  • This study aims to visualize the friction and wear behaviors of metal coatings in real time. The main mechanism of wear is identified by observing all the processes in which wear occurs. The friction coefficients of the moments are monitored to confirm the relationship between the friction and wear characteristics of the coating. Thin Ag coatings, which are several hundred nanometers in thickness, are prepared by depositing Ag atoms on silicon substrates through a sputtering method. A pin-on-disk-type tribo-tester is installed inside a scanning electron microscope (SEM) to evaluate the friction and wear characteristics of the Ag coating. A fine diamond pin is brought into contact with the Ag coating surface, and a load of 20 mN is applied. The contact pressure is calculated to be approximately 15 GPa. The moments of wear caused by the sliding motion are visualized, and the changes in the friction characteristics according to each step of wear generation are monitored. The Ag coating can be confirmed to exhibit a wear phenomenon by gradually peeling off the surface of the coating on observing the friction and wear characteristics of the coating in real time inside the SEM. This can be explained by a typical plowing-type wear mechanism.

자동차용 마찰재에 사용되는 결합제와 강화섬유에 따른 마찰 및 마모특성에 관한 연구 (A Study of Binder Resins and Reinforcing Fibers in Automotive Friction Materials on Friction and Wear)

  • 김성진;장호
    • Tribology and Lubricants
    • /
    • 제15권4호
    • /
    • pp.314-320
    • /
    • 1999
  • Friction and wear characteristics of phenolic resin-based friction materials reinforced with aramid pulp and potassium titanate were investigated using a pad-on-disk type friction tester. Friction characteristics such as friction stability, thermal stability, and wear rate varied according to the type of phenolic resins and the relative amount of aramid pulp and potassium titanate. The modified novolac resin-based friction materials showed better heat resistance and friction stability than those with the unmodified(straight) novolac resin. Compared with friction materials filled with potassium titanate or aramid pulp only, the friction materials reinforced with both aramid pulp and potassium titanate showed good friction stability and wear resistance. Increment of aramid pulp from 10 to 20 vol.% however, showed little difference in friction stability.

고성능 금속마찰재의 트라이볼로지적 특성 (Tribological Characteristics for High Perfomance Metallic Friction Materials)

  • 김석삼;김재호;안효준
    • Tribology and Lubricants
    • /
    • 제14권1호
    • /
    • pp.45-53
    • /
    • 1998
  • Friction and wear test for two kinds of Cu-based sintered metallic friction material against cast iron disk was carried out by plate-on-disk type friction and wear tester to investigate the friction and wear characteristics of brake system in severe condition. In this experimental study, the counter specimen was cast iron which is being used generally in brakes of heavy duty equipments. Test friction materials were A type which was manufactured by foreign company and B type by domestic company. Friction coefficient and wear volume were measured and compared with each other. The experiment was performed under room temperature. The worn surface of cast iron disk and friction material were observed by scanning electron microscope. The temperature of surface of disk was measured continuously by the non-contacting thermometer. It was found that A type friction material had stable friction coefficient over the wide range of sliding condition, but B type friction material had unstable friction coefficient and lower value of 0.2 under the severe sliding condition.

침탄처리한 Ni-Cr-Mo강의 마찰-마모특성 (Friction-Wear Properties of Carburized SNCM)

  • 백승호
    • 열처리공학회지
    • /
    • 제11권3호
    • /
    • pp.159-167
    • /
    • 1998
  • In this study, friction-wear test was carried out on the carburized layer depth of a mechanical structure steel SNCM carburized with RX and LPG for 7hrs at $930^{\circ}C$ and also the wear properties of wear loss, wear rate, coefficient of friction, friction force and friction temperature were investigated. The wear properties for carburized layer of SNCM were tested on dry condition at the room temperature by the thrust load of 49~245N range at sliding speed of 0.2m/sec and the sliding speed of 0.2~1.0m/sec range at thrust load of 98N. Wear loss on the depth of carburizing layer was increased with increasing of thrust load and sliding speed, and with decreasing of hardness. The condition of worn surfaces were showed mild wear at less than the thrust load of 98N and sliding speed of 0.6m/sec but were showed severe wear at more than 98N and 0.6m/sec. The friction load and temperature were increased with increasing of thrust load but with increasing sliding speed was appeared minimum at 0.6m/sec. With increasing thrust load the wear rate was increased and the coefficient of friction was decreased, but with increasing sliding speed the wear rate and the coefficient of friction were decreased in 0.2~0.6m/sec and increased in 0.6~1.0m/sec, therefore 0.6m/sec in this testing is a transition velocity.

