• Title/Summary/Keyword: superconducting powder

Search Result 177, Processing Time 0.024 seconds

Fabrication of $YBa_2Cu_3O_{7-{\delta}}$ Superconducting Coils with Polymer Binder (유기물 바인더를 사용한 $YBa_2Cu_3O_{7-{\delta}}$ 초전도 Coil의 제조)

  • 정해원;박승만;김재묵;김성수
    • Journal of the Korean Ceramic Society
    • /
    • v.27 no.3
    • /
    • pp.355-360
    • /
    • 1990
  • One of the possible ways to make a flexible wire of high-Tc superconductiong ceramics is the extrusion of a mixture slurry of superconducting powder with an appropriate polymer binder. The fabrication procedure for $YBa_2Cu_3O_{7-{\delta}}$ superconducting coils with this plastic mass is described. The major factors limiting the formation of extruded wire are the binder content, powder size, and entrapped gas in the mixture slurries. The optimum content of binder for both good flexbility and strength of wire was estimated to be 30wt%. The finer the powder size is, the more homogeneous structure the extruded wire has. The vacuum degassing before extrusion was necessary to remove the entrapped gas in as-extruded wire. The formability of wire depends greatly on the wire radius and binder content. After burning out the binder and the successive sintering, the contacts between the superconducting grains could be made. The resistivity vs. temperature behavior measured in the final wire showed the transition temperature of 90K with narrow transition width. However, the critical current densities of these wires are much lower in comparison to those of conventional bulk specimens.

  • PDF

Effects of Nano FexC Addition on Superconducting Properties of MgB2 (MgB2 초전도 특성에 대한 나노 FexC 첨가 효과)

  • Lee, Dong-Gun;Lee, Ji-Hyun;Jun, Byung-Hyuk;Park, Soon-Dong;Uhm, Young-Rang;Park, Hai-Woong;Kim, Chan-Joong
    • Journal of Powder Materials
    • /
    • v.19 no.2
    • /
    • pp.146-150
    • /
    • 2012
  • The effects of nano $Fe_xC$ addition to superconducting properties of $in$ $situ$ processed $MgB_2$ superconductors was examined. 0.1 wt.% and 1 wt.% nano $Fe_xC$ powders were mixed with boron and magnesium powders by ball milling. The powder mixtures were made into pellets by uniaxial pressing. The pellets were heat-treated at $700^{\circ}C-900^{\circ}C$ in argon atmosphere for $MgB_2$ formation. It was found by powder X-ray diffraction that the raw powders were completely converted into $MgB_2$ after the heat treatment. The superconducting transition temperature ($T_c$) and critical current density ($J_c$), estimated from susceptibility-temperature and $M-H$ curves, were decreased by nano $Fe_xC$ addition. The $T_c$ and $J_c$ decrease by nano $Fe_xC$ addition are attributed to the incorporation of iron and carbon with $MgB_2$ lattices (Fe substitution for Mg and C substitution for B) due to the high reactivity of the nano $Fe_xC$ powder.

Design, Manufacture and Characteristic Experiment of a Superconducting power Supply with Superconducting Excitation Coil (초전도여자기를 이용한 초전도전원장치의 설계.제작 및 특성해석)

  • Chu, Yong;Kim, Ho-Min;Yoon, Yong-Soo;Ko, Tae-Kuk;Han, Tae-Su
    • Progress in Superconductivity and Cryogenics
    • /
    • v.2 no.1
    • /
    • pp.14-18
    • /
    • 2000
  • This paper describes a series of experiments to investigate the operational characteristics of a superconducting power supply with superconducting excitation coil. In this experiment, the superconducting excitation coil is introduced to control the pole-flex in the air gap of the machine. The operating current of the superconducting powder supply is designed to have the value of 300 [A] for the rotational speed of 600 rpm. Sensors installed on the Nb sheet yield the information on the spatial and temporal behaviors of the magnetic field in spot and on the characteristics of the superconducting power supply.

