온간단조용 금형에 있어서 고속도 공구강의 적용 (Application of High Speed Tool Steel in Warm Forging)

  • 김동진
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2000년도 춘계학술대회논문집
    • /
    • pp.75-78
    • /
    • 2000
  • There are several effective factors to influence die life in the warm forging process. For instance process design die design and die materials etc This study presented heat treatment method which could improve toughness and wear resistance simultaneously in high temperature to apply high speed tool steels like SKH51 to die material for warm forging process. To verify the feasibility of application of heat treatment method mentioned above wear test was performed under the condition of constant time in 40$0^{\circ}C$ Wear coefficient was examined to search a relation between wear amount and time for each material and heat treatment method in 30, 60, and 130 minutes. To quantify the toughness-behavior between room and high temperature impact test was performed and heat fatigue test also fulfilled to compare with the resistance of heat check in room, 200, 400, and $600^{\circ}C$ temperature. On the basis of experimental results mentioned above high speed tool steel was applied to verify appropriateness of newly proposed heat treatment method for die of rotor pole used in automobile alternator. As a result die life of high speed tool steel applied newly proposed heat treatment is longer than that of STD61.

  • PDF

나노다이아몬드가 첨가된 윤활제의 마모 특성 연구 (Study on Wear Characteristics of Lubricants with Nano-diamond Additives)

  • 김승택;김승목;박태희;이정석;이영제
    • Tribology and Lubricants
    • /
    • 제30권5호
    • /
    • pp.291-294
    • /
    • 2014
  • Multiple additives can help improve the performance of generally used lubricants. These additives include MoS2, cadmium, chloride, indium, sulfide, and phosphide, which are harmful to both humans and the environment. Thus, researchers in this industry have been trying to reduce the use of these additives by finding alternatives. Nanodiamonds are one of these candidates. Nanodiamond particles are very hard, chemically stable, and highly heat-conductive. This research involved uniformly dispersing nanodiamond particles in marine engine oils via a matrix synthesis method at various concentrations (0, 0.1, 0.3, 0.5, and 1.0 wt). Friction and wear tests involved constant loads on ball-on-disk specimens, where the ball was AISI 51200 steel, the disk was AISI 1020 steel, and the sliding speed was 0.217 m/s. The lowest wear occurred at a suitable concentration of nanodiamonds (0.3 wt). However, excessive amounts of nanodiamonds caused them to act as abrasive debris because of their hardness, which increased the wear amount. The friction coefficient decreased as the nanodiamond concentration increased because their octagonal, almost spherical shape caused them to act as rolling contact elements between two surfaces.

노멀라이징 열처리한 구상 흑연 주철의 마찰.마모특성 평가에 관한 연구 (A Study on the Evaluation of the Friction and Wear Properties for Normalized Ductile Cast Iron)

  • 김윤해
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제23권4호
    • /
    • pp.440-446
    • /
    • 1999
  • This study is mainly concerned with the friction and wear properties for the specimens of crank shaft which are made of ductile cast iron. The friction and wear tests were carried out for the nor-malized ductile cast iron specimens and their properties were compared with each other at reheat-ing temperatures(550^{\circC,\; 600^{\circ}C,\; 650^{\circ}$) and in dry condition at different friction velocity(0.94 m/s 1.88m/s 2.83m/s) range. After austenized at $910^{\circ}C$ it is observed that the higher the reheating temperature is the hardness becomes decrease which is supposedly attributed to the fact that the amount of pearlite austenite matrix is rduced by reheating after normalizing and that as the reheating temperature goes up the pearlite generated is less and the interval between the pearlites were widened at last to make pearlite globular. At the low velocity the friction coefficient increase in the beginning and gets stabilized as the sliding distance increases. As the friction velocity grows the friction coefficient decreases suppos-edly since the abrasive wear is heavier at low velocity than at the high velocity as the friction tem-perature at low velocity is lower than at high velocity.

