• 제목/요약/키워드: stone deterioration

검색결과 120건 처리시간 0.028초

보물 제955호 선암사 금동팔각원당형사리탑 보존처리 (The conservation of a gilt-bronze Sarira Reliquary, Treasure No. 955)

  • 고형순;유재은
    • 보존과학연구
    • /
    • 통권24호
    • /
    • pp.215-227
    • /
    • 2003
  • The gilt-bronze Sarira Reliquary was discovered when repairing three-stories east stone pagoda (Treasure No. 395) at Seungju-eup in Suncheon city in Jeollanam-do Province in August, 1986. Then it was appointed as Treasure in 1988. The Sarira Reliquary had been held in Seonamsa temple, but deterioration on the surface and corrosion had appeared affecting its surface detail. Consequently, the conservation treatment was carried out from November 2002 to March 2003.The corrosion and dirt on the surface of the Sarira Reliquary were cleaned with ethyl alcohol and Benzotriazole was applied to prevent further corrosion. Finally, NAD-10(Paraloid NAD-10), acrylic resin, was used to consolidate the structure. Moreover, after non-destructive analysis to confirm element of alloy, copper, gold, silver and mercury were discovered and this result tells us that it was plated with gold by amalgam. Fibers at the pedestal were examined under the microscope and identified as silk. The total height of this Sarira Reliquary is 6.0cm, the height of lotus pedestal and the roof is 2.7cm and 1.8cm, respectively. The roof and body are joined together, and the lotus pedestal can be separated, on which the octagonal reliquary is impaled. The pedestal consists of 3layers of petals and the surface is decorated with flower pattern. The reliquary is presumed to be created in the 14th century, and it becomes valuable historical material to reveal the secret of metal work in the late Goryeo Dynasty.

  • PDF

공기 유압식 브레이크 라인 파손 사례 및 파손 분석 연구 (A Case Study on Failure and Analysis of Air Over Hydraulic Brake Line)

  • 박정만;박종진
    • 자동차안전학회지
    • /
    • 제12권2호
    • /
    • pp.47-55
    • /
    • 2020
  • In this case study, the brake line failure of air over hydraulic(AOH) brake system is described. AOH brake system is applied to commercial vehicles between 5 to 8 tons. It consists of a hydraulic system using compressed air and operates the air master to form hydraulic pressure to transfer braking power to the wheels. When the brake lines of the system applied to vehicles with high load capacity are damaged, the braking force of one shaft is lost, and the braking distance increases rapidly, leading to a big accident. Failure of the brake line occurs due to various causes such as road surface fragmentation, corrosion of the line, and aged deterioration of air brake hose. The braking force could be decreased even when a very small break in the form of a pin-hole occurs. However, it is difficult to find a part where the thickness of the line is thin due to stone pecking or corrosion generated in the pin-hole formed on the brake line located under the lower part of the vehicle by the sensory evaluation or the conventional braking force test. Accordingly, it is necessary to analyze the condition and cause of the failure of the brake line more precisely when the accident investigation of the heavy vehicles, and also to examine the necessity of the advanced test for the aged brake line.

창녕 물계서원 원정비의 재질특성 및 손상도 평가와 균열심도 측정 (Material Characteristics, Deterioration Evaluation and Crack Depth Estimation for Mulgyeseowon Stele in Changnyeong, Korea)

  • 유지현;이찬희;전유근
    • 보존과학회지
    • /
    • 제30권4호
    • /
    • pp.427-438
    • /
    • 2014
  • 이 연구에서는 석조문화재의 표면 균열에 대한 깊이와 연장성을 측정하기 위해 창녕 물계서원 원정비를 대상으로 초음파 속도를 활용하였다. 또한 이 원정비의 장기적인 보존관리 방안을 수립하기 위해 재질 및 손상현황을 조사하고, 다양한 비파괴 기법을 활용하여 정밀진단을 수행하였다. 원정비를 이루고 있는 주요 구성암석은 비석의 부위에 따라 달리 알칼리장석화강암, 반려암 및 섬록암으로 이루어져 있다. 손상도 평가 결과, 특히 균열이 비신의 모든 방향에서 두드러진 분포를 보여 안정성을 저해하는 중요한 손상인자로 나타났다. 원정비 재질의 물성평가를 위한 초음파 측정에서는 비신, 대좌, 옥개석 순으로 속도가 빠르게 나타났다. 원정비에 다양한 형태로 발생한 균열들의 현황과 산출상태를 정량적으로 산출하기 위해 초음파를 이용한 To-Tc법으로 균열의 심도를 측정한 결과, 0.6~24.1cm로 다양한 깊이를 보였다.

