졸겔법과 자가조립법을 통해 제조된 메조포러스 $SiO_2$ 박막의 트라이볼로지 특성 (The Tribological Behaviors of Mesoporous $SiO_2$ Thin Film Formed by Sol-Gel and Self-Assembly Method)

  • 이영제;신윤하;김지훈;김지만;김태성
    • Tribology and Lubricants
    • /
    • 제23권6호
    • /
    • pp.298-300
    • /
    • 2007
  • Frictional characteristics of mesoporous $SiO_2$ thin films were evaluated with different pore sizes. The films were manufactured by sol-gel and self-assembly methods to have a porous structure. The pores on the surface may play as the outlet of wear particle and the storage of lubricant so that the surface interactions could be improved. The pores were exposed on the surface by chemical mechanical polishing (CMP) or plasma-etching after forming the porous films. The ball-on-disk tests with mesoporous $SiO_2$ thin films on glass specimen were conducted at sliding speed of 15 rpm and a load of 0.26 N. The results show considerable dependency of friction on pore size of mesoporous $SiO_2$ thin films. The friction coefficient decreased as increasing the pore size. CMP process was very useful to expose the pores on the surface.

급속응고한 Ag-Sn-In 합금의 산화반응에 미치는 Sn-In 첨가량 비율에 관한 연구 (The Study of the Sn-In Ratio on the Oxidation Reaction of Rapidly Solidified Ag-Sn-In Alloys)

  • 장대정;권기봉;조대형;김정수;남태운
    • 한국주조공학회지
    • /
    • 제27권2호
    • /
    • pp.72-76
    • /
    • 2007
  • Contact materials are widely used as electrical parts. Ag-Cd alloy has a good wear resistance and stable contact resistance. But the Cd exists as coarse oxide in alloy so it have an effect on mechanical properties badly. Moreover, the Cd is an injury material to environment. Nowadays, the use of Cd is strictly restricted. Because of these disadvantage, Ag-Sn-In alloy has been developed. In Ag-Sn-In alloy, the Sn : In ratio affects the internal oxidation properties, such as the formation of the oxide layer on the surface. In this work, we changed and optimized the Sn : In ratio variety for good internal oxidation properties. We have shown that a internal oxidation process did not fully completed when the Sn : In ratio is over 4 : 1 because of the Sn oxide layer at surface. The increase of In decelerates the formation of Sn oxide layer.

탄화물(SiC, TiC, $B_4C$ ) 입자 강화 7075 Al 합금 기지 복합재료의 건식 미끄럼 마멸 거동 (Dry Sliding Wear Behavior of Carbide-Particle-Reinforced 7075 Al Alloy Matrix Composites)

  • 강석하;박형철;강신철;김용석
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2003년도 춘계학술발표강연 및 논문개요집
    • /
    • pp.27-27
    • /
    • 2003
  • 무가압침투법으로 제조된 부피분율 10~24% SiC, TiC, B$_4$C 탄화물 입자강화 7075 Al 합금 기지 복합재료의 건식 미끄럼 마멸거동을 강화입자의 종류, 크기 및 부피 분율을 변수로 연구하였다. 미끄럼 마멸 시험은 pin-on-disk 형태의 마멸 시험기를 사용하여, AISI 52100 베어링강을 상대재로 상온 대기 중에서 실시되었다. 마멸특성의 분석과 마멸기구의 규명을 위하여 마멸면과 마멸단면을 SEM, EDS를 이용하여 분석하였다. 제조된 복합재료의 압축 시험을 통하여 측정된 항복강도와 가공경화지수는 서로 반비례하였고, 각 시편간의 경도 차는 크지 않았다. 마멸 시험결과, 크기 및 부피 분율이 7$\mu\textrm{m}$ !0%인 SiC 입자로 강화된 복합재료를 제외하고, 전체 복합재료 시편은 7075 Al 기지 합금에 비해 낮은 마멸 속도를 보였다. 10N 이하의 저하 중에서는 강화상의 종류와 상관없이 복합재료는 낮은 마멸 속도를 보였고, 25N 이상의 고하중에서는 TiC 입자강화 복합재료가 가장 낮은 마멸 속도를, SiC 입자강화 복합재료가 가장 높은 마멸 속도를 나타내었다. 강화 입자의 크기 및 부피 분율이 동일한 경우 SiC 입자로 강화된 복합재료가 가장 낮은 내마멸성을 나타내었다. 강화상의 크기 및 부피 분율이 증가함에 따라 미소 마멸에서 격렬 마멸로의 천이 하중이 증가하였다.