  • PDF

Effect of Chemically Etched Surface Microstructure on Tribological Behaviors

  • Hye-Min Kwon;Sung-Jun Lee;Chang-Lae Kim
    • Tribology and Lubricants
    • /
    • 제40권3호
    • /
    • pp.84-90
    • /
    • 2024
  • This study investigates the effect of the surface microstructure on the tribological characteristics of glass substrates. Chemical etching using hydrofluoric acid and ammonium hydrogen fluoride was employed to create controlled asperity structures on glass surfaces. By varying the etching time from 10 to 50 min, different surface morphologies were obtained and characterized using optical microscopy, surface roughness measurements, and water contact angle analysis. Friction tests were performed using a stainless steel ball as the counter surface to evaluate the tribological behavior of the etched specimens. The results showed that the specimen etched for 20 min exhibited the lowest and most stable friction coefficient, which was attributed to the formation of a uniform and dense asperity structure that effectively reduced the stress concentration and wear at the contact interface. In contrast, specimens etched for shorter (10 min) or longer (30-50 min) durations displayed higher friction coefficients and accelerated wear owing to nonuniform asperity structures that led to local stress concentration. Optical microscopy of the wear tracks further confirmed the superior wear resistance of the 20-minute etched specimen. These findings highlight the importance of optimizing the etching process parameters to achieve the desired surface morphology for enhanced tribological performance, suggesting the potential of chemical etching as a surface modification technique for various materials in tribological applications.

The Effect of TiN and CrN Coatings on the Fretting Wear of Tubes against Supports in a Nuclear Steam Generators

  • Park, Dong-Shin;Park, Jung-Min;Kim, Jin-Seon;Lee, Young-Ze
    • KSTLE International Journal
    • /
    • 제10권1_2호
    • /
    • pp.33-36
    • /
    • 2009
  • The nuclear steam generator is composed of a bundle of tubes. The length of these tubes is very long, but their diameter is small. Fluid exists inside of the steam generator and its flow causes vibration, therefore these tubes are supported by anti-vibration bars. The wear damage due to the vibration is known as fretting wear, which should be minimized to ensure the safety of the plants. Research needs to be done about decreasing the amount of fretting wear. Hard coatings have proven to be very effective in reducing the amount of wear. The commercial coatings of TiN and CrN have excellent wear resistance and are used to protect the Inconel tube from fretting wear. The tube-on-flat type tester was used for conducting the fretting wear tests. It was found that the wear amounts of the coated tubes decreased depending on the coating thickness. CrN was found to be very effective in reducing the wear, while the wear amounts were dependent on the coating thickness in the case of TiN and a thick coating of TiN was very effective on wear resistance.

Al계 준결정 분말의 제조 및 응용

  • Kim, W. T.;Kim, D.H.;Lee, S.M.;E.Fleury;H.S. Ahn
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2002년도 제3회 최신 분말제품 응용기술 Workshop
    • /
    • pp.133-155
    • /
    • 2002
  • 1. Quasicrystalline powders shows exotic physical and mechanical p properties 2. Applications: structural application: strengthening particles for composites C Coating application: wear resistance, low friction coefficient 3. For thermal spaying: material loss during process should be c considered to control chemical composition of deposit 4. Friction coefficient is strongly dependent on contact geometry F Friction coefficient from pin on plate: 0.1-0.2 Friction coe야icient from flat on plate: about 0.46. 5. Quasicrystalline materials show lower friction coefficient but higher w wear rate than corresponding values of $Cr_20_3$ coated layer. 6. Amorphous coating seems to be promising

  • PDF

인산화 전분 ER 유체의 트라이볼로지 특성 (Tribological Characteristics of Phosphorated Starch Based Electrorheological Fluid)

  • 장민규;이철희;최재영;손정우;최승복
    • Tribology and Lubricants
    • /
    • 제26권1호
    • /
    • pp.7-13
    • /
    • 2010
  • This experimental study presents tribological characteristics under boundary lubrication contacts associated with electrorheolocal (ER) fluid. ER fluid is prepared by using phosphorated starch particles and silicone oil. Experimental apparatus of tribological tester is designed and constructed to evaluate tribological characteristics of pin specimens. Wear tests under boundary lubrication of ER fluid are experimentally performed under consideration of several operational factors such as normal load, sliding distance, sliding speed and specimen materials: steel, copper and aluminum. After wear test, microscopic surface changes of the worn pin specimens are analyzed in order to investigate measured wear characteristics by using the scanning electron microscope (SEM) as well as surface profilometer. In addition, the chemical wear characteristics are investigated by using energy dispersive x-ray spectroscopy (EDS). Moreover, friction coefficient measurements under different materials of pin specimens are conducted for the tribological investigations. In order to verify the effect of starch phosphate particles in ER fluid, the wear test results with ER fluid are compared with test results with only silicone oil. The results clearly present that the phosphorated starch based ER fluid shows the stabilized wear as well as friction characteristics after run-in operations, but the wear rate under ER fluid is increased.

