Corrosion of Fe-Cr Steels at 600-800℃ in NaCl Salts

  • Lee, Dong Bok;Kim, Min Jung;Yadav, Poonam;Xiao, Xiao
    • Journal of the Korean institute of surface engineering
    • /
    • v.51 no.6
    • /
    • pp.354-359
    • /
    • 2018
  • NaCl-induced hot corrosion behavior of ASTM T22 (Fe-2.25Cr-1Mo), T91 (Fe-9Cr-1Mo), T92 (Fe-9Cr-1.8W-0.5Mo), 347HFG (Fe-18-Cr-11Ni), and 310H (Fe-25Cr-19Ni) steels was studied after spraying NaCl on the surface. During corrosion at $600-800^{\circ}C$ for 50-100 h, thick, non-adherent, fragile, somewhat porous oxide scales formed. All the alloys corroded fast with large weight gains owing to fast scaling and destruction of protective oxide scales. Corrosion rates increased progressively as the corrosion temperature and time increased. Corrosion resistance increased in the order of T22, T91, T92, 347HFG, and 310H, suggesting that the alloying elements of Cr, Ni, and W beneficially improved the corrosion resistance of steels. Basically, Fe oxidized to $Fe_2O_3$, and Cr oxidized to $Cr_2O_3$, some of which further reacted with FeO to form $FeCr_2O_4$ or with NiO to form $NiCr_2O_4$.

Investigation of Electronic Structures of TCr2O4 (T = Fe, Co, Ni) Spinel Oxides by Employing Soft X ray Synchrotron Radiation Spectroscopy (연 X선 방사광 분광법을 이용한 TCr2O4(T = Fe, Co, Ni) 스피넬 산화물의 전자구조 연구)

  • Kim, Hyun Woo;Hwang, Jihoon;Kim, D.H.;Lee, Eunsook;Kang, J.S.
    • Journal of the Korean Magnetics Society
    • /
    • v.23 no.5
    • /
    • pp.149-153
    • /
    • 2013
  • The electronic structures of $TCr_2O_4$ (T = Fe, Co, Ni) spinel oxides have been investigated by employing synchrotron radiation-based soft X ray absorption spectroscopy (XAS). The measured 2p XAS spectra of transition-metal ions reveal that Cr ions are trivalent ($Cr^{3+}$), and all the T (T = Fe, Co, Ni) ions are divalent ($Fe^{2+}$, $Co^{2+}$, $Ni^{2+}$). It is also found that most of T (T = Fe, Co, Ni) ions occupy the A sites under the tetrahedral symmetry, while Cr ions occupy mainly the B sites under the octahedral symmetry. These findings show that the structures of $TCr_2O_4$ (T = Fe, Co, Ni) are very close to the normal spinel structures. Based on these findings, it is expected that Jahn-Teller (JT) effects are important in $FeCr_2O_4$ and $NiCr_2O_4$. In contrast, $CoCr_2O_4$ maintains the cubic structure without having the JT distortion since both $Cr^{3+}$ and $Co^{2+}$ ions are non-JT ions. This work suggests that the antiferromagnetic interaction between $Cr^{3+}$ and $T^{2+}$ ions plays an important role in determining the magnetic properties of $TCr_2O_4$ (T = Fe, Co, Ni).

Dielectric and Piezoelectric Characteristics of PSS-PZT Piezoelectric Ceramics with CrS12TOS13t Addition (Cr2O3 첨가에 따른 PSS-PZT 압전 세라믹스의 유전 및 압전 특성)

  • 홍재일;이개명;윤석진;유주현;박창엽
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.41 no.6
    • /
    • pp.687-693
    • /
    • 1992
  • To improve dielectric, piezoelectric and temperature stability in 0.50Pb(SnS11/2TSbS11/2T)OS13T - 0.35PbTiOS13T - 0.60PbZrOS13T + 0.4[wt%]MnOS12T piezoelectric ceramics which is used for surface acoustic wave devices, CrS12TOS13T was added and the specimens were fabricated by Hot Press method, and their characteristics were measured with CrS12TOS13T addition. From the results, in the specimen added by 0.2[wt%]CrS12TOS13T, dielectric constant and mechanical quality factor were 380 and 2307, respectively, and it was suited for surface acoustic wave device and the temperature coefficient of the resonant frequency in the specimen added by 0.4[wt%]CrS12TOS13T was the least value of 74.96[ppm/$^{\circ}C$].