통영 세병관 초석의 암석학적 특성 및 비파괴 손상평가 (Petrological Characteristics and Nondestructive Deterioration Assessments for Foundation Stones of the Sebyeonggwan Hall in Tongyeong, Korea)

  • 한두루;김성한;박석태;이찬희
    • 자원환경지질
    • /
    • 제54권2호
    • /
    • pp.199-212
    • /
    • 2021
  • 세병관(국보 제305호)은 통영 삼도수군통제영에 위치하며, 1605년에 창건한 이래 최근까지 수차례의 중건, 중수, 보수 및 복원을 거쳤다. 연구대상인 세병관 초석은 모두 50개로 다양한 표면손상이 나타난다. 이 초석은 총 6개의 암종으로 구성되어 있으며, 대부분은 석영안산암질 래피리 응회암이다. 보수용 대체석 수급을 위한 산지해석 결과, 대부분의 암석은 초석과 산출상태, 기재적, 광물학적 및 전암대자율 등 암석학적으로 높은 동질성을 갖는 것으로 나타났다. 초석의 손상유형 중에는 표면의 박리와 박락이 가장 심한 것으로 나타났으며, 무기오염물 분석을 통한 손상메커니즘으로 볼 때 해풍 및 복합적인 환경에 의한 염풍화가 주된 원인으로 판단된다. 초석의 기계적 내구성으로 보아 현재 물성 저하로 부재의 교체가 필요한 것은 없으나 표면적인 손상을 늦추기 위한 보존처리가 필요할 것으로 보인다. 이 초석은 표면에 발생한 물리적 손상과 내부 결함을 유발하는 암석학적 요인이 복합적으로 작용하였다. 따라서 세병관의 장기적 보존을 위해서는 주기적인 상태 진단과 모니터링이 요구된다.

영천 신월동삼층석탑의 재질특성과 훼손도 정량평가 (Material Characteristics and Quantitative Deterioration Assessment of the Sinwoldong Three-storied Stone Pagoda in Yeongcheon, Korea)

  • 이정은;이찬희;채성태;정영동
    • 보존과학회지
    • /
    • 제26권4호
    • /
    • pp.349-360
    • /
    • 2010
  • 영천 신월동삼층석탑(보물 제465호)은 주로 담회색의 정동질 알칼리화강암으로 구성되어 있다. 주요 구성광물은 흑운모, 석영, 각섬석, 정장석 및 사장석이다. 이 탑은 기단부의 팔부중상을 중심으로 황갈색 및 흑색 변색이 심하며, 옥개석은 조각된 부분을 중심으로 탈락된 암편 등을 시멘트 몰탈로 보수한 흔적이 많다. 이 석탑의 전면에 걸쳐 적외선열화상분석을 실시한 결과, 미세균열과 박리 및 박락 현상은 심하지 않은 것으로 나타났다. 표면 변색 부위에 대한 휴대용 XRF 측정 결과, 변색 지점을 중심으로 Fe(평균 5,599ppm)와 S(평균 3,270ppm) 농도가 높게 나타났다. 또한 흑색 오염물로 피복된 부위는 Mn 함량(평균 2,155ppm)이 높게 검출되었다. 이는 암석 성분의 유리에 의한 무기오염물과 생물체의 고사에 의한 유기오염물이 공존하는 것이다. 전체적인 물리적 풍화는 북면(42.6%)과 남면(40.5%)에서 높게 나타나며 서면(30.6%)와 동면(34.0%)은 비슷한 훼손 양상을 보였다. 또한 변색 및 생물학적 풍화는 각각 북면(31.8%)과 동면(11.8%)이 가장 심하였다. 따라서 이 석탑은 생물 오염에 대한 세정과 약화된 재질에 대한 보존처리 및 지속적인 모니터링이 필요한 것으로 나타났다.

