Evaluation of mechanical properties for high strength and ultrahigh strength concretes

  • Murthy, A. Ramachandra;Iyer, Nagesh R.;Prasad, B.K. Raghu
    • Advances in concrete construction
    • /
    • v.1 no.4
    • /
    • pp.341-358
    • /
    • 2013
  • Due to fast growth in urbanisation, a highly developed infrastructure is essential for economic growth and prosperity. One of the major problems is to preserve, maintain, and retrofit these structures. To meet the requirements of construction industry, the basic information on all the mechanical properties of various concretes is essential. This paper presents the details of development of various concretes, namely, normal strength concrete (around 50 MPa), high strength concrete (around 85 MPa) and ultra high strength concrete (UHSC) (around 120 MPa) including their mechanical properties. The various mechanical properties such as compressive strength, split tensile strength, modulus of elasticity, fracture energy and tensile stress vs crack width have been obtained from the respective test results. It is observed from the studies that a higher value of compressive strength, split tensile strength and fracture energy is achieved in the case of UHSC, which can be attributed to the contribution at different scales viz., at the meso scale due to the fibers and at the micro scale due to the close packing of grains which is on account of good grading of the particles. Micro structure of UHSC mix has been examined for various magnifications to identify the pores if any present in the mix. Brief note on characteristic length and brittleness number has been given.

Mock-up Test of Concrete Using AE Water Reducing Agent of Early-Strength Type in Construction Field (조기강도발현형 AE감수제를 사용한 콘크리트의 현장 Mock-up 실험)

  • 황인성;김기훈;김규동;이승훈;한천구
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2004.05a
    • /
    • pp.1-4
    • /
    • 2004
  • In this paper. applicability of high early strength type AE water reducing agent(HESAEWA) developed by the authors is discussed by applying Mock-up test. For fresh concrete properties, concrete using existing AE water reducing agent(EAEWRA) and HESAEW A meets the target slump and air content at jobsite. Setting time of concrete using HESAEWA is shorter than that using EAEWRA. Remarkable variance of bleeding and settlement is not observed with type of AE water reducing agent. For hardened concrete properties, use of HESAEW A results in higher strength development compared with that of EAEWRA at standard curing and in field curing condition. Reaching time to accomplish 5MPa of compressive strength. which is possible to remove side form. is taken using HESAEWA earlier than that of EAEWRA by 1day. Therefore, it is confirmed that use of HESAEWA can meet the requirements of general quality of concrete and achieve high early strength development as well as has a desirable field applicability.

  • PDF

The Mechanical Properties of High Strength Concrete in Massive Structures

  • Park, Ki-Bong
    • Architectural research
    • /
    • v.15 no.1
    • /
    • pp.53-58
    • /
    • 2013
  • High strength concrete is being used increasingly in mass structure projects. The purpose of this study is to investigate the influence of temperature during mixing, placing and curing on the strength development, hydration products and pore structures of high strength concrete in mass structures. The experiments were conducted with two different model walls, viz.: 1.5 m and 0.3 m under typical summer and winter weather conditions. The final part of this study deal with the clarification of the relationship between the long-term strength loss and the microstructure of the high strength concrete at high temperatures. Test results indicated that high elevated temperatures in mass concrete structures significantly accelerate the strength development of concrete at the early ages, while the long-term strength development is decreased. The long-term strength loss is caused by the decomposition of ettringite and increased the total porosity and amount of small pores.

Long-term development of compressive strength and elastic modulus of concrete

  • Yang, Shuzhen;Liu, Baodong;Yang, Mingzhe;Li, Yuzhong
    • Structural Engineering and Mechanics
    • /
    • v.66 no.2
    • /
    • pp.263-271
    • /
    • 2018
  • Compressive strength and elastic modulus of concrete are constantly changing with age. In order to determine long-term development of compressive strength and elastic modulus of concrete, an investigation of C30 concrete cured in air conditions was carried out. Changes of compressive strength and elastic modulus up to 975 days were given. The results indicated that compressive strength and elastic modulus of concrete rapidly increased with age during the initial 150 days and then increased slowly. The gain in elastic modulus was slower than that of compressive strength. Then relationships of time-compressive strength, time-elastic modulus and compressive strength-elastic modulus were proposed by regression analysis and compared with other investigations. The trends of time-compressive strength and time-elastic modulus with age agreed best with ACI 209R-92. Finally, factors contributed to long-term development of compressive strength and elastic modulus of concrete were proposed and briefly analyzed.

Mechanical Properties of Concrete with Different Curing Temperatures (양생온도변화에 따른 콘크리트의 재료역학적 특성)

  • 김진근;한상훈;양은익;송영철;방기성
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1998.10c
    • /
    • pp.42-47
    • /
    • 1998
  • Experimental investigation was undertaken to determine early-age strength development and the relationships between the mechanical properties of type I, V and V/fly ash cement concrete with different curing temperature. The tests for mechanical properties, i.e., compressive strength, splitting tensile strength and modulus of elasticity were carried out for type, I, V and V with 15% replacement with fly ash cement concrete. For this purpose 480 concrete cylinders cured at isothermal conditions of 10, 23, 35 and 5$0^{\circ}C$ were tested at ages of 1, 3, 7 and 28days. According to the experiments, the concrete subjected to high temperature at early age got greater strength at early age, however eventually lower strength at late age. The derived relationships between compressive strength and splitting tensile strength and elastic modulus of elasticity appeared to be identical for all types of cement.

