• Title/Summary/Keyword: waste tire rubber

Search Result 56, Processing Time 0.023 seconds

Application of waste tire rubber aggregate in porous concrete

  • Shariati, Mahdi;Heyrati, Arian;Zandi, Yousef;Laka, Hossein;Toghroli, Ali;Kianmehr, Peiman;Safa, Maryam;Salih, Musab N.A.;Poi-Ngian, Shek
    • Smart Structures and Systems
    • /
    • v.24 no.4
    • /
    • pp.553-566
    • /
    • 2019
  • This study aimed to categorize pervious rubberized concrete into fresh and hardened concrete analyzing its durability, permeability and strength. During the globalization of modern life, growing population and industry rate have signified a sustainable approach to all aspects of modern life. In recent years, pervious concrete (porous concrete) has significantly substituted for pavements due to its mechanical and environmental properties. On the other hand, scrap rubber tire has been also contributed with several disposal challenges. Considering the huge amount of annually tire wastes tossing out, the conditions become worse. Pervious concrete (PC) gap has graded surface assisted with storm water management, recharging groundwater sources and alleviate water run-offs. The results have shown that the use of waste tires as aggregate built into pervious concrete has tremendously reduced the scrap tire wastes enhancing environmental compliance.

Effects of a Crosslinking Agent and a Compatibilizer on the Mechanical and Rheological Properties of Waste PP and Waste Ground Rubber Tire Composites

  • Kim, Donghak;Kim, Seonggil;Lee, Minji;Lee, Chanhee;Lee, Horyong;Lee, Seongwoo;Lee, Suhyeon;Moon, Myeongsuk;Bang, Daesuk
    • Elastomers and Composites
    • /
    • v.50 no.1
    • /
    • pp.24-29
    • /
    • 2015
  • In this study, we investigated the effects of a crosslinking agent and a compatibilizer on the mechanical and rheological properties of waste PP and waste ground rubber tire (WGRT) composites. In order to simulate a commercial TPV, the component of waste PP and WGRT was fixed at 30 and 70 wt%, respectively. With the simple addition of SEBS-g-MA into the waste PP/WGRT composites, the tensile strength of the composite was decreased, whereas both the elongation at break and impact strength were significantly increased because of rubbery characteristics of SEBS-g-MA. In order to further improve the properties of the composites, the waste PP/WGRT/SEBS-g-MA composites was revulcanized with dicumyl peroxide (DCP). As expected, mechanical properties of the revulcanized composites was generally improved. Especially, with 15 and 1 phr of SEBS-g-MA and DCP, elongation at break was highest value of about 183% because of the recross-linking of WGRT without chain scission of the main chain. It was found that complex viscosity of the revulcanized composite increased which might verify further vulcanization of the WGRT.

Post-fire flexural behavior of functionally graded fiber-reinforced concrete containing rubber

  • Nematzadeh, Mahdi;Mousavi, Reza
    • Computers and Concrete
    • /
    • v.27 no.5
    • /
    • pp.417-435
    • /
    • 2021
  • The optimal distribution of steel fibers over different layers of concrete can be considered as an appropriate method in improving the structural performance and reducing the cost of fiber-reinforced concrete members. In addition, the use of waste tire rubber in concrete mixes, as one of the practical ways to address environmental problems, is highly significant. Thus, this study aimed to evaluate the flexural behavior of functionally graded steel fiber-reinforced concrete containing recycled tire crumb rubber, as a volume replacement of sand, after exposure to elevated temperatures. Little information is available in the literature regarding this subject. To achieve this goal, a set of 54 one-, two-, and three-layer concrete beam specimens with different fiber volume fractions (0, 0.25, 0.5, 1, and 1.25%), but the same overall fiber content, and different volume percentages of the waste tire rubber (0, 5, and 10%) were exposed to different temperatures (23, 300, and 600℃). Afterward, the parameters affecting the post-heating flexural performance of concrete, including flexural strength and stiffness, toughness, fracture energy, and load-deflection diagrams, along with the compressive strength and weight loss of concrete specimens, were evaluated. The results indicated that the flexural strength and stiffness of the three-layer concrete beams respectively increased by 10 and 7%, compared to the one-layer beam specimens with the same fiber content. However, the flexural performance of the two-layer beams was reduced relative to those with one layer and equal fiber content. Besides, the flexural strength, toughness, fracture energy, and stiffness were reduced by approximately 10% when a 10% of natural sand was replaced with tire rubber in the three-layer specimens compared to the corresponding beams without crumb rubber. Although the flexural properties of concrete specimens increased with increasing the temperature up to 300℃, these properties degraded significantly with elevating the temperature up to 600℃, leading to a sharp increase in the deflection at peak load.