목조문화재 열화 및 보존기술에 관한 연구(제1보) -장경각 구조부재중 큰기둥의 생물적 열화 특성 - (Deterioration and Preservation Technique of Wooden Cultural Properties (Part I) -Biodeterioration of Wooden Round Columns, Janggeongpanjeon, Built in 15 century-)

  • 김영숙;윤정희;강호양;박상진
    • Journal of the Korean Wood Science and Technology
    • /
    • 제35권1호
    • /
    • pp.51-63
    • /
    • 2007
  • 국보 제32호인 팔만대장경을 보관하고 있으며 UNESCO가 정한 세계문화유산이기도 한 장경판전의 목재 구조부재중 큰기둥에 대한 생물인자에 의한 열화 특성을 조사 연구하였다. 장경판전의 법보전과 수다라장의 목재부재를 대상으로 연구 검토한 결과, 목재 부재 및 부위 그리고 주변 환경에 따라 다양한 열화 현상이 있음이 밝혀졌다. 부재의 주요 열화는 미생물에 의한 부후현상으로 밝혀졌으나, 부후가 나타난 부분들은 하나의 부재에서 매우 국부적으로 발생하고 있었으며 이들을 잘 조치하면 대부분의 부재는 건전한 상태로 더 유지 할 수 있는 상황으로 고찰되었다. 수다라장 큰기둥의 부후지수가 더 심했다. 큰기둥의 소재로 사용된 수종의 내구성은 소나무, 전나무 및 상수리나무보다는 느티나무가 큰 것으로 조사되었다. 그러나 느티나무의 경우 일부 기둥에서 해충의 피해가 발견되었다. 기둥 위치에 따른 생물적 열화는 동북, 서북, 북향에 위치한 기둥이 다른 방향에 위치한 기둥에 비해 심한 경향을 보였다.

기능을 상실한 보 철거를 통한 하천생태통로 복원 - 곡릉천 곡릉2보 철거를 대상으로 - (Stream Eco-corridor Restoration by Out-aged Small Dam Removal - Focused on Gokreung River Gokreung 2 Small Dam Removal -)

  • 안홍규;우효섭;이동섭;김규호
    • 한국환경복원기술학회지
    • /
    • 제11권2호
    • /
    • pp.40-54
    • /
    • 2008
  • Small and large dams are installed in the course of a stream for maintaining the water level of the stream or obtaining agricultural water. Currently about 18,000 of them are installed in Korea to supply water. However, the environmental problems of small dams are well known : the interruption of stream eco-corridors, deterioration of water quality in the upper reaches of the small dam, changes in the habitats of riparian organisms, damages to the stream scenery. In a very few of these small dams artificial eco-corridors like fishways are installed, but the number is very minimal.Accordingly, to efficiently restore stream eco-corridors by removing these small dams, it will be necessary to closely examine physical impacts, such as changes in the riverbed and changes in the shape of the stream caused by the removal, chemical impacts, such as changes in water quality, and transport and accumulation of contaminated sediments and biological impacts, such as changes in the habitats of organisms, and develop related technologies in advance, and have these technologies verified through demonstration application in the sites. In this study, we analyzed the physical, chemical and ecological impacts of the removal of the above-mentioned small dams, and conducted a research on the demonstration small dam removal project for a spot investigation. As a result, the small dam removal will restore the eco-corridor, there by improving the habitat of fishes and crustaceans. The number of major underwater organisms inhabiting the Gokreungcheon, such as Korean spotted sleepers, Chinese minnows, Microphysogobio yaluensis, Abbottina rivularis, stone morokos, striped shinners, long-nosed barbels, and Chinese mitten crabs, is expected to increase, and the food chain in the ecosystem will improve so that species diversity will improve as well.

서울 홍지문 오간수문의 암석기재적 분석과 손상도 평가 및 보존처리 (Conservation Treatment, Deterioration Assessment and Petrography of the Hongjimun Ogansumun (Five-arched Floodgates) in Seoul)

