• Title/Summary/Keyword: tensile stress region

Search Result 202, Processing Time 0.032 seconds

Tensile Behavior Analyses of Tubular Column to H-Beam Connections with T-Stiffeners (외부 T 스티프너를 이용한 각형강관기둥-H 형강보 접합부의 인장거동 해석)

  • Shin, Kyung Jae;Kwon, Young Ran
    • Journal of Korean Society of Steel Construction
    • /
    • v.14 no.1
    • /
    • pp.69-78
    • /
    • 2002
  • This paper describes the analysis results for tensile behavior of tubular column to H-beam connection with T stiffeners. Using the elasto-plastic finite element method, analysis results are compare with experimental results. Parametric analyses with different size of T-stiffener have conducted to understand the stress distribution at the connections. Stress concentration in elastic region and PEEQ distribution in plastic region are plotted for different shape. The results of analysis were applied to design equations and were checked for the applicability of design equations.

A Study on the Microstructures and Tensile Properties of Heat-Treated Cast Ti-(44-54)at.%Al Alloys (Ti-(44-54)at.%Al 열처리 주조합금의 미세조직과 인장특성에 관한 연구)

  • Jung, Jae-Young
    • Journal of Korea Foundry Society
    • /
    • v.37 no.6
    • /
    • pp.199-206
    • /
    • 2017
  • In this study, the variations of microstructures and tensile properties of Ti-(44-54)at.%Al binary alloys were investigated. The heat-treated microstructure depended greatly on their solidification structure and annealing temperature. We measured the variations of volume fractions of primary and secondary lamellar structure as a function of the heat treatment temperature in a Ti-47at.%Al alloy. The variation of ductility as a function of Al content was in good agreement with the change of fracture mode in the tensile fracture surface. It can be inferred that the variations of yield stress and hardness of ${\gamma}$ phase in a single ${\gamma}$-phase field region are enhanced by anti-site defects created by deviations from the stoichiometric composition. In a Ti-47at.%Al alloy within the (${\alpha}_2+{\gamma}$) two-phase field, the yield stress tended to be the maximum at a near equal volume fraction of lamellar and ${\gamma}$ grains. The ductility depended sensitively on the overall grain size and Al content. The calculation of fracture strain using Chan's model indicated that the change of ductility as a function of annealing temperature was primarily determined by the variations in the overall grain size and lamellar volume fraction.

Fatigue Strength of Al-5052 Tensile-Shear Specimens using a SPR Joining Method (SPR 접합법을 이용한 Al-5052 인장-전단 시험편의 피로강도)

  • Lee, Man Suk;Kim, Taek Young;Kang, Se Hyung;Kim, Ho Kyung
    • Journal of the Korean Society of Safety
    • /
    • v.29 no.4
    • /
    • pp.9-14
    • /
    • 2014
  • Self-piercing riveting(SPR) is a mechanical fastening technique which is put pressure on the rivet for joining the sheets. Unlike a spot welding, SPR joining does not make the harmful gas and $CO_2$ and needs less energy consumption. In this study, static and fatigue tests were conducted using tensile-shear specimens with Al-5052 plates for evaluation of fatigue strength of the SPR joints. During SPR joining process for the specimen, using the current sheet thickness and a rivet, the optimal applied punching force was found to be 21 kN. And, the maximum static strength of the specimen produced at the optimal punching force was 3430 N. During the fatigue tests for the specimens, interface failure mode occurred on the top substrate close to the rivet head in the most high-loading range region, but on the bottom substrate close to the rivet tail in the low -loading range region. There was a relationship between applied load amplitude $P_{amp}$ and lifetime of cycle N for the tensile-shear, $P_{amp}=3395.5{\times}N^{-0.078}$. Using the stress-strain curve of the Al-5052 from tensile test, the simulations for fatigue specimens have been carried out using the implicit finite element code ABAQUS. The relation between von-Mises equivalent stress amplitude and number of cycles was found to be ${\sigma}_{eq}=514.7{\times}N^{-0.033}$.

