• Title/Summary/Keyword: submerged arc welding

Search Result 81, Processing Time 0.021 seconds

A study on the correlation between V charpy absorbed energy and critical COD value in the welded parts of high tensil strength steel under various welding methods (고장력강 용접부에 있어서 한계 COD값과 V charpy충격치와의 상관성에 관한 연구)

  • 김영식;김충해
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.12 no.3
    • /
    • pp.57-67
    • /
    • 1988
  • Although handicapped by the inability to bridge the size gap between small laboratory sample and large engineering component, the V charpy test sample method does possess certain advantages, such as each of preparation, simplicity of test method, speed, low cost in test machinery, and low cost per test. On the other hand, the COD test method does posses advantages, which reduce the size gap between the laboratory sample and actual engineering component. Consequently, the correlation between V charpy absorbed energy and the critical COD value is required for estimating critical COD value from the simple V charpy test results. In this paper, the high tensile strength steel AH36 plate specimens having a single edge cracked notch were investigated to find out the correlation between V charpy absorbed energy and critical COD value in the welded parts under such various welding methods as shielded metal arc welding, the submerged arc welding and the electro gas welding by means of V charpy impact test and static 3-point bending test. Main results obtained are as follow ; 1. The relationships between V charpy absorbed energy Wc' and critical COD value ($\delta_c$)show; $\delta_c$=0.0065 Wc'+0.1906. 2. Ductile- brittle transition behaviours can be estimated by means of fracture appearance and general yielding behaviours. 3. The V charpy absorbed energy of SMAW is higher than that of SAW, EGW and similar relationships are obtained in the COD tests.

  • PDF

Prediction of Chemical Composition of Pure Weld Metal in SAW

  • Kim Y.;Ryu D. H.;Kim J. S.;Lee B. Y.
    • International Journal of Korean Welding Society
    • /
    • v.5 no.1
    • /
    • pp.10-14
    • /
    • 2005
  • An element of Pure Weld Metal(PWM) is important factor to understand the Flux's conduct in Submerged Arc Welding(SAW). To get the element of PWM, pile-up welding over than 10 layers have been used in the past. But, it took a long time to analyze the elements of PWM in this method. Therefore, in this study, instead of pile-up welding over than 10 layers, one pass bead welding is used to predict an element of PWM using mathematical formula which got to be derived. As a results that applied the formula, there was no differences between theoretical and experimental value except the element Mn and Si.

  • PDF

An Evaluation of Dynamic Crack Initiation Toughness in SS41 Steel Welding (SS41강 용접부의 동적균열개시인성 평가)

  • 정재강;김건호
    • Journal of Welding and Joining
    • /
    • v.12 no.2
    • /
    • pp.108-118
    • /
    • 1994
  • In the present study, the dynamic crack initiation toughness and total absorbed energy behavior of Heat Affected Zone(HAZ) was experimentally evaluated for SS41 steel welding. The materials were submerged arc-welded SS41 steel plate with thickness 19mm. The test temperature range was from $20^{\circ}C$(room temperature) to $-70^{\circ}C$ The HAZ of welding were divided into three sub-zones for analysis; H1, H2, H3, according to the distance from the fushion line. From the experimental studies, the reference value of dynamic crack initiation toughness $(J_{Id(R)})$ can be use to estimate dynamic fracture toughness characteristics of steel welding.

  • PDF

Hardness prediction based on microstructure evolution and residual stress evaluation during high tensile thick plate butt welding

  • Zhou, Hong;Zhang, Qingya;Yi, Bin;Wang, Jiangchao
    • International Journal of Naval Architecture and Ocean Engineering
    • /
    • v.12 no.1
    • /
    • pp.146-156
    • /
    • 2020
  • Two High Tensile Strength Steel (EH47) plates with thickness of 70 mm were butt-welded together by multi-pass Submerged Arc Welding (SAW), also the hardness and welding residual stress were investigated experimentally. Based on Thermal-Elastic-Plastic Finite Element (TEP FE) computation, the thermal cycles during entire welding process were obtained, and the HAZ hardness of multi-pass butt welded joint was computed by the hardenability algorithm with considering microstructure evolution. Good agreement of HAZ hardness between the measurement and computational result is observed. The evolution of each phase was drawn to clarify the influence mechanism of thermal cycle on HAZ hardness. Welding residual stress was predicted with considering mechanical response, which was dominantly determined by last cap welds through analyzing its formation process.