  • PDF

An Experimental Investigation on the Contamination Sensitivity of an Automotive Fuel Pump

  • Lee Jae-Cheon;Shin Hyun-Myng
    • International Journal of Precision Engineering and Manufacturing
    • /
    • 제6권3호
    • /
    • pp.51-55
    • /
    • 2005
  • This study addresses the contamination sensitivity test of a typical fuel pump for an automotive vehicle. The objective of the study is to find the contamination sensitivity coefficient of a fuel pump on specific contaminant particle sizes so that an optimal fuel filter could be selected. To achieve the objective, the degradation of discharge flow rate of the fuel pump is measured under the experiments of various contaminants size ranges of ISO test dust up to $80\;{\mu}m$. The fundamental theory of contamination sensitivity is introduced and the contamination sensitivity coefficients are estimated using the experimental data. Maximum contamination sensitivity coefficient of $5\chi\;10^{-6}\;L/min{\cdot}Ea$ is found in the contaminant size range of $40\;{\mu}m\~50\;{\mu}m$. The magnified picture of the surface of vane disc reveals that the abrasive wear is the principal cause of discharge flow rate degradation. Hence, this study reveals that a high efficiency filter for contaminant particles especially in the size range of $30\;{\mu}m\~70\;{\mu}m$ especially should be used to maintain the service life of the fuel filter.

Effect of graphite particulate on mechanical properties of glass fibre reinforced composite

  • Bhattacharjee, Antara;Roy, Kanchan;Nanda, B.K.
    • International Journal of Aerospace System Engineering
    • /
    • 제7권1호
    • /
    • pp.16-20
    • /
    • 2020
  • The recent trend is increasing towards the usage of polymer matrix composites since they have a wide variety of applications. They have applications in the field of aircraft and space industry, sporting goods, medical devices, marine and automotive applications and also in commercial usage. The most commonly used fibre-reinforced polymer matrix composite is Glass fibre reinforced epoxy (GFRE) composite which is used in aviation, sports and automotive industries. However, the strength of GFRE composites is not adequate for structural applications. Therefore, the current research focuses on increasing the strength of GFRE composites by reinforcing with micro Graphite (Gr) particulates. The Gr used is an ultra-fine powder with particle size 250 ㎛. Gr is known to have good wear resistance, thermal conductivity and can operate at high temperatures. Gr particulates are mixed with the epoxy matrix in various weight ratios. Hand-lay technique is used for fabricating the composites. Mechanical properties such as tensile strength, elongation, compressive strength and flexural strength are obtained experimentally to study the effect of change in Gr content (0-5 wt. %). The tests were done as per ASTM standards.

나노 윤활유를 이용한 압축기 습동부 재질의 경도에 따른 윤활특성 평가 (Lubrication Characteristics of Nano-oil with Different Surface Hardness of Sliding Members)

  • 한영철;구본철;이광호;황유진;이재근
    • 대한설비공학회:학술대회논문집
    • /
    • 대한설비공학회 2009년도 하계학술발표대회 논문집
    • /
    • pp.916-921
    • /
    • 2009
  • In this study, lubrication characteristics of sliding members were compared with the change of the hardness of friction surfaces and the application of nano-oil. The materials of the specimens were gray cast iron (AISI 35, AISI 60) and nickel chromium molybdenum steel (AISI 4320). The Friction coefficients and the temperature variations of on the frictional surfaces were measured by disk-on-disk tribotester under the condition of fixed rotating speed. The friction surfaces were observed by scanning electron microscope (SEM). In the results, the friction coefficients of the disk surface were increased as hardness difference was increased. The friction coefficient lubricated in nano-oil was less than mineral oil. This is because a spherical nano particle plays a tiny ball bearing between the frictional surfaces, improved the lubrication characteristics.

  • PDF

Changing PEO coating formation on Mg alloys by particle additions to the treatment electrolyte

  • Blawert, Carsten;Srinivasan, Bala;Liang, Jun;Huang, Yuanding;Hoche, Daniel;Scharnagl, Nico;Heitmann, Volker;Burmester, Ulrich
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2012년도 추계총회 및 학술대회 논문집
    • /
    • pp.7-11
    • /
    • 2012
  • Plasma electrolytic oxidation of magnesium alloys is a well known technique to produce corrosion and wear resistant coatings. The addition of particles to the electrolyte provides a possibility to produce coatings with an increasing range of composition by in-situ incorporation of those particles into the coating. An extensive literature review has revealed that the mode of incorporation depends mainly on the melting point of the used particles and the energy provided by the discharges of the PEO process. The spectrum ranges from inert to partly reactive incorporation, but a complete reactive incorporation and a formation of a new single phase coating was not observed so far. Thus a new approach in PEO processing is introduced using specific particles as a kind of sintering additive, changing not only the composition but lowering the melting temperature and increase the liquid phase fraction during the discharges, resulting in a new amorphous coating.

