• Title/Summary/Keyword: silicate glass

Search Result 208, Processing Time 0.035 seconds

A Solid-state 27Al MAS and 3QMAS NMR Study of Basaltic and Phonolitic Silicate Glasses (현무암과 포놀라이트 비정질 규산염의 원자구조 차이에 대한 고상핵자기 공명 분광분석 연구)

  • Park, Sun Young;Lee, Sung Keun
    • Journal of the Mineralogical Society of Korea
    • /
    • v.28 no.1
    • /
    • pp.61-69
    • /
    • 2015
  • While the macroscopic properties and eruption style of basaltic and phonolitic melts are different, the microscopic origins including atomic structures are not well understood. Here we report the atomic structure differences of glass in diopside-anorthite eutectic composition (basaltic glass) and phonolitic glass using high-resolution 1D and 2D solid-state Nuclear Magnetic Resonance (NMR). The $^{27}Al$ MAS NMR spectra for basaltic glass and phonolitic glass show that the full width at half maximum (FWHM) of Al for basaltic glass is about twice than phonolitic glass, suggesting the topological disorder of basaltic magma is larger than that of phonolitic magma. The $^{27}Al$ 3QMAS NMR spectra for basaltic glass and phonolite glass show much improved resolution than the 1D MAS NMR, resolving Al and Al. Approximately 3.3% of Al is observed for basaltic glass, demonstrating the configurational disorder of basaltic magma is larger than phonolitic magma. This result confirms that the topological disorder of Al in basaltic glass is larger than that of phonolitic glass. The observed structural differences between basaltic glass and phonolitic glass can provide an atomistic origin for change of the macroscopic properties with composition including viscosity.

Consolidation of Quartz Powder by the Geopolymer Technique

  • Ikeda, Ko;Nakamura, Yoshinori
    • The Korean Journal of Ceramics
    • /
    • v.6 no.2
    • /
    • pp.120-123
    • /
    • 2000
  • The geopolymer technique may be a future-oriented technology for saving energies and resources. This technique requires 3 fundamental elements so-called filler, hardener and geopolymer liquor being generally an alkaline silicate solution. Quartz powder, water quenched granulated blast furnace slag and sodium silicate solution prepared from $Na_2O\cdot2SiO_2$were chosen for these three elements. After mixing these starting materials in appropriate proportions, monoliths were prepared by casting at room temperature. Strength tests showed the following results for 28d age speciment: 7.9-12.7 MPa in flexural strength and 20.2-32.8 MPa in compressive strength, depending on geopolymer liquor/solid ratio, P/S and fineness of the quartz powders used.

  • PDF

Effect of partial sintering of silicate soots on refractive index of the silcate glass films deposited by FHD Process (FHD 공정으로 Si wafer에 증착된 silicate soot의 부분 소결 처리가 굴절률 변화에 미치는 영향)

  • 유성우;정우영;백운출;한원택
    • Proceedings of the Optical Society of Korea Conference
    • /
    • 2002.07a
    • /
    • pp.46-47
    • /
    • 2002
  • Flame Hydrolysis Deposition (FHD) 공정은 SiC1$_4$, GeCl$_4$, POC1$_3$, BCl$_3$ 등의 원료를 사용하여 Si wafer 및 유리기판 위에 silicate soot를 증착하는 방법이며, 증착된 soot는 고온에서 소결과정을 거쳐 B$_2$O$_3$-P$_2$O$_{5}$ -GeO$_2$-SiO$_2$(BPGS)계 유리막으로 형성된다. 유리막의 굴절률은 SiC1$_4$, GeCl$_4$, POC1$_3$, BCl$_3$ 등의 원료 유량을 조절하여 변화가능하며 이를 이용하여 광도파로를 제작할 수 있다 특히 광통신에 사용할 수 있는 광증폭기 등의 능동형 광소자 제작을 위해서는 FHD공정을 통해 형성된 soot에 Er$^{3+}$ 등의 희토류 원소를 첨가하여야 한다. (중략)