Irradiation Behavior of Reactor Pressure Vessel SA508 class 3 Steel Weld Metals (압력용기강재 SA508 class 3 용착금속의 조사거동)

  • Koh, Jin-Hyun;Park, Hyoung-Keun;Kim, Soo-Sung;Hwang, Yong-Hwa;Seo, Yun-Seok
    • Journal of Welding and Joining
    • /
    • v.28 no.5
    • /
    • pp.69-74
    • /
    • 2010
  • Irradiation behavior of the reactor pressure vessel SA508 class 3 steel weld metals was examined by Charpy V Notch impact specimens. The specimens were exposed to a fluence of $2.8{\times}1019$ neutrons(n)/$cm^2$(E>1 MeV) at $288^{\circ}C$. The irradiation damage of weld metal was evaluated by comparison between unirradiated and irradiated specimens in terms of absorbed energy and lateral expansion. The specimens for neutron irradiation were welded by submerged arc welding process at a heat input of 3.2 kJ/mm which showed good toughness in terms of weld microstructure, absorbed energy and lateral expansion. The post-irradiation Charpy V notch 41J and 68J transition temperature elevation were $65^{\circ}C$ and $70^{\circ}C$, respectively. This elevation was accompanied by a 20% reduction in Charpy V notch upper shelf energy level. The lateral expansion at 0.9mm irradiated Charpy specimens showed temperature elevation of $65^{\circ}C$ and was greatly decreased due to radiation damage.

Microstructure and CTOD (crack tip opening displacement) of Deposit Weld Metal in 30 mm Thick Plate

  • Lee Hae-Woo;Kim Hyok-Ju;Park Jeong-Ung;Kang Chang-Yong;Sung Jang-Hyun
    • Korean Journal of Materials Research
    • /
    • v.14 no.9
    • /
    • pp.642-648
    • /
    • 2004
  • The microstructure and crack tip opening displacement (CTOD) of deposit weld metal were investigated for a 30 mm- thick plate welded with flux cored arc welding (FCAW) and submerged arc welding (SAW) processes. The CTOD test was carried out both as welded condition and as stress-relieved specimen by local compression. The crack growth rates in FCAW were faster than those in a SAW, and the acicular ferrite content by the SAW process was increased relatively more than that by the FCAW process. The fatigue crack growth rate in a welded specimen was faster than that in locally compressed specimen. The CTOD value of locally compressed specimens was lower than that of as welded specimen. Furthermore, the CTOD value tested with the SAW process was higher than that tested with the FCAW process.

AUTOMATIC MULTITORCH WELDING SYSTEM WITH HIGH SPEED

  • Moon, H.S;Kim, J.S.;Jung, M.Y.;Kweon, H.J.;Kim, H.S.;Youn, J.G.
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.320-323
    • /
    • 2002
  • This paper presents a new generation of system for pressure vessel and shipbuilding. Typical pressure vessel and ship building weld joint preparations are either traditional V, butt, fillet grooves or have narrow or semi narrow gap profiles. The fillet and U groove are prevalently used in heavy industries and shipbuilding to melt and join the parts. Since the wall thickness can be up to 6" or greater, welds must be made in many layers, each layer containing several passes. However, the welding time for the conventional processes such as SAW(Submerged Arc Welding) and FCAW(Flux Cored Arc Welding) can be many hours. Although SAW and FCAW are normally a mechanized process, pressure vessel and ship structures welding up to now have usually been controlled by a full time operator. The operator has typically been responsible for positioning each individual weld run, for setting weld process parameters, for maintaining flux and wire levels, for removing slag and so on. The aim of the system is to develop a high speed welding system with multitorch for increasing the production speed on the line and to remove the need for the operator so that the system can run automatically for the complete multi-torch multi-layer weld. To achieve this, a laser vision sensor, a rotating torch and an image processing algorithm have been made. Also, the multitorch welding system can be applicable for the fine grained steel because of the high welding speed and lower heat input compare to a conventional welding process.