  • PDF

Friction and Wear of Polyimide-PTFE-Diamond Composites

  • Umeda, K.;Tanaka, A.;Takatsu, S.
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 proceedings of the second asia international conference on tribology
    • /
    • pp.233-234
    • /
    • 2002
  • Diamond composites hold promise as a tribological material because of low friction and high wear resistance. We studied friction and wear of polyimide-20vol% PTFE-diamond composites in open air at room temperature, focusing on the effects of diamond size, and diamond content, sliding conditions, and mating material. Friction coefficient and wear tend to Increase with increasing diamond size and content. Composites of appropriate diamond size and content showed a friction coefficient below 0.1 and specific wear of $10^{-7}\;mm^3/Nm$. Friction and wear of composites sliding against stainless steel were higher than those of Al_2O_3$ an increase that became increasingly not able with increasing diamond size.

  • PDF

프레팅 마멸계수 및 마찰계수 측정에 관한 연구 (Measurement of Wear and Friction Coefficients for the Prediction of Fretting Wear)

  • 조용주;김태완
    • Tribology and Lubricants
    • /
    • 제28권3호
    • /
    • pp.124-129
    • /
    • 2012
  • The prediction of fretting wear is a significant issue for the design of contacting mechanical components such as flexible couplings and splines, jointed structures and so on. In our earlier study, we developed a numerical model to predict the fretting wear using boundary element method. The developed algorithm needs experimental fretting wear coefficients and friction coefficients between two moving materials to get more reliable results. In this study, therefore, we demonstrated the measurement method of the fretting wear coefficients and friction coefficients using disk on plate tribometer with piazo actuator and gap sensor. For four different material combinations, the fretting wear coefficients and friction coefficients are acquired through the fretting wear experiment and the analysis of the measured values. Thess results are useful to predict the quantative fretting wear rate in the developed algorithm.

탄소 섬유 보강 폴리에테르에테르케톤의 마찰 및 마모 거동에 관한 연구 (A Study on Friction and Wear Behavior of Carbon Fiber Reinforced Polyetheretherketone)

  • 류성국;김경웅
    • 대한기계학회논문집A
    • /
    • 제25권6호
    • /
    • pp.930-937
    • /
    • 2001
  • The friction and wear behavior of short carbon fiber reinforced polyetheretherketone was studied experimentally under dry sliding conditions against SCM440(AISI 4140) disks with different surface roughness and hardness at the low sliding speeds and the high pressures on a pin-on-disk apparatus. Under the low disk surface roughness value the earsplitting noise and stick-slip were occurred. The increased adhesion friction and wear factor with stick-slip made the friction and wear behavior worse. Under the high disk surface hardness the break and falling-off of carbon fibers were accelerated. The carbon fibers fallen off from the matrix were ground into powder between two wear surfaces and this phenomenon caused abrasive friction and wear factor to increase. So the friction and wear behavior became worse. With the transfer film made of wear particles formed on a disk, the carbon powder film formed on a pin lowered a friction coefficient.

