Sound Absorption Rate and Sound Transmission Loss of CLT Wall Panels Composed of Larch Square Timber Core and Plywood Cross Band

  • Kang, Chun Won;Jang, Sang Sik;Kang, Ho Yang;Li, Chengyuan
    • Journal of the Korean Wood Science and Technology
    • /
    • v.47 no.1
    • /
    • pp.33-39
    • /
    • 2019
  • The square timbers of larch having cross section of $90mm{\times}90mm$ were glued laterally to be formed $1,200mm{\times}2,400mm$ panels which were used as cores for CLT wall panels. Then, structural plywood panels having size of $1,200mm{\times}2,400mm$ were used as cross band covering the small square timber cores to manufacture CLT wall panels. The sound absorption rate of CLT wall panels and polyester board attached CLT wall panels were investigated. The mean sound absorption coefficients of the former and the latter in the frequency range of 100-6400 Hz were 0.21 and 0.74, respectively. The noise reduction coefficients (NRC) of those were 0.21 and 0.40, respectively. Also, the mean sound transmission loss of CLT wood panel in the frequency range of 50-1600 Hz was 45.12 dB and that value at the frequency of 500 Hz was 42.49 dB. It was suggested that the polyester board attached CLT wall panels could be used as housing wall because of its high sound absorption rate and high sound transmission loss.

Study on the Long-Term Demand Projections for Timber in Korea (우리나라 목재수요(木材需要)의 장기여측에(長期予測) 관(関)한 연구(硏究))

  • Kim, Jang Soo;Park, Ho Tak
    • Journal of Korean Society of Forest Science
    • /
    • v.50 no.1
    • /
    • pp.29-35
    • /
    • 1980
  • The purpose of this study is to analyze and to forecast the long-term domestic demand and export demand for timber in Korea by regression models with time series data during 1962~1978. The method applied in this study was econometric analysis using Time Series Processor. The most important explanatory variables of timber demand were found to be the production activities of wood products industries to the prices of substitute goods. On the basis of the long-term forecast made according to the guidelines of the Fifth Five-Year Plan. According to the projection, domestic timber demand is projected at 8 million cubic meters in 1987 and 10.6 million cubic meters in 1991. On the other hand, the total demand (domestic demand plus export demand) for timber is projected 21.4 million cubic meters in 1987 and 27.2 million cubic meters in 1991.

  • PDF

A Study on Utilization of the Sawed Products by 1, 2 and 3-Sided Sawing Methods from Thinning of Japanese Larch and Pitch Pine (낙엽송(落葉松), 리기다소나무 간벌재(間伐材)의 1, 2및 3면(面) 제재이용(製材利用) 시험(試驗)에 관(關)한 연구(硏究))

  • Lee, Choon-Taek;Kang, Dae-Hun;Chung, Doo-Jin;Lee, Yong-Dae;Joe, Jae-Myung
    • Journal of the Korean Wood Science and Technology
    • /
    • v.13 no.3
    • /
    • pp.41-48
    • /
    • 1985
  • In near future about 500,000 hectares of Japanese larch and pitch pine need thinning to improve crop-tree spacing and reasonable species composition in Korea. Although thinned trees show very little high quality wood, in fact, all the sawed products are suitable for construction and farming materials. Studies on the utilization of thinned small-diameter trees have been implemented in order to increase lumber yield and display the skeleton of farm buildings. The results obtained in this study were summarized as follows: 1. According to Korean Conifers Log Grading System, log grade 3 was 87.4 percent in Japanese larch bolts and 95.8 percent in pitch pine bolts from thinned trees. The ability to identify defects was essential for grading logs. 2. Cutting diagrams of sawing were developed for 1-sided sawing, 2-sided sawing and 3-sided sawing by small end diameter class of bolt and cutting sizes also were found to use effectively lumber with wane. 3. Lumber recovery of Pitch pine was a little higher than that of Japanese larch. The maximum lumber yields of pitch pine by sawing patterns were 87.2 percent for 1-sided sawing, 80.8 percent for 2-sided sawing an 64.1 percent for 3-sided sawing, up yield compared with 58.1 percent for 4-sided sawing. The lumber yield of 1, 2 and 3-sided sawing significantly was higher value than that of 4-sided sawing. 4. Lumber was inspected and graded. Lumber quality of diameter class 12cm was a little better than that of diameter class 8cm, but 90 percent of lumber in diameter c1ass 16cm fell into grade 3. The lumber grade was classified by Korean standard grades of confiers lumber. 5. Lumber from 1, 2 and 3-sided sawing was used to build the skeleton of a farm house ($53m^2$) and greenhouse ($60m^2$) in order to display more efficient use of small diameter trees from thinning 6. Total volume of timber for building a farm house was $8.1m^3$ of imported timber. Timber of $7m^3$, 70 percent of total volume would be substituted imported timber for domestic timber.