  • 이명성;김지영;이찬희;김영택;한병일
    • 보존과학회지
    • /
    • 제29권1호
    • /
    • pp.1-14
    • /
    • 2013
  • 홍지문 오간수문은 홍지문에 부속된 홍예 수문이다. 이들의 주요 구성암석은 흑운모화강암, 홍장석화강암, 화강섬록암으로서 서울 인근에 분포하는 화강암류와 암석기재적 특징이 매우 유사하다. 오간수문에 나타난 손상현상은 주로 백색, 흑색 및 황색 변색이며 백화현상이 가장 심각하다. 5기의 홍예 수문에서 공통적으로 측벽의 변색이 천장보다 심하고, 천장에서는 종유석이 성장하고 있다. 오염물 분석 결과, 백화현상을 야기하는 물질은 다양한 형태를 보이는 방해석으로 판명되었다. 보존처리는 오간수문 전면에 대한 건식세정과 표면에 피각되어 있는 백화물질을 제거하기 위해 부분적으로 고압세척 및 백화제거제 등을 사용하였다. 현재는 일차적인 보존처리가 완료되어 양호한 상태를 보이고 있으나 향후 오간수문의 훼손을 저감하기 위해서는 수문 상부에 배수로를 확보하여 수분의 이동과 배출을 제어하는 것이 필요하다.

의치 연성이장재에 대한 Candida albicans의 부착과 침투연구 (IN VITRO STUDY ON THE ADHERENCE AND PENETRATION OF CANDIDA ALBICANS INTO DENTURE SOFT LINING MATERIALS)

  • 김민주;신상완;이정열
    • 대한치과보철학회지
    • /
    • 제44권4호
    • /
    • pp.466-476
    • /
    • 2006
  • Purpose : Colonization of denture soft lining materials by Candida albicans can result in clinical problem, and deterioration of the materials. This study aimed to compare the retention and penetration of C. albicans into four denture soft lining materials commonly used. Materials and methods : Four denture soft lining materials (Coe-comfort$^{(R)}$, Coe-soft$^{(R)}$, GC soft liner$^{(R)}$, and Tissue conditioner$^{(R)}$) discs were prepared to glass slide and dental stone. Adherence of yeast to surfaces was monitored after one hour incubation of standardized washed cell suspension with test disc surfaces. Adherent cells stained with acridine orange were counted fluorescence microscopy. Penetration of yeast into materials bonded with acrylic resin after 1, 2, 3,4, 5, 6 and 7 days incubation was observed through sections stained using acridine orange and estimated to quantitative analysis using radioisotope. Results : There was statistical significance in cell numbers between smooth and rough surfaces(p<0.05). Higher numbers of cells were observed on rough surfaces. There was statistical significance in adherent cell numbers into smooth and rough surfaces individually(p<0.05). According to the increase of incubation periods, the cells penetrated into denture soft lining materials were shown to increase. The differences among all kinds of soft liner were statistically significant(p<0.05),and the largest number of cells penetrated into soft liners was observed in the Coe-soft$^{(R)}$. Conclusion : Initial adherence and penetration of yeast into denture soft lining materials has been influenced by surface roughness and chemical composition of them. The selection of appropriate materials and their fabrication may promote clinical performance.

765 kV용 400 kN 현수애자 개발 (Development of Extra High Voltage(400kN) Porcelain Insulator for Transmission Lines)

  • 최인혁;최장현;이동일;최연규
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제52권8호
    • /
    • pp.348-353
    • /
    • 2003
  • This paper was the research of high voltage suspension insulator (400 [kN]) including pottery stone, feldspar, clay and alumina of 17 [wt%]. The slurry was fabricated after ball milling mixed raw materials. Green compacts were made by the extrusion of jiggering method and were sintered at 1300[$^{\circ}C$] for 50 [min.] in the tunnel kiln. The sintered density was reached to 97% of theoretical density, and the bending strength was 1658 [k $g_{f}$/$\textrm{cm}^2$] and hardness and fracture toughness which was measured by ICL( indentation crack length ) method were 1658 (kgf/$\textrm{cm}^2$) and 27.5 [Gpa], respectively. In measurement of tana and insulation break voltage of 400 (kN) porcelain, tan$\delta$ took some numerical value between 17${\times}$10$_{-3}$ and 61${\times}$10$_{-3}$ and insulation break voltage value was 19.9$\pm$1.4 [㎸/mm]. The test was performed to research whether the shape of pin affect a overvoltage break load or not As a consequence, when a pin was designed a pin diameter 51 [mm] with the bottom form of two-step constructed with straight in the suspension insulator, Insulator showed overvoltage break load 52 [ton] of the highest value and reflected a fine characteristic in aged deterioration test which is one of the accelerated aging test. Also it could be confirmed a fine characteristic through performing the test that electrical property of insulator was established correctly in accordance with IEC 60383-1 standards.s.