Mechanical Properties of Polyethylene/Polypropylene/Waste Tire Rubber Powder Composites (폴리에틸렌/폴리프로필렌/폐타이어고무분말 복합체의 기계적 특성)

  • Choi, Jeong-Su;Park, Cha-Cheol
    • Elastomers and Composites
    • /
    • v.46 no.4
    • /
    • pp.318-323
    • /
    • 2011
  • To recycle the waste tire rubber powder, rubber powder composite for waterproof sheet was prepared, and analyzed the effect of the kind of resin and the amount of crosslinking agent on the mechanical property of the composites. The elongation-at-break of the PE composite increased more than 3 times as EPDM was added into rubber composites. As the content of the crosslinking agent increased, the tensile strength of composite increased as well. When recycled polypropylene was used, the increase in composite's tensile strength was more than 3 times. Therefore to use the recycled PP in composite is more effective rather than PP in term mechanical properties.

A study on the Characteristic of Waste Ground Rubber Tire Powders with Pre-treatment Process for Recycling (전처리 공정에 따른 폐타이어 재생 고무분말의 특성연구)

  • Park, Jongmoon;An, Ju-Young;Park, Jin-Eui;Bang, DaeSuk;Kim, Bong-Suk;Oh, Myung-Hoon
    • Resources Recycling
    • /
    • v.24 no.2
    • /
    • pp.55-61
    • /
    • 2015
  • In this study, mechanical properties of waste ground rubber tire powder were investigated to evaluate the influence of pre-treatment process for recycling. The tensile test, fracture test and morphology observation were carried out using various kinds of waste ground tire powders, which were produced by grinding and devulcanization process, respectively. As a results, it was found that the produced rubber powder through grinding process increased its tensile strength and elongation with decreasing particle size because of decreasing surface area. Devulcanized rubber powder also increased its tensile strength and elongation by de-crosslink with sulfur. It could be also suggested that devulcanization treatment after grinding process was more efficient recycling process for both increasing tensile property and fracture elongation of waste ground rubber tire powders.

Effect of the Curing Conditions on the Recycling of the Scrap Waste Tire (폐타이어 재활용에 있어서 가공조건의 영향)

  • Cho, Ha-Na;Kim, Jin-Kuk
    • Elastomers and Composites
    • /
    • v.31 no.2
    • /
    • pp.95-103
    • /
    • 1996
  • Nowadays, recycling of waste materials is one of great attention among all industries. Especially, the waste tires become a significant problem with increasing in a number of automobiles. For recycling of the waste tires, a polyurethane binder was mixed with the scrapped rubber powders obtained from tread part of the waste tire. This study covered the effect of processing conditions;curing temperature and curing time;on the mechanical properties of the blend. We also compared the experimental results from labors-tory scale with those from scale-up.

  • PDF

Characteristics Studies of Waste Tire Rubber Powders using the Different Grinding Methods (분쇄 방식에 따른 폐타이어 고무분말의 특성 연구)

  • Park, Jong-Moon;An, Ju-Young;Bang, Daesuk;Kim, Bong-Seok;Oh, Myung-Hoon
    • Resources Recycling
    • /
    • v.23 no.3
    • /
    • pp.44-50
    • /
    • 2014
  • In this study, a method of shear crushing and a two-stage disk mill were introduced to grind the waste tire powder. Rubber chips with various size were obtained during the crushing or grinding step. The two-stage disk mill was composed of two drum-type blades rotating at various speed and in opposite directions. Therefore, more roughly surfaced particles of micronized waste tire powder were obtained using shear crushing rather than using conventional cutting crushing. In this study, the shape of shear-crushed waste tire particles was compared with conventional cutting crushing particles by scanning electron microscope. In addition, the particle size analyzer was employed to determine the appropriate particle size of waste ground tire powders obtained in this study.