Fabrication of Graded-Boundary Ni/Steel Material by Laser Beam (레이저빔에 의한 조성구배계면 Ni/Steel 재료의 제조)

  • 안재모;김도훈
    • Laser Solutions
    • /
    • v.2 no.1
    • /
    • pp.22-29
    • /
    • 1999
  • This work was carried out as a fundamental experiment to fabricate a Graded-Boundary Ni/Steel material using a laser beam. A Ni sheet was placed on a steel substrate, and then a series of high power $CO_2$ laser beams were irradiated on the surface in order to produce a homogeneous alloyed layer. The processing parameters were : 4 ㎾ laser power, 2m/min traverse speeds, -2mm defocuing, 17 l/min sheiding gas flow rates. The sequential repetition of the laser surface alloying treatment up to 4 times, resulted in about 5mm thick of fair compositional gradient systems. In order to determine the microstructure, phase and compositional profiles in this material, optical microscopy, XRD and EDS were used. The compositions varied from 66% to 0% for Ni and 34% to 100% for Fe in this material The microstructures were typical morphologies of rapid solidification and solid-state cooling. Since compressive stress was formed in the heat affected region due to martensitic transformation, while relative tensile stress was developed in the alloyed region, cracks were formed between the alloyed region and the substrate region.

  • PDF

Effect of Process Parameters on the Residual Stress Distribution in p+ Films (공정변수가 p+ 박막의 잔류응력 분포에 미치는 영향)

  • Yang, E.H.;Yang, S.S.
    • Proceedings of the KIEE Conference
    • /
    • 1995.07c
    • /
    • pp.1437-1439
    • /
    • 1995
  • This paper investigates the effect of thermal oxidation on the profile of the residual stress along the depth of p+ silicon films by quantitative determination method. Two examples for the application of this method illustrate that most of p+ region is subjected to the tensile stress except the region near the front surface and that the stress gradient of the film oxidized at $1100^{\circ}C$ is more steep than that of the film oxidized at $1000^{\circ}C$.

  • PDF

A Study on Tensile Behavior of Transparent Polycarbonate (PC) Plate in the High Temperature (투명 폴리카보네이트 판재의 고온 인장 거동에 관한 연구)

  • Lee, Ho Jin;Ahn, Dong-Gyu
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.31 no.1
    • /
    • pp.21-28
    • /
    • 2014
  • Recently, several researchers made their endeavor to manufacture the photobioreactor(PBR) with characteristic shapes form vacuum and blow forming process. Hence, behaviors of the transparent polycarbonate(PC) plate in the high temperature region should be examined to obtain the desired PBR case via vacuum and blow forming processes. The aim of this paper is to investigate tensile behavior of PC plate in the high temperature. Various tensile tests were performed using high temperature tensile testing machine. The influence of tensile speed, thickness and ambient temperature on tensile behavior in the high temperature was examined. The flow stress and tensile strength augmented when the tensile speed increased. In order to obtain proper flow curves with strain rate effects for different temperature of specimen, G'sell-Jonas model was adopted. The material constants of the G'sell-Jonas model were estimated. The flow curves of the PC plate considering the tensile speed, specimen thickness and temperature were obtained.

Stress Analysis of Steam Generator Row-1 Tubes (증기발생기 제1열 전열관의 응력 해석)

  • Kim, Woo-Gon;Ryu, Woo-Seog;Lee, Ho-Jin;Kim, Sung-Chung
    • Proceedings of the KSME Conference
    • /
    • 2000.04a
    • /
    • pp.25-30
    • /
    • 2000
  • Residual stresses induced in U-bending and tube-to-tubesheet joining processes of PWR's steam generator row-1 tube were measured by X-ray method and Hole-Drilling Method(HDM). The stresses resulting from the Internal pressure and the temperature gradient in the steam generator were also estimated theoretically. In U-bent lesions, the residual stresses at extrados were induced with compressive stress(-), and its maximum value reached -319 MPa in axial direction at ${\psi}=0^{\circ}$ in position. Maximum tensile residual stress of 170MPa was found to be at the flank side at Position of${\psi}=90^{\circ}$, i.e., at apex region. In tube-to-tubesheet fouling methods, the residual stresses induced by the explosive joint method were found to be lower than that by the mechanical roll method. The gradient of residual stress along the expanded tube was highest at the. transition region, and the residual stress in circumferential direction was found to be higher than the residual stress in axial direction. Hoop stress due to an internal pressure between primary and secondary side was analyzed to be 76 MPa and thermal stress was 45 MPa.