  • PDF

Insulation Details and Energy Performance of Post-Beam Timber House for Insulation Standards (단열 기준에 따른 기둥-보 목조주택의 단열 상세 및 에너지 성능)

  • Kim, Sejong;Park, Joo-Saeng
    • Journal of the Korean Wood Science and Technology
    • /
    • v.43 no.6
    • /
    • pp.876-883
    • /
    • 2015
  • Han-green project, which pursues Korean style post and beam timber house with traditional construction technique of Han-ok, has been carried out in KFRI (Korea Forest Research Institute) since 2006. Recently, the improvement of its building energy performance was studied with energy-saving elements. This study was conducted to provide the insulation details of building envelopes in a post-beam timber house for recent enhanced insulation standards and following effect on building energy performance. The level of thermal transmittance (U-value) values of building envelopes was composed of two stages: present Korean insulation standards and passive house. To evaluate building energy performance, the building airtightness values of two stages was ACH50 = $3.0h^{-1}$ for common domestic timber house constructed recently, and ACH50 = $0.6h^{-1}$ for passive house. Consequently, four cases of the building energy performance according to the combination of U-value with airtightness were evaluated. The test house for evaluation was located in Seoul and its energy performance was evaluated with CE3 commercial building energy simulation program. The result showed that enhanced insulation from level I to II reduced $14kWh/(m^2{\cdot}a)$ of annual heating energy demand regardless of airtightness.

Feasibility of Ultrasonic Log Sorting in Manufacturing Structural Lamination from Japanese Cedar Logs

  • Oh, Jung-Kwon;Yeo, Hwan-Myeong;Choi, In-Gyu;Lee, Jun-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • v.39 no.2
    • /
    • pp.163-171
    • /
    • 2011
  • Because Japanese cedar shows lower mechanical performance, glued-laminated timber (glulam) can be a better way to utilize Japanese cedar for structural purpose. However, low yield of higher grade lamination from log makes it difficult to design structural glulam. This study was aimed to increase the yield of higher grade lamination and provide higher efficiency of manufacturing structural lamination by ultrasonic log sorting technology. Logs were sorted by an existing log grading rule regulated by Korea Forest Research Institute (KFRI). It was found that the KFRI log grading rule contributed to finding better logs in viewpoint of the volumetric yield and it can reduce the number of rejected lumber by visual grading. However, it could not identify better logs to produce higher-grade products. To find an appropriate log-sorting-method for structural products, log diameter and ultrasonic time of flight (TOF) for the log were considered as factors to affect mechanical performance of resulting products. However, it was found that influence of log diameter on mechanical performance of resulting products was very small. The TOF showed a possibility to sort logs by mechanical performance of resulting products even though a coefficient of correlation was not strong (R = 0.6). In a case study, the log selection based on the ultrasonic TOF of the log increased the yield of the outermost tension lamination (E8 or better grade, KS F 3021) from 2.6% to 12.5% and reduced LTE5 (lower than E5 grade) lamination from 43.6% to 10.3%, compared with the existing KFRI log grading rule.

Lightweight Floor Systems for Tall Buildings: A Comparative Analysis of Structural Material Efficiencies

  • Piyush Khairnar
    • International Journal of High-Rise Buildings
    • /
    • v.12 no.2
    • /
    • pp.145-152
    • /
    • 2023
  • Typical floor systems in contemporary tall buildings consist of reinforced concrete or composite metal deck over framing members and account for a majority of the structural weight of the building. The use of high-density materials, such as reinforced concrete and steel, increases the weight of floor systems, reducing the system's overall efficiency. With the introduction of high-performance materials, mainly mass timber products, and fiber-reinforced composites, in the construction industry, designers and engineers have multiple options to choose from when selecting structural materials. This paper discusses the application of mass timber and carbon fiber composites as structural materials in floor systems of tall buildings. The research focused on a comparative analysis of the structural system efficiency for five different design options for tall building floor systems. Finite Element Analysis (FEA) method was adopted to develop a simulation framework, and parametric structural models were simulated to evaluate the structural performance under specific loading conditions. Simulation results revealed the advantages of lightweight structural materials to improve system efficiency and reduce material consumption. The impact of mechanical properties of materials, loading conditions, and issues related to fire engineering and construction were briefly discussed, and future research topics were identified in conclusion.

Structures and Competitiveness of Softwood Products in Korean Import Market (우리나라 수입(輸入) 침엽수재(針葉樹材) 시장구조(市場構造) 및 수종별(樹種別) 경쟁력(競爭力))

