  • In this study, we evaluated the early strength of red clay soil with the polymer aqueous solution at rammed earth construction. In order to satisfy the demolding strength of the formwork be due to the rammed of red clay soil, the polymer aqueous solution was added to evaluate the compressive strength at the early age according to the consolidation level. As a result, a high compressive strength was exhibited with the formulation to which the polymer aqueous solution was added.

  • PDF

Study properties of soft subgrade soil stabilized by sewage sludge/lime and nano-SiO2

  • Lin, Deng-Fong;Luo, Huan-Lin;Chen, Chien-Ta;Cai, Ming-Du
    • Geomechanics and Engineering
    • /
    • 제10권6호
    • /
    • pp.793-806
    • /
    • 2016
  • The pozzolanic characteristics of a sludge incinerated into ash were determined in this study. Lime is commonly used as a stabilizer for the treatment of soils, whereas sewage sludge ash (SSA) is often applied with lime to improve soft subgrade soil. In this study, a cohesive soil categorized as A-4 (low-plasticity clay) by AASHTO classifications was mixed with SSA/lime with a 3:1 ratio. Nano-$SiO_2$ was also added to the soil. To identify changes in the workability, strength, permeability, and shear strength of the soft subgrade soil, basic soil tests were conducted, and the microstructure of the treated soil was analyzed. The results indicate that SSA/lime mixtures improve the properties of soft subgrade soil and transform the soil from "poor subgrade soil" to "good to excellent subgrade soil" with a CBR > 8. Additionally, the addition of 2% nano-$SiO_2$ increases the unconfined compressive strength of soft subgrade soil treated with SSA/lime mixture by approximately 17 kPa. However, the swelling of the treated soil increased by approximately 0.1% after the addition of nano-$SiO_2$ and lime. Thus, soil swelling should be considered before lime and nano-$SiO_2$ are applied to soft subgrade soil.

저시멘트 소일콘크리트의 유동성 및 압축강도 특성 (Flow and Compressive Strength Properties of Low-Cement Soil Concrete)

  • 박종범;양근혁;황철성
    • 한국건설순환자원학회논문집
    • /
    • 제6권1호
    • /
    • pp.1-7
    • /
    • 2018
  • 본 연구에서는 산업부산물을 다량 활용한 소일콘크리트의 유동성 및 강도발현에 대한 결합재-흙의 비(B/S) 및 물-결합재비(W/B)의 영향을 평가하였다. 보통 포틀랜드 시멘트의 부분 치환재로서 바이패스 더스트 10%, 고로슬래그미분말 40%, 순환유동층 플라이애시 25%가 사용되었다. 저시멘트 결합재와 함께 사질토 또는 점성토를 사용하여 18 소일콘크리트 배합이 실험되었다. 실험결과 소일콘크리트의 유동성은 대상토(점성토 또는 사질토)의 종류에 관계없이 동일한 W/B에서 B/S가 클수록 증가하였다. 압축강도는 점성토 콘크리트보다 동일 배합조건을 갖는 사질토 콘크리트에서 컸다. 산업부산물 다량 활용 소일콘크리트의 배합은 압축강도 및 고유동성을 고려하면 대상토에 관계없이 B/S가 0.35 그리고 W/B는 175%가 추천될 수 있었다.

폴리아크릴아마이드를 기반으로 하는 다기능성 토양안정제의 특성에 관한 연구 (Research on Characteristics of Multifunctional Soil Binder Based on Polyacrylamide)

  • 김진경;김대호;주상현;이명천
    • 공업화학
    • /
    • 제29권2호
    • /
    • pp.155-161
    • /
    • 2018
  • 훼손된 비탈면을 효율적으로 복구하고 토양을 견고하게 지지하고 식물 생장을 도울 수 있는 토양바인더 사용이 매우 중요하다고 할 수 있다. 이러한 토양바인더는 토양을 오염시키지 않는 친환경 소재이면서 토양의 생태를 복원할 수 있어야 한다. 본 연구에서는 토양바인더 외에 흡수제와 응집제를 첨가하여, 최적의 함수율, 투수계수, 직접전단강도 값을 갖는 조건을 도출하였다. 토양바인더로는 다양한 음이온강도의 polyacrylamide (PAM)를, 흡수제로는 super absorbent polymer (SAP), 응집제로는 cellulose ether (CE)를 사용하여 그 효과를 관찰하였다. 그 결과 우선 토양바인더를 사용한 경우 토양시험편의 직접전단강도와 함수율을 각각 수십 배 이상 그리고 두 배 이상 증가시킬 수 있었으며 변수위 투수계수를 낮춤으로 인해 방수의 효과가 증가함을 관찰되었다. 첨가제로서 SAP를 사용한 경우 그 효과를 더욱 높일 수 있었고 SAP의 응집력을 높이기 위해 첨가된 CE 역시 직접전단강도와 함수율을 높임을 관찰할 수 있었다.

