• 제목/요약/키워드: urea formaldehyde resin

검색결과 123건 처리시간 0.028초

요소수지합판(尿素樹脂合板)의 증량(增量)에 관(關)한 연구(硏究) (A study on the extension of urea-formaldehyde resin plywood)

  • 김용재;김은섭;이필우
    • Journal of the Korean Wood Science and Technology
    • /
    • 제4권1호
    • /
    • pp.28-32
    • /
    • 1976
  • This study was carried out to know the adaptability of barley flour, potato flour and white ash as extender and filler of urea-formaldehyde resin for plywood as a substitute material of wheat flour. The extenders and filler used at this study were extended by several groups of percentages. Shear strength, moisture contents, and specific gravities were compared among tested groups. The results obtained are summarized as follows. 1) Wet and dry shear strength of plywoods extended by 10% barley flour, 30% potato flour, and wheat flours were shown better results than non extended plywoods. 2) There was no significant difference between plywoods extended until 50% barley flours and non extended plywoods. 3) Shear strength of plywoods extended by 50% potato and 100% barley flours were shown worse result than non extended. 4) Dry and wet shear strength of plywoods extended by white ash were shown worst result. 5) The plywoods extended by potato flours were shown not only better shear strength, but also considered more profitable cost for extending.

  • PDF

황산알미늄용액의 단판(單板) 전처리(前處理)에 따른 합판용(合板用) 요소수지(尿素樹脂) 도포량의 감소에 관한 연구(硏究) (The Study of the Veneer Pretreatment with Aluminum Sulfate Solution on the Reduction of Urea Formaldehyde Resin Spreading Content for the Manufacture of Plywood)

  • 이화형
    • Journal of the Korean Wood Science and Technology
    • /
    • 제16권1호
    • /
    • pp.3-8
    • /
    • 1988
  • This study was carried out to examine the effect of pretreatment of veneer with aluminum sulfate solution for the manufacture of the kapur plywood on the reduction of urea resin spread. The results were as follows: 1. Specific gravities of plywoods made of the kapur veneers ranged from 0.83 to 0.84 and their moisture contents based on air dry weight showed from 10.6% to 11.4%. These met the Korean Industrial Standards. 2. In the case of dry shear strength for the 3rd class plywood, 40% reduction- spread met K S as well as normal urea resin spread. pH of the aluminum sulfate solution gave better result at pH 4.5 and pH 6 than at pH 3. For the manufacture of the 2nd class plywood, hot and cold water-wet shear strength show the best results at the following conditions; such as 20% reduction spread, pH 4.5 of aluminum sulfate solution and all veneer treatment.

  • PDF

Research on Flame Retardant Plywood with Different Flame Retardants

  • LIU, Yang;XU, Jun-xian;WEN, Ming-yu;PARK, Hee-Jun;ZHU, Jia-zhi;LIU, Yu-nan
    • Journal of the Korean Wood Science and Technology
    • /
    • 제49권6호
    • /
    • pp.667-678
    • /
    • 2021
  • The flame retardancy of plywood should be improved as much as possible while minimizing the impact on the bonding strength of plywood. Six commercial flame retardants and three laboratory synthesized phosphorous nitrogen flame retardants were selected. E0, E1 and E2 grade commercial formaldehyde resins (UF) were applied in this study to evaluate the effect of different flame retardants on the curing time of resin, bonding strength, flame retardant performance, and formaldehyde emission of plywood. The results show that the effect of the addition of different flame retardants on the bonding strength of plywood gradually decreased with the increase of the formaldehyde molar ratio of the resin. The effect of flame retardants on the curing time of UF gradually decreased as the mole ratio of formaldehyde increasing, while the amount of formaldehyde emission varied according to the content of formaldehyde in the flame retardant. Compared with plywood without flame retardant, flame retardant of plywood added with phosphorous nitrogen flame retardant was improved.

Effects of Hardener and Extender Contents on Curing Behavior of Urea-Melamine-Formaldehyde Resin

  • Eom, Young-Geun;XU, Guang-Zhu;Lee, Young-Kyu;Kim, Hyun-Joong
    • Journal of the Korean Wood Science and Technology
    • /
    • 제36권5호
    • /
    • pp.42-48
    • /
    • 2008
  • This study was conducted to discuss the effects of hardener and extender contents on peak temperature, reaction enthalpy (${\Delta}H$), gelation time, viscosity change, and pH value in three types of UMF (urea-melamine- formaldehyde) resin with the help of perpHecT LogR meter, differential scanning calorimetry (DSC), and advanced rheometric expansion system (ARES), The results indicated that the pH value of Control A steeply decreased to 5,2 in the early stage but relatively remained constant thereafter as in Synthesis 1 and Synthesis 2, The peak temperature and time decreased as well, whereas ${\Delta}H$ and viscosity increased with the increase of hardener content. On the other hand, ${\Delta}H$ was not changed up to the extender content of 5% and then decreased with its further addition, And the pH value and peak temperature showed no change with the increase of extender content at the hardener content of 5% in three types of UMF resin, The effect of hardener content in this experiment, however, appeared more conspicuous in Control A than in the other two types of Synthesis 1 and Synthesis 2, These results might be caused by higher molecular weight with longer chains of methylene ($-CH_2-$) and methylene ($-CH_2-O-CH_2-$) ether bridges or much more branched chains in Control A.

