• Title/Summary/Keyword: siloxane-containing polymers

Search Result 5, Processing Time 0.021 seconds

Control of Molecular Weight, Stereochemistry and Higher Order Structure of Siloxane-containing Polymers and Their Functional Design

  • Yusuke Kawakami;Yuning Li;Yang Liu;Makoto Seino;Chitsakon Pakjamsai;Motoi Oishi;Cho, Yeong-Bee;Ichiro Imae
    • Macromolecular Research
    • /
    • v.12 no.2
    • /
    • pp.156-171
    • /
    • 2004
  • We describe the precision synthesis schemes of siloxane-containing polymers, i.e., the control of their molecular weight, stereoregularity, and higher-order structures. First, we found a new catalytic dehydrocoupling reaction of water with bis(dimethylsilyl)benzene to give poly(phenylene-disiloxane). Together with this reaction, we applied hetero-condensations to the synthesis of thermally stable poly(arylene-siloxane)s. The dehydrocoupling reaction was applied to the synthesis of syndiotactic poly(methylphenylsiloxane) and poly(silsesquioxane)s, which we also prepared by hydrolysis and deaminative condensation reactions. We discuss the tendency for loop formation to occur in the synthesis of poly(silsesquioxane) by hydrolysis, and provide comments on the design of functionality of the polymers produced. By taking advantage of the low energy barrier to rotation in the silicon-oxygen bond, we designed selective oxygen-permeable membrane materials and liquid crystalline materials. The low surface free energy of siloxane-containing systems allows surface modification of a blend film and the design of holographic grating materials.

The Preparation of Polysiloxaneimide Membranes and their Pervaporation Properties (폴리실록산이미드 막의 제조와 투과증발특성)

  • Chang, Yeon-Hee;Kim, Jeong-Hoon;Lee, Soo-Bok;Rhee, Hee-Woo
    • Applied Chemistry for Engineering
    • /
    • v.10 no.7
    • /
    • pp.1041-1045
    • /
    • 1999
  • Three polysiloxaneimide(PSI) as membrane material were prepared by polycondensation of three aromatic dianhydrides(6FDA, BTDA, PMDA) with one siloxane-containing diamine(SIDA, aver. MW. 800). The PSIs were rubbery polymers containing 30~40 wt % of flexible siloxane chains and exhibited low density, high fractional free volume and low surface energy. They were used for pervaporation experiments with 0.05 wt % of four organic aqueous solutions containing ethyl acetate, methylene chloride, trichloroethylene, and toluene, respectively. With increasing hydrophobicity of organic solvents, both pervaporation selectivity and pemeation flux increase.

  • PDF

Gas Separation Properties of Microporous Carbon Membranes Containing Mesopores (중간기공을 갖는 미세다공성 탄소 분리막의 기체 투과 특성)

  • Shin, Jae Eun;Park, Ho Bum
    • Membrane Journal
    • /
    • v.28 no.4
    • /
    • pp.221-232
    • /
    • 2018
  • The silica containing carbon ($C-SiO_2$) membranes were fabricated using poly(imide siloxane)(Si-PI) and polyvinylpyrrolidone (PVP) blended polymer. The characteristics of porous carbon structures prepared by the pyrolysis of polymer blends were related with the micro-phase separation behaviors of the two polymers. The glass transition temperatures ($T_g$) of the mixed polymer blends of Si-PI and PVP were observed with a single $T_g$ using differential scanning calorimetry. Furthermore, the nitrogen adsorption isotherms of the $C-SiO_2$ membranes were investigated to define the characteristics of porous carbon structures. The $C-SiO_2$ membranes derived from Si-PI/PVP showed the type IV isotherm and possessed the hysteresis loop, which was associated with the mesoporous carbon structures. For the molecular sieving probe, the $C-SiO_2$ membranes were prepared with the ratio of Si-PI/PVP and the pyrolysis conditions, such as the pyrolysis temperature and the isothermal times. Consequently, the $C-SiO_2$ membranes prepared by the pyrolysis of Si-PI/PVP at $550^{\circ}C$ with the isothermal time of 120 min showed the $O_2$ permeability of 820 Barrer ($1{\times}10^{-10}cm^3(STP)cm/cm^2{\cdot}s{\cdot}cmHg$) and $O_2/N_2$ selectivity of 14.