PTFE-폴리이미드 복합 재료의 마찰과 마모 특성 (Friction and Wear Characteristics of PTFE-Polyimide Composite)

  • 심현해;권오관
    • Tribology and Lubricants
    • /
    • 제11권4호
    • /
    • pp.28-34
    • /
    • 1995
  • PTFE has good mechanical and chemical stability at wide temperature range, and more over, shows a low value of friction coefficient. On the other hand, it shows cold flow and high wear rate. However, these short comings can be overcome by adding various fillers. In this experiment, PTFE and polyimide powder were mixed into composite and its tribological characteristics was investigated. 100% polyimide was also tested for comparison. The countefface material was a stainless steel (SUS304). Friction and wear tester of ring-on-block type was used at room temperature and under atmosphere. After the wear test, the worn surfaces were examined by optical microscope. The test results show that PTFE-polyimide composite generates. the wear transfer film on both sides of the friction surfaces, and, the friction coefficient and the wear rates are relatively low. 100% polyimide generated little wear transfer films, showed high friction and wear rates, and also showed some problems of vibration and noise. It even damaged the stainless steel countefface. It was concluded that 100% polyimide does not generate transfer film well because its shear resistanbe is high and it stickslips, thus, friction coefficients and wear rates are high. In case of PTFE-polyimide composite, on the other hand, transfer film containing sufficient PTFE adheres and remains on both wear surfaces well enough because PTFE has low shear resistance. Polyimide particles in the composite were proved to be able to bear normal load and does not show stick-slip because they are covered with transfer film containing much PTFE.

흑연과 지르콘의 상대적 함량에 따른 마찰재의 고온 마찰 및 마모특성 (High temperature Friction and Wear of Friction Material; The Effect of the Relative Amount of Graphite and Zirconium Silicate (ZrSiO$_4$))

  • 김성진;장호
    • Tribology and Lubricants
    • /
    • 제16권5호
    • /
    • pp.365-372
    • /
    • 2000
  • Tribological behavior of novolac resin-based friction materials with three different relative amounts of graphite and zirconium silicate was investigated by using a pad-on-disk type friction tester. The goal of this paper is to examine the effects of the relative amount of a lubricant and an abrasive in the automotive friction material on friction and wear characteristics at elevated temperature. Friction and wear of friction materials were affected by the existence of transfer film(3$\^$rd/ body layer) at friction interface and the composition of friction material, especially lubricant amount. The friction material with higher content of graphite indicated homogenized and durable transfer film, and resulted in stable friction coefficient regardless of the increase in friction heat. The experimental result also showed that the higher concentration of ZrSiO$_4$ in friction material aggravated friction stability and wear resistance due to the higher friction heat generated at fiction interface during high temperature friction test.

PTFE 복합재료의 마찰 . 마모 특성에 미치는 첨가제의 영향 (Effects of Additives on the Friction and Wear Properties of PTFE Composites)

  • 김용직;엄수현;김윤해
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 1999년도 추계학술발표대회 논문집
    • /
    • pp.88-94
    • /
    • 1999
  • Recently, PTFE-polyimide composites are being used self-lubricating parts for industrial field. Thus, this study is mainly concerned with friction and wear properties for the piston ring of non-lubricating air compressor which made of PTFE-polyimide composites. The friction and wear test was carried out for the different composition ratio under the atmosphere room temperature and constant load of 7.69N and their friction and wear properties were compared with each other at various sliding speed. Notable results are summarized as follows. PTFE 100% showed that friction coefficient was almost same values at 0.94 and 1.88m/s but the value was decreased at 2.83m/s because the friction temperature is higher than low speed. PTFE 80%-PI 20% showed the lowest mean friction coefficient at 2.83m/s. PTFE 20%-PI 80% showed the highest friction coefficient at 0.94m/s and the value was decreased at high speed but the value is higher than other materials except PTFE 100 %. PI 100% showed the highest friction coefficient at 0.94 and 1.88m/s because adhesive wear mainly occurred that speed. PTFE 100% showed highest specific wear rate on the whole. Specific wear rate of PTFE 80%-PI 20% was almost the same value with PTFE 20%-PI 80%. PI 100% showed the lowest value at high sliding speed because the friction surface was thicken and carbonated by high friction temperature.