition showed the smallest values. 4. The Archcoat 502B coating is fitted to the dynamic instruments in the range of low speed and middle speed. Rigspray coating is fitted to the dynamic instruments in the range of high speed. 5. The wear mass of five kinds of coating materials at the range of low speed was very small, and those of the Archcoat S02B, Archcoat 402B and Rigspray coating at high speed range were quitely smaller than those of the Modified Epoxy and Tar Epoxy.

  • PDF

탄소섬유와 SiC 휘스커를 혼합한 $Al/Al_2O_3$ 복합재료의 마멸특성 (Wear Characterization of $Al/Al_2O_3$ Composites Reinforced with Hybrid of Carbon Fibers and SiC Whiskers)

  • 봉하동;송정일;한경섭
    • 대한기계학회논문집
    • /
    • 제19권7호
    • /
    • pp.1619-1629
    • /
    • 1995
  • The Al/Al$_{2}$O$_{3}$ SiC and Al/Al$_{2}$O$_{3}$/C hybrid metal matrix composites (MMCs) were fabricated by squeeze infiltration method. Uniform distribution of reinforcements were found in the microstructure of metal matrix composites. Mechanical tests were carried out under various test conditions to clearly identify mechanical behavior of MMCs, and the wear mechanism of Al/Al$_{2}$O$_{3}$/(SiC or C) hybrid metal matrix composites were investigated. The tensile strength and hardness of hybrid composites was resulted in increasing compared with those of the unreinforced matrix alloy. Wear resistance was strongly dependent upon kinds of fiber, volume fraction and sliding speed. The wear resistance of metal matrix composites was remarkably improved by the addition of reinforcements. Especially, the wear resistance of the hybrid composites of carbon fibers was more effective than in the composites reinforced with alumina and SiC whiskers of reinforcements. This was due to the effect of carbon fiber on the solid lubrication. Wear mechanisms of hybrid composites were suggested from wear surface analyses. The major wear mechanism of hybrid composites was the abrasive wear at low to intermediate sliding speed, and the melting wear at intermediate to high sliding speed.

경부고속열차의 기존선 주행시 차륜마멸특성에 관한 연구 (A Study on the Wheel Wear of High Speed Train Running on the Conventional Line)

  • 강부병;이희성
    • Tribology and Lubricants
    • /
    • 제19권4호
    • /
    • pp.187-194
    • /
    • 2003
  • This paper describes the characteristics of wheel wear of high speed train running on the conventional line. Conventional line has many curved tracks that cause severe wheel flange wear. The influences of lubrication, cant deficiency, curve radius on wheel wear are also described considering the operation performance of the highspeed trainset. A method of calculation using contact patch work model is presented for determination of the evolution by wear of railway wheels.

고속열차 차륜 플랜지 마모 (Flange Wear of the High Speed Train)

  • 이희성;강부병
    • Tribology and Lubricants
    • /
    • 제22권1호
    • /
    • pp.33-39
    • /
    • 2006
  • During the high speed train operation in the conventional line, it was found to have extremely severe flange wear, due to the curvy routes. This paper looks at the actions that have been taken to bring the wear to an acceptable level. In particular, it have been presented for flange wear variation depending on curve radius, cant, transition curve length by using numerical method. And the impacts on the flange wear by the application of stick type solid lubricant are also presented.

PMMA(Poly Methyl Methacrylate) 코팅층 두께 및 적용하중에 따른 마멸기구 분석 (Effects of thickness and applied load on wear mechanisms of PMMA (Poly Methyl Methacrylate) coating layers)

  • 강석하;김용석
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 춘계학술대회 논문집
    • /
    • pp.152-155
    • /
    • 2004
  • Effects of sliding speed, applied load, counterpart radius and thickness of PMMA (Poly Methyl Methacrylate) coating layers on their dry sliding frictional and wear behavior were investigated. Sliding wear tests were carried out using a pin-on-disk wear tester. The PMMA layer was coated on Si wafer by a sol-gel technique with two different thicknesses, $1.5{\mu}m\;and\;0.8{\mu}m$. AISI 52100 bearing steel balls were used as a counterpart of the PMMA coating during the wear. Normal applied load and sliding speed were varied. Wear mechanisms were investigated by examining worn surfaces by an SEM. Under most of sliding test conditions, the thicker layer with the thickness of $1.5{\mu}m$ showed lower fiction coefficient than the thinner layer. Effects of sliding speed and counterpart's radius on the frictional behavior were varied depending on the thickness of the coating layer.