표층처리를 위한 현장의 강도적용에 관한 연구 (A Study on Applicability of Soil Strength for Surface Treatment)

  • 양태선;김병호
    • 한국지반신소재학회논문집
    • /
    • 제4권3호
    • /
    • pp.45-52
    • /
    • 2005
  • 대부분의 항만구조물은 초연약 지반상에 축조되고 있으며 도로나 건물부지에는 지반개량이 필요하다. 이 논문에서는 여러 사례연구를 통하여 표층처리후의 복토사례에 대하여 몇가지 고려사항을 언급하였다. 또한, 모래나 산토를 이용한 복토공법에 대하여 강도적용이 고려되었다. 국내 복토공법 토목섬유 인장강도는 15t/m, 복토두께는 1.6~3.1m, 점토지반의 표층강도는 $0.2{\sim}1.2t/m^2$이 대표적이다. 표층처리공 시공시 발생되는 지반교란, 점토유출, 장비전도 등의 사고를 최소화하기 위한 연구가 필요하다.

  • PDF

Predicting strength development of RMSM using ultrasonic pulse velocity and artificial neural network

  • Sheen, Nain Y.;Huang, Jeng L.;Le, Hien D.
    • Computers and Concrete
    • /
    • 제12권6호
    • /
    • pp.785-802
    • /
    • 2013
  • Ready-mixed soil material, known as a kind of controlled low-strength material, is a new way of soil cement combination. It can be used as backfill materials. In this paper, artificial neural network and nonlinear regression approach were applied to predict the compressive strength of ready-mixed soil material containing Portland cement, slag, sand, and soil in mixture. The data used for analyzing were obtained from our testing program. In the experiment, we carried out a mix design with three proportions of sand to soil (e.g., 6:4, 5:5, and 4:6). In addition, blast furnace slag partially replaced cement to improve workability, whereas the water-to-binder ratio was fixed. Testing was conducted on samples to estimate its engineering properties as per ASTM such as flowability, strength, and pulse velocity. Based on testing data, the empirical pulse velocity-strength correlation was established by regression method. Next, three topologies of neural network were developed to predict the strength, namely ANN-I, ANN-II, and ANN-III. The first two models are back-propagation feed-forward networks, and the other one is radial basis neural network. The results show that the compressive strength of ready-mixed soil material can be well-predicted from neural networks. Among all currently proposed neural network models, the ANN-I gives the best prediction because it is closest to the actual strength. Moreover, considering combination of pulse velocity and other factors, viz. curing time, and material contents in mixture, the proposed neural networks offer better evaluation than interpolated from pulse velocity only.

풍화잔적토의 불포화전단강도에 미치는 순연직응력의 영향 (Influence of net normal stresses on the shear strength of unsaturated residual soils)

  • 성상규;이인모
    • 한국지반공학회:학술대회논문집
    • /
    • 한국지반공학회 2002년도 봄 학술발표회 논문집
    • /
    • pp.139-146
    • /
    • 2002
  • The characteristics and prediction model for the shear strength of unsaturated residual soils was studied. In order to investigate the influence of the net normal stress on the shear strength, unsaturated triaxial tests and SWCC tests were carried out varying the net normal stress, and the experimental data for unsaturated shear strength tests were compared with predicted shear strength envelopes using existing prediction models. It was shown that the soil - water characteristic curve and the shear strength of the unsaturated soil varied with the change of the net normal stress. Therefore, to achieve a truly descriptive shear strength envelope for unsaturated soils, tile effect of the normal stress on the contribution of matric suction to the shear strength has to be taken into consideration. In this paper, a modified prediction model for the unsaturated shear strength was proposed.

  • PDF

시멘트함량 및 다짐함수비가 Soil Cement의 압축강도에 미치는 영향에 관한 연구 (A Study on the Effects of Molding Water Content and Cement Content on Unconfined Compressive Strength of Soil Cement Mixtures)

  • 김재영;강예묵
    • 한국농공학회지
    • /
    • 제17권1호
    • /
    • pp.3685-3701
    • /
    • 1975
  • This study was conducted to investigate the strength of soil cements for varied molding water content and cement content(3,6,9,12%) in four cementstabilized soils(KY: sand, MH: sad, SS: sandy loam, JJ: loam). The eoperimental results obtainedfrom unconfined compressive strength tests are asfollows: 1. The optimum moisture content increased in accordance with the increase of the cement while maximum dry density didn't change uniformly. 2. The moisture content for maximum strength was higher than the optimum moisture content in the higher cement content. Moisture-density curves showed a dull peak in the higher cement contents, on the other hand, a sharp peak in the lower cement contents. 3. In molding the specimen with the approximate optimum moisture content, the maximum strength showed at the wet side of the optimum moisture content. 4. SS and JJ maybe used as cement-stabilized base of road to require 300PSI of compressive strength cured seven days, but MH and KY may be not adequate. 5. In soil cement, the better the grain size distribution was, the stronger the compressive strength was itn general. 6. The relation between 28-day strengh and 7-day strength in the cementstabilized four soils may be expressed as follows: q28=1.55q7+1.5 in which q28:28-day strength. q7:7-day strength.