  • PDF

고액공존 과공정 Al-Si합금의 교반응고시 미세조직변화 (Microstructural changes during semi-solid state processing of hypereutectic Al-Si alloys)

  • 유영호;김도향
    • 한국주조공학회지
    • /
    • 제15권5호
    • /
    • pp.483-493
    • /
    • 1995
  • The microstructural changes during semi-solid state processing of hypereutectic Al-Si alloy has been investigated in the present study. Stirring of semi-solid slurry results in the morphological changes of the primary Si particles, i.e. from angular rod shape to near-spherical shape. Besides the spherodization of primary Si particles, the average particle size increases, especially, at much higher rate in the final stage than that in the early stage of stirring. Various microstructure characterization techniques, such as anisotropic etching, SEM imaging and ECP analysis, reveal that the spherodization of primary Si particles occurs by the combinations of the mechanisms of coalescence, fracture, and wear of the individual particles. Isothermal shearing of hypereutectic Al-Si at $580^{\circ}C$ shows that spherical ${\alpha}-Al$ particles are formed by the dissociation of Al-Si eutectic structure at the early stage of isothermal shearing. The spherical ${\alpha}-Al$ particles gradually grow by the mechanisms of Ostwald ripening and coalescence of the particles.

  • PDF

용융 Al의 치환반응에 의한 $Al_2O_3/Al$ 복합체의 제조 (Fabrication of $Al_2O_3/Al$ Composites by Replacement Reaction of Molten Metal Al)

  • 정두화;김용진;배원태
    • 한국세라믹학회지
    • /
    • 제34권6호
    • /
    • pp.591-600
    • /
    • 1997
  • Al2O3/Al composites were produced by displacement reaction method, which was carried out by immersing the sintered silica preform, which was prepared from fused silica powder, in molten aluminum. Because the molten aluminum did not penetrate into the silica preform with higher than 20% of porosity when the displacement reaction was accomplished at 100$0^{\circ}C$ for 10 hours in air atmosphere, the optimum range of sintering temperature of silica preform was from 135$0^{\circ}C$ to 140$0^{\circ}C$. The microstructure of this Al2O3/Al composites showed three-dimentionally co-continuous alumina, which provides wear resistance and high stiffness, and aluminium which acts as a toughnening phase. The grain size of the alumina in composites did not change with the particle size of the silica preform. The exact shape of the preform was retained and a net-shaped composite was produced. The representative Al2O3/Al composite prepared in this study showed 3.30mg/㎤ of bulk density, 350-430 MPa of flexural strength, 7.0 MPa.m1/2 of fracture toughness, and good machinability.

  • PDF

SHS 합성에 의한 몰리브덴계 용사용 복합분말의 제조 (Fabrication of Mo based Thermal Spray Composite Powder by Self- propagating High- temperature Synthesis)

  • 박제신;심건주
    • 한국재료학회지
    • /
    • 제11권9호
    • /
    • pp.763-768
    • /
    • 2001
  • Molybdenum-based thermal spray powder is widely used for coating the moving parts of the internal combustion engines due to its excellent wear resistance. A composite powder of the $Mo_{40}(Al_{1-x}Si_x)_{60}$ system was synthesized using the SHS method. The synthesized bulk was pulverized and specially treated to produce thermal spray powder. It was found that the synthesis reaction consisted of two-steps: the formation of $Al_8/Mo_3$ and the formation of Mo(Al,Si)$_2$. Both the temperature and the rate of the SHS reaction linearly increased with the increase of the value of x in $Mo_{40}(Al_{1-x}Si_x)_{60}$, The temperature and the rate of the reaction were also affected by the compacting density of the specimens, exhibiting the maximum valves at 62% and 60%, respectively. Since spherical shape is advantageous to the thermal spraying process, shape-control of the powder was attempted with PVA as a binding additive, resulting in the successful production of almost perfectly spherical powder of 80 $\mu\textrm{m}$ Ø$(d_{50})$ mean particle size.