A study on the fabrication of soda-lime glass by using refused coal ore and its properties (석탄 폐석을 이용한 소다라임계 유리의 제조 및 특성 연구)

  • Lim, Tae-Young;Jeong, Sang-Su;Hwang, Jong-Hee;Kim, Jin-Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.20 no.1
    • /
    • pp.43-52
    • /
    • 2010
  • Glass was fabricated by using refused coal ore obtained from Dogye coal mine in Samchuk. We additionally used soda ash and calcium carbonate as raw materials to make a glass with the chemical composition of soda-lime glass. And the properties of glass were measured when limestone was used as natural raw materials instead of calcium carbonate as chemical raw materials. Transparent glass was fabricated by melting raw materials at $1550^{\circ}C$ for 1 hr in an electrical furnace. The various kinds of glass samples were fabricated according to the kinds of refused coal ore and glass cullet. The optical properties of transmittance and color chromaticity were measured by UV/VIS/NIR spectrometer and the thermal properties of thermal expansion coefficient and softening point were measured. Transparent glass with the transmittance of over 70% in visible range was fabricated by using normal refused coal ore and black colored glass with the transmittance of 0~35% was fabricated by using shel1 type refused coal ore. Therefore, it is concluded that refused coal ore can be used for raw materials to manufacture secondary glass products such as a glass tile and foamed glass panel for construction material.

Formant-broadened CMS Using the Log-spectrum Transformed from the Cepstrum (켑스트럼으로부터 변환된 로그 스펙트럼을 이용한 포먼트 평활화 켑스트럴 평균 차감법)

  • 김유진;정혜경;정재호
    • The Journal of the Acoustical Society of Korea
    • /
    • v.21 no.4
    • /
    • pp.361-373
    • /
    • 2002
  • In this paper, we propose a channel normalization method to improve the performance of CMS (cepstral mean subtraction) which is widely adopted to normalize a channel variation for speech and speaker recognition. CMS which estimates the channel effects by averaging long-term cepstrum has a weak point that the estimated channel is biased by the formants of voiced speech which include a useful speech information. The proposed Formant-broadened Cepstral Mean Subtraction (FBCMS) is based on the facts that the formants can be found easily in log spectrum which is transformed from the cepstrum by fourier transform and the formants correspond to the dominant poles of all-pole model which is usually modeled vocal tract. The FBCMS evaluates only poles to be broadened from the log spectrum without polynomial factorization and makes a formant-broadened cepstrum by broadening the bandwidths of formant poles. We can estimate the channel cepstrum effectively by averaging formant-broadened cepstral coefficients. We performed the experiments to compare FBCMS with CMS, PFCMS using 4 simulated telephone channels. In the experiment of channel estimation, we evaluated the distance cepstrum of real channel from the cepstrum of estimated channel and found that we were able to get the mean cepstrum closer to the channel cepstrum due to an softening the bias of mean cepstrum to speech. In the experiment of text-independent speaker identification, we showed the result that the proposed method was superior than the conventional CMS and comparable to the pole-filtered CMS. Consequently, we showed the proposed method was efficiently able to normalize the channel variation based on the conventional CMS.

Adhesion Performance of Natural Rubber-based Pressure-Sensitive Adhesives for Protecting of Opto-functionalized Sheet (광기능성시트 보호용 천연고무계 점착제의 점착 물성)

  • Park, Young-Jun;Lim, Dong-Hyuk;Kim, Hyun-Joong;Song, Hyun-Suk;Kwon, Hyuk-Jin
    • Journal of Adhesion and Interface
    • /
    • v.8 no.2
    • /
    • pp.15-21
    • /
    • 2007
  • To prepare a natural rubber-based pressure-sensitive adhesive (PSA) for protection film of opto- functionalized sheet, natural rubber (NR) was blended with a DCPD type tackifier and three types of aliphatic hydrocarbon resins, respectively. Also, to supply low cohesion strength of NR, in the fixed ratio of tackifier, synthetic rubber, styrene-isoprene-styrene (SIS) block copolymer was blended with NR as a function of SIS contents. PSA performance of prepared PSAs was evaluated using probe tack and peel strength. Probe tack of NR/tackifier blends was increased with increasing tackifier contents, and showed maximum peak. In addition, probe tack of NR/tackifier blends slightly increased with increasing softening point of aliphatic hydrocarbon resins. Their peel strength increased up to 50 wt% of tackifier contents, but in the over contents of tackifier, they showed stick-slip failure mode. Finally, probe tack of NR/SIS/tackifier blends showed the maximum values at 20~40 wt% of tackifier contents, but at 20 wt% of tackifier contents, they showed fibrillation. For this reason, peel strength showed maximum values at 40 wt% of tackifier contents.

