• 제목/요약/키워드: thinning system

검색결과 246건 처리시간 0.031초

Pipe thinning model development for direct current potential drop data with machine learning approach

  • Ryu, Kyungha;Lee, Taehyun;Baek, Dong-cheon;Park, Jong-won
    • Nuclear Engineering and Technology
    • /
    • 제52권4호
    • /
    • pp.784-790
    • /
    • 2020
  • The accelerated corrosion by Flow Accelerated Corrosion (FAC) has caused unexpected rupture of piping, hindering the safety of nuclear power plants (NPPs) and sometimes causing personal injury. For the safety, it may be necessary to select some pipes in terms of condition monitoring and to measure the change in thickness of pipes in real time. Direct current potential drop (DCPD) method has advantages in on-line monitoring of pipe wall thinning. However, it has a disadvantage in that it is difficult to quantify thinning due to various thinning shapes and thus there is a limitation in application. The machine learning approach has advantages in that it can be easily applied because the machine can learn the signals of various thinning shapes and can identify the thinning using these. In this paper, finite element analysis (FEA) was performed by applying direct current to a carbon steel pipe and measuring the potential drop. The fundamental machine learning was carried out and the piping thinning model was developed. In this process, the features of DCPD to thinning were proposed.

원전 2차계통의 수화학 변화가 배관감육에 미치는 영향 분석 (Analysis of Pipe Wall-thinning Caused by Water Chemistry Change in Secondary System of Nuclear Power Plant)

  • 윤훈;황경모;문승재
    • Corrosion Science and Technology
    • /
    • 제14권6호
    • /
    • pp.325-330
    • /
    • 2015
  • Pipe wall-thinning by flow-accelerated corrosion (FAC) is a significant and costly damage of secondary system piping in nuclear power plants (NPPs). All NPPs have their management programs to ensure pipe integrity from wall-thinning. This study analyzed the pipe wall-thinning caused by changing the amine, which is used for adjusting the water chemistry in the secondary system of NPPs. The pH change was analyzed according to the addition of amine. Then, the wear rate calculated in two different amines was compared at the steam cycle in NPPs. As a result, increasing the pH at operating temperature (Hot pH) can reduce the rate of FAC damage significantly. Wall-thinning is affected by amine characteristics depending on temperature and quality of water.

감육을 가지는 배관 용접부의 파괴거동 (Fracture Behavior of Welded Pipes with Local Wall Thinning)

  • 안석환;남기우;정정환;김용운
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2003년도 춘계학술대회
    • /
    • pp.90-95
    • /
    • 2003
  • Fracture behaviors of pipes with local wall thinning are very important for the integrity of nuclear power plant. In pipes of energy plants, sometimes, the local wall thinning may result from severe erosion-corrosion (E/C) damage. However, the effects of local wall thinning on strength and fracture behaviors of piping system were not well studied. In this paper, the monotonic bending tests were performed of full-scale welded and unwelded carbon steel pipes with local wall thinning. A monotonic bending load was applied to straight pipe specimens by four-point loading at ambient temperature without internal pressure. The observed failure modes were divided into four types; ovalization, crack initiation/growth after ovalization, local buckling and crack initiation/growth after local buckling. Also, the strengths of welded and unwelded piping system with local wall thinning were evaluated.

  • PDF

낙엽송 간벌 임분의 공간 이미지 분석 (Spatial Images toward Thinning Systems on Larix Forest Stands)

