The Fundamental Properties of High-Strength Concrete Using Pre-mixed Cement Corresponding to Water Binder Ratio (물 결합재비 변화에 따른 프리믹스 시멘트를 사용한 고강도 콘크리트의 기초적 특성)

  • Jin, Cheong-Ri;Han, Dong-Yeop;Kim, Ki-Hoon;Hwang, Yin-Seong;Kim, Sung-Su;Han, Cheon-Goo
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.04a
    • /
    • pp.369-372
    • /
    • 2008
  • This study analysis fundamental properties of high-strength concrete corresponding to W/B ratio for suggested table of high strength concrete, mixed with premixed cement. As a result of this study, the amount of using air entraining and high-range water reducing agent for intended slump flow and air content decreased as W/B increased, and the setting time corresponding to the W/B ratio delayed as W/B ratio increased except 20% W/B ratio. The compressive strength according to W/B ratio decreased as W/B ratio increased, and there was no great deferent as the intended slump flow. Also it could possible to use this study at work as the correlation coefficient is high enough as 0.9646 substituting B/W and compressive strength for the regression formula.

  • PDF

Modelling the performance of self-compacting SIFCON of cement slurries using genetic programming technique

  • Cevik, Abdulkadir;Sonebi, Mohammed
    • Computers and Concrete
    • /
    • v.5 no.5
    • /
    • pp.475-490
    • /
    • 2008
  • The paper explores the potential of applicability of Genetic programming approach (GP), adopted in this investigation, to model the combined effects of five independent variables to predict the mini-slump, the plate cohesion meter, the induced bleeding test, the J-fiber penetration value, and the compressive strength at 7 and 28 days of self-compacting slurry infiltrated fiber concrete (SIFCON). The variables investigated were the proportions of limestone powder (LSP) and sand, the dosage rates of superplasticiser (SP) and viscosity modifying agent (VMA), and water-to-binder ratio (W/B). Twenty eight mixtures were made with 10-50% LSP as replacement of cement, 0.02-0.06% VMA by mass of cement, 0.6-1.2% SP and 50-150% sand (% mass of binder) and 0.42-0.48 W/B. The proposed genetic models of the self-compacting SIFCON offer useful modelling approach regarding the mix optimisation in predicting the fluidity, the cohesion, the bleeding, the penetration, and the compressive strength.

Clustering-based identification for the prediction of splitting tensile strength of concrete

  • Tutmez, Bulent
    • Computers and Concrete
    • /
    • v.6 no.2
    • /
    • pp.155-165
    • /
    • 2009
  • Splitting tensile strength (STS) of high-performance concrete (HPC) is one of the important mechanical properties for structural design. This property is related to compressive strength (CS), water/binder (W/B) ratio and concrete age. This paper presents a clustering-based fuzzy model for the prediction of STS based on the CS and (W/B) at a fixed age (28 days). The data driven fuzzy model consists of three main steps: fuzzy clustering, inference system, and prediction. The system can be analyzed directly by the model from measured data. The performance evaluations showed that the fuzzy model is more accurate than the other prediction models concerned.

Effect of temperature on the behavior of self-compacting concretes and their durability

  • Salhi, M.;Li, A.;Ghrici, M.;Bliard, C.
    • Advances in concrete construction
    • /
    • v.7 no.4
    • /
    • pp.277-288
    • /
    • 2019
  • The formulation of self-compacting concretes (SCC) and the study of their properties at the laboratory level were currently well mastered. The aim of this work is to characterize SCC under hot climatic conditions and their effects on the properties of fresh and hardened SCC. Particularly, the effect of the initial wet curing time on the mechanical behavior such as the compressive strength and the durability of the SCCs (acid and sulfate attack) as well as the microstructure of SCCs mixtures. In this study, we used two types of cement, Portland cement and slag cement, three water/binder (W/B) ratio (0.32, 0.38 and 0.44) and five curing modes. The obtained results shows that the compressive strength is strongly influenced by the curing methods, 7-days of curing in the water and then followed by a maturing in a hot climate was the optimal duration for the development of a better compressive strength, regardless of the type of binder and the W/B ratio.

Autogenous Shrinkage of Ultra-high Strength Concrete according to W/B and Aggregate Kinds (W/B 및 골재암종 변화에 따른 초고강도 콘크리트의 자기수축특성)

  • Jung, Sang-Woon;Kim, Tae-Seon;Lee, Hong-Kyu;Han, Dong-Yeop;Han, Min-Cheol;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2014.11a
    • /
    • pp.127-128
    • /
    • 2014
  • The aim of this research is selecting an economical aggregate type for ultra-high strength concrete with 80 to 120 MPa of compressive strength. As the tests, the effect of water-to-binder ratios and types of aggregate on autogenous shrinkage of ultra-high strength concrete were evaluated. as the results of a series of tests performed, the slump flow was satisfied the target range of 600 ± 100 mm, and the concrete mixture with RLA showed higher elastic modulus than the other cases. For the autogenous shrinkage preventing performance, in the case of water-to-binder ratio of 15, and 20 %, the mixture with BA showed slightly improved autogenous shrinkage reducing effect than the mixture with RLA while the mixture with RLA showed better performance at 25 % of water-to-binder ratio. Therefore, based on the tests results of slump flow, elastic modulus, and autogenous shrinkage, the RLA is considered as a better aggregate type for this purpose.

