Effects of Spinning Conditions on Properties of Polyester Yarn Prepared using an Ultra-high-speed Melt Spinning Technique Equipped with a Steam Chamber

  • Ho, Yo-Seung;Kim, Hak-Yong;Jin, Fan-Long;Park, Soo-Jin
    • Bulletin of the Korean Chemical Society
    • /
    • 제31권11호
    • /
    • pp.3252-3258
    • /
    • 2010
  • In this study, the effects of the various parameters of spinning and drawing processes on the properties of polyester full drawn yarn (FDY) prepared by steam processing during high-speed spinning were investigated using several techniques. The wet shrinkage ratio of the FDY was able to be manipulated by controlling the temperature and draw ratio. The FDY made using the steam high speed spinning technique exhibited identical properties (such as tenacity, elongation, and wet shrinkage ratio) to that of regular FDY, made using the spin-draw process. FDY prepared using the steam process during high-speed spinning showed excellent dyeability. The dye pick-up of the polyester yarn spun at high-speed spinning was found to be improved when dyed under an atmospheric pressure of $100^{\circ}C$. This result was the same as regular FDY dyed under a high pressure of $130^{\circ}C$.

Rayon-like 섬유의 최적 방사 조건 (Optimum Condition of Spinning for Rayon-like Yarn)

  • 안영무
    • 패션비즈니스
    • /
    • 제12권1호
    • /
    • pp.120-128
    • /
    • 2008
  • Rayon fiber as clothing material has silk-like property which relates to other synthetic fibers. It has many advantages that is required to women's clothes. However rayon has many shortcomings. Therefore this research is to spin rayon-like polyester which has high contraction property to be synthesized by previous research to solve those shortcomings and to maintain advantages of rayon. The contraction ratio of regular polyester is 30% and the contraction ratio of this synthesized polyester is over 60%. The spinning temperature of regular polyester ranges from $285^{\circ}C$ to $300^{\circ}C$. However, this copolymer is set range from $270^{\circ}C$ to $290^{\circ}C$, which is $10^{\circ}C$ less than regular polyester due to decreasing melting temperature. The spinning velocity effects the tensile strength and elongation of yarn magnificently. The high velocity of spinning makes yarn highly oriented, increases the tensile strength and decreases the elongation. This research defines the condition as following; draw ratio 2.734, First roller temperature $85^{\circ}C$, Slit heater temperature $175^{\circ}C$.