  • PDF

고속철도 차륜답면의 마모 특성에 관한 연구 (A Study on the Wear Characteristics of Wheel Profile for High Speed Rolling-stock)

  • 허현무;유원희
    • 한국철도학회논문집
    • /
    • 제8권5호
    • /
    • pp.477-482
    • /
    • 2005
  • Through a year's commercial operation, Korea High Speed Railway has solved defectives from several breakages at the beginning and is going into the stage of stable operation. Among issues, wheel wear becomes a matter of primary concerns in view of vehicle's stability and maintenance. It was understood as above that wear status has been improved in the test by which railway system including vehicles and tracks was stabilized during a year's commercial operation, comparing to that with excessive wear in the trial operation prior to opening to the public. To make out wheel's wear status and characteristics of equivalent conicity at present when the service has been introduced a year ago and the average cumulative mileage of vehicles reach almost 500,000km, wheel's wear types were analyzed with the current vehicles in service.

탄소/탄소 복합재료의 마찰 및 마모 거동과 신경회로망에의 적용에 관한 연구 (Friction and Wear Behavior of Carbon/carbon Composite Materials and its Application to a Neural Network)

  • 류병진;윤재륜;권익환
    • Tribology and Lubricants
    • /
    • 제10권4호
    • /
    • pp.13-26
    • /
    • 1994
  • Effects of resin contents, number of carbonization, graphitization, sliding speed, and oxidation on friction and wear behavior of carbon/carbon composite materials were investigated. Friction and wear tests were carried out under various sliding conditions. An experimental setup was designed and built in the laboratory. Stainless steel disks were used as the counterface material. Friction coefficient, emperature, and wear factor were measured with a data acquisition system. Wear surfaces were observed by the scanning electron microscope. It has been shown that the average friction coefficient was increased with the sliding speed in the range of 1.43~6.10 m/s, but it as decreased in the range of 6.10~17.35 m/s. Specimens prepared by different numbers of carbonization. showed variations in friction coefficient and friction coefficient of the graphitized specimen was the highest. Friction coefficients depended on contribution of the plowing and adhesive components. As the number of carbonization was increased, wear factor was reduced. Wear factor of the graphitized specimens dropped further. In the case of graphitized specimens, sliding speed had a large influence on wear behavior. When the tribological experiments were conducted in nitrogen atmosphere, the wear factor was decreased to two thirds of the wear factor obtained in air. It is obvious that the difference was affected by oxidation. Results of friction and wear tests were applied to a neural network system based on the backpropagation algorithm. A neural network may be a valuable tool for prediction of tribological behavior of the carbon/carbon composite material if ample data are present.

CBN 공구를 이용한 고속 정면밀링시의 공구마멸 (Tool Wear in High Speed Face Milling Using CBN Tool)

  • 최종순
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2000년도 춘계학술대회논문집 - 한국공작기계학회
    • /
    • pp.332-338
    • /
    • 2000
  • The high speed machining is now one of the most effective manufacturing methods to achive higher productivity. However, due to the increased cutting temperatures caused by increased cutting speed, tool wear become larger. Especially in high speed face milling, cutting tools are exposed not only to high cutting temperatures, but also to mechanical and thermal shock stresses. It is essential, therefore, to know the wear characteristics of tool materials in high speed machining. This study presents an experimental investigation of the cutting performance of CBN tools in high speed face milling of gray cast iron FC25. The effect of cutting conditions and cutting length on flank wear of CBN tools and roughness of machined surfaces is investigated. The cutting parameters involved were ; cutting speeds in the range of 600to 1800 m/min, feed of 0.1 mm/tooth, and depth of cut of 0.3mm.

  • PDF

중탄소 Boron강의 가스침질탄화처리에 의해 형성된 화합물층의 마모특성에 관한 연구 (A Study on the Wear Characteristics of Compound Layers Formed during Gaseous Nitrocarburizing in Medium Carbon Boron Steels)

  • 박기원;오도원;조효석;이해우;이준범;이상윤
    • 열처리공학회지
    • /
    • 제12권2호
    • /
    • pp.136-144
    • /
    • 1999
  • The study on the wear characteristics of compound layers formed during gaseous nitrocarburising in the medium carbon boron steels and the plain carbon steel has been carried out by using a pin-on-disc type wear test machine under the oil lubricating condition at room temperature and by varying applied loads, sliding speeds and wear distances. Values of friction coefficient measured at the sliding speed of 0.4m/sec under the oil lubricating condition have been shown to decrease considerably with increasing applied load and become gradually a constant value as load is increased to a higher value, showing that the transition load for friction coefficient appears at an applied load of 247.2N. The length and volume wear rates of compound layer have been revealed to relatively constantly increase, also showing that the wear life per unit thickness of compound layer turns out to be superior as porous layer has a denser and thinner appearance. As the sliding speed increases during wear test performed by varying sliding speed at a load of 63.2N under the oil lubricating condition for medium carbon boron steel nitrocarburised in gas atmosphere, the wear rate has been found to increase, the friction coefficient to decrease and the wear life per unit thickness of compound layer to decrease considerably.

  • PDF