악기 향판재의 최적공진비에 미치는 접착제의 영향 (Effect of Adhesives on the Best Acoustic Radiation Ratio of Sound board for Musical Instrument)

  • 이화형
    • 한국가구학회지
    • /
    • 제11권1호
    • /
    • pp.25-29
    • /
    • 2000
  • This study was carried out to analyze the ultrasonic properties of sound board which was glued with various adhesives and to evaluate which adhesive is the best for the acoustic radiation of the musical instrument. The results are as follows: 1. Animal glue is the best adhesive for the sound board with respect to the acoustic radiation ratio of the musical instruments. Epoxy resin and polyvinyl acetate resin are the next group, urea formaldehyde resin and Hot melt are the third group, polychloroprene(CR) resin is the lowest. 2. Epoxy resin, animal glue and Titebond(PVA) give the highest shear strength and the highest wood failure relatively Hot melt and polychloroprene(CR) resin do not meet the standard because of low wood failure.

  • PDF

Soybean-based Green Adhesive for Environment-friendly Furniture Material

  • Jeon, Ji-Soo;Lee, Jeong-Hun;Kim, Su-Min
    • 한국가구학회지
    • /
    • 제22권3호
    • /
    • pp.174-182
    • /
    • 2011
  • Over the last decade, Sick Building Syndrome has become a significant social issue in Korea and many methods have been considered to maintain comfortable indoor air quality. To reduce toxic substances emitted from wood composite products, the source control is an efficient method through the reduction of formaldehyde content by using natural material-based adhesives for composite wood products production. Among alternative materials, soybean protein is considered an appropriate natural material to replace formaldehyde-based resin and many efforts have been made to produce new products, such as soap, shampoo, ink, resin, adhesive and textile through changing the chemical or physical properties of soybean. To process soybeans into these useful products, the beans are dehulled and the oil is removed by crushing at very high pressure or by solvent extraction. For use soybean as an adhesive, it is processed at temperatures below $70^{\circ}C$ to preserve the alkaline solubility of the proteins. In addition, soybean-based adhesive is undergone treatment process to improve mechanical properties using urea, urease inhibitor N-(n-butyl) thiophosphoric triamide and sodium dodecyl sulfate. The modified soybean-based adhesive exhibited sufficient mechanical properties to use as an adhesive for composite wood products. This paper is a review article to discuss the possibilities of soybean-based adhesive for environment-friendly furniture materials.

  • PDF

옥촉서간(玉蜀黍幹), 송수피(松樹皮), 소맥(小麥), 리기다송엽(松葉), 잣나무엽(葉) 및 목분말(木粉末)을 이용(利用)한 합판(合板)의 접착증량(接着增量)에 관(關)한 연구(硏究) (The Utilization of Corn Stalk, Pine Bark, Pine Leaves, Wheat and Wood Flour as an Extender for Plywood Bonding)