  • PDF

Low Temperature Sintering of PZTN by the Liquid Phase Transient Processing (액상천이공정에 의한 PZTN의 저온소결에 관한 연구)

  • Kim, Chan-Yeong
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.50 no.12
    • /
    • pp.593-598
    • /
    • 2001
  • Transient liquid phase processing was investigated to decrease processing temperatures while maintaining useful piezoelectric properties in the lead zirconate titanate (PZT) system. Niobium oxide$(Nb_2O_5)$ modified crystalline PZT (PZTN) powder was combined with lead silicate $(PS; PbO-SiO_2)$ glass powder and crystalline titania, zirconia, and niobia. Firing above the melting temperature of the lead silicate $(PS; Tm \risingdotseq\; 714^{\circk}C)$ resulted in liquid phase densification of the PZTN followed by dissolution of the titania, zirconia, and niobia into the liquid phase, and crystallization of additional PZTN. The addition of crystalline titania, zirconia, and niobia to react with the lead oxide from the lead silicate phase resulted in an increase in the dielectric and Piezoelectric properties.

  • PDF

Formation and Structure of $CaO-P_2O_5-SiO_2$ Glasses ($CaO-P_2O_5-SiO_2$계 유리의 형성 및 구조)

  • 조정식;김철영
    • Journal of the Korean Ceramic Society
    • /
    • v.29 no.9
    • /
    • pp.729-738
    • /
    • 1992
  • The glass formation and structural change with the glass compositions were investigated in the CaO-P2O5-SiO2 system with less than 40 wt% of P2O5. The glass formation range was determined by XRD, SEM and EDS techniques for water quenched specimens. The structural analyses were made for binary CaO-SiO2 glasses and ternary CaO-P2O5-SiO2 glasses by using FT-IR and Raman spectroscopy. The glass formation was affected by CaO/SiO2 mole ratio, P2O5 content and primary crystalline phase. The stable glass formation range was found when the transformed CaO/SiO2 mole ratio (new factor derived from structural changes) was in the range of 0.72~1.15 with less than 10 mol% of P2O5. The structural analyses of CaO-SiO2 glasses indicated that as the CaO/SiO2 ratio was increased, the nonbridging oxygens in the structural unit of the glasses were increased. With addition of P2O5 to CaO-SiO2 glasses, the P2O5 enhanced the polymerization of [SiO4] tetrahedra unit in CaO-SiO2 glasses, which contained a large portion of nonbridging oxygen. The phosphate eliminated nonbridging oxygens from silicate species, forcing polymerization of silicate structures and produced in [PO4] monomer in glasses. When added P2O5 was kept constant, the structural change with various CaO/SiO2 ratio was very similar to that of CaO-SiO2 glasses.

  • PDF

Crystallization in Li$_2$O-A1$_2$O$_3$-SiO$_2$ Glass induced by 355 nm Nd:YAG Laser Irradiation

  • Lee, Yong-Su;Kang, Won-Ho
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.7 no.2
    • /
    • pp.43-46
    • /
    • 2000
  • Nd:YAG laser of 355 nm wavelength, which amounts to 3.5 eV, produced by a harmonic generator was used to create Ag metallic particles as seeds for nucleation in photosensitive glass containing $Ag^+$ and $Ce^{3+}$ . The pulse widths and frequency of the laser were 8ns and 10 Hz, respectively. For crystalline growth, heat-treatment following laser irradiation was carried out at $570^{\circ}C$ for 1h. Then, the $LiAlSi_3O^8$ crystal phase appeared in the laser irradiated lithium aluminum silicate glass. We present the effect of laser-induced nucleation compared with spontaneous nucleation by heat treatment fur crystallization in the glass.

