  • This paper presents the prediction of shear strength of oil contaminated clay using fall cone test used to determine the liquid limit of soil. The penetration depth of fall cone is related to water content of soil. Laboratory vane shear can also be related to water content. To explore the relative correlation between penetration depth of fall cone and laboratory vane shear, both fall cone tests and laboratory vane shear test were carried out with water contents of soil. The developed empirical relationships in this studys showed that the shear strength is reduced to 3.9% with 1% increase of oil content. And, the lesser initial water content of contaminated clay, the more shear strength of contaminated clay is affected by oil content.

북동태평양 심해저 퇴적물의 베인전단강도 측정에 관한 연구 (A Study on Vane Shear Strength Measurement of Deep-sea Sediment in the Northeast Equatorial Pacific)

  • 지상범;박정기;손승규;이경용;이현복
    • 자원환경지질
    • /
    • 제37권2호
    • /
    • pp.235-244
    • /
    • 2004
  • 북동태평양 심해저퇴적물 전단강도 측정의 정확성을 위하여 측정 방법에 따른 전단강도 측정 결과들을 비교하였다. 비교 항목들은 1) 동일한 시료를 두 종류의 베인 전단강도 측정기(수동 베인, 전동 베인)를 이용하여 측정한 결과, 2) 시료채취 후 즉시 선상에서 측정한 결과와 3개월 뒤 육상의 실험실에서 측정한 결과, 3) 동일한 정점에서 채취된 두개시료를 측정한 결과, 그리고 4) 동일한 코어 내에서 4회 반복 실험한 결과이다. 측정 결과, 전단강도 값은 퇴적깊이에 따라 뚜렷한 변화 양상을 보였다. 또한, 동일한 정점에서 채취한 두개의 코어 퇴적물에 대한 전단강도를 비교한 결과, 두 시료에서 측정된 변화폭이 장비차이에 따른 변화와 보관 조건에 의한 변화보다 높게 나타났다. 이와 같은 결과는 퇴적 깊이에 따른 전단강토의 변화가 지질공학적 물성변화에 의해 야기되었음을 지시한다.

순결형 그라우트의 초기 전단강도 특성에 대한 연구 (A Study on the Initial Shear Strength Characteristics of Sudden Gelation Grout)

  • 허형석;박인준
    • 한국지반공학회논문집
    • /
    • 제36권9호
    • /
    • pp.33-44
    • /
    • 2020
  • 순결 특성을 갖는 그라우트에 대한 경화 전 소성상태의 전단강도 특성을 분석하기 위하여 혼합물의 점도와 실내 베인전단시험을 수행하였다. 그라우트를 물-시멘트비(w/c) 별로 제조하고 전단강도시험을 실시하였다. 그라우트의 소성상태 전단강도는 물-시멘트비에 영향을 많이 받아 물-시멘트비가 낮을수록 초기에 높은 전단강도가 발현되었으며, 양생 시간이 길어질수록 높은 전단강도를 나타내었다. 최대전단강도는 그 값이 클수록 작은 회전각에서 발현되고, 최대전단강도 값이 작을수록 큰 회전각에서 발현되었다. 또한, 겔 상태의 그라우트는 최대 전단강도가 발현 이후 급격히 전단강도가 저하되고 베인날의 회전각이 약 70°~90°이후에는 일정한 수준으로 수렴되는 것을 확인할 수 있었다.

인천 재성형 해성점토의 비배수 전단강도 특성에 대한 연구 (A Study on Characteristics of Undrained Shear Strength of Remolded Marine Clays at Incheon)

  • 유남재;이한솔;전상현
    • 산업기술연구
    • /
    • 제29권B호
    • /
    • pp.81-88
    • /
    • 2009
  • The main purpose of this work is to determine characteristics of undrained shear strength of remolded marine clay at Incheon. Laboratory vane tests with remolded marine clay sampled from west coast at Incheon were performed to investigate the undrained shear strength of them being dumped for reclamation after dredging from the sea bottom. Test results were compared with the predicted values of undrained shear strength proposed by many researchers. It was found that measured results about undrained shear strength with water content was in good agreements with values proposed by Mikasa and Modified Mikasa's empirical formula.