  • PDF

An Experimental Study on appropriate water-binder ratio for development of ultra high strength concrete (초고강도 콘크리트 개발을 위한 적정 물-결합재비 선정에 관한 실험적 연구)

  • Jang, Jong-Min;Jang, Hyun-O;Lee, Han-Seung
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2016.10a
    • /
    • pp.79-80
    • /
    • 2016
  • In this study, we measured the relative density and the compressive strength in order to select the appropriate W/ B for the ultra-high strength concrete development. If W/B is lowered than the W/B of highest relative density, it was confirmed that the strength is lowered. However, if water is increased than the W/B of highest relative density, the relative density is decreased compressive strength was similar. The selection of the W/B of the lower than the highest relative density is not appropriate. Appropriate W/B is selected to be more than the maximum relative density of W/B.

  • PDF

Strength and Some Durability Properties of Concrete Containing Rice Husk Ash Produced in a Charcoal Incinerator at Low Specific Surface

  • Abalaka, A.E.
    • International Journal of Concrete Structures and Materials
    • /
    • v.7 no.4
    • /
    • pp.287-293
    • /
    • 2013
  • Strength and some durability properties of concrete containing rice husk ash (RHA) predominantly composed of amorphous silica at a specific surface of 235 $m^2/kg$ produced using a charcoal incinerator were determined. The maximum ordinary Portland cement (OPC) replacement with the RHA increased with increase in water/binder (w/b) ratio of the concrete mixes. The results show that 15 % OPC could be substituted by the RHAwithout strength loss at w/b ratio of 0.50. The split tensile strength generally increased with increase in RHA content for the mixes.

A Study on the Choice of Optimal Mixtures and Sensibility Properties of High Strength Concrete and Mass Concrete to apply the High Rising Building (초고층구조물에 적용하기 위한 고강도콘크리트 및 매스콘크리트의 최적배합선정 및 민감도특성에 관한 연구)

  • Lee, Sang-Soo;Song, Ha-Young;Kim, Eul-Yong
    • Journal of the Korea Institute of Building Construction
    • /
    • v.5 no.2 s.16
    • /
    • pp.153-159
    • /
    • 2005
  • This study is to choose the optimal mixture and to analyze the sensibility properties of High strength concrete and mass concrete to apply the high rising building. The main experimental variables were water/binder ratio $39\%,\;33\%,\;35\%\;and\;37\%$, replacement ratio of fly ash $5\%,\;10\%\;and\;15\%$, in the high strength concrete and water/binder ratio $39\%,\;41\%\;and\;43\%$, replacement ratio of fly ash $10\%,\;20\%\;and\;30\%$, in the man concrete. According to the test results, the principal conclusions are summarized as follows. 1) The slump(or slump flow) and air content of fresh concrete were found to be the highest in the elapsed time 30 minutes. 2) The optimal mixture conditions are W/B $40\%$, FA $25\%$ in the mass concrete and W/B $33.4\%$, FA $15\%$ in the high strength concrete. 3) The ranges of sensibility are satisfied in the moisture content ${\pm}l\%\;and\;S/a\;{\pm}2\%$.

Effects of Crushed Coal Bottom Ash on the Properties of Mortar with Various Water-to-binder Ratios (다양한 물-결합재비를 갖는 모르타르의 물성에 대한 파쇄 바텀애시의 영향)

  • Tafesse, Million;Kim, Hyeong-Ki
    • Resources Recycling
    • /
    • v.25 no.6
    • /
    • pp.29-40
    • /
    • 2016
  • Effects of crushed coal bottom ash (CBA) with maximum size of 1 mm on the properties of mortar with various water-to-binder ratios (w/b) were evaluated. The present work is a fundamental study to establish a method of mix proportion design for mortar and concrete with CBA. The workability, air contents, and compressive strength of mortar were measured. Efficiency of CBA on the compressive strength at 28 days, which was adopted for mix proportion design, was evaluated based on concepts of 'equivalent strength' in CEN/TR 16637. It was found that the CBA could be contributed as a binder in mortar in some cases, while in other cases act as at aggregates. The efficiency of CBA was influenced by types of CBA and their replacement ratio, and w/b of mortar.

The Effects of Void Ratio on Extrudability and Buildability of Cement-based Composites Produced by 3D Printers (3D 프린터용 시멘트 복합체의 간극비가 출력성과 적층성에 미치는 영향)

  • Seo, Ji-Seok;Lee, Bong-Chun;Kim, Yun-Yong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.7
    • /
    • pp.104-112
    • /
    • 2019
  • The material properties of the 3D printing cement composite mortar were evaluated, and the performance range in which printing was possible was calculated using the void ratio in a fresh state as a single index. As a results of the tests, as the water-binder ratio (W/B) increased, the mortar flow value increased and the density and strength decreased. As the sand-binder ratio (SS/B) increased, the mortar flow value decreased. However, strength and density increased and decreased up to a certain SS/B. As admixture-binder ratio (Ad/B) increased, mortar flow value, density, and strength decreased. These trends make it difficult to mix-design to meet the target performances of 3D printing mortars, represented by extrudability and buildability. The value of mortar flow increased proportionally with the void ratio, while the density and strength apparently decreased as the void ratio increased. This indicates that void ratio can be utilized as a single index for controlling the material properties in the design of mortar mixtures. It was found that mortar mixture could be printed by a 3D printer when the void ratio was in the range from 0.6 to 0.7. This was verified by printing a mortar which has the void ratio of 0.634. The mortar was produced with the mixture design of W/B 35.0%, SS/B 60.0%, and Ad/B 0.1%. Further research applying diverse admixtures is needed to improve the quality of 3D printing output mortars.