• Title/Summary/Keyword: transient dynamic

Search Result 1,023, Processing Time 0.021 seconds

Elastic Wave Propagation in Nuclear Power Plant Containment Building Walls Considering Liner Plate and Concrete Cavity (라이너 플레이트 및 콘크리트 공동을 고려한 원전 격납건물 벽체의 탄성파 전파 해석)

  • Kim, Eunyoung;Kim, Boyoung;Kang, Jun Won;Lee, Hongpyo
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.34 no.3
    • /
    • pp.167-174
    • /
    • 2021
  • Recent investigation into the integrity of nuclear containment buildings has highlighted the importance of developing an elaborate diagnostic method to evaluate the distribution and size of cavities inside concrete walls. As part of developing such a method, this paper presents a finite element approach to modeling elastic waves propagating in the containment building walls of a nuclear power plant. We introduce a perfectly matched layer (PML) wave-absorbing boundary to limit the large-scale nuclear containment wall to the region of interest. The formulation results in a semi-discrete form with symmetric damping and stiffness matrices. The transient elastic wave equations for a mixed unsplit-field PML were solved for displacement and stresses in the time domain. Numerical results show that the sensitivity of displacement, velocity, acceleration, and stresses is large depending on the size and location of the cavity. The dynamic response of the wall slightly differs depending on the existence of the containment liner plate. The results of this study can be applied to a full-waveform inversion approach for characterizing cavities inside a containment wall.

A Study on the Calculation of Optimal Compensation Capacity of Reactive Power for Grid Connection of Offshore Wind Farms (해상풍력단지 전력계통 연계를 위한 무효전력 최적 보상용량 계산에 관한 연구)

  • Seong-Min Han;Joo-Hyuk Park;Chang-Hyun Hwang;Chae-Joo Moon
    • The Journal of the Korea institute of electronic communication sciences
    • /
    • v.19 no.1
    • /
    • pp.65-76
    • /
    • 2024
  • With the recent activation of the offshore wind power industry, there has been a development of power plants with a scale exceeding 400MW, comparable to traditional thermal power plants. Renewable energy, characterized by intermittency depending on the energy source, is a prominent feature of modern renewable power generation facilities, which are structured based on controllable inverter technology. As the integration of renewable energy sources into the grid expands, the grid codes for power system connection are progressively becoming more defined, leading to active discussions and evaluations in this area. In this paper, we propose a method for selecting optimal reactive power compensation capacity when multiple offshore wind farms are integrated and connected through a shared interconnection facility to comply with grid codes. Based on the requirements of the grid code, we analyze the reactive power compensation and excessive stability of the 400MW wind power generation site under development in the southwest sea of Jeonbuk. This analysis involves constructing a generation site database using PSS/E (Power System Simulation for Engineering), incorporating turbine layouts and cable data. The study calculates reactive power due to charging current in internal and external network cables and determines the reactive power compensation capacity at the interconnection point. Additionally, static and dynamic stability assessments are conducted by integrating with the power system database.

Electrochemical Characteristics of Cu3Si as Negative Electrode for Lithium Secondary Batteries at Elevated Temperatures (리튬 이차전지 음극용 Cu3Si의 고온에서의 전기화학적 특성)

  • Kwon, Ji-Y.;Ryu, Ji-Heon;Kim, Jun-Ho;Chae, Oh-B.;Oh, Seung-M.
    • Journal of the Korean Electrochemical Society
    • /
    • v.13 no.2
    • /
    • pp.116-122
    • /
    • 2010
  • A $Cu_3Si$ film electrode is obtained by Si deposition on a Cu foil using DC magnetron sputtering, which is followed by annealing at $800^{\circ}C$ for 10 h. The Si component in $Cu_3Si$ is inactive for lithiation at ambient temperature. The linear sweep thermammetry (LSTA) and galvano-static charge/discharge cycling, however, consistently illustrate that $Cu_3Si$ becomes active for the conversion-type lithiation reaction at elevated temperatures (> $85^{\circ}C$). The $Cu_3Si$ electrode that is short-circuited with Li metal for one week is converted to a mixture of $Li_{21}Si_5$ and metallic Cu, implying that the Li-Si alloy phase generated at 0.0 V (vs. Li/$Li^+$) at the quasi-equilibrium condition is the most Li-rich $Li_{21}Si_5$. However, the lithiation is not extended to this phase in the constant-current charging (transient or dynamic condition). Upon de-lithiation, the metallic Cu and Si react to be restored back to $Cu_3Si$. The $Cu_3Si$ electrode shows a better cycle performance than an amorphous Si electrode at $120^{\circ}C$, which can be ascribed to the favorable roles provided by the Cu component in $Cu_3Si$. The inactive element (Cu) plays as a buffer against the volume change of Si component, which can minimize the electrode failure by suppressing the detachment of Si from the Cu substrate.