  • PDF

Evaluation on Mechanical Properties with Welding Processes for Off Shore Wind Tower Application (TMCP강을 적용한 해상용 풍력타워의 용접 공정에 따른 기계적 물성 평가)

  • Ji, Changwook;Choi, Chul Young;Nam, Dae-Geun;Kim, Hyoung Chan;Jang, Jae Ho;Kim, Ki Hyuk;Park, Yeong-Do
    • Journal of Welding and Joining
    • /
    • v.32 no.1
    • /
    • pp.15-21
    • /
    • 2014
  • FCAW(Flux Cored Arc Welding), SAW(Submerged Arc Welding), EGW(Electro Gas Welding), and three-pole SAW are applicable in manufacturing the offshore wind tower. In this paper, mechanical properties of these welded-joints for TMCP steels were evaluated in all above welding processes. The tensile strength of welded-joints for all the welding methods satisfied the standard guideline (KS D 3515). No cracking on weldment was found after the bending test. Changes of weldedments hardness with welding processes were observed. In a weld HAZ (heat-affected zone), a softened HAZ-zone was formed with high heat input welding processes (SAW and EGW). However, the welded-joint fractures were found in the base metal for all cases and small decrease in welded-joint strength was caused by a softened zone. The multi-pole SAW welds exhibited similar mechanical properties comparing to the one with one-pole SAW process.

TMCP 강의 용접열영향부 인성에 관한 연구

  • 신민태;윤중근;김희진
    • Journal of Welding and Joining
    • /
    • v.4 no.3
    • /
    • pp.43-49
    • /
    • 1986
  • Weldability of the TMCP steel manufactured by controlled rolling followed by accelerated cooling process was investigated. For comparison, two other steel plates produced by different manufacturing processes were selected; normalized and controlled rolled. Tandem submerged arc welding with both side one run technique was carried out. The results of this study can be summarized as follows; TMCP steel having the lowest carbon equivalent shows the best combination of mechanical properties, not only in the base metal but also in the heat affected zone. In the HAZ, the accelerated colling effect imarted on the trengthis releved by the weld thermal cycles, and thus the strength of the welded joint decrease substantially accompanied with the fracture in the HAZ. On the other hand, not only the softening but the fine microstructure can preserve the high toughness of TMCP steel in the HAZ.

  • PDF

Status and Prospect of Site Welding Technology for LNG Strorage Tank (LNG 저장탱크의 현장용접 시공기술의 현상 및 전망)

  • 이광희;전혁성
    • Journal of Welding and Joining
    • /
    • v.13 no.3
    • /
    • pp.8-17
    • /
    • 1995
  • LNG를 저장할 수 있는 탱크는 주로 지상식이거나 반지하식이며 그 용량은 매우 다양하다. 우리나라에서는 지상식 탱크가 평택 인수기지에 10만m$^{3}$급 Membrane Type 6기가 건설되었고 1기는 거의 완성단계이며, 현재 추가로 건설 중인 3기를 포함하면 총 10기의 탱크를 확보하게 된다. 또한 제2인수기지인 인천에도 동급 으로서 9%Ni강을 사용하는 Double Wall Type LNG 탱크 3기를 건설 중이다. 전세계적 으로 볼 때 LNG 저장 탱크의 78%는 지상식으로 Double Wall Type 또는 Membrane 저장 탱크 형식을 취하고 있으나, 최근에는 안전성 측면, 토지 가격의 상승, 토지의 합리적 이용 측면 등을 감안하여 LNG 탱크를 지하화, 대형화하는 추세이다. 본고에서는 Fig. 1과 같은 구조의 Double Wall Type LNG 저장탱크 중 초저온의 LNG에 직접 접하는 저 온용 재료(9%니켈강)로 만들어지는 내조 용접에 대해서 중점적으로 논하기로 하며, 특히 9% 니켈강 Shell Plate Horizontal Joint에 채용되는 Automatic Submerged ARC 용접에 대해 실제 현장 용접 시공상태를 나타내고자 한다.

  • PDF