  • PDF

인천 및 부산 재성형 해성점토의 비배수 전단강도 특성에 대한 연구 (A Study on Characteristics of Undrained Shear Strength of Remolded Marine Clays at Incheon and Busan)

  • 유남재;이한솔;전상현
    • 산업기술연구
    • /
    • 제30권A호
    • /
    • pp.103-109
    • /
    • 2010
  • This research is to determine characteristics of undrained shear strength of remolded marine clay at Incheon and Busan, representing typical marine clays in Korea. Laboratory vane tests with remolded marine clays sampled from coasts at Incheon and Busan were performed to investigate the undrained shear strength of them. Test results were compared with the predicted values of undrained shear strength proposed by many researchers. It was found that measured results about undrained shear strength with water content was in good agreements with values proposed by Terzaghi empirical formula.

  • PDF

부산점토의 Fall Cone Test에 의한 지수 및 강도특성 (Index Properties and Undrained Shear Strength of the Pusan Clays by Fall Cone Test)

  • 정승원;정성교;;곽정민;김무겸
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2000년도 가을 학술발표회 논문집
    • /
    • pp.391-398
    • /
    • 2000
  • The index properties of cohesive soils play an important role to examine entire tendency of soil properties. Especially, the Atterberg limits have a good correlation with compression and shear strength of cohesive soils. However, these values strongly depend on their testing methods. In this study, for Pusan clays the Atterberg limits were peformed under different conditions; for example, four kinds of specimen preparation, two kinds of testing equipment, and four kinds of estimating method. And a laboratory vane test was peformed to compare the undrained shear strength with that of the fall cone test. As experimental results, the value of liquid limit performed for oven-dried sample, followed in ASTM D4318, underestimated by about 10% compared to those of another three methods, irrespective to the used equipments. But the value of plastic limit was not influenced by sample preparation methods and equipments. The liquid limits by one-point methods(Leroueil et al., 1996; Nagaraj et al., 1981) were agreed well with those of different methods. Finally, the undrained shear strength by laboratory vane test was relatively larger than that of fall cone test, and the relationship between both showed a bad trend.

  • PDF

북동태평양 KODOS지역 심해 퇴적물의 베인 전단강도 측정 방법에 따른 결과 비교 (Comparison of Vane-shear Strength Measured by Different Methods in Deep-sea Sediments from KODOS area, NE Equatorial Pacific)

  • 지상범;정회수;김현섭;문재운
    • 한국해양학회지:바다
    • /
    • 제4권4호
    • /
    • pp.390-399
    • /
    • 1999
  • 북동태평양 심해저 생물자원 퇴적물에서 서로 다른 두 종류의 측정기 그리고 선상 및 육상 실험실에서 획득한 베인전단강도(vane shear strength) 자료의 비교 연구를 위하여 다중주상시료 채취기(multiple corer)로 규질 및 탄산질 퇴적물 시료를 채취하였다. 전단강도는 $2.0{\times}2.0$ cm의 베인($90^{\circ}$ four blade vane)이 장착된 수동베인측정기(hand-held vane apparatus, 수동베인) 그리고 회전식 점도계 (rotational viscometer)에 $1.0{\times}0.88$ cm의 베인을 장착하여 구성한 전동베인 측정기(motorized shear vane system, 전동베인)로 측정되었다. 수동베인과 전동베인으로 측정된 전단강도 값들은 코어 깊이에 따라 증가하는 동일한 변화 양상을 보이며, 절대 값도 유의한 차이를 보이지 않는다. 그리고 선상에서 측정된 전단강도 값에 비하여 3개훨월후 실험실에서 동일 장비에 의해 측정한 값들 또한 큰 차를 나타내지 않는다. 한편, 실험실에서 전동베인으로 동일한 코어를 2~4회 반복 측정한 결과 동일한 깊이에서도 측정 지점(hole)에 따라 차이가 나타난다. 또한 한 정점 내에서 서로 다른 코어 시료중 전단강도 값은 상당한 차이를 보이는 경우도 있다. 이는 심해저 주상 퇴적물의 물리적 특성이 생물 교란 작용 등의 영향으로 국부적으로 다르기 때문에 나타난 결과로 판단된다. 즉 심해저 퇴적물의 전단강도는 선상에서 또는 3개월이 지난 후 실험실에서, 그리고 두 종류의 기기를 사용하여도 깊이에 따른 유의한 차이를 보이지 않고, 오히려 한 코어시료 내의 국부적 물성차이 또는 한 정점 내 지점별 물성차이에 의한 변화 폭이 더 크게 나타낸다.