Effects of $Cr_2O_3$ Addition in PSS-PZT Piezoelectric Ceramics for Surface Acoustic Wave Filter ($Cr_2O_3$가 탄성 표면파 필터용 PSS-PZT계 압전 세라믹스에 미치는 영향)

  • 홍재일;손은영;박창엽
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.41 no.5
    • /
    • pp.502-507
    • /
    • 1992
  • To improve temperature stability, 0.05Pb(SnS11/2TSbS11/2T)OS13T-0.35PbTiOS13T-0.60PbZrOS13T+0.4[wt%]MnO S12T piezoelectic ceramics were manufactured with the addition of CrS12TOS13T by Hot Press method. And the SAW delay line was fabricated and effects of CrS12TOS13T to the propagation characteristics of SAW was investigated, and the SAW filter was fabricated on C4 specimen added by 0.2[wt%] CrS12TOS13T whose propagation characteriatics of surface acoustic wave were the bast and its frequency characteristics was investigated. Electromechancal coupling factor(kS1sTS02T) was 3.11[%] and its temperature coefficient of the center frequency(CS1foT)was -21.27[ppm/$^{\circ}C$] in C4. The 31[MHz]]SAW IF filter of C4 scarcely had diffraction phenomena and therefore it was proper.

  • PDF

How to Combine Diffusion-Weighted and T2-Weighted Imaging for MRI Assessment of Pathologic Complete Response to Neoadjuvant Chemoradiotherapy in Patients with Rectal Cancer?

  • Jong Keon Jang;Chul-min Lee;Seong Ho Park;Jong Hoon Kim;Jihun Kim;Seok-Byung Lim;Chang Sik Yu;Jin Cheon Kim
    • Korean Journal of Radiology
    • /
    • v.22 no.9
    • /
    • pp.1451-1461
    • /
    • 2021
  • Objective: Adequate methods of combining T2-weighted imaging (T2WI) and diffusion-weighted imaging (DWI) to assess complete response (CR) to chemoradiotherapy (CRT) for rectal cancer are obscure. We aimed to determine an algorithm for combining T2WI and DWI to optimally suggest CR on MRI using visual assessment. Materials and Methods: We included 376 patients (male:female, 256:120; mean age ± standard deviation, 59.7 ± 11.1 years) who had undergone long-course CRT for rectal cancer and both pre- and post-CRT high-resolution rectal MRI during 2017-2018. Two experienced radiologists independently evaluated whether a tumor signal was absent, representing CR, on both post-CRT T2WI and DWI, and whether the pre-treatment DWI showed homogeneous hyperintensity throughout the lesion. Algorithms for combining T2WI and DWI were as follows: 'AND,' if both showed CR; 'OR,' if any one showed CR; and 'conditional OR,' if T2WI showed CR or DWI showed CR after the pre-treatment DWI showed homogeneous hyperintensity. Their efficacies for diagnosing pathologic CR (pCR) were determined in comparison with T2WI alone. Results: Sixty-nine patients (18.4%) had pCR. AND had a lower sensitivity without statistical significance (vs. 62.3% [43/69]; 59.4% [41/69], p = 0.500) and a significantly higher specificity (vs. 87.0% [267/307]; 90.2% [277/307], p = 0.002) than those of T2WI. Both OR and conditional OR combinations resulted in a large increase in sensitivity (vs. 62.3% [43/69]; 81.2% [56/69], p < 0.001; and 73.9% [51/69], p = 0.008, respectively) and a large decrease in specificity (vs. 87.0% [267/307]; 57.0% [175/307], p < 0.001; and 69.1% [212/307], p < 0.001, respectively) as compared with T2WI, ultimately creating additional false interpretations of CR more frequently than additional identification of patients with pCR. Conclusion: AND combination of T2WI and DWI is an appropriate strategy for suggesting CR using visual assessment of MRI after CRT for rectal cancer.

Microstructure and Liquid Al Erosion Property of Tribaloy T-800 Coating Material Manufactured by Laser Cladding Process (Laser Cladding 공정으로 제조된 Tribaloy T-800 코팅 소재의 미세조직 및 용융 Al 침식 특성)

  • Kim, Kyoung-Wook;Ham, Gi-Su;Park, Sun-Hong;Lee, Kee-Ahn
    • Journal of Powder Materials
    • /
    • v.27 no.3
    • /
    • pp.210-218
    • /
    • 2020
  • A T-800 (Co-Mo-Cr) coating material is fabricated using Co-Mo-Cr powder feedstock and laser cladding. The microstructure and melted Al erosion properties of the laser-cladded T-800 coating material are investigated. The Al erosion properties of the HVOF-sprayed MoB-CoCr and bulk T-800 material are also examined and compared with the laser-cladded T-800 coating material. Co and lave phases (Co2MoCr and Co3Mo2Si) are detected in both the laser-cladded T-800 coating and the bulk T-800 materials. However, the sizes of the lave phases are measured as 7.9 ㎛ and 60.6 ㎛ for the laser-cladded and bulk T-800 materials, respectively. After the Al erosion tests, the erosion layer thicknesses of the three materials are measured as 91.50 ㎛ (HVOF MoB-CoCr coating), 204.83 ㎛ (laser cladded T-800), and 226.33 ㎛ (bulk T-800). In the HVOF MoB-CoCr coating material, coarse cracks and delamination of the coating layer are observed. On the other hand, no cracks or local delamination of the coating layer are detected in the laser T-800 material even after the Al erosion test. Based on the above results, the authors discuss the appropriate material and process that could replace conventional bulk T-800 materials used as molten Al pots.