  • 이필우;권진헌
    • 한국산림과학회지
    • /
    • 제51권1호
    • /
    • pp.41-50
    • /
    • 1981
  • 본연구(本硏究)의 목적(目的)은 현재(現在) 증량제(增量剤)로 사용(使用)하고 있는 도인소맥분(導人小麥粉)을 국내(国內)에서 값싸게 생산(生産)할 수 있는 다른 증량제(增量剤)로 대체(代替)키 위한 가능성(可能性)을 규명하는데 있다. 증량재료(増量材料)는 옥촉서간(玉蜀黍幹), 송수피(松樹皮), 소맥(小麥), 리기다송엽(松葉), 잣나무엽(葉) 및 목분말(木粉末)을 택(択)해서 $103{\pm}2^{\circ}C$에서 24시간(時間)동안 전건(全乾)시킨 다음 60~100mesh로 분쇄(粉碎)하였다. 증량방법(増量方法)에 있어서 요소수지(尿素樹脂)는 10, 20, 30, 50%로 증량(増量)하였으며 수용성석탄산수지(水溶性石炭酸樹脂)는 5, 10, 15, 20%로 증량(増量)하였다. 본연구(本硏究)에서 얻은 결론(結論)은 다음과 같이 요약(要約)할 수 있다. 1. 요소수지(尿素樹脂)에 있어서 상태접착력(常態接着力)은 소맥분(小麥粉)이 가장 양호(良好)하였다. 2. 요소수지(尿素樹脂)에 있어서 내수접착력(耐水接着力)은 10%와 20%증량(増量)의 경우 소맥분(小麥粉)보다 목분(木粉)이 더 양호(良好)하였으나 이들 사이의 유의적(有意的)인 차이(差異)는 없었다. 3. 석탄산수지(石炭酸樹脂)의 상태접착력(常態接着力)에 있어서 5%증량((増量)의 경우 잣나무엽분(葉粉)이 가장 양호(良好)하였으나 10, 15, 20% 증량((増量)의 경우는 소맥분(小麥粉)이 가장 양호(良好)하였다. 4. 석탄산수지(石炭酸樹脂)의 내수접착력(耐水接着力)에 있어서는 소맥분(小麥粉)이 가장 양호(良好)하였다. 5. 석탄산수지(石炭酸樹脂)의 상태(常態) 및 내수접착력(耐水接着力)에 있어서 15와 20%증량((増量)의 경우 옥촉서간(玉蜀黍幹)이 소맥분(小麥粉) 다음으로 양호(良好)한 결과(結果)를 나타내었다.

  • PDF

섬유판(纖維板)의 증강(增强)사이즈제(齊)가 재질(材質)에 미치는 영향(影響) (Effect of Strength Increasing Sizes on the Quality of Fiberboard)

  • 신동소;이화형
    • 한국산림과학회지
    • /
    • 제30권1호
    • /
    • pp.19-29
    • /
    • 1976
  • 습식(濕式) 경질섬유판(硬質纖維板) 제조(製造)를 위(爲)한 보강용(補强用) 사이징제(劑)로서 실험실(實驗室) 제조(製造) 석탄산수지(石炭酸樹脂), 요소수지(尿素樹脂)(음(陰)이온 형(型), 양(陽)이온 형(型)), 요소(尿素) 메라민 공축합수지(共縮合樹脂)와 일본(日本) M사(社)의 변성(變性)메라민수지(樹脂)(P-6100)와 변성(變性) 양(陽)이온형(型) 요소수지(尿素樹脂)(P-1500)등을 사용(使用)하여 섬유판(纖維板) 재질(材質)에 미치는 영향(影響)을 검토(檢討)하였다. 공시재(供試材)는 라왕(20%)+소나무(80%)로 사용(使用)하였고 침착제(沈着劑)는 황산알미늄을 사용(使用)하였으며 열압조건(熱壓條件)은 전기가열(電氣加熱) 푸레스로 $180^{\circ}C$, $50-6-50kg/cm^2$, 시간(時間)은 1-2-7분(分)으로 S-1-S 경질섬유판(硬質纖維板)을 제조(製造)하여 일주일 기건(氣乾)시킨 후(後) 그 성질(性質)을 조사(調査)한 결과(結果)를 요약(要約)하면 다음과 같다. 1. 섬유판(纖維板)의 비중(比重)은 각(各) 보강제(補强劑)의 처리량(處理量)에 따른 비중(比重)의 차(差)는 없으나 보강제(補强劑) 간(間)에는 고도(高度)의 유의차(有意差)가 있어 변성(變性)메라민수지(樹脂)가 제일 높고 양(陽)이온형(型), 음(陰)이온형(型) 및 요소(尿素) 메라민 공축합수지(共縮合樹脂)가 중간(中間)이며 석탄산수지(石炭酸樹脂)가 제일 낮았다. 2. 섬유판(纖維板)의 함수율(含水率)은 보강제(補强劑) 간(間)의 차(差)와 보강제(補强劑) 처리량(處理量)에 따른 함수율(含水率)의 차(差)가 전부(全部) 유의성(有意性)이 있었으며 전체적(全體的)으로 처리량(處理量)이 증가(增加)할 수록 함수율(含水率)은 떨어지나 2%와 3% 처리(處理) 간(間)의 함수율(含水率) 차(差)는 없었다. 3. 섬유판(纖維板)의 흡수율(吸水率)은 보강제(補强劑) 간(間) 및 파라핀 왁스유탁액(乳濁液) 처리량(處理量) 간(間) 모두 다 유의차(有意差)를 보이고 있다. 파라핀 왁스유탁액(乳濁液) 처리량(處理量)을 늘일수록 흡수율(吸水率)은 떨어져 내수성(耐水性)이 증가(增加)함을 보이고 있으며 P-6100 및 P-1500은 무처리(無處理)에도 표준규격(標準規格)을 만족시켜 주며 음(陰)이온형(型) 요소수지(尿素樹脂), 양(陽)이온형(型) 요소수지(尿素樹脂), 요소(尿素) 메라민 공축합수지(共縮合樹脂)의 산(酸)콜로이드는 내수제(耐水劑)를 1% 요구하고 석탄산수지(石炭酸樹脂)는 2%에 합격(合格)되고 있었다. 4. 섬유판(纖維板)의 곡강도(曲强度)는 보강제(補强劑) 간(間) 및 보강제(補强劑) 처리량(處理量) 간(間)에 모두 유의차(有意差)가 있으며 처리량(處理量)이 증가(增加)할 수록 곡강도(曲强度)는 증가(增加)하였다. P-6100이 가장 곡강도(曲强度)가 높고 P-1500, 양(陽)이온형(型) 및 음(陰)이온형(型) 요소수지(尿素樹脂), 요소(尿素) 메라민 공축합수지(共縮合樹脂)의 산(酸)콜로이드등(等)이 중간(中間)이며, 석탄산수지(石炭酸樹脂)가 곡강도(曲强度)는 제일 낮았다. 5. 섬유판(纖維板)의 품질(品質)과 경제적(經濟的)인 면(面)을 고려한다면 석탄산수지(石炭酸樹指)의 대체(代替)로서 산(酸)콜로이드 방법(方法)에 의한 요소(尿素) 메라민 공축합수지(共縮合樹脂)와 양(陽)이온형(型) 요소수지(尿素樹脂)를 사용(使用)하는 것이 가장 바람직하며 이들 변성수지(變性樹脂)에 대(對)한 개선(改善) 연구(硏究)가 계속 필요(必要)하다 하겠다.