  • PDF

함수비, 양생온도 및 흙의 입도가 Soil-Cement의 압축강도에 미치는 영향에 관한 연구(I) (Studies on the Effect of Water Content, Curing Temperature and Grain Size Distribution of Soils on Unconfined Compressive Strength of Soil-Cement Mixtures.)

  • 김재영;강신업
    • 한국농공학회지
    • /
    • 제19권1호
    • /
    • pp.4312-4322
    • /
    • 1977
  • In order to investigate the effect of the water content and the accelerated curing on the strength of the soil-cement mixtures, laboratory test of soil cement mixtures was performed at five levels of water content, four levels of accelerated curing temperatures, three levels of normal curing periods, and six levels of accelerated curing time. Also this study was carried out to investigate the effect of grain size distribution of 21 types of soils on the strength of soil-cement mixtures at four levels of cement content and three levels of curing time. The results are summarized as follows: 1. Optimum moisture content increased with increase of the cement content, but maximum dry density was changed ununiformly with cement content. Water content corresponding to the maximum strength was a little higher than the optimum moisture content along the increase of cement content. 2. In molding the specimens with the optimum moisture content, the maximum strength appeared at the wet side of the optimum moisture content. 3. According to increase of curing temperature as 30, 40, 50, and 60$^{\circ}C$, unconiiend compressive strength of soil-cement mixtures increased, the rate of increase at the early curing period was large, and approximately 120 hours was suifficient to harden soil-cement mixtures completely. 4. The strength of soil-cement mixtures at the curing temperature of 10$^{\circ}C$ decreased at the rate of 30 to 50 percent than at the curing temperature of 20$^{\circ}C$, and the strength of soil-cement mixtures at the curing temperature of 0$^{\circ}C$ increased a little with increase of curing time. 5. Although the strength of soil-cement mixtures seemed to be a little affected by the temperature difference between day time and night, it was recommended that reasonable working period was the duration from July to August of which average maximum temperature of Korea was approximately 30$^{\circ}C$. 6. Accelerated curing time corresponding to the normal curing time of 28-day was shorten with increase of curing temperature, also it was a little affected by the cement. Accelerated curing time that the strength of soil-cement mixtures for the cement of 9 percent and the curing temperature of 60was shorten with increase of curing temperature, also it was a little affected by the cement. Accelerated curing time that the strength of soil-cement mix- tures for the cement of 9 percent and the curing temperature of 60$^{\circ}C$ was 45 hours at the KY sample, 50 hours at the MH, 40 hours at the SS, and 34 hours at the JJ respectively. 7. Accelerated curing time was depended upon the grain size distribution of soil, it decreased with increase the percent passing of No. 200 sieve. 8. Relationship between the normal curing times and the accelerated curing times showed that there was a linear relationship between them, its slope decreased with increase of curing temperature. 9. The most reasonable soil of the soil-cement mixtures was the sandy loam which was a well graded soil. Assuming the base of road requiring 7-day strength of 21 kg/$\textrm{cm}^2$ being used, the soil-cement mixtures could be obtained with adding 6 percent of cement in such a sails S-7, S-8, S-9, S-10, S-11, S-12, S-13. 10. The regression equation between the 28-day and the 7-day strength was obtained as follow; q28=1.12q7,+6.5(r=0.96).

  • PDF

유류 오염 점성토의 강도 특성 (The Strength Characteristic of Oil Contaminated Clayey Soil)

  • 권무남;김현기;남효석;구정민
    • 한국농공학회:학술대회논문집
    • /
    • 한국농공학회 2003년도 학술발표논문집
    • /
    • pp.183-186
    • /
    • 2003
  • This study was conducted to evaluate effects by adding oil to clay soil and influences of remained oil in soil as time elapsed. Unconfined compression test and direct shear test were performed to analyze strength properties of contaminants in clayey soil. As a results of $q_u$ test for kerosene and diesel contaminated clayey soil indicate that were decreased from near 5% oil content rapidly and the declination of strength were blunt as oil content over 10%. The cohesions(c) and internal friction angle(${\psi}$) of kerosene contaminated clayey soil were not varied as quantities of kerosene in clayey soil increased. In the case of diesel contaminated clayey soil, the cohesions(c) were decreased and the internal friction angle(${\psi}$) were increased.

  • PDF