• 제목/요약/키워드: sulfuric acid corrosion

검색결과 106건 처리시간 0.026초

Preparation of Novel Sorbents for Gas-phase Mercury Removal

  • Lee, Si-Hyun;Rhim, Young-Jun;Park, Young-Ok
    • Carbon letters
    • /
    • 제3권4호
    • /
    • pp.187-191
    • /
    • 2002
  • In the present research, we prepared the activated carbon (AC) sorbents to remove gas-phase mercury. The mercury adsorption of virgin AC, chemically treated AC and fly ash was performed. Sulfur impregnated and sulfuric acid impregnated ACs were used as the chemically treated ACs. A simulated flue gas was made of SOx, NOx and mercury vapor in nitrogen balance. A reduced mercury adsorption capacity was obtained with the simulated gas as compared with that containing only mercury vapor in nitrogen. With the simulated gas, the sulfuric acid treated AC showed the highest performance, but it might have the problem of corrosion due to the emission of sulfuric acid. It was also found that the high sulfur impregnated AC also released a portion of sulfur at $140^{\circ}C$. Thus, it was concluded that the low sulfur impregnated AC was suitable for the treatment of flue gas in terms of stability and efficiency.

  • PDF

Effectiveness of fibers and binders in high-strength concrete under chemical corrosion

  • Nematzadeh, Mahdi;Fallah-Valukolaee, Saber
    • Structural Engineering and Mechanics
    • /
    • 제64권2호
    • /
    • pp.243-257
    • /
    • 2017
  • Investigating the properties and durability of high-strength concrete exposed to sulfuric acid attack for the purpose of its application in structures exposed to this acid is of outmost importance. In this research, the resistance and durability of high-strength concrete containing macro-polymeric or steel fibers together with the pozzolans of silica fume or nano-silica against sulfuric acid attack are explored. To accomplish this goal, in total, 108 high-strength concrete specimens were made with 9 different mix designs containing macro-polymeric and steel fibers at the volume fractions of 0.5, 0.75, and 1.0%, as well as the pozzolans of silica fume and nano-silica with the replacement levels of 10 and 2%, respectively. After placing the specimens inside a 5% sulfuric acid solution in the periods of 7, 21, and 63 days of immersion, the effect of adding the fibers and pozzolans on the compressive properties, ultrasonic pulse velocity (UPV), and weight loss of high-strength concrete was investigated and the respective results were compared with those of the reference specimens. The obtained results suggest the dependency of the resistance and durability loss of high-strength concrete against sulfuric acid attack to the properties of fibers as well as their fraction in concrete volume. Moreover, compared with using nano-silica, using silica fume in the fibrous concrete mix leads to more durable specimens against sulfuric acid attack. Finally, an optimum solution for the design parameters where the crushing load of high-strength fibrous concrete is maximized was found using response surface method (RSM).

UNS N08810 합금의 입계부식손상과 원인 분석 (Elucidation of Intergranular Corrosion of UNS N08810 alloys)

  • 김영식;황보덕
    • Corrosion Science and Technology
    • /
    • 제11권5호
    • /
    • pp.196-204
    • /
    • 2012
  • Corrosion failure of petrochemical facilities is one of the difficulties in maintenance, since operating conditions of crude oil production, storage, and refinement are very aggressive. UNS N08810, which has been used for crude oil transportation pipes and storage tanks in petrochemical industries, shows good resistance to general corrosion and localized corrosion in several environments. Among its environments, UNS N08810 showed better corrosion resistance in fuel gas containing sulfuric acid and phosphoric acid and sulfur. However, ductility and toughness at high temperature over about $500^{\circ}C$ were greatly reduced due to microstructural change. In general, welding process is the representative method to join the parts in industrial components. Because the alloy by welding can be sensitized and corroded, the manufacturing process should be controlled. In this work, UNS N08810 was used and heat treatment conditions including solution and stabilization treatments were controlled. Oxalic acid etch test by ASTM A262 Practice A was done to evaluate the qualitative sensitization in room temperature. Huey test by ASTM A262 Practice C was done to evaluate the intergranular corrosion rate in boiling 65% $HNO_3$ solution. Also, the microstructure by thermal history was analyzed. Experimental alloy showed high intergranular corrosion rate and its corrosion mechanism was elucidated.

산성안개 환경하에서 Ni-Cr-Mo 강의 피로크랙전파거동 (Fatigue Crack Growth Behavior of Ni-Cr-Mo Steel under Acid Fog Environment)

  • 김민건;임용호;김만구
    • 대한기계학회논문집A
    • /
    • 제24권7호
    • /
    • pp.1841-1846
    • /
    • 2000
  • To examine the effect of acid fog on the corrosion fatigue behavior in structural steel, fatigue tests under acid fog atmosphere were carried out in comparison with distilled water. The corrosive c omponents contained in acid fog pile up the corrosion products on crack face and show a crack branching and crack tip blunting. Therefore, due to these workings crack growth rate was reduced by decreasing the effective stress range in crack tip rather than under distilled water. Also the effect of sulfuric acid, which is the main component of acid fog, and testing speed on fatigue crack growth were examined. It was found that corrosion behavior was remarkably dependent upon pH and Hz rather than components of acid fog. According as pH and testing speed decrease below a specific value, crack growth was accelerated in comparison with distilled water. This reveals that due to liquid having strong acidity and slow speed of test the crack face dissolution was promoted, so crack closure was disturbed in the process of stress descent.