  • 송형섭;명재갑;박민우;손종은;이선
    • 농업과학연구
    • /
    • 제27권1호
    • /
    • pp.5-12
    • /
    • 2000
  • The main purpose of this study is to obtain spatial image information toward forest thinning process in Larix forest stands. Thirteen different alternatives were simulated to visualize on the basis of actual thinning work photos. The options were illustrated as photos produced by photoshop program. Each alternatives were evaluated by forest visitor group with total 244 respondents after reliability test. Spatial images of 13 thinning photos were measured by 12 semantic differential scale as broad -narrow, ordered-tangled, friendly-unfriendly, monotonous-divers, dry-refreshing, relieved -stifling, healthy-sickly, uniform-scattered, dead-alive, opened-closed, bent-straight, and beautiful-ugly. In comparison with thinning stands and natural stands, thinning works were visual improvement effects of spatial images. Seemingly, this trend is due to definite form beauty, straight and clear length form of coniferous forest, As can be expected, slash and downwood were negatively related to improvement effects of spatial images. The 60% ratio of stem/ tree height and 450-950 trees/ha was positive in attraction of spatial images. Results indicate how to conduct forest thinning system for spatial images on Larix forest stands.

  • PDF

감육배관의 굽힘하중에 의한 손상모드와 파괴거동 평가 (Failure Mode and Fracture Behavior Evaluation of Pipes with Local Wall Thinning Subjected to Bending Load)

  • 안석환;남기우;김선진;김진환;김현수;도재윤
    • 대한기계학회논문집A
    • /
    • 제27권1호
    • /
    • pp.8-17
    • /
    • 2003
  • Fracture behaviors of pipes with local wall thinning are very important for the integrity of nuclear Power Plant. In Pipes of energy Plants, sometimes, the local wall thinning may result from severe erosion-corrosion (E/C) damage. However, the effects of local wall thinning on strength and fracture behaviors of piping system were not well studied. In this paper, the monotonic bending tests were performed of full-scale carbon steel pipes with local wall thinning. A monotonic bending load was applied to straight pipe specimens by four-point loading at ambient temperature without internal pressure. From the tests, fracture behaviors and fracture strength of locally thinned pipe were manifested systematically. The observed failure modes were divided into four types; ovalization. crack initiation/growth after ovalization, local buckling and crack initiation/growth after local buckling. Also, the strength and the allowable limit of piping system with local wall thinning were evaluated.

내압을 받는 내/외부 국부 감육 곡관의 파손거동 (Damage Behavior of Elbow Pipe with Inner or Outer Local Wall Thinning under Internal Pressure)

  • 김수영;남기우
    • 동력기계공학회지
    • /
    • 제18권5호
    • /
    • pp.66-73
    • /
    • 2014
  • This study was considered to occur the local wall thinning at elbow which is flowing the steam and high-pressure water of high-temperature. The angle of elbow is ${\Theta}=45^{\circ}$ and $67.545^{\circ}$. The damage behaviors of inner or outer wall thinning elbow under internal pressure were calculated by FEA(finite element analysis). We compared the simulated results by FEA with experimental data. The FEA results are as follows: In the FEA results of three types of wall thinning ratio, the circumferential and longitudinal stresses show the similar values regardless of the angle of elbow, respectively. The circumferential strain was greater at elbow of small angle, but the longitudinal strain was nearly same. The FEM stress of outer wall thinning elbow was slightly higher than that of the inner wall thinning elbow, and strain was also slightly higher. In the experiments, the circumferential strain was increased with the increase in the internal pressure, and increased rapidly on about 0.2% of strain. The longitudinal strain was small. The strain at break was much smaller than 0.2%. In the relation between pressure and eroded ratio, the criteria that can be used safely under operating pressure and design pressure were obtained. The results of FEA were in relatively good agreement with those of the experiment.

Thinning Processor for 160 X 192 Pixel Array Fingerprint Recognition

  • Jung, Seung-Min
    • Journal of information and communication convergence engineering
    • /
    • 제8권5호
    • /
    • pp.570-574
    • /
    • 2010
  • A thinning algorithm changes a binary fingerprint image to one pixel width. A thinning stage occupies 40% cycle of 32-bit RISC microprocessor system for a fingerprint identification algorithm. Hardware block processing is more effective than software one in speed, because a thinning algorithm is iteration of simple instructions. This paper describes an effective hardware scheme for thinning stage processing using the Verilog-HDL in $160\times192$ Pixel Array. The ZS algorithm was applied for a thinning stage. The hardware scheme was designed and simulated in RTL. The logic was also synthesized by XST in FPGA environment. Experimental results show the performance of the proposed scheme.