  • PDF

Characteristics of Bi(Pb)-Sr-Ca-Cu-O Superconductor Wire Fabricated using the Billet Insertion Method (Billet 장입 방식을 이용 제조한 Bi(Pb)-Sr-Ca-Cu-O 초전도 선재의 특성)

  • 장건익;유재근;홍계원
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.4
    • /
    • pp.471-477
    • /
    • 1996
  • During Bi(Pb)-Sr-Ca-Cu-O superconductor wire fabrication the effect of the initial packing density on the final characteristics of superconductor wire was systematically studied. To increase the powder packing density with uniform distribution of superconducting core a billet insertion method processed by CIP was applied instead of the commonly used vibration and ramming method of powder insertion into silver sheath. Compared with the vibration and ramming method the billent insertion technique processed by CIP cause the 30% incre-specimen with 130${\mu}{\textrm}{m}$(core thickness : 45 ${\mu}{\textrm}{m}$)and 5.24 mm width processed at 84$0^{\circ}C$for 200hrs. shows specimen with 130${\mu}{\textrm}{m}$ (core thickness ; 45${\mu}{\textrm}{m}$)and 5.24 mm width processed at 84$0^{\circ}C$ for 200 hrs. shows maximum 34A for Ic and 16, 700 A/cm2 for Ic measured at 77K and 0T. Also the sample rolled 3 times shows maximum 7, 2A for Ic and 11, 000 A/cm2 for 77K and 0T. Based on X-ray experimental results the formation of Bi-2223 and texture were significantly well developed at the interface between the superconducting core and silver sheath as compared with those of the interior area of superconducting core.

  • PDF

Development of multi filament cable with Bi high-Tc superconducting system (Bi계 고온초전도 다심케이블 제작에 관한 연구)

  • 김민기;강형곤;최효상;한병성
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1993.11a
    • /
    • pp.43-46
    • /
    • 1993
  • Superconducting cable (Ic: 60 A at 77K. 10 filaments) with Bi high-Tc superconducting system was developed by powder - in - tube method. Pressing and sintering process of the cables were repeated for growth of 2223 high-Tc superconducting phase. The cable can be fabricate by twist method that is nessary for high current density and cooled circulative system. This cab1e system can be used for commercial.

  • PDF

Preparation of YBa2Cu3O6+x Superconducting Wires Prepared by Pyrophoric Synthetic Technique (발화합성법에 의한 YBa2Cu3O6+x 초전도 선재의 제조)

  • Yang, Suk-Woo;Lee, Young-Min;Kim, Young-Soon;Park, Jeong-Shik;Kim, Chan-Joong;Hong, Gye-Won;Shin, Hyung-Shik
    • Applied Chemistry for Engineering
    • /
    • v.9 no.7
    • /
    • pp.1011-1017
    • /
    • 1998
  • $YBa_2Cu_3O_{6+x}(Y123)-Ag$ high-Tc superconducting wires were fabricated by plastic extrusion technique using pyrophoric synthetic and mechanical mixing powder with and without Ag addition(20 wt.%). This method involves powder preparation, plastic paste making, die extrusion, binder burn-out and the sintering process. In order to fabricate a good-quality superconducting body, it is required to use homogeneous and fine-size power as a starting materials. $Y_2O_3-BaCO_3-CuO$ precursor powders with/without Ag addition were prepared both by pyrophoric synthetic(PS) and mechanical mixing(MM) method of raw powders. The formation kinetics of the powder mixtures into Y123 phase was investigated at various temperatures and times in air atmosphere. The powder prepared by PS method was more easily converted into a Y123 phase than the MM powder. The fine size and good chemical homogeneity of the powder prepared by PS method is attributable to the fast formation into a Y123 phase. The critical current density($J_c$) of the Y123-Ag superconducting wires made by plastic extrusion method were in the range of $150A/cm^2{\sim}230A/cm^2$. depending on the charateristics of starting material powders. $J_c$ of the wire prepared by pyrophoric synthetic powder with 20 wt.% Ag addition was $230A/cm^2$.

