High Temperature Tensile Properties of Heat-resistant Cast Ferritic Stainless Steels (고내열 페라이트계 스테인레스 주강의 고온인장특성 평가)

  • Jeong, Hyeon Kyeong;Lee, Dong-Geun
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.34 no.1
    • /
    • pp.10-16
    • /
    • 2021
  • Exhaust manifold is a very important component that is directly connected to air environment pollution and that requires strict mechanical properties such as high temperature fatigue and oxidation. Among stainless steels, the ferritic stainless steel with body-centered cubic structure shows excellent resistance of stress-corrosion cracking, ferromagnetic at room temperature, very excellent cold workability and may not be enhanced by heat treatment. The microstructural characteristics of four cast ferritic stainless steels which are high heat-resistant materials, were analyzed. By comparing and evaluating the mechanical properties at room temperature and high temperature in a range of 400℃~800℃, a database was established to control and predict the required properties and the mechanical properties of the final product. The precipitates of cast ferritic stainless steels were analyzed and the high-temperature deformation characteristics were evaluated by comparative analysis of hardness and tensile characteristics of four steels at room temperature and from 400℃ to 800℃.

Evaluation of fiberization of rice hull by autohydrolysis conditons (자기가수분해 조건에 따른 농산부산물 왕겨의 섬유화 특성 평가)

  • Lee, Young-Ju;Jung, Woong-Ki;Sung, Yong-Joo
    • Korean Journal of Agricultural Science
    • /
    • v.38 no.1
    • /
    • pp.95-100
    • /
    • 2011
  • In the present study, effects of autohydrolysis treatment on the properties of rice hull were investigated. Two temperature condition such as $160^{\circ}C$ and $180^{\circ}C$ and thee treatment time such as 15 min, 30 min and 45 min were applied for autohydrolysis treatment. The pH of extract after autohydrolysis treatment decreased as increasing of the temperature and the treatment time. The ash content and the lignin content of rice hull were not decreased by the autohydrolysis treatment. The structure of rice hull after autohydrolysis treatment became more weak, the better efficiency of the fiberization with PFI-Mill was shown for the autohydrolysis treated rice hull with the higher temperature and the longer treatment time.

Improving the Dimensional Stability of Spruce and Birch Boards by Heat-Treatment at 190 and $210^{\circ}C$

  • Kang, Ho-Yang
    • Journal of the Korea Furniture Society
    • /
    • v.20 no.6
    • /
    • pp.560-565
    • /
    • 2009
  • It is known that heat treatment decreases the hygroscopicity of wood. Thus heat-treated wood is good for outdoor construction due to its improved dimensional stability. This study is to investigate the hygroscopicity and discoloration of spruce and birch boards heat-treated above $190^{\circ}C$. The equilibrium moisture contents (EMCs) at all relative humidities decreased with the increase of heat treatment temperature and/or time for both spruce and birch. It was revealed that heat-treatment temperature affected more on the hygroscopicity thaan heat-treatment time. The average basic densities decreased for the spruce specimens, but increased for the birch specimens with an increase of the treatment time and/or temperature. The same heat treatment condition (190-8) made the birch specimens darker than the spruce specimens.

  • PDF

Effect of Subzero Treatment on the Mechanical Properties and Damping Capacity of Austempered Ductile Cast Ironn (오스템퍼드 구상흑연주철의 기계적 성질 및 감쇠능에 미치는 서브제로처리의 영향)

  • Lee, K.H.;Kwon, M.K.;Kim, C.G.;Kang, C.Y.
    • Journal of Power System Engineering
    • /
    • v.11 no.4
    • /
    • pp.86-91
    • /
    • 2007
  • This study was investigated to know the effect of subzero treatment in austempered ductile cast iron. Retained austenite transformed to martensite by subzero treatment. With decreasing subzero treatment temperature, more volume fraction of retained austenite transformed to martensite and transformed to martensite above 30% by subzero treatment temperature at $-196^{\circ}C$. With decreasing subzero treatment temperature, the value of strength and hardness increased but the value of elongation and impact value decreased. In case of subzero treatment at $-196^{\circ}C$, hardness value increased about 18% and impact value decreased by above 20%. We could find that subzero treated specimens had a little of effect on the tensile properties but had very much effect on the hardness and value of the impact.