  • PDF

A Study on the Improvement of the Electrochemical Performance of Graphite Anode by Controlling Properties of the Coating Pitch (코팅 피치의 물성제어를 통한 흑연 음극재의 전기화학 성능 향상 연구)

  • Kim, Bo Ra;Kim, Ji Hong;Kang, Seok Chang;Im, Ji Sun
    • Applied Chemistry for Engineering
    • /
    • v.33 no.5
    • /
    • pp.459-465
    • /
    • 2022
  • A pitch coating method was proposed for the purpose of improving the electrochemical properties of natural graphite. The synthesis conditions of pitch coating were optimized via measuring electrochemical properties of pitch-coated graphite anodes. As the synthesis temperature increased, the thermal stability was improved in addition to an increase in the softening point and residual carbon weight. However, the synthesis temperature of 430 ℃ resulted in the synthesis of a large amount of NI (NMP Insoluble) due to excessive condensation reaction. As the surface uniformity and coating thickness increased due to high thermal stability, the initial coulombic efficiency and rate capability of the pitch-coated graphite were improved. However, the graphite coated with the pitch containing excessive NI showed lower electrochemical properties than the uncoated graphite. NI had low dispersibility and formed spheres after heat treatment, so it formed the heterogeneous and thicker SEI layer. The optimum conditions for forming a uniform surface and an appropriate coating layer were investigated.

A Study on the Bituminization Process of Radiative Liquid Waste (II)

  • Lee, Sang-Hoon;Yoon, Myung-Hwan;Lee, Moon-Deuk
    • Nuclear Engineering and Technology
    • /
    • v.8 no.4
    • /
    • pp.231-242
    • /
    • 1976
  • The effects of temperature and pressure of leaching water on the leaching of radionuclides from bitumen-waste products were studied. The principal results are as follows: The fraction of $^{90}$ Sr and $^{137}$ Cs leached for periods of up to 120 days at 8atm was 2.1$\times$10$^{-6}$ ($\textrm{cm}^2$/g)$^{-1}$ , day$^{-1}$ and 6.02$\times$10$^{-5}$ ($\textrm{cm}^2$/g)$^{-1}$ day$^{-1}$ respectively and at 5$^{\circ}C$, 1.7$\times$10$^{-5}$ ($\textrm{cm}^2$/g)$^{-1}$ day$^{-1}$ and 4.01$\times$10$^{-5}$ ($\textrm{cm}^2$/g)$^{-1}$ day$^{-1}$ respectively. These values were lower than those in atmospheric pressure and room temperature. No diffence in the leaching rate with sea and distilled water was observed for the bitumen-waste products containing 40wt% salts. It appears that these results could be saved by improving safety in the dumping of sea. The effect of the softening point of pure asphalt or bitumen-waste product by $^{60}$ Co irradiation was increased with increasing total dose. Irradiation of asphalts at a total dose of 5.8$\times$10$^{8}$ rad showed no evidence of volume and caused no swelling. The functional groups of blown asphalt by infrared spectra are also identified.