  • PDF

The Preparation of Bi-2223 Superconducting Powder and Tape by Emulsion Drying Method (에멀젼 건조법에 의한 Bi-2223 초전도 분말과 테이프 제조)

  • 장중철;이응상;이희균;홍계원
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.2
    • /
    • pp.115-122
    • /
    • 1997
  • The powder preparation by using emulsion drying method, one of the chemical powder fabrication methods has the advantages; easy to control the chemical stoichiometry and to fabricate homogeneously fine particles. In the present study, the initial morphology and size distribution of the powder fabricated by using emulsion dry-ing method were controlled and were improved the homogeneity. By carefully controlling the mixing ratio of oil phase and aqueous solution and surfactant of preventing emulsion separation, the Bi(Pb)-Sr-Ca-Cu-O su-perconducting powders were prepared. The properties of the superconducting powder fabricated by this method and the microstructures and superconducting properties of the pelletized samples were investigated. The microstructures and electric properties of the tapes prepared by oxide powder-in-tube method were in-vestigated. The fabricated powder was spherical with less than 1$\mu$m but most of them was agglomerated with 2~5$\mu$m in size. The critical temperature of the pelletized sample annealed at 84$0^{\circ}C$ for 72 hours in oxygen par-tial pressure of 1/13atm in Ar atmosphere was 108K. And the critical current of the first and second annealed tapes in air prepared by oxide powder-in-tube process were 0.4A and 1.5A, respectively.

  • PDF

Reaction temperature dependence of MgB2 superconducting bulks using the different sizes of Mg raw powders

  • K.C., Chung
    • Progress in Superconductivity and Cryogenics
    • /
    • v.24 no.4
    • /
    • pp.36-39
    • /
    • 2022
  • Since the MgB2 superconductor is simply composed of two constituents of Mg and B, its performance can be monitored easily with the change of one ingredient compared to the other. With the powder size of B less than 100 nm, two different sizes of Mg powders are used to investigate the reaction temperature dependence of MgB2 bulk samples. In the range of 630-700℃ for the duration of 30 min., the un-reacted Mg is seen only at 630℃ with Mg powder size of <5 ㎛, whereas Mg traces are detected at all the temperature range with Mg powder size of <45 ㎛. The reaction temperature dependence of MgB2 superconducting transition temperature, Tc, shows little difference whether Mg powder size is large or small in this range except for the 630℃. It is worthy of notice that the critical current densities of MgB2 show higher performance with the small size of Mg compared to the large one at all field ranges. With the Mg powder size of <45 ㎛, flux pinning is enhanced with decreasing the reaction temperature, whereas flux pinning properties is quite similar in the Mg powder size of <5 ㎛ except for the 630℃, where Mg is left behind after the reaction.

Effects of F-doping on perparation and superconducting characteristics of ag-sheathed Tl-1223 tapes

  • 정대영;김희권;이준호;차무경;김영철;이호섭
    • Progress in Superconductivity and Cryogenics
    • /
    • v.2 no.1
    • /
    • pp.1-6
    • /
    • 2000
  • The effects of partial substitution of fluorine on physical properties were studied in Ag-sheathes tapes of $Tl_{0.8}Pb_{0.2}Sr_{1.8}Ba_{0.2} Ca_{2.2}Cu_3O_yF_x (0{\leq}x{\leq}1)$ nominal compositions. The tapes were prepared using the powder-in-tube method incorporating an in-situ reaction method. $CuF_2$ was used as a source of F. It was found that F-doping in Tl-1223 system resulted in a decrease in formation temperatire of Tl-1223 phase. and thus significantly deteriorated their superconducting properties. Such disadvantages seem to originate by the fromation of non-beneficial phases such as SrF2 in the early stage of the powder preparation process.

  • PDF