  • PDF

Effect of Temperature and Pre-treatment for Elutriated Acidogenic Fermentation of Piggery Waste (돈사폐수의 세정산발효시 온도와 전처리의 영향)

  • Bae, Jin-Yeon;Min, Kyung-Sok
    • Journal of Korean Society on Water Environment
    • /
    • v.21 no.1
    • /
    • pp.34-39
    • /
    • 2005
  • The performance of elutriated acid fermentation with slurry-type piggery waste was investigated, especially to evaluate the effects of temperature and pre-treatment. In the first phase, the acid elutriation reactor with piggery waste after centrifugation operated at both mesophilic and thermophilic conditions to evaluate the effect of temperature. Solubilization yield($gVFAs/gSCOD_{prod.}$) and acidification rate($gVFAs/gSCOD_{prod.}$) in the thermophilic digestion were 0.45 and 0.55, which were higher than those of the mesophilic digestion, 0.25 and 0.45. In addition, the acid elutriation reactor at thermophilic temperature is more effective in removing e-coli. In the second phase, the acid elutriation reactor was fed with piggery waste before centrifugation. With piggery wastes before centrifugation, the solubilization yield and the acidificaton rate were 0.40 and 0.80, respectively, which were higher than the rates using piggery waste after centrifugation at both mesophilic and thermophilic conditions. The higher sludge volume reduction of 80% benefits sludge management. Furthermore, economical advantages can be achieved by removing the pre-treatment process, such as centrifugation. Consequently, the treatment with piggery waste before centrifugation proved to be effective. Also, the optimum temperature condition was estimated at mesophilic or thermophilic conditions, considering solubilization yields and acidification rates, though the system should be heated.

Dielectric Properties of SCT Ceramics with the Sintering Temperature and the Thermal Treatment Time (소결온도와 열처리시간에 따른 SCT 세라믹스의 유전특성)

  • Gang, Jae-Hun;Choe, Un-Sik
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.50 no.11
    • /
    • pp.539-543
    • /
    • 2001
  • ln this paper, the $Sr_{l-x}Ca_xTiO_3(0\leqx\leq0.2)-based$ grain boundary layer ceramics were fabricated to measure dielectric properties with the sintering temperature and the thermal treatment time. The sintering temperature and time were $1420~15206{\circ}C$, 4hours, and the thermal treatment temperature and time of the specimen were $l150^{\circ}C$, 1, 2, 3hours, respectively. The structural and the dielectric properties were investigated by SEM, X-ray, HP4194A and K6517. The average grain size was increased with increasing the sintering temperature, but it decreased up to 15mo1% with increasing content of Ca. X-ray diffraction analysis results showed that all specimens were the cubic structure, and the main peaks were moved to right and the lattice constant were decreased with increasing content of Ca. The appropriate thermal treatment time and temperature of CuO to obtain dielectric properties of $\varepsilon_r>50000,\; tan \delta<0.05\; and \;\DeltaC<\pm10%$ were 2hrs and $l150^{\circ}C$, respectively.

  • PDF

Low Temperature Tensile Properties of High Temperature Gas-nitrided Duplex Stainless Steel

  • On, Han-Yong;Kong, Jung-Hyun;Kim, Mi-Jeong;Park, Sang-Joon;Kang, Chang-Yong;Sung, Jang-Hyun
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.23 no.5
    • /
    • pp.263-268
    • /
    • 2010
  • This investigation was focused on the low temperature tensile properties, phase change, changes in nitrogen content and corrosion resistance in the 22Cr-5Ni-3Mo duplex stainless steel after high temperature gas nitriding and solution annealing (HTGN-SA). From the HTGN-SA treatment, the duplex (ferrite + austenite) phase changed into austenite single phase. The nitrogen content of austenite single-phase steel showed a value of ~0.54%. For the HTGN-SA treated austenitic steel, tensile strength increased with lowering test temperature, on the other hand elongation showed the maximum value of 28.2% at $-100^{\circ}C$. The strain-induced martensitic transformation gave rise to lead the maximum elongation. After HTGN-SA treatment, corrosion resistance of the austenite single-phase steel increased remarkably compared with HTGN- treated steel.

