Strength Development of Low Heat Portland Cement Concrete in High Strength Range (저열 포틀랜드 시멘트 콘크리트의 고강도 영역에서의 강도발현 특성)

  • Ha Jae Dam;Um Tai Sun;Lee Jong Ryul;Kwon Young Ho
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.05b
    • /
    • pp.353-356
    • /
    • 2005
  • Strength development of low heat portland cement(Type IV) concrete in high strength range is tested. In this study strength development according to water-binder ratio, strength development according to age, effect of fly ash and super plasticizer are tested. This study tests effect of low heat portland cement in high strength range concrete and provide guide line concrete mix design for later study and/or construction.

  • PDF

Modeling the compressive strength of cement mortar nano-composites

  • Alavi, Reza;Mirzadeh, Hamed
    • Computers and Concrete
    • /
    • v.10 no.1
    • /
    • pp.49-57
    • /
    • 2012
  • Nano-particle-reinforced cement mortars have been the basis of research in recent years and a significant growth is expected in the future. Therefore, optimization and quantification of the effect of processing parameters and mixture ingredients on the performance of cement mortars are quite important. In this work, the effects of nano-silica, water/binder ratio, sand/binder ratio and aging (curing) time on the compressive strength of cement mortars were modeled by means of artificial neural network (ANN). The developed model can be conveniently used as a rough estimate at the stage of mix design in order to produce high quality and economical cement mortars.

Concrete mix design for service life of RC structures exposed to chloride attack

  • Kwon, Seung-Jun;Kim, Sang-Chel
    • Computers and Concrete
    • /
    • v.10 no.6
    • /
    • pp.587-607
    • /
    • 2012
  • The purpose of this research is to propose a design technique of concrete mix proportions satisfying service life through genetic algorithm (GA) and neural network (NN). For this, thirty mix proportions and the related diffusion coefficients in high performance concrete are analyzed and fitness function for diffusion coefficient is obtained considering mix components like w/b (water to binder ratio), cement content, mineral admixture (slag, flay ash and silica fume) content, sand and coarse aggregate content. Through averaging the results of 10 times GA simulations, relative errors to the previous data decrease lower than 5.0% and the simulated mix proportions are verified with the experimental results. Assuming the durability design parameters, intended diffusion coefficient for intended service life is derived and mix proportions satisfying the service life are obtained. Among the mix proportions, the most optimized case which satisfies required concrete strength and the lowest cost is selected through GA algorithm. The proposed technique would be improved with the enhancement of comprehensive data set including wider the range of diffusion coefficients.

Fundamental Study on High Strength and High Durability Cement Concrete Pavement : Part I Optimum Mix Proportions (시멘트콘크리트 포장의 고강도 고내구성을 위한 기초 연구 : Part I 최적배합에 관한 연구)

  • Yun, Kyong-Ku;Park, Cheol-Woo
    • International Journal of Highway Engineering
    • /
    • v.11 no.3
    • /
    • pp.41-49
    • /
    • 2009
  • Cement concrete pavement has become more common in Korean highway systems. However, as its service period increases, there are some technical problems occurs and no clear solution is available primarily due to the lack of active researches. This research, hence, aims to develop a new mix proportion that may provide better strength and durability with extended service life. Based on a variety of literature reviews, the experimental variables were determined as unit cement content, S/a ratio and W/C ratio. From the experimental works, it is recommended to increase the unit cement content up to 375kg/$m^3$, 400kg/$m^3$ and 425kg/$m^3$. The target slump and air content were set 40mm and 5%, respectively. The maximum size of coarse aggregate was decided to be 25mm because of the easiness of supply in the field. The reduction of W/C ratio was necessarily required and decreased to 0.4 which was proven not to cause any mixing problem with the increased unit cement contents along with polycarbon-based high range water reducing agent. In addition, it was known that the S/a ratio could be reduced to 0.34. The lowered S/a might be possible because of the increased cement paste and hence increased cohesiveness and workability.

  • PDF

Effect of polyolefin fibers on the permeability of cement-based composites

  • Hsu, Hui-Mi;Lin, Wei-Ting;Cheng, An
    • Computers and Concrete
    • /
    • v.9 no.6
    • /
    • pp.457-467
    • /
    • 2012
  • This study evaluates the permeability of cement-based composites, which are a mix of polyolefin fibers and silica fume. Test results indicate that permeability increases as the water/cementitious ratio increases. Silica fume in cement-based composites produced hydrated calcium silicate and filled the pores. However, permeability decreased as the addition of silica fume increased. Specimens containing polyolefin fibers also provided higher permeability resistance. The polyolefin fiber length did not have a significant effect on permeability. The decrease in the permeability is mainly due to the addition of silica fume and lower water/cementitious ratio. Addition of fibers marginally decreases the permeability. Incorporating polyolefin fiber and silica fume in composites achieved more significant decreases in permeability. The correlated test results reveal the interrelationship between them.

Effect of fly ash and plastic waste on mechanical and durability properties of concrete

  • Paliwal, Gopal;Maru, Savita
    • Advances in concrete construction
    • /
    • v.5 no.6
    • /
    • pp.575-586
    • /
    • 2017
  • The disposal of polythene waste and fly ash is causing serious threat to the environment. Aim of this study is to decrease environmental pollution by using polythene waste and fly ash in concrete. In this study, cement was partially replaced with 0%, 5%, 10%, 15% and 20% fly ash (by weight) and plastic waste was added in shredded form at 0.6% by weight of concrete. The specimens were prepared for the concrete mix of M25 grade and water to cementitious material ratio (w/c) was maintained as 0.45. Fresh concrete property like workability was examined during casting the specimens. Hardened properties were found out by carrying out the experimental work on cubes, cylinders and beams which were cast in laboratory and their behavior under test were observed at 7 & 28 days for compressive strength and at 28 days for density, flexural strength, dynamic modulus of elasticity, abrasion resistance, water permeability and impact resistance. Overall results of this study show that addition of 0.6% (by weight of the concrete) plastic waste with 10% (by weight of cement) replacement of cement by fly ash result an improvement in properties of the concrete than conventional mix.