탄소 섬유 복합재의 마찰 및 마모 특성에 미치는 속도 효과 (Effect of sliding velocity on the wear and friction characteristics of a carbon fiber composites)

  • 고성위;양병춘
    • 수산해양기술연구
    • /
    • 제40권4호
    • /
    • pp.337-343
    • /
    • 2004
  • 탄소 섬유강화 에폭시기지 복합재의 경면 가공한 스테인레스 강 상대재와 마찰과 마모에 바탕을 둔 연구에서 다음과 같은 결론을 얻었다. (1) 일방향 탄소섬유 강화 복합재의 마모 거동에 미치는 미끄럼 방향의 효과는 다르며 작용하는 마모 메커니즘의 형태에 의존한다. (2) 상온에서 경면 가공한 스테인리스 스틸에 대하여 미끄럼이 일어나면 AP 방향에서 높은 마모 저항과 낮은 마찰계수가 관찰되었다. (3) 복합재의 비마모율은 미끄럼 속도가 증가하면 N방향과 P방향에서는 감소하는 경향을 보이며, AP 방향에서는 증가하다가 감소한다. 이것은 마모 메카니즘의 영향으로 속도가 증가하면 마모 이착막의 생성이 빨라져 이착막 속의 탄소섬유가 윤활제의 역할을 하기 때문이다. (4) 복합재의 마찰계수는 미끄럼 속도가 증가하면 3방향 모두 증가하다가 일정한 값에 수렴하면 N방향이 가장 크며, P방향과 AP방향 순이다. 이는 N방향에서 마찰초반에 발생한 섬유의 쟁기질에 의한 상대재 표면의 손상과 돌기변형에 따른 것이며, AP방향의 마찰계수가 가장 낮다.

회전각가속도가 가스 포일 스러스트 베어링의 마찰 및 마모 특성에 미치는 영향 (Effects of Angular Acceleration on the Friction and Wear Characteristics of Gas Foil Thrust Bearings)

  • 황성호;김대연;김태호
    • Tribology and Lubricants
    • /
    • 제39권5호
    • /
    • pp.203-211
    • /
    • 2023
  • This study experimentally investigates the effects of angular acceleration on the friction and wear performances of a gas foil thrust bearing (GFTB) using a typical GFTB with six pads. The outer radius of the bearing is 31.5 mm, the total bearing area is 2,041 mm2 , and the bump foil and incline (ramp) height are both 500 ㎛. The newly developed GFTB test rig for measuring the friction torque and coefficient measures the axial load, drag torque, lift-off speed, and touch-down speed. The experiment is conducted for angular accelerations of 78.5, 314.2, and 328.3 rad/s2 at axial loads of 5, 10, and 15 N, respectively. The test shows that the start-up friction coefficient increases with increasing axial load at the same angular acceleration, and the friction coefficient decreases with increasing angular acceleration under the same axial load. As the angular acceleration increases, the lift-off speed at the motor start-up increases, and the touch-down speed at the motor stop decreases. The wear distance of the GFTB for a single on/off cycle increases with increasing axial load at the same angular acceleration and decreases nonlinearly with increasing angular acceleration under the same axial load. The test results suggest that adjusting the rotational angular acceleration helps reduce bearing friction and wear.

PECVD 공정에 의한 TiC, TiN 및 Ti(CN)의 마찰 마모 특성 연구 (A Study on the Friction and Wear Characteristics of TiC, TiN and Ti(CN) with PECVD Process)

  • 이봉구;전찬열;김정기;김동현;오성모
    • 한국공작기계학회논문집
    • /
    • 제14권2호
    • /
    • pp.1-7
    • /
    • 2005
  • In order to determine the wear Properties of PECVD ceramic coatings, wear process was evaluated using the coated pin of Falex Tribosystem. Coating materials deposited wear the TiC, TiN and Ti(CN). An experimental process was established to determine the tribological characteristics of friction and wear behavior under the variation of applied load, temperature and sliding distance by the Falex test machine. The experimental results indicate that TiN coating compared with TiC coating on e materials have e excellent friction and wear characteristics. However TiC coating compared i친 TiN coatings have a low friction coefficient with steel and good thermal stability, and Ti(CN) has the excellent anti-wear properly as well as the superiority of extreme pressure property. Compound coating compared wi simple coatings show improved tribological characteristics.