Role of Phytoecdysteroid Treatment Time in the Maturation Process of $Multi{\times}Bivoltine$ ($BL67{\times}CSR101$) Hybrid Silkworm, Bombyx mori L. When Maintained at Low, Medium and High Temperature

  • Kumar S. Nirmal;Nair K. Sashindran;Rabha Jagat
    • International Journal of Industrial Entomology and Biomaterials
    • /
    • v.12 no.2
    • /
    • pp.51-56
    • /
    • 2006
  • Use of products containing phytoecdysteroid (PE) as active principle has become popular in prominent sericultural areas of India for hastening larval maturation events and synchronizing cocoon spinning activities as an obvious advantage is assured. At times, the present recommendation of administering PE at the onset of spinning results in peak labour requirement at odd hrs. To enable making recommendation for the use of PE on $multi{\times}bivoltine$ silkworm hybrids based on the climatic conditions prevailing in different areas especially with regard to temperature, the experiment was taken up to determine proper treatment times so that the induced spinning will be more orderly and the labour can be leveraged more efficiently. Different brackets of low ($18-22^{\circ}C$), medium ($24-28^{\circ}C$) and high ($29-32^{\circ}C$) temperature were simulated during the latter half of V larval instar and cocoon spinning. PE was administered to $multi{\times}bivoltine$ silkworm ($BL67{\times}CSR101$) hybrid batches as per the recommended dose at three different times viz., 10 am, 4 pm and 10 pm. Three replicates of 100 larvae were maintained for each treatment. Absolute controls were also maintained in each temperature range to compare the results. Cumulative maturation percentage was recorded at 6 hrs interval to ascertain peak mounting span. The influence of the treatment on the cocoon traits also was studied. Based on the peak mounting span, it was evident that in low temperature 10 pm treatment would be better. In medium and high temperature, treatment at 4 pm proved to be a better option. The influence of the treatment times at different temperature range on labour management is discussed.

Effect of Heat-treatment on Microstructure and Tensile Properties in Cast Alloy 718 (주조 합금 Alloy 718에서 미세조직과 인장특성에 미치는 열처리의 영향)

  • Do, Jeong-Hyeon;Kim, In-Soo;Choi, Baig-Gyu;Jung, Joong-Eun;Jung, In-Yong;Jo, Chang-Yong
    • Journal of Korea Foundry Society
    • /
    • v.36 no.5
    • /
    • pp.167-173
    • /
    • 2016
  • The effect of various types of heat-treatment on the mechanical properties of cast Alloy 718 has been investigated. Cast Alloy 718 bars were subjected to 'standard heat-treatment'_(SHT), 'HIP (Hot Isostatic Pressing) heat-treatment'_(HHT), and 'HIP-simulated heat-treatment'_(HS). In the absence of long time high temperature heat-treatment, a small amount of Laves phase remained in the 'SHT' specimen, and needle shaped ${\delta}$ precipitated in the vicinity of the Laves phase. Due to the formation of the Laves and ${\delta}$ phases in the 'SHT' specimen, it exhibited lower tensile properties than those of the others_specimens. On the other hand, the Laves phase was completely dissolved into the matrix after 'HHT' and 'HS' treatments. It is known that isostatic pressure reduces the self-diffusion coefficient, because of the lower self-diffusivity under HIP conditions in the interdendritic region, Nb segregation and the high amount of ${\gamma}^{{\prime}{\prime}}$ precipitation that occurs. Due to the higher fraction of coarse ${\gamma}^{{\prime}{\prime}}$ phases, the 'HHT' treated Alloy 718 showed excellent tensile strength.

Effect of Passive Temperature Therapy of the Femoral Muscles on the Countermovement Jump Performance

  • Lee, Jintaek;Panday, Siddhartha Bikram;Byun, Kyungseok;Lee, Jusung;Hwang, Jinny;Moon, Jeheon
    • Korean Journal of Applied Biomechanics
    • /
    • v.29 no.4
    • /
    • pp.227-235
    • /
    • 2019
  • Objective: The purpose of this study was to evaluate the effect of passive-acute temperature therapy of the femoral muscle and dynamic warm-up on the countermovement jump performance. Method: Twenty male track and field athletes from national team underwent three treatments applied on the femoral muscles; cold temperature treatment, thermal treatment and dynamic warm-up. The variables extracted at 2 time points (pre-measurement and post measurement) were the temperature of the left and right femoral muscle, displacement & velocity of centre of mass, peak power out, range of motion and moment & power of the knee joint. Results: There was a statistically significant difference in the temperature of the femoral muscle according to measurement time which was high in the order of thermal treatment, dynamic treatment and cold treatment. The jump height was the highest in the dynamic warm-up with no statistically significant difference for the range of motion of the knee joint. The peak power out at dynamic warm-up and the power of the knee joint were statistically significant according to the treatment and measurement time. Conclusion: Local cold and thermal treatment of femoral muscles at ambient temperature did not improve jump performance, while dynamic warm-up was considered to be effective for maintaining the performance of the activities that require strong muscular power.