Properties of recycled green building materials applied in lightweight aggregate concrete

  • Wang, Her-Yung;Hsiao, Darn-Horng;Wang, Shi-Yang
    • Computers and Concrete
    • /
    • v.10 no.2
    • /
    • pp.95-104
    • /
    • 2012
  • This study uses recycled green building materials based on a Taiwan-made recycled mineral admixture (including fly ash, slag, glass sand and rubber powder) as replacements for fine aggregates in concrete and tests the properties of the resulting mixtures. Fine aggregate contents of 5% and 10% were replaced by waste LCD glass sand and waste tire rubber powder, respectively. According to ACI concrete-mixture design, the above materials were mixed into lightweight aggregate concrete at a constant water-to-binder ratio (W/B = 0.4). Hardening (mechanical), non-destructive and durability tests were then performed at curing ages of 7, 28, 56 and 91 days and the engineering properties were studied. The results of these experiments showed that, although they vary with the type of recycling green building material added, the slumps of these admixtures meet design requirements. Lightweight aggregate yields better hardened properties than normal-weight concrete, indicating that green building materials can be successfully applied in lightweight aggregate concrete, enabling an increase in the use of green building materials, the improved utilization of waste resources, and environmental protection. In addition to representing an important part of a "sustainable cycle of development", green building materials represent a beneficial reutilization of waste resources.

A Study on Recycling Technology of Waste Tire Powder by Particle Size Distribution Analysis (입도분포해석에 의한 폐타이어 분말의 재활용 연구)

  • Hwang, Sung-Hyuk;Jung, Jae-Hum;Pack, So-Yoon;Kim, Jin-Kuk
    • Elastomers and Composites
    • /
    • v.38 no.2
    • /
    • pp.128-138
    • /
    • 2003
  • It goes to be serious with environmental pollution because of great number of waste tires scrapped each you. That is why there are lots of studies for efficient recycle. We tried to reduce particle size of the waste tire powder using a new technology of self-designed grinding machine (SDGM) and ultrasonic treatment. The purpose of this study is to improve the physical properties of reduced waste tire powder. We investigated the fine powder by particle size distribution(PSD) analysis. And also we examined the physical and mechanical properties and cross-link density at various particle sire. Also we carried out morphological studies after making the products by SEM.

Effect of rubber fiber size fraction on static and impact behavior of self-compacting concrete

  • Thakare, Akshay A.;Siddique, Salman;Singh, Amardeep;Gupta, Trilok;Chaudhary, Sandeep
    • Advances in concrete construction
    • /
    • v.13 no.6
    • /
    • pp.433-450
    • /
    • 2022
  • The conventional disposal methods of waste tires are harmful to the environment. Moreover, the recycling/reuse of waste tires in domestic and industrial applications is limited due to parent product's quality control and environmental concerns. Additionally, the recycling industry often prefers powdered rubber particles (<0.60 mm). However, the processing of waste tires yields both powdered and coarser (>0.60 mm) size fractions. Reprocessing of coarser rubber requires higher energy increasing the product cost. Therefore, the waste tire rubber (WTR) less favored by the recycling industry is encouraged for use in construction products as one of the environment-friendly disposal methods. In this study, WTR fiber >0.60 mm size fraction is collected from the industry and sorted into 0.60-1.18, 1.18-2.36-, and 2.36-4.75-mm sizes. The effects of different fiber size fractions are studied by incorporating it as fine aggregates at 10%, 20%, and 30% in the self-compacting rubberized concrete (SCRC). The experimental investigations are carried out by performing fresh and hardened state tests. As the fresh state tests, the slump-flow, T500, V-funnel, and L-box are performed. As the hardened state tests, the scanning electron microscope, compressive strength, flexural strength and split tensile strength tests are conducted. Also, the water absorption, porosity, and ultrasonic pulse velocity tests are performed to measure durability. Furthermore, SCRC's energy absorption capacity is evaluated using the falling weight impact test. The statistical significance of content and size fraction of WTR fiber on SCRC is evaluated using the analysis of variance (ANOVA). As the general conclusion, implementation of various size fraction WTR fiber as fine aggregate showed potential for producing concrete for construction applications. Thus, use of WTR fiber in concrete is suggested for safe, and feasible waste tire disposal.