  • PDF

Studies on the Glaze for High Expansion Glass Ceramics (고팽창 결정화 유리의 유약에 관한 연구)

  • 박용완;강은태;박찬성;전문덕
    • Journal of the Korean Ceramic Society
    • /
    • v.17 no.4
    • /
    • pp.213-216
    • /
    • 1980
  • A glass-ceramics material of composition %SiO_2$: 38.50, $Al_2O_3$: 26.00, $Na_2O$: 18.00, CaO: 6.00, MgO: 4.00, $TiO_2$: 7.50 was strengthened by coating a series of glazes$(SiO_2-B_2O_3-Al_2O_3-CaO-PbO-Na_2O-)$, which has lower thermal expansion coefficient than that of the glass-ceramics. The thermal expansion coefficient of the glazes ranges $80~90{\times}10^{-7}$cm/cm/$^{\circ}C$, whereas that of the glass-ceramics is $115{\times}10^{-7}$cm/cm/$^{\circ}C$. The glass-ceramics was identified to be composed of nepheline, carnegieite low form, and meta sodium silicate crystal by X-ray diffraction phase analysis. The glaze, having lower melting point and appropriate thermal expansion coefficient, was tried to be stable and good at secondary heat treatment.

  • PDF

Ambient Pressure Dried Silica Aerogel Thin Film from Water Glass

  • Cha, Young-Chul;Yoon, Jong-Seol;Lee, Jun;Hwang, Hae-Jin;Moon, Ji-Woong
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.2
    • /
    • pp.87-89
    • /
    • 2008
  • A nano structured silica aerogel thin film was manufactured from inexpensive sodium silicate (water glass) using an ambient pressure drying method. High purity silicic sol was prepared by passing a water glass solution through an ion exchange resin, and the gel films were prepared on a modified glass substrate via dip coating. The dip coating conditions, such as coating time and solvent, were optimized. The optical and physical properties of the obtained silica aerogel thin film were characterized using a UV-visable spectrometer and a scanning electron microscope.

New Glass Ceramics for Hard Disk Substrates with Improved Surface Flatness

  • Utsuno, Futoshi;Yamada, Yusuke;Takeya, Huminori;Yasui, Itaru
    • The Korean Journal of Ceramics
    • /
    • v.5 no.4
    • /
    • pp.363-367
    • /
    • 1999
  • New glass ceramics were investigated for the application as substrates to be used in hard disk devices. The glass system to precipitate lithium di-silicate was studied so as to optimize the composition to realize very high surface flatness. The addition of small amount of several metal oxides with high valences had very drastic effects on the microstructure, because they played a role of crystallization agents, and consequently it determined surface flatness even after the polishing process. The possible mechanism changes of crystal growth due to the addition of metal oxides were discussed in relation to the final micro-texture development. The glass ceramics with very high surface flatness(Ra=7.1 $\AA$) was obtained by the addition of the mixture of $P-2O_5 \;and \;MoO_3$ as crystallization agents.

  • PDF

Crystallization in Li20-A1203-Si02 Glass induced by 355nm Nd:YAG Laser Irradiation

  • Lee, Yong-Su;Kang, Won-Ho;Song, Sun-Dal
    • Proceedings of the International Microelectronics And Packaging Society Conference
    • /
    • 2000.04a
    • /
    • pp.112-117
    • /
    • 2000
  • Nd:YAG laser of 355nm wavelength, which amounts to 3.5eV, produced by a harmonic generator was used to create Ag metallic particles as seeds for nucleation in photosensitive glass containing Ag+ and Ce3+. The pulse widths and frequency of the laser were 8ns and 10Hz, respectively. For crystalline growth, heat-treatment following laser irradiation was carried out at $570^{\circ}C$ fur 1h. Then, the LiAlSi3O8. crystal phase appeared in the laser irradiated lithium aluminum silicate glass. We present the effect of laser-induced nucleation compared with spontaneous nucleation by heat treatment for crystallization in the glass.

  • PDF