GENERALIZED CR-SUBMANIFOLDS OF A T-MANIFOLD

  • De, U.C.;Matsuyama, Y.;Sengupta, Anup-Kumar
    • The Pure and Applied Mathematics
    • /
    • v.11 no.3
    • /
    • pp.175-187
    • /
    • 2004
  • The purpose of the present paper is to study the generalized CR-sub manifold of a T-manifold. After preliminaries we have studied the integrability of the distributions and obtained the conditions for integrability. Then geometry of leaves are being studied. Finally it is proved that every totally umbilical generalized CR-submanifold of a T-manifold is totally geodesic.

  • PDF

Interpretation of Complete Tumor Response on MRI Following Chemoradiotherapy of Rectal Cancer: Inter-Reader Agreement and Associated Factors in Multi-Center Clinical Practice

  • Hae Young Kim;Seung Hyun Cho;Jong Keon Jang;Bohyun Kim;Chul-min Lee;Joon Seok Lim;Sung Kyoung Moon;Soon Nam Oh;Nieun Seo;Seong Ho Park
    • Korean Journal of Radiology
    • /
    • v.25 no.4
    • /
    • pp.351-362
    • /
    • 2024
  • Objective: To measure inter-reader agreement and identify associated factors in interpreting complete response (CR) on magnetic resonance imaging (MRI) following chemoradiotherapy (CRT) for rectal cancer. Materials and Methods: This retrospective study involved 10 readers from seven hospitals with experience of 80-10210 cases, and 149 patients who underwent surgery after CRT for rectal cancer. Using MRI-based tumor regression grading (mrTRG) and methods employed in daily practice, the readers independently assessed mrTRG, CR on T2-weighted images (T2WI) denoted as mrCRT2W, and CR on all images including diffusion-weighted images (DWI) denoted as mrCRoverall. The readers described their interpretation patterns and how they utilized DWI. Inter-reader agreement was measured using multi-rater kappa, and associated factors were analyzed using multivariable regression. Correlation between sensitivity and specificity of each reader was analyzed using Spearman coefficient. Results: The mrCRT2W and mrCRoverall rates varied widely among the readers, ranging 18.8%-40.3% and 18.1%-34.9%, respectively. Nine readers used DWI as a supplement sequence, which modified interpretations on T2WI in 2.7% of cases (36/1341 [149 patients × 9 readers]) and mostly (33/36) changed mrCRT2W to non-mrCRoverall. The kappa values for mrTRG, mrCRT2W, and mrCRoverall were 0.56 (95% confidence interval: 0.49, 0.62), 0.55 (0.52, 0.57), and 0.54 (0.51, 0.57), respectively. No use of rectal gel, larger initial tumor size, and higher initial cT stage exhibited significant association with a higher interreader agreement for assessing mrCRoverall (P ≤ 0.042). Strong negative correlations were observed between the sensitivity and specificity of individual readers (coefficient, -0.718 to -0.963; P ≤ 0.019). Conclusion: Inter-reader agreement was moderate for assessing CR on post-CRT MRI. Readers' varying standards on MRI interpretation (i.e., threshold effect), along with the use of rectal gel, initial tumor size, and initial cT stage, were significant factors associated with inter-reader agreement.

Effects of Deposition Conditions on Magnetic Properties of SmCo/Cr (스퍼터 제조조건에 따르는 SmCo/Cr 박막의 자기적 특성에 관한 연구)

  • 나태준;고광식;이성래
    • Journal of the Korean Magnetics Society
    • /
    • v.9 no.6
    • /
    • pp.312-320
    • /
    • 1999
  • Effect of deposition conditions on the magnetic properties of SmCo/Cr prepared by a RF magnetron sputtering method was studied. We obtained the maximum coercivity of 3.2 kOe in the sample of Cr(50 nm)/SmCo(40 nm, 50W, 20 mT)/Cr(150 nm, 100 W, 30 mT). The coercivity of the SmCo/Cr depends largely on the roughness of the Cr underlayer and the composition of SmCo. The roughness of the Cr underlayer increased with increasing the Ar pressure and thickness, and promoted the isolation of SmCo grains which resulted in an enhanced coercivity. The composition of the SmCo was changed with RF power and Ar pressure due to the mass difference between Sm and Co and the resputtering phenomena. The maximum coercivity was obtained in the composition of about 20 at.% Sm. The mechanism of magnetization reversal of the present SmCo films changed from domain wall motion to domain rotation as the RF power and the Ar pressure increase. This was though to be due to the defects, such as the roughness of Cr surface, porous column boundaries etc., which inhibit domain wall movement.