  • PDF

Influence of ITO Thickness on the Deformation and Cracking Behaviors of ITO/PET Sheets (ITO층의 두께에 따른 ITO/PET sheet의 변형거동 및 균열 형성 거동)

  • Kim, Jin-Yeol;Hong, Sun-Ig
    • Korean Journal of Materials Research
    • /
    • v.19 no.1
    • /
    • pp.1-6
    • /
    • 2009
  • In this study, the stress-strain response and the cracking behaviors of ITO film on a PET substrate are investigated. The cracking behaviors of ITO thin films deposited on a thermoplastic semi-crystalline polymer developed for flexible display applications was investigated by means of tensile experiments equipped with an electrical measurement apparatus and an in-situ optical microscope. Electrical resistance increased gradually in the elastic-to-plastic transition region of the stress strain curves and cracks formed. Numerous cracks were found in this region, and the increase of the resistance was linked to the cracking of ITO thin films. Upon loading, the initial cracks perpendicular to the tensile axis were observed at about 1% of the total strain. They propagated to the entire sample width as the strain increased. The spacing between the horizontal cracks is thought to be determined by the fracture strength and the thickness of the ITO film as well as by the interfacial strength between the ITO and PET. The effect of the strain rate on the cracking behavior was also investigated. The crack density increased as the strain increased. The spacing between the horizontal cracks (perpendicular to the stress axis) increased as the strain rate decreased. The increase of the crack density as the strain rate decreased can be attributed to the higher fraction of the plastic strain to the total strain at a given total strain. The higher critical strain for the onset of the increase in the resistance and the crack initiation of the ITO/PET with a thinner ITO film (300 ohms/sq.) suggests a higher strength of the thinner ITO film.

Variation in the Residual Stress of Hastelloy X Superalloy Fabricated by the Laser Powder Bed Fusion Process with Sample Thickness and Support Structure (레이저 분말 베드 용융법으로 제작된 Hastelloy X 적층 소재의 시편 두께 및 서포트 구조에 따른 잔류응력 변화)

  • Jang, J. E.;Park, S. H.;Kim, D. H.
    • Transactions of Materials Processing
    • /
    • v.31 no.3
    • /
    • pp.136-142
    • /
    • 2022
  • The purpose of this study was to investigate the effects of sample thickness and support structure on the residual stress of Hastelloy X superalloy samples fabricated by laser powder bed fusion (LPBF), which is an additive manufacturing process. The residual stresses of LPBF samples with different thicknesses and support structures were measured using X-ray diffraction. The results revealed that as the thickness of sample increased from 2.5 mm to 20 mm, its tensile residual stress gradually decreased from 443.5 MPa to 182.2 MPa. Additionally, the residual stress in the bottom region of sample was higher than that in the top region, and the residual stress difference in the bottom and top regions became more pronounced as the sample thickness decreased. The residual stress of LPBF sample also varied depending on the structure of support. The residual stress of sample decreased with increasing contract area between the sample and the support, because the larger contract area led to smaller temperature gradient throughout the sample.

Crystallization behavior of Cu-base bulk metallic glass in supercooled liquid region during compression and tension (과냉각 액상구간에서 압축.인장시 Cu기 비정질 합금의 결정화 거동)

  • Park, E.S.;Kim, S.H.;Huh, M.Y.;Kim, H.W.;Bae, J.C.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.10a
    • /
    • pp.215-217
    • /
    • 2008
  • Crystallization behavior of the bulk metallic glass (BMG) during compression and tension was studied in the supercooled liquid region (SLR). Rod samples of the BMG alloy were produced by consolidating gas atomized powders of $Cu_{54}Zr_{22}Ti_{18}Ni_6$ using spark plasma sintering. The crystallization behavior in these samples was examined by tackling changes in thermal property during heating the samples in DSC. The present BMG alloy was firstly decomposed and then crystallized during annealing in the SLR. The phase decomposition from the original amorphous phase was retarded by the compressive stress, while it was accelerated by the tensile stress.

  • PDF