감육 배관의 손상모드에 미치는 감육부 길이의 영향 (Effects of Thinning Length on Failure Mode of Local Wall Thinned Pipe)

  • 김진원;박치용;이성호;강태경
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집A
    • /
    • pp.357-362
    • /
    • 2001
  • The pipe fracture tests were performed on 102mm-Sch.80 carbon steel pipe with various local wall thinning shapes, in order to understand failure behavior of thinned pipe. Pipe specimens were subjected to monotonic bending moment, using 4-points loading system, under internally pressurized condition. From the results of experiment, the failure mode, load carrying capacity, and deformability of local wall thinning pipe were investigated. Failure mode of thinned pipe depended on magnitude of internal pressure and thinning length as well as loading direction and thinning depth and angle. The variation in load carrying capacity and deformability of thinned pipe with length of thinned area was determined by stress type appled to thinning region and circumferential thinning angle. Also, the effect of internal pressure on failure behavior was dependent on failure mode of thinned pipe, and it promoted crack occurrence and mitigated local buckling at thinned area.

  • PDF

펄스와전류를 이용한 보온재 비해체식 배관감육 평가기술 (Nondestructive evaluation of wall thinning covered with insulation using pulsed eddy current)

  • 박덕근;;이덕현
    • 한국압력기기공학회 논문집
    • /
    • 제10권1호
    • /
    • pp.90-95
    • /
    • 2014
  • Local wall thinning is a point of concern in almost all steel structures such as pipe lines covered with a thermal insulator made up of materials with low thermal conductivity(fiberglass or mineral wool); hence, Non Destructive Technique(NDT) methods that are capable of detecting the wall thinning and defects without removing the insulation are necessary. In this study we developed a Pulsed Eddy Current(PEC) system to detect the wall thinning of Ferro magnetic steel pipes covered with fiber glass thermal insulator and shielded with Aluminum plate. The developed system is capable of detecting the wall thickness change through an insulation of thickness 10cm and 0.4mm aluminum shielding. In order to confirm the thickness change due to wall thinning, two different sensors, a hall sensor and coil sensor were used as a detecting element. In both cases, the results show a very good change corresponding to the thickness change of the test specimen. During these experiments a carbon steel tube of diameter 210mm and a length of 620mm, which is covered with insulator of 95mm thickness was used. To simulate the wall thinning, the thickness of the tube is changed for a specified length such as 2.5mm, 5mm and 8 mm from the inner surface of the tube. A 0.4mm thick Aluminum plate was covered on the Test specimen to simulate the shielding of the insulated pipelines. For both hall sensor and coil detection methods Fast Fourier transform(FFT) was calculated using window approach and the results for the test specimen without Aluminum shielding were summarized which shows a clear identification of thickness change in the test specimen by comparing the magnitude spectra. The PEC system can detect the wall thinning under the 95 mm thickness insulation and 0.4 mm Al shielding, and the output signal showed linear relation with tube wall thickness.

감육된 증기발생기 전열관의 유한요소 해석 (Finite Element Analysis for Wall Thinned Steam Generator Tubes)

  • 성기용;안석환;남기우
    • 동력기계공학회지
    • /
    • 제10권3호
    • /
    • pp.38-44
    • /
    • 2006
  • Failure assessment of steam generator tube are very important for the integrity of energy plants. In pipes of energy plants, sometimes, the local wall thinning may result from severe erosion-corrosion damage. Recently, the effects of local wall thinning on fracture strength and fracture behavior of piping system have been well studied. In this paper, the elasto-plastic analysis is performed by FE code ANSIS on steam generator tube with wall thinning. We evaluated the failure mode, fracture strength and fracture behavior from FE analysis. It was possible to predict the crack initiation point by estimating true fracture ductility under multi-axial stress conditions at the center of the thinned area.

  • PDF