  • PDF

사면파괴 하부 점토지반 비배수강도의 평가 (Estimation of Undrained Shear Strength of Clay under Failed Slope)

  • 이승현;한진태
    • 한국산학기술학회논문지
    • /
    • 제13권11호
    • /
    • pp.5572-5577
    • /
    • 2012
  • 사면파괴가 발생한 사면의 하부 연약지반에 대한 현장원치시험결과와 실내시험결과 그리고 강도 추정식에 의한 결과를 상호 비교분석해 보았다. 사면 하부연약지반에 대한 콘관입시험결과와 현장베인시험결과의 비교를 통해 결정된 연약지반의 콘계수값은 12였다. 콘관입시험자료로부터 콘계수 추정식을 적용하여 구한 연약지반의 비배수강도는 현장베인시험에 의한 그것보다 보수적인 값을 주었다. 압밀시험결과를 이용한 추정식을 통해 연약지반의 비배수강도를 추정하고 현장베인시험에 의한 비배수강도와 비교해 보았다. 세 가지 방법을 통한 추정결과에 따르면 Jamiolkowsky 방법에 의한 결과가 시험을 통해 구한 결과에 가장 근접하였으며 현장베인시험에 의한 비배수강도에 비해 0.88~1.23 범위의 값을 보였다.

Shear behavior of foam-conditioned gravelly sands: Insights from pressurized vane shear tests

  • Shuying Wang;Jiazheng Zhong;Qiujing Pan;Tongming Qu;Fanlin Ling
    • Geomechanics and Engineering
    • /
    • 제34권6호
    • /
    • pp.637-648
    • /
    • 2023
  • When an earth pressure balance (EPB) shield machine bores a tunnel in gravelly sand stratum, the excavated natural soil is normally transformed using foam and water to reduce cutter wear and the risk of direct muck squeezing out of the screw conveyor (i.e., muck spewing). Understanding the undrained shear behavior of conditioned soils under pressure is a potential perspective for optimizing the earth pressure balance shield tunnelling strategies. Owing to the unconventional properties of conditioned soil, a pressurized vane shear apparatus was utilized to investigate the undrained shear behavior of foam-conditioned gravelly sands under normal pressure. The results showed that the shear stress-displacement curves exhibited strain-softening behavior only when the initial void ratio (e0) of the foam-conditioned sand was less than the maximum void ratio (emax) of the unconditioned sand. The peak and residual strength increased with an increase in normal pressure and a decrease in foam injection ratio. A unique relation between the void ratio and the shear strength in the residual stage was observed in the e-ln(τ) space. When e0 was greater than emax, the fluid-like specimens had quite low strengths. Besides, the stick-slip behavior, characterized by the variation coefficient of measured shear stress in the residual stage, was more evident under lower pressure but it appeared to be independent of the foam injection. A comparison between the results of pressurized vane shear tests and those of slump tests indicated that the slump test has its limitations to characterize the chamber muck fluidity and build the optimal conditioning parameters.