티타늄과 금합금의 레이저 용접부의 인장강도 (TENSILE STRENGTH OF LASER WELDED-TITANIUM AND GOLD ALLOYS)

  • 송윤관;송광엽;하일수
    • 대한치과보철학회지
    • /
    • 제38권2호
    • /
    • pp.200-213
    • /
    • 2000
  • Lasers have given dentistry a new rapid, economic, and accurate technique for metal joining. Although laser welding has been recommended as an accurate technique, there are some limitations with this technique. For example, the two joining surfaces must have a tight-fitting contact, which may be difficult to achieve in some situations. The tensile samples used for this study were made from a custom-made pure titanium and type III gold alloy plates. 27 of 33 specimens were sectioned perpendicular to their long axis with a carborundum disk and water coolant. Six specimens remained and served as the control group. A group of 6 specimens was posed as butt joints in custom parallel positioning device with a feeler gauge at each of three gaps : 0.00, 0.25. and 0.50mm. All specimens were then machined to produce a uniform cross-sectional dimension, none of the specimens was subjected to any subsequent form of heat treatment. Scanning electron microscopy was performed on representative tested specimens at fractured surfaces in both the parent metal and the weld. Vickers hardness was measured at the center of the welds with a micropenetrometer using a force of 300gm for 15 seconds. Measurement was made at approximately $200{\mu}m\;and\;500{\mu}m$ deep from each surface. One-way analysis of variance (ANOVA) and Scheffe's test was calculated to detect differences between groups. The purpose of this study is to compare the strength and properties of the joint achieved at various butt Joint gaps by the laser welding of type III gold alloy and pure titanium tensile specimens in an argon atmosphere. The results of this study were as follows : 1. When indexing and welding pure titanium, there was no decrease in ultimate tensile strength as compared with the unsectioned alloys for indexing gaps of 0.00 to 0.50mm, although with increasing gap size may come increased distortion (p>0.05). 2. When indexing and welding type III gold alloy, there were significant differences in ultimate tensile strength among groups with weld gaps of 0.00mm, 0.25 and 0.50mm, and the control group. Group with butt contact without weld gap demonstrated a significant higher ultimate tensile strength than groups with weld gaps of 0.25 and 0.50mm (p<0.05). 3. When indexing and welding the different metal combination of type III gold alloy and pure titanium, there were significant differences in ultimate tensile strength between groups with weld gaps of 0.00, 0.25, and 0.50mm. However, the mechanical properties of the welded joint would become too brittle to be acceptable clinically (p<0.05). 4. The presence of large pores in the laser welded joint appears to be the most important factor in controlling the tensile strength of the weld in both pure titanium and type III gold alloy.

  • PDF

철근구속을 받는 고강도 콘크리트의 자기수축저감에 관한 실험 연구 (An experimental study on the reduction of autogenous shrinkage of high strength concrete with bar restricted specimen)

  • 최진영;전철송;임병호;김화중
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.431-436
    • /
    • 2002
  • In this paper, to seek a solution of reducing autogenous shrinkage three types of bar restricted concrete specimens which have similar compressive strength were tested. The three type of concrete were plain concrete-P25 type, $10^{\circ}C$ fly-ash replaced concrete-F10 type, and $1^{\circ}C$ expansion admixture replaced concrete-SP1 type, and with the test result an experimental study was conducted to gain the tensile stress of concrete. From the result of P25, SP1, F10 tests, it was found that by the age of 14 the ratios of tensile stress to tensile strength of three specimens are $75^{\circ}C$, $47^{\circ}C$, $52^{\circ}C$ respectively. so we came to a conclusion that the SP1-type concrete has better capacity to reduce autogenous shrinkage than F10-type concrete at similar compressive strength condition.

  • PDF

쉬트형 FRP와 콘크리트의 부착특성에 관한 실험적 연구 (Experimental Study on the Bond Charateristics for FRP Sheet-Concrete Interface)

  • 고훈범;고만영
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 춘계 학술발표회 논문집(II)
    • /
    • pp.361-364
    • /
    • 2006
  • In this study, six specimens were prepared for two type FRP sheets(carbon and polyacetal) to evaluate the behavior of FRP-concrete interfacial bond. A direct tensile test was conducted and the test results show that fiber type influences both bond strength and the shape of strain distribution. The failure mode for carbon type specimens seems to bond failure between concrete and FRP, but for polyacetal type indicates interface failure between FRP and expoxy. The local bond stress-slip relations were obtained from test results, and it was shown good shape for the polyacetal type. But for the carbon type it was scattered.