  • PDF

Effects of Boliing, Steaming, and Chemical Treatment on Solid Wood Bending of Quercus acutissima Carr. and Pinus densiflora S. et. Z. (자비(煮沸), 증자(蒸煮) 및 약제처리(藥劑處理)가 상수리나무와 소나무의 휨가공성(加工性)에 미치는 영향(影響))

  • So, Won-Tek
    • Journal of the Korean Wood Science and Technology
    • /
    • v.13 no.1
    • /
    • pp.19-62
    • /
    • 1985
  • This study was performed to investigate: (i) the bending processing properties of silk worm oak (Quercus acutissima Carr.) and Korean red pine (Pinus densiflora S. et Z.) by boiling and steaming treatments; (ii) the effects of interrelated factors - sapwood and heartwood, annual ring placement, softening temperature and time, moisture content. and wood defects on bending processing properties; (iii) the changing rates of bending radii after release from a tension strap, and (iv) the improving methods of bending process by treatment with chemicals. The size of specimens tested was $15{\times}15{\times}350mm$ for boiling and steaming treatments and $5{\times}10{\times}200mm$ for treatments with chemicals. The specimens were green for boiling treatments and dried to 15 percent for steaming treatments. The specimens for treatments with chemicals were soaked in saturated urea solution, 35 percent formaldehyde solution, 25 percent polyethylene glycol -400 solution, and 25 percent ammonium hydroxide solution for 5 days and immediately followed the bending process, respectively. The results obtained were as follows: 1. The internal temperature of silk worm oak and Korean red pine by boiling and steaming time was raised slowly to $30^{\circ}C$ but rapidly from $30^{\circ}C$ to $80-90^{\circ}C$ and then slowly from $80-90^{\circ}C$ to $100^{\circ}C$. 2. The softening time required to the final temperature was directly proportional to the thickness of specimen. The time required from $25^{\circ}C$ to $100^{\circ}C$ for 15mm-squared specimen was 9.6-11.2 minutes in silk worm oak and 7.6-8.1 minutes in Korean red pine. 3. The moisture content (M.C.) of specimen by steaming time was increased rapidly first 4 minutes in the both species, and moderately from 4 to 20 minutes and then slowly and constantly in silk worm oak, and moderately from 4 to 15 minutes and then slowly and constantly in Korean red pine. The M.C. of 15mm-squared specimen in 50 minutes of steaming was increased to 18.0 percent in the oak and 22.4 percent in the pine from the initial conditioned M.C. of 15 percent The rate of moisture adsorption measured was therefore faster in the pine than in the oak. 4. The mechanical properties of the both species were decreased significantly with the increase of boiling rime. The decrement by the boiling treatment for 60 minutes was measured to 36.6-45.0 percent in compressive strength, 12.5-17.5 percent in tensile strength, 31.6-40.9 percent in modulus of rupture, and 23.3-34.6 percent in modulus of elasticity. 5. The minimum bending radius (M.B.R.) of sapwood and heartwood was 60-80 mm and 90 mm in silk worm oak, and 260 - 300 mm and 280 - 300 mm in Korean red pine, respectively. Therefore, the both species showed better bending processing properties in sapwood than in heartwood. 6. The M.B.R. of edge-grained and flat-grained specimen in suk worm oak was 60-80 mm, but the M.B.R. in Korean red pine was 240-280 mm and 260-360 mm, respectively. Comparing the M.B.R. of edge-grained with flat-grained specimen, in the pine the edge-grained showed better bending processing property than the flat-grained. 7. The bending processing properties of the both species were improved by the rising of softening temperature from $40^{\circ}C$ to $100^{\circ}C$. The minimum softening temperature for bending was $90^{\circ}C$ in silk worm oak and $80^{\circ}C$ in Korean red pine, and the dependency of softening temperature for bending was therefore higher in the oak than in the pine. 8. The bending processing properties of the both species were improved by the increase of softening time as well as temperature, but even after the internal temperature of specimen reaching to the final temperature, somewhat prolonged softening was required to obtain the best plastic conditions. The minimum softening time for bending of 15 mm-squared silk worm oak and Korean red pine specimen was 15 and 10 minutes in the boiling treatment, and 30 and 20 minutes in the steaming treatment, respectively. 9. The optimum M.C. for bending of silk worm oak was 20 percent, and the M.C. above fiber saturation point rather degraded the bending processing property, whereas the optimum M.C. of Korean red pine needed to be above 30 percent. 10. The bending works in the optimum conditions obtained as seen in Table 24 showed that the M.B.R. of silk worm oak and Korean red pine was 80 mm and 240 mm in the boiling treatment, and 50 mm and 280 mm in the steaming treatment, respectively. Therefore, the bending processing property of the oak was better in the steaming than in the boiling treatment, but that of the pine better in the boiling than in the steaming treatment. 11. In the bending without a tension strap, the radio r/t of the minimum bending radius t to the thickness t of silk worm oak and Korean red pine specimen amounted to 16.0 and 21.3 in the boiling treatment, and 17.3 and 24.0 in the steaming treatment, respectively. But in the bending with a tension strap, the r/t of the oak and the pine specimen decreased to 5.3 and 16.0 in t he boiling treatment, and 3.3 and 18.7 in the steaming treatment, respectively. Therefore, the bending processing properties of the both species were significantly improved by the strap. 12. The effect of pin knot on the degradation of bending processing property was very severe in silk worm oak by side, e.g. 90 percent of the oak specimens with pin knot on the concave side were ruptured when bent to a 100 mm radius but only 10 percent of the other specimens with pin knot on the convex side were ruptured. 13. The changing rate in the bending radius of specimen bent to a 300 mm radius after 30 days of exposure to room temperature conditions was measured to 4.0-10.3 percent in the boiling treatment and 13,0-15.0 percent in the steaming treatment. Therefore, the degree of spring back after release was higher in the steaming than in the boiling treatment. And the changing rate of moisture-proofing treated specimen by expoxy resin coating was only -1.0.0 percent. 14. Formaldehyde, 35 percent solution, and 25 percent polyethylene glycol-400 solution found no effect on the plasticization of the both species, but saturated urea solution and 25 percent ammonium hydroxide solution found significant effect in comparison to non-treated specimen. But the effect of the treatment with chemicals alone was inferior to that of the steaming treatment, and the steaming treatment after the treatment with chemicals improved 10-24 percent over the bending processing property of steam-bent specimen. 15. Three plasticity coefficients - load-strain coefficient, strain coefficient, and energy coefficient - were evaluated to be appropriate for the index of bending processing property because the coefficients had highly significant correlation with the bending radius. The fitness of the coefficients as the index was good at load-strain coefficient, energy coefficient, and strain coefficient, in order.