  • PDF

Mechanical Strength Properties of Hanger Insulator for Arrestor (피뢰기 절연행거의 기계적 강도 특성)

  • 박기호;조한구;한동희
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.589-592
    • /
    • 2001
  • Generally, hanger insulator for polymer arrestor have to be good insulation properties and mechanical strength and weatherability, But many remark and repairs have been to think about low cost and light weight. The Paper is used Polymer arrestor for post and performance analysis and mechanical strength insulator hanger according to development of simplest product. To enhance the efficiency of experimental modal analysis, we proposed the process which is the selection of the locations and the number of measurement points for pre-test.

  • PDF

Fundamental Properties of Antiwashout Underwater Concrete Mixed with Mineral Admixtures

  • Han-Young, Moon;Kook-Jae, Shin;Yong-Kyu, Song
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2003.11a
    • /
    • pp.457-460
    • /
    • 2003
  • This paper discusses laboratory evaluations to assess the physical properties of antiwashout underwater concrete (AWC) containing pozzolanic materials such as fly ash (FA), blast furnace slag (SG) and metakaolin(MK). For the experiments, pH value, suspended solids, slump flow, efflux time and compressive strength were tested. According to the results from compressive strength test, MK10 showed the very high compressive strength characteristic during the entire curing days, but the rate of strength development was decreased as time goes by.

  • PDF

Development of Strength and Durability Properties of Latex-Modified Concrete with Rapid-Setting Cement (초속경 시멘트를 사용한 라텍스 개질 콘크리트의 강도발현 및 내구특성)

  • 최성욱;홍창우;김동호;최상릉;장홍균
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.11a
    • /
    • pp.1029-1034
    • /
    • 2001
  • The purpose of this research is to develop rapid setting cement latex modified concrete (RSLMC) which will be used to overlay bridge deck for maintaining and repairing. The main experimental variables were the types of rapid setting cement and variation of latex and antifoam agent contents were selected as admixture factor, then the properties of workability and strength development and durability properties were investigated. The results of this study show that latex content give increment of a slump due to surface tension in polymer particles and reduce unit weight of water for preservation of workability. In addition, When no and 1.6~3.2% antifoam agent were mixed, 8%, 2.0~3.8% were respectively obtained. An increasing the amount of latex produced concrete with increased flexural strength, but with slightly lower compressive strength. Rapid chloride permeability and freezing-thawing test carried out. As a results, according to increment of containing ratio antifoamer, strength of RSLMC increase, permeability showed lower value than ignorable 100 coulombs. Also, in the case of more than antifoamer 1.6%, the relativity dynamic modulus is mantained more than 90%, but in case of 0, 5%, it decrease. In consequence, with the view of strength and workability of RSLMC, it is considered that appropriate content ratio of antifoam agent and latex solid are respectively 1.6% by latex weight, 15% by cement weight.

  • PDF

An Experimental Study on the Early Strength Development Properties of Concrete According to Curing Condition and Used Materials (사용재료 및 양생조건에 따른 콘크리트의 조기강도발현 특성에 관한 실험적 연구)

  • Lee, Sang-Soo;Song, Ha-Young;Lee, Ji-Hwan
    • Journal of the Korea Concrete Institute
    • /
    • v.20 no.6
    • /
    • pp.721-729
    • /
    • 2008
  • The purpose of this study is to investigate the engineering properties of concrete for the early strength development. As a result of reviewing it by establishing each experimental factor and level, the cement had more excellent quality performance in CHC and HESPC than OPC. This study has shown that the PC series admixture was more excellent in side of elapsed time (aging) and early strength development than PNS series admixture. In addition, there was much difference according to the curing temperature, but the early strength development showed the considerable vulnerability in curing temperature below $12^{\circ}C$. To satisfy the strength requirements of 5 MPa/18 hr this study has shown that it needed the curing temperature over $17^{\circ}C$ to the minimum in OPC, over $14^{\circ}C$ in CHC, and over $11^{\circ}C$ in HESPC. On the other hand, as to the strength properties according to W/C, the less W/C was, the more strength development was excellent. If this study is to be used in construction filed on a basis of this result, this researcher is considered as possible of the economic execution of construction by advancing the early strength and by the reduction of construction cost according to shortening construction duration.

Mechanical Properties of Concrete Containing Silicic Wastes (규사성분의 산업폐기물을 혼입한 콘크리트의 역학적 특성)

  • 박제선;김태경;이주형;백민경
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1996.04a
    • /
    • pp.192-197
    • /
    • 1996
  • An experimental study was performed to examine the feasibility of using silicic wastes as construction materials for civil structures, and investigate its utility as a replacement for the favored nature resource to prevent the economic loss. In order to achieve this objective, mechnical properties of concrete containing silicic wastes is tested by investigating the strength development through parameters of water-binder ratios replacement 10 percent ratio with respect to curting conditions. The effect of stringth development is investigated for curing conditions when silicic wastes of 10 percent of cement-binder ratios is containde. Comparision on compressive strength of normal concrete and concrete containing silicic wastes at 28 day is conducted. The concrete with silicic wastes have larger compressive strength than of normal concrete by about 20 percent, when cured at 80 degree. The wastes concrete using silica sand shows increased strength, fracture toughness, elastic modulus and strain than the normal concrete, although the silicic wastes concrete could be able to satisfy the generally required strength for conventional concrete structures.

  • PDF