The Effect of Solution Treatment on Intergranular Corrosion Resistance of a New Type Ultra Low Carbon Stainless Steel

  • Julin, Wang;Nannan, Ni;Qingling, Yan;Lingli, Liu
    • Corrosion Science and Technology
    • /
    • 제6권3호
    • /
    • pp.140-146
    • /
    • 2007
  • In the paper, with corrosion velocity measurement and metallographic observation on specimens after sulfuric acid/ferric sulfate boiling experiment, intergranular corrosion tendency of the new type ultra low carbon stainless steel developed by ourselves which experienced solution treatment at different temperatures was evaluated. A VHX 500 super depth field tridimensional microscope was used to observe corrosion patterns on the sample surfaces. The depth and width of grain boundary corrosion groove were measured by the tridimensional microscope, which indicated that the corrosion degrees of the samples which received solution treatment at different temperatures are quite different. Transgranular corrosion at different degree occurred along with forged glide lines. After comparison it was proved that the stainless steel treated at $1100^{\circ}C$ performs very well against intergranular corrosion.

고분자 전해질 연료전지 금속분리판용 316L 스테인리스강의 양극작동조건에서 염화물 농도에 따른 부식 특성 (Corrosion Characteristics of 316L Stainless Steel with Chloride Concentrations in Cathode Operating Conditions of Metallic Bipolar Plate for PEMFC)

  • 신동호;김성종
    • Corrosion Science and Technology
    • /
    • 제20권6호
    • /
    • pp.435-450
    • /
    • 2021
  • The interest in eco-friendly energy is increasing, and polymer electrolyte membrane fuel cell (PEMFC) is attracting attention as alternative power sources. Research on metallic bipolar plates, a fuel cell component, is being actively conducted. However, since the operating conditions of PEMFC, in which sulfuric acid (H2SO4) and hydrofluoric acid (HF) are mixed, are strong acidity, the durability of the metallic bipolar plate is very important. In this research, the electrochemical characteristics and corrosion damage behavior of 316L stainless steel, a material for metallic bipolar plates, were analyzed through potentiostatic corrosion tests with test times and chloride concentrations. As the test times and chloride concentrations increased, the current density and corrosion damage increased. As a result of observation with scanning electron microscope(SEM) and 3D microscope, both the depth and width of pitting corrosion increased with increases in test times and chloride concentrations. In particular, the pitting corrosion damage depth at test conditions of 6 hours and 1000 ppm chloride increased the most. The growth of the pitting corrosion damage was not directly proportional to time and increased significantly after a certain period.

Corrosion resistance improvement of 6061 aluminum alloy using anodizing process

  • Zuraidawani Che Daud;Muhammad Faidzi Shukri;Mohd Nazree Derman
    • Advances in materials Research
    • /
    • 제13권3호
    • /
    • pp.195-202
    • /
    • 2024
  • Aluminum alloy is a material that is frequently used in the aerospace and transportation industries due to its high mechanical and corrosion resistance qualities. Unfortunately, aluminum alloys are prone to corrosion, limiting their application in some harsh situations such as when submerged in aqueous environments. The purpose of this study is to investigate how anodizing can increase the corrosion resistance of 6061 Aluminum alloy. The anodizing process was carried out using two different parameters which are voltage (5V, 10V, 15V) and electrolyte sulfuric acid (H2SO4) concentration (0.3M, 0.5M) for 1 hour. The anodized samples were performed using several analyses such as X-ray diffraction (XRD) analysis, morphology analysis, and corrosion test. From this study, it is found that the difference in anodizing parameters affects the corrosion resistance of the samples. Sample anodized at 15V, 0.5M gives the best corrosion resistance.

Electrochemical Adsorption Properties and Inhibition of Zinc Corrosion by Two Chromones in Sulfuric Acid Solutions

  • Fouda, Abd El-Aziz S.;Nazeer, Ahmed Abdel;Saber, Ahmed
    • 대한화학회지
    • /
    • 제58권2호
    • /
    • pp.160-168
    • /
    • 2014
  • The electrochemical behavior and corrosion inhibition of zinc in 0.5 M $H_2SO_4$ in the absence and presence of some chromones has been investigated using weight loss, potentiodynamic polarization, electrochemical impedance spectroscopy (EIS) and electrochemical frequency modulation (EFM) techniques. The presence of these investigated compounds in the corrosive solutions decrease the weight loss, the corrosion current density, and double layer capacitance but increases the charge transfer resistance. Polarization studies were carried out at room temperature, and showed that all the studied compounds act as mixed type inhibitors with a slight predominance of cathodic character. The effect of temperature on corrosion inhibition has been studied and the thermodynamic activation and adsorption parameters were determined and discussed. The adsorption of the investigated compounds on zinc was found to obey Langmuir adsorption isotherm.

Ni-Px/C 다층 도금층의 내식성과 표면 전기저항 평가 (Evaluation of Corrosion and Surface Resistance of Ni-Px/C Multi Layer)

  • 박제식;정은경;이철경
    • 한국표면공학회지
    • /
    • 제45권4호
    • /
    • pp.162-167
    • /
    • 2012
  • Ni-P/C multi-layer was synthesized by electroless plating and paste coating for better corrosion and surface conductance as a metallic bipolar plate. The Ni-P layer could be synthesized with the range of 2.6~22.4 at.% P contents and it's surface morphology and corrosion resistance depend on content of P. Corrosion resistance of the Ni-P layer in sulfuric acid by electrochemical test is similar with pure Ni. Surface resistance of pure Ni after corrosion was increased about 8% compared to pure Ni. On the other hand, that of the Ni-P/C composite with 20% carbon content was increased only 1%.