Chemical Compositions and Thermal Characteristics of Rice Husk and Rice Husk Ash in Korea (왕겨 및 왕겨재의 화학적 조성 성분과 열적 특성)

  • Park S. J.;Kim M. H.;Shin H. M.
    • Journal of Biosystems Engineering
    • /
    • v.30 no.4 s.111
    • /
    • pp.235-241
    • /
    • 2005
  • For better and large utilization of rice husk, the production and consumption status, differences in chemical composition and heating value due to region and variety, and thermogravimetric characteristic of rice husk were studied. In addition, the differences in chemical composition due to region and variety and the crystallization characteristic of rice husk ash were also studied. Approximately 800,000 M/T of rice husk was produced per year in Korea, which is about $18\%$ of the paddy production by weight. Noticeable varietal and regional difference pattern in chemical composition was not found among the domestic rice husk samples. Their average ash content and higher heating value were $16.4\%$ and 16,660 kJ/kg by dry basis, respectively. A relation seemed to exist between the carbon content and higher heating value. Noticeable difference pattern in chemical composition was not found among the domestic rice husk ash samples. The $SiO_2$ contents were a little low, the maximum being $92.9\%,$ and the contents of major components such as CaO, MgO, and $K_2O$ were also lower compared with foreign rice husk ash due to the deficiency of compost matters in domestic soils. Thermogravimetry study showed the thermal decomposition of rice husk started at about $250^{\circ}C,$ followed by relatively fast combustion of combustible gas until the temperature rose to $350^{\circ}C.$ After $350^{\circ}C,$ combustion of the carbon component proceeded relatively slowly as the temperature increased. Therefore, the ignition temperature of the rice husk could be estimated around $300^{\circ}C$. Crystallization of $SiO_2$ in the rice husk ash was found from the combustion temperature of $750^{\circ}C$ and became distinctly when the combustion temperature exceeded $900^{\circ}C$. The ash became darker with $SiO_2$ crystallization.

Tensile Properties and Thermal Stability of Cellulose Nanofibril/Clay Nanocomposites

  • Park, Byung-Dae;Singh, Adya P.;Um, In Chul
    • Current Research on Agriculture and Life Sciences
    • /
    • v.31 no.1
    • /
    • pp.18-24
    • /
    • 2013
  • This work attempted to fabricate organic/inorganic nanocomposite by combining organic cellulose nanofibrils (CNFs), isolated by 2,2,6,6-tetramethylpiperidine-1-oxy radical (TEMPO)-mediated oxidation of native cellulose with inorganic nanoclay. The morphology and dimension of CNFs, and tensile properties and thermal stability of CNF/clay nanocomposites were characterized by transmission electron microscope (TEM), tensile test, and thermogravimetry (TG), respectively. TEM observation showed that CNFs were fibrillated structure with a diameter of about $4.86{\pm}1.341nm$. Tensile strength and modulus of the hybrid nanocomposite decreased as the clay content of the nanocomposite increased, indicating a poor dispersion of CNFs or inefficient stress transfer between the CNFs and clay. The elongation at break increased at 1% clay level and then continuously decreased as the clay content increased, suggesting increased brittleness. Analysis of TG and derivative thermogravimetry (DTG) curves of the nanocomposites identified two thermal degradation peak temperatures ($T_{p1}$ and $T_{p2}$), which suggested thermal decomposition of the nanocomposites to be a two steps-process. We think that $T_{p1}$ values from $219.6^{\circ}C$ to $235^{\circ}C$ resulted from the sodium carboxylate groups in the CNFs, and that $T_{p2}$ values from $267^{\circ}C$ to $273.5^{\circ}C$ were mainly responsible for the thermal decomposition of crystalline cellulose in the nanocomposite. An increase in the clay level of the CNF/clay nanocomposite predominately affected $T_{p2}$ values, which continuously increased as the clay content increased. These results indicate that the addition of clay improved thermal stability of the CNF/clay nanocomposite but at the expense of nanocomposite's tensile properties.