  • Kim, Wae-Jung
    • Journal of the Korean Wood Science and Technology
    • /
    • v.19 no.4
    • /
    • pp.34-42
    • /
    • 1991
  • Protection of tropical forest affects on significant reduce of tropical hardwood supply, and softwood resources will be increasingly important for the timber security in Korea. U.S. softwood log was most favorite species for Korean softwood log importers in overall import conditions except price stablization and consistency of export policy. Reduced export volume from Pacific Northwest to Korean market has been immediately replenished by rediata pine from New Zealand and Chilean plantation. Siberian timber will hardly play major roles in Korean timber market unless budding structure. softwood plywood and softwood furniture uses are enhanced. Recent rapid rise of labor cost and reducing tariff rrate in Korea provided better opportunities for import lumber in building materials market. Dry dimension lumber was relatively profitable when processed from import U.S. soft-wood log while green lumber was favorable products processed from radiata pine log in Korean lumber market. This means U.S. softwood lumber would have better opportunity to market for '2${\times}$'4 studs when wood frame housing is introduced. On the other hand while radiata pine is competitive on temporary construction lumber such as supporter and concrete forming frame in Korea. Shortage of raw material for the new capacity of board plants in Korea will be it bottle neck. Major log export countries to Korea as U.S. New Zealand and Chile showed high trade intensity indices of composite hoard produces for Korean market. As Korea efforts to diversify import sources, and tariffs are reduced to 8% as scheduled by 1994. countries of scoring higher comparative advantages as Portugal. Brazil, Austria as well as New Zealand will have better opportunity to penetrate into promised Korean composites hoard market.

  • PDF

Influence of Composition of Layer Layout on Bending and Compression Strength Performance of Larix Cross-Laminated Timber (CLT)

  • Da-Bin SONG;Keon-Ho KIM
    • Journal of the Korean Wood Science and Technology
    • /
    • v.51 no.4
    • /
    • pp.239-252
    • /
    • 2023
  • In this study, bending and compression strength tests were performed to investigate effect of composition of layer layout of Larix cross-laminated timber (CLT) on mechanical properties. The Larix CLT consists of five laminae, and specimens were classified into four types according to grade and composition of layer. The layer's layout were composited as follows 1) cross-laminating layers in major and minor direction (Type A), and 2) cross-laminating external layer in major direction and internal layer applied grade of layer in minor direction (Type B). E12 and E16 were used as grades of lamina for major direction layer of Type A and external layer of Type B according to KS F 3020. In results of the bending test of CLT using same grade layer according to layer composition, the modulus of elasticity (MOE) of Type B was higher than Type A. In case of prediction of bending MOE of Larix CLT, the experimental MOE was higher than 1.00 to 1.09 times for Shear analogy method and 1.14 to 1.25 times for Gamma method. Therefore, it is recommended to predict the bending MOE for Larix CLT by shear analogy method. Compression strength of CLT in accordance with layer composition was measured to be 2% and 9% higher for Type A using E12 and E16 layers than Type B, respectively. In failure mode of Type A, progress direction of failure generated under compression load was confirmed to transfer from major layer to minor layer by rolling shear or bonding line failure due to the middle lamina in major direction.

A Study Scope of Optimal Heating and Drying Process of Timber Heated by Microwave (초고주파 가열 목재의 최적 가열 및 건조 공정범위 도출에 관한 연구)

  • Shin, Ki-Hoon;Park, Cheul-Woo;Son, Dong-Won;Lim, Nam-Gi
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.18 no.4
    • /
    • pp.126-137
    • /
    • 2014
  • Characteristics of heating and drying of Canadian-imported Douglas-fir timber using microwave in order to secure convenience and quality of drying timber and to get basic data for secondary conservation treatment are as follows: As the results of analysis of change curves of internal temperature of the timber after irradiating it, round timber and board timber showed stable heat distribution, heat consumption and surface water-content in heating with 30kW for 30 minutes and 120 minutes and with 40kW for 3 minutes and 9 minutes, respectively. Especially, surface water-content distribution according to heating by microwave showed very even leveling and water-content decrease rate was also more 30% compared to its weight showing excellent dry efficiency. And in case of soaking timbers into liquid chemicals for secondary conservation according to the analysis results of heat consumption, it is expected that large amount of preservative will be permeated. Therefore, timber heated by microwave is remarkably available for using industrial materials and developing secondary utilized products with its fast water-content decrease and dryness and higher heat consumption.

Influence of Manufacturing Environment on Delamination of Mixed Cross Laminated Timber Using Polyurethane Adhesive

  • SONG, Dabin;KIM, Keonho
    • Journal of the Korean Wood Science and Technology
    • /
    • v.50 no.3
    • /
    • pp.167-178
    • /
    • 2022
  • To investigate the influence of manufacturing environment on bonding performance of mixed cross laminated wood (CLT) using polyurethane (PUR) adhesive, a boiling water soak delamination test according to the temperature and relative humidity was conducted. The 5-ply mixed CLT consisted of Japanese Larch for external and middle layer and yellow poplar for internal layer. The PUR adhesives with different opening times of 10 and 30 minutes were used. The mixed CLT was manufactured according to pressing times of PUR and manufacturing environments of summer and winter. In case of summer environment, the delamination rate of the mixed CLT with pressing time of 4 hours using a PUR adhesive with open time of 10 minutes met the requirements of KS F 2081. In case of winter environment, the delamination rate of the mixed CLT didn't meet the requirements of KS standard. However, it was possible to confirm the effect of improving the adhesive performance by adjusting the pressing time according to the open time of the adhesive under the manufacturing conditions. The delamination rate of CLT with open time 30 minutes PUR, manufactured by indirect moisture supply methods was 11.2% better than direct moisture supply methods. As a result of delamination test in the same condition of relative humidity and adhesive, it was found that the temperature of manufacturing environment influences the adhesive performance.