  • PDF

Physical and Mechanical Properties of Three-layer Particleboards Bonded With UF and UMF Adhesives

  • Iswanto, Apri Heri;Simarmata, Janrahman;Fatriasari, Widya;Azhar, Irawati;Sucipto, Tito;Hartono, Rudi
    • Journal of the Korean Wood Science and Technology
    • /
    • 제45권6호
    • /
    • pp.787-796
    • /
    • 2017
  • A low dimensional stability and poor bending strength properties were main problems in particleboard manufacturing. The objective of this research was to evaluate the effect of mixed wood species and urea-formaldehyde (UF) or urea-melamine-formaldehyde (UMF) resins on the physical and mechanical properties of three-layer particleboards. The ratio of face/core/back layer was 1 : 2 : 1. The resin content of 12% for both UF resins and UMF resins (UF/MF = 70/30% w/w) was used. The results of this study showed that the utilization of S.mahagony shaving using both UF and UMF resins caused a decrease in the thickness swelling and water absorption of the boards. Thickness swellings of particleboard made of Sengon/Sengon/Sengon (SSS), Mahogany/Mahogany/Mahogany (MMM), Sengon/Mahogany/Sengon (SMS), and Mahogany/Sengon/Mahogany (MSM) were in the range of 23%, 12~16%, 14~16%, and 13~21%, respectively. The board bonded with UMF resin demonstrated better dimensional stability than that bonded with UF resin alone. Modulus of elasticity (MOE) and modulus of rupture (MOR) of particleboards made of S. mahagony shaving in the surface layer in both MMM and MSM boards were better than those of the SSS and SMS. MOE of MMM and MSM board was in the ranges of 24,000 to $26,000kg.cm^{-2}$ and 18,000 to $21,000kg.cm^{-2}$ respectively. Meanwhile, the MOR of board was in the ranges of 200 to $240kg.cm^{-2}$ and 190 to $228kg.cm^{-2}$, respectively.

Phenol-Formaldehyde (PF) Resin Bonded Medium Density Fiberboard

  • Park, Byung-Dae;Riedl, Bernard;Park, Sang-Jin
    • Journal of the Korean Wood Science and Technology
    • /
    • 제27권1호
    • /
    • pp.64-71
    • /
    • 1999
  • 본 연구는 통상적으로 충밀도 섬유판 제조에 사용되고있는 요소수지를 페놀수지로 대체함으로써 그 장단점을 찾아 보기 위해 실행되었다. 페놀수지을 이용해 제조한 중밀도 섬유판의 성능은 표준 요건을 충족시켰으며 높은 내구성을 보였다. 아울러 24 시간 냉수 침적후 두께팽창은 2 퍼센트 이하로 낮게 나타났다. 요소수지를 페놀수지로 대체했을 경우 단점들은 비교적 높은 수지함량 (8% 섬유전건종량기준)과 긴 열압시간 (7 분)으로 판명되었다. 이러한 결과들은 페놀수지을 사용한 중밀도 섬유판제조시 열압공정의 최적화가 되어야함을 시사하였다.

  • PDF