  • PDF

Thermo-decomposition behavior of GaAs scrap by thermogravimetry (열중량분석법에 의하 GaAs Scrap의 열분해거동)

  • 이영기;손용운;남철우;최여윤;홍성웅
    • Resources Recycling
    • /
    • v.4 no.3
    • /
    • pp.10-18
    • /
    • 1995
  • Recycling of GaAs scrap which occurs durmg the manufachre of GaAs waters is. therefore, required to solve the environmentalproblcrns caused by arsenic metal and to reutilize gallium which is a expensive metal. A thema-analyticalstudy (thermogravimeg. and derivative thermogravimetry) tor the evaporation behavior of Fa, As from Gak\ulcorner scrap powdersat vacuum atmosphere(2-2.5X 10'mmHg); was primarily performed to identi j the possibility of Ga extraction. Until79YC, the weight change of G d s porvder does not take place, at 800-970C range GaAs vaporizes as the GaAs compound,and over 1WO"C it decamposes mto Ga and As md then As vaporizes rapidly as a result of the difference af vaporprcssure for Ga and As, liquid Ga rcmains eventually.mains eventually.

  • PDF

Preparation and Properties of Poly($\varepsilon$-caprolactone) Nanocapsules Containing Phytoncide Oil by Emulsion-diffusion Method(1) (유화확산법을 이용한 피톤치드오일 함유 폴리입실론카프로락톤 나노캡슐의 제조와 성질(1))

  • Jeong, Cheon-Hee;Kim, Hea-In;Park, Soo-Min
    • Proceedings of the Korean Society of Dyers and Finishers Conference
    • /
    • 2008.04a
    • /
    • pp.114-116
    • /
    • 2008
  • Poly(${\varepsilon}$-caprolactone) nanocapsules(nanoPCL) containing phytoncide oil were synthesized by emulsion diffusion method using ethyl acetate as organic solvent. The influence of the degree of hydrolyzation of poly(vinyl acohol) used as an emulsion stabilizer, and the different weight ratio of core material to wall material on the particle size, morphology, and emulsion stability was investigated to design nanocapsules. The encapsulated nanoPCL were characterized by FT-IR spetrometry, Scanning electron microscope, Differential scanning calorimetry, and Thermogravimetry analysis, respectively.

  • PDF

Electrospun $SiO_2$ membrane using covalently cross-linked SPEEK/HPA by impregnation for high temperature PEMFC

  • Na, Heesoo;Hwang, Hyungkwon;Lee, Chanmin;Shul, Yonggun
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2010.11a
    • /
    • pp.85.2-85.2
    • /
    • 2010
  • There is widespread effort to develop polymer membranes in place of Nafion for high temperature polymer electrolyte membrane fuel cell(PEMFC). In our study, SiO2 membranes are arranged by electrospinning method. For impregnation solution, the modified sulfonated poly(ether ether ketone)(SPEEK) polymer is prepared from sulfonation, sulfochlorination, partial reduction and lithiation reaction. The modified polymer is cross-linked with 1,4-diiodobetane in NMP solvent and then blended with Heteropoly acid(HPA). The characterization of membranes is confimed by FT-IR, Thermogravimetry(TGA), water uptake test and single cell performance test for PEMFC, etc. The composite membrane shows satisfactory thermal and mechanical properties. Beside, The membrane exhibits good ion exchange capacity and high proton conductivity. As a result, The composite membrane is promising as an alternative membrane in high temperature PEMFC.

  • PDF

Behavior of Mn Ions in Spinel-type Mn-Zn-Fe Oxide System (스피넬계 Mn-Zn 페라이트의 망간이온이 미치는 영향)

  • 권오흥
    • Resources Recycling
    • /
    • v.9 no.5
    • /
    • pp.11-15
    • /
    • 2000
  • The sample made of $Mn_3O_4$ indicated an excellent frequency dependency for intial permeability and core loss. Moreover the homogeneity of cation configuration in he spinel structure was confirmed by X-ray diffraction analysis. The result of homogeneity of the spinel structural coincided with the analytical results of temperature dependence of magnetization. Furthermore, the influence of manganese oxide as starting material, on homogeneity of spinel structure was examined by using thermogravimetry-differential thermal analysis. It may be concluded that the reaction between $Mn_3O_4$ and Fe-Zn oxide mixture proceeds at fist in all combination of manganese oxide and oxie mixture, and then Mn-Zn-Fe spinel was formed.