  • PDF

망사 및 스틱 형태의 유리섬유 보강재를 삽입한 의치상용 레진의 굴곡강도 및 굴곡계수 비교 평가 (Comparative evaluation of flexural strength and modulus of denture base resin with mesh and stick type glass fiber reinforcement)

  • 김동연;김재홍
    • 대한치과기공학회지
    • /
    • 제42권2호
    • /
    • pp.91-98
    • /
    • 2020
  • Purpose: This study is to compare the flexural strength and modulus by inserting a mesh and stick type fiberglass reinforcement into resin specimens. Methods: Wax specimens (length 64 mm, width 39 mm, thickness 5 mm) are prepared according to ISO 20795-1:2013. Mesh type and stick type glass fiber reinforcements were prepared. The prepared wax specimens were used plaster and flask for investment. The flask was separated and the wax was removed. The heat curing resin was injected into the flask, and then a mesh type and stick type fiberglass reinforcement were inserted. The prepared resin specimen was cut into three equal parts (length 64 mm, width 10 mm, thickness 3.3 mm). The mesh type glass fiber reinforcement (MT group) and the stick type glass fiber reinforcement (ST group) were classified into two groups. The prepared specimen was measured using a universal testing machine (UTM). The data were analyzed by Mann-Whitney U test, and the significance level was set to 0.05. Results: In the flexural strength, the ST group was higher than the MT group, and there was a significant difference between the two groups (p<0.05). In the flexural modulus, the ST group was higher than the MT group, and there was a significant difference between the two groups (p<0.05). Conclusion: The stick-type glass fiber inreased the flexural strength than the mesh-type glass fiber reinforcement.

점용접시편의 과부하해석 및 유효 J-적분에 의한 피로수명예측 (Overload Analysis and Fatigue Life Prediction Using an Effective J-Integral of Spot Welded Specimens)

  • 이형일;최진용
    • 대한기계학회논문집A
    • /
    • 제24권3호
    • /
    • pp.567-580
    • /
    • 2000
  • This paper proposes an integrated approach, which is independent of specimen geometry and loading type, for predicting the fatigue life of spot welded specimens. We first establish finite element models reflecting the actual specimen behaviors observed on the experimental load-deflection curves of 4 types of single spot welded specimens. Using finite element models elaborately established, we then evaluate fracture parameter J-integral to describe the effects of specimen geometry and loading type on the fatigue life in a comprehensive manner. It is confirmed, however, that J-integral concept alone is insufficient to clearly explain the generalized relationship between load and fatigue life of spot welded specimens. On this ground, we introduce another effective parameter $J_e$ composed of $J_I$, $J_{II}$, $J_{III}$, which has been demonstrated here to more sharply define the relationship between load and fatigue life of 4 types of spot welded specimens. The crack surface displacement method is adopted for decomposition of J, and the mechanism of the mixed mode fracture is also discussed in detail as a motivation of using $J_e$.

고강도 확대머리 이형철근의 정착길이 효과에 관한 실험적 연구 (Development Length Effects of High Strength Headed Bar)

  • 문정호;오영훈
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제19권5호
    • /
    • pp.75-82
    • /
    • 2015
  • 본 연구는 고강도 철근을 확대머리 이형철근으로 사용하는 경우 정착길이 효과에 관한 실험 연구이다. 현행 기준에서는 확대머리 이형철근의 정착길이를 산정하는 식에서 철근의 설계기준강도를 400 MPa로 한정하고 있다. 고강도 철근에 대한 연구결과가 충분하지 않기 때문에 이러한 규정이 명시된 것이다. 따라서 본 연구에서는 설계기준 항목강도 600 MPa의 철근으로 확대머리 이형철근을 제작하여, 변수별 실험연구를 수행하였다. 실험은 철근의 정착길이, 철근의 개수, 그리고 확대머리의 형상 등의 변수로 계획하였다. 실험체는 정착길이가 긴 L형과 정착길이가 짧은 S형으로 분류하고, 확대머리의 형상은 원판형(A형)과 원뿔형(B형)으로 구분하였다. L형 실험체는 원판형 확대머리를 대상으로 철근 개수가 1~3으로 변하는 3개의 실험체와 S형 실험체는 원판과 원뿔형 확대머리 형상에 대하여 정착길이를 L형의 50%, 45%, 40%, 35%로 변화한 실험체를 계획하였다. L형(LA형) 3개, SA형 4개, SB형 4개 등 총 11개의 실험체를 인발실험을 하였다. 실험결과는 콘크리트구조기준(부록 II)의 정착길이 산정 규정에 따라 평가하였으며, 그 결과 항복강도 600 MPa의 철근을 사용한 확대머리 이형철근은 현행기준의 설계식을 적용하여 설계할 수 있음을 보였다.