A Study on the Properties of Condensed Ethyl Silicate Synthesized according to Water Contents in Ethanol (에탄올의 수분함량에 따라 합성된 Condensed Ethyl Silicate의 물성에 관한 연구)

  • Rho, Jae-Seong;Hong, Seong-Su;Seo, Shin-Seok
    • Applied Chemistry for Engineering
    • /
    • v.7 no.1
    • /
    • pp.91-100
    • /
    • 1996
  • Condensed ethyl silicate(CES) solutions were prepared from $SiCl_4$ and ethanol which is different in water content(2.5, 5.0 and 7.0wt.% ). To investigate the sol-gel transition behaviors of CES and PHT(partially hydrolyzed TEOS) solutions, the measurement of volume change, density, $SiO_2$ content, intrinsic viscosity and number average molecular weight were conducted with elapsed time. The polymer shapes of CES were discussed from the relation between the intrinsic viscosity[$\eta$] and the number average molecular weight($\bar{Mn}$). CES-3 prepared from ethanol containing 7.0wt.% $H_2O$ had different sol-gel transition behaviors from CES-1 (2.5wt.% $H_2O$) and CES-2(5.Owt.% $H_2O$), but similar behaviors to those of PHT which is used for controlling the hydrolysis rata of TEOS when composite ceramic materials were manufactured from silicon alkoxides. On the basis of Mark-Hawink relation, $[{\eta}]=K\bar{Mn}^{{\alpha}}$, the polymer shape of CES solutions were determined linear siloxane polymers because all solutions had ${\alpha}$ values in the range from 0.53 to 0.84. Especially, CES-3 showed to be a favorable raw materials for composite ceramics due to its similar properties to those of PHT.

  • PDF

Development of Immediate Face Lifting Technology for Reducing Wrinkles by Using Film-Forming Agent (피막 형성제를 이용한 즉각 리프팅 기술 개발)

  • Jun, Ji hyun;Ko, Eun ah;Han, Sang Gun;Kang, Hakhee
    • Journal of the Society of Cosmetic Scientists of Korea
    • /
    • v.44 no.3
    • /
    • pp.211-218
    • /
    • 2018
  • Instant face lifting cosmetics contain various film forming agents for stretching the wrinkles on the skin surface. But, most of the film-forming polymers have sticky feels. And they are easily scrubbed out when skin is rubbed on. In this study, we focused on the influence of sodium silicate that has rapid film forming effect on skin surface and immediate wrinkle reducing effect. Sodium silicate, also known as water glass or soluble glass, is a compound containing sodium oxide and silica. Sodium silicate is a white powder that is readily soluble in water, producing an alkaline solution. Sodium silicate is stable in neutral and alkaline solutions. The sodium silicate solution hardens by drying in air and rapidly forms a thin film. When the solution is applied to the skin, the fine membrane coating is formed by water evaporation and ionic bond re-formation. It also makes the strong siloxane (Si-O) bonding on the skin surface. When these fixation properties are applied to cosmetics, they can give remarkable skin tightening effect. The sodium silicate solution can provide the lifting effect by forming a film on skin at a proper concentration. But, skin irritation may be caused with too high concentration of sodium silicate. We studied a desirable range of the sodium silicate concentration and combination with other fixatives for skin care formulation that has no sticky feels and no scrubbing out phenomenon. Immediate lifting gel was developed by using sodium silicate and various thickening systems. Among of the various thickeners, aluminum magnesium silicate showed the best compatibility with sodium silicate for rapid lifting effect. This instant physical lifting gel was confirmed as a low stimulating formula by skin clinical test.