  • PDF

A Study on the Environmental Properties of Polyimide/Silica Composites Prepared by Sol-Gel Method (졸-겔법으로 합성된 폴리이미드/실리카 복합체의 환경적 물성에 관한 연구)

  • 박성수;홍성수;이성환;김성완;박재현;김지경;박희찬
    • Journal of Environmental Science International
    • /
    • v.12 no.4
    • /
    • pp.481-485
    • /
    • 2003
  • Two types of polyimide/silica composite films were prepared using sol-gel method through hydrolysis and polycondensation of tetraethoxysilane (TEOS) with the polyamic acid (PAA) and end-capped PAA solution. Samples were characterized by the means of differential thermogravimetry, X-ray diffractometry, scanning electron microscopy, universal test, impedance analyzer, chemical resistance test, etc. All of the PAA/silanol solutions heat-treated at 300$^{\circ}C$ for 6h were transformed to polyimide/silica composites. It has been demonstrated that the properties of polyimide/silica composites were affected by the amount of silica addition and the bend type existed between polyimide and silica.

Synthesis of $Zn(BH_4)_2$ powders by mechanochemical reaction and study of thermal decomposition behavior (기계 화학적 반응법을 이용한 $Zn(BH_4)_2$ 분말의 합성과 열분해 특성)

  • Jeon Eun;Jo Yeong Hwan
    • 한국전기화학회:학술대회논문집
    • /
    • 2005.07a
    • /
    • pp.373-378
    • /
    • 2005
  • [ $Zn(BH_4)_2$ ] ($8.4\;wt\%$ theoretical hydrogen storage capacity) powders have been successfully synthesized by mechanochemical reaction from mixtures of $ZnCl_2$ and $NaBH_4$ powders in a 1:2 molar ratio in different times. $$ZnCl_2\;+\;2NaBH_4\rightarrow\;Zn(BH_4)_2\;+\;2NaCl\;(1)$$ $Zn(BH_4)_2$ powders were characterized by X-ray diffractometry(XRD), and Furier Transform Infrared spectrometry(FT-IR). The thermal stabilities of $Zn(BH_4)_2$ powders were studied by Differential scanning calorimetry(DSC), Thermogravimetry analysis(TGA), and Mass spectrometry(MS). $Zn(BH_4)_2$ can be tested for hydrogen evolution without further purification. The reaction to yield hydrogen is irreversible, the other products being compounds of Zn, and borane. $Zn(BH_4)_2$ thermally decomposes to release borane and hydrogen gas between about 85 and $150^{\circ}C$.

  • PDF

Synthesis of Acrylic Pressure-Sensitive Adhesive by Emulsion Polymerization (유화중합에 의한 수성 아크릴계 접착제의 합성)

  • Kim, Dong-yeub
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.9 no.1
    • /
    • pp.45-50
    • /
    • 2006
  • In order to analyse the properties of the fiber-adhesive that was used as Flocking process we synthesized quaterpolymer with the variation of the types of monomer ratio by emulsion polymerization. We characterized the properties of this adhesive: Differential Scanning Calorimeter(DSC), Thermogravimetry Analysis(TGA), Raman spectroscopy. The polymer was synthesized by changing the using amount of 2-EHAM, and then we investigated the characteristics of glass transition temperature(Tg), melting temperature(Tm), thermal stability and hydroxyl group respectively. The optimum monomer composition was 36.84% EAM, 15.79% MAM, 42.1% 2-EHAM and 5.26% AAc.

  • PDF

The Effect of Composition on Hydrogen Reduction Behavior of Ball-milled WO3-CuO Nanocomposite Powders (볼밀링한 WO3-CuO 나노복합분말의 조성에 따른 수소환원 거동)

  • Jung Sung-Soo;Kang Yun-Sung;Lee Jai-Sung
    • Journal of Powder Materials
    • /
    • v.13 no.3 s.56
    • /
    • pp.205-210
    • /
    • 2006
  • The effect of Cu content on hydrogen reduction behavior of ball-milled $WO_3$-CuO nanocomposite powders was investigated. Hydrogen reduction behavior and reduction percent(${\alpha}$) of nanopowders were characterized by thermogravimetry (TG) and hygrometry measurements. Activation energy for hydrogen reduction of $WO_3$ nanopowders with different Cu content was calculated at each heating rate and reduction percent(${\alpha}$). The activation energy for reduction of $WO_3$ obtained in this study existed in the ranging from 129 to 139 kJ/mol, which was in accordance with the activation energy for $WO_3$ powder reduction of conventional micron-sized.