복합재료 스킨-보강재 접합 시편의 파손 특성에 대한 시험 연구 (Experimental Debonding Failure Behaviors of Composite Skin-Stiffener Bonded Specimens)

  • 김광수;안재모;장영순;이영무
    • Composites Research
    • /
    • 제20권6호
    • /
    • pp.8-14
    • /
    • 2007
  • 스킨-보강재 시편 시험을 통해 스킨과 보강재의 분리 파손 특성을 살펴보고 접합방법, 보강재 단면 및 이차 접합 파라미터의 영향을 조사하였다. 본 시험 결과와 이전 시험[1]의 결과를 종합해 볼 때, 보강패널의 스킨-보강재 분리 파손 강도를 판단하는 기준으로 스킨-보강재 시편의 파손 변위를 이용하는 것이 타당하며 동일한 접합 방법을 사용할 경우, closed형 보다 open형 보강재를 사용하는 것이 복합재 보강 패널에서 스킨과 보강재의 분리파손을 방지하는데 유리함을 알 수 있었다. 접합방법으로는 이차접합 및 접착제를 사용한 동시성형이 좋은 파손 강도를 보였으며 접착제 없는 동시성형이 가장 나쁜 파손 강도를 나타내었다. 파손 모드는 이차접합 시편은 주로 계면 파손이 발생하였으며 동시성형 시편은 복합재료의 층간분리 파손이 발생하였다. 이차 접합 시편에서는 접착제 두께가 작을수록 높은 파손 강도를 보였다. Fillet은 시편의 강도에 영향을 미치지 않았다. 표면 조도의 영향은 open형 및 closed형 시편이 다르게 나타났다.

AE파형분류에 의한 용사코팅재의 파손해석 (Fracture Analysis of Plasma Spray Coating by Classification of AE Signals)

  • 김귀식;박경석;홍용의
    • 동력기계공학회지
    • /
    • 제6권3호
    • /
    • pp.24-30
    • /
    • 2002
  • The deformation and fracture behaviors of both Al2O3 and Ni 4.5wt.%Al plasma thermal spray coating were investigated by an acoustic emission method. Plasma thermal spray coating is formed by a process in which melted particles flying with high speed towards substrate, then crash and spread on the substrate surface cooled and solidified in a very short time, stacking of the particles makes coating. A tensile test is conducted on notch specimens in a stress range below the elastic limit of substrate. A bendind test is done on smooth specimens. The waveforms of AE generated from the both test coating specimens can be classified by FFT analysis into two types which low frequency(type I) and high frequency(type II). The type I waveform is considered to corresponds exfoliation of coating layers and type II waveform corresponds the plastic deformation of notch tip. The fracture of the coating layers can estimate by AE event and amplitude, because AE features increase when the deformation generates.

  • PDF

구조용 집성판(CLT)-콘크리트 경계면의 전단성능 평가 (Shear Performance Evaluation at the Interface Between CLT and Concrete)

  • 박금성
    • 한국공간구조학회논문집
    • /
    • 제21권3호
    • /
    • pp.35-42
    • /
    • 2021
  • An experimental study was carried out to evaluate the shear performance at the interface composed of structural laminates and concrete. The main variables are the number of CLT layers and the shape of the shear connector. The number of CLT layers consisted of 3 and 5 layers. A total of 6 test specimens for shear performance evaluation were prepared in the form of a shear connector, a direct screw type and a vertically embedded type. As a result of the experiment, similar behavior was shown in all specimens, regardless of the number of layers, including direct screw type (SC series) and vertically embedded type (VE series). The behavior at the joint surface was damaged due to the occurrence of initial shear cracks, expansion of shear groove cracks, and splaying at the interface after the maximum load.After the maximum load, the shear strength decreased gradually due to the effect of the shear connector. It can be seen that the shear strength of all specimens is determined by shear and compression stress failure of concrete at the interface of the notch joint.

철근을 이용한 충전 강관기둥 접합부의 인장거동 (Tensile Behavior of Concrete-Filled Column Connections Using Re-bars)

  • 이영렬;유영찬;신경재;오영석;이승준;문태섭
    • 한국강구조학회 논문집
    • /
    • 제8권3호통권28호
    • /
    • pp.89-96
    • /
    • 1996
  • The objective of this study is to investigate the structural behavior of Concrete-Filled Steel Tubular Column connections using reinforced bar. The parameter of specimens is the area of each reinforced bar (SD40 : D13, D16, D19, D22, D25). The simple tensile experiment is conducted to 5 kinds of specimens. Estimating the load, displacement, and strain from each kind, we compared them to basic elementary type (Flange Type, Basic Type, DPA Type, DPB Type). In each specimen, We can get the yielding load obtained by the theoretical three failure modes which make it possible to predict the experimental results. Actually, through the comparison and analysis, we come to know that the experimental results and theoretical results are nealy the same. Further, we will exert to apply the connections using reinforced bar to construction of high-rise building.

  • PDF