  • PDF

Thermal Conductivity and Pore Characteristics of Low-Temperature Sintered Lightweight Aggregates Mode from Waste Glass and Bottom Ash (바텀애쉬와 폐유리를 사용하여 제조한 저온소성 경량골재의 열전도율과 기공특성)

  • Lee, Han-Baek;Ji, Suk-Won;Seo, Chee-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.22 no.6
    • /
    • pp.851-858
    • /
    • 2010
  • In this study, waste glass and bottom ash were used as basic materials in order to secure a recycling technology of by-products which was mostly discarded and reclaimed. In addition, because softening point of waste glass is less than $700^{\circ}C$ and bottom ash includes combustible material, it was possible to manufacture low-temperature sintering lightweight aggregates for energy saving at $800{\sim}900^{\circ}C$ that it is as much as 20~30% lower than sintering temperature of existing lightweight aggregates. Thermal conductivity of newly-developed lightweight aggregates was 0.056~0.105W/m. K and its porosity was 40.36~84.89%. A coefficient of correlation between thermal conductivity and porosity was -0.97, it showed very high negative correlationship. With this, we were able to verify that porosity is key factor to affect thermal conductivity. Microstructure of lightweight aggregates by $CaCO_3$ content and replacement ratio of bottom ash in the variation of temperature were that $CaCO_3$ content increased along with pore size while replacement ratio of bottom ash increased as pore size decreased. Specially, most pores were open pore instead of closed pore of globular shape when replacement ratio of bottom ash was 30%, and pore size was small about 1/10~1/5 as compared with case in bottom ash 0~20%. In addition, open pore shapes were remarkably more irregular form of open pore in $900^{\circ}C$ than $700^{\circ}C$ or $800^{\circ}C$ when replacement ratio of bottom ash was 30%. We reasoned hereby that these results will influence on absorption increase, strength and thermal conductivity decrease of lightweight aggregates.