A Study on the Improvements of Strengths of Water-Permeable Concrete (투수성 콘크리트의 강도개선에 관한 연구)

  • 은재기;이철웅;김완기;조영국;소양섭
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1999.04a
    • /
    • pp.307-312
    • /
    • 1999
  • The purpose of this study is to ascertain the strength properties of water-permeable concrete with redispersible polymer powder, silica fume and polypropylene fibers. The water-permeable concrete using rediapersibel polymer powder with a water-cement ratio of 25%, polymer-cement ratios of 0 to 10%, silica fume contents of 0 to 10% and fiber contents of 0 to 1.5% are prepared, and tested for flexural strength, compressive strength and water permeability. From the test results, improvements in the strength properties of the water-permeable concrete due to the addition of the redispersible polymer powder, silica fume and fibers are discussed. It is concluded from the test results that the superior flexural and compressive strengths of water-permeable concretes are obtained at a propylene fiber content of 1.0% with a void filling ratio of 50%. And, the water-permeable concrete having a flexural strength of 15.6~28.4kgf/$\textrm{cm}^2$, a compressive strength of 63.5~120.6kgf/$\textrm{cm}^2$, and a coefficient of permeability of 1.14~1.70cm/s at a void filling ratio of 30% can be prepared. Also water-permeable concrete having a flexural strength of 35.6~57.9kgf/$\textrm{cm}^2$, a compressive strength of 164.0~290.0kgf/$\textrm{cm}^2$, and a coefficient of permeability of 0.19~1.04cm/s at a void filling ratio of 50% can be prepared in the consideration of the mix proprotioning factors.

  • PDF

Influences of Water to Cement Ratio and Chemical Admixtures on the Quality of Inter-Locking Block (인터로킹 블록의 품질에 미치는 물시멘트비와 화학혼화제의 영향)

  • 이상태;김기철;신병철;김진선;한천구
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.10c
    • /
    • pp.157-160
    • /
    • 1998
  • KS F 4419, which is dealt with the Inter-Locking block, states that water to cement ratio for manufacturing inter-locking block should be less than 25% and in KS F4419, the use of admixture is shown to be reluctant to recommend. In this paper, reinvestigation of some regulations in KS F 4419 are carried out. According to the experimental results, as W/C increases, flexural strength and compressive strength are tended to decrease, whereas they increases within certain range, Flexural strength and compressive strength have higher values in 1:2(W/C=35%), 1:4(W/C=45%) and 1:6(W/C=55%) of mix proportions. Moreover they have rather higher values with the containment of high range AE water-reducing agent. The absorption ratios decrease with the increase of W/C and the containment of high range AE water-reducing agent. Therefore, the regulations on the W/C and admixture in KS F 4419 reguire revision.

  • PDF

An Experimental Study on the Mechanical Properties of Fiber Reinforced Cement Composites Utilizing by-Products(II) (산업부산물을 활용한 섬유보강 시멘트 복합체의 역학적 특성에 관한 실험적 연구(II))

  • 박승범;윤의식;조청휘
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1993.10a
    • /
    • pp.144-149
    • /
    • 1993
  • The results of an experimental study on the manufacture and the mechanical properties of carbon fiber reinforced silica fume.cement composites and light weight fly ash.cement composites are presented in this paper. The CF reinforced silica fume.cement composites using silica fume early strength cement were prepared with Pan-derived or Pitch-derived CF, and Lt. Wt, fly ash.cement composites using fly ash, early strength cement, perlite and a small amount of foaming agent. As the test results show, the flexural strength, toughness and ductility of CF reinforced silica fume .cement composites were remarkably increased by fiber contents. Also, the manufacturing process technology of Lt. Wt. fly ash.cement composites was developed and its optimum mix proportions were proposed. And the compressive and flexural strength of the fly ash.cement composites by hot water cured were improved even more than by moist cured, but are decreased by increasing fly ash replaced ratio for cement.

  • PDF

Hydration properties of cement pastes containing high-volume mineral admixtures

  • Tang, Chao-Wei
    • Computers and Concrete
    • /
    • v.7 no.1
    • /
    • pp.17-38
    • /
    • 2010
  • This research aimed to investigate the influence of high-volume mineral admixtures (MAs), i.e., fly ash and slag, on the hydration characteristics and microstructures of cement pastes. Degree of cement hydration was quantified by the loss-on-ignition technique and degree of pozzolanic reaction was determined by a selective dissolution method. The influence of MAs on the pore structure of paste was measured by mercury intrusion porosimetry. The results showed that the hydration properties of the blended pastes were a function of water to binder ratio, cement replacement level by MAs, and curing age. Pastes containing fly ash exhibited strongly reduced early strength, especially for mix with 45% fly ash. Moreover, at a similar cement replacement level, slag incorporated cement paste showed higher degrees of cement hydration and pozzolanic reaction than that of fly ash incorporated cement paste. Thus, the present study demonstrates that high substitution rates of slag for cement result in better effects on the short- and long-term hydration properties of cement pastes.