Self-healing Anticorrosion Coatings for Gas Pipelines and Storage Tanks

  • Luckachan, G.E.;Mittal, V.
    • Corrosion Science and Technology
    • /
    • v.15 no.5
    • /
    • pp.209-216
    • /
    • 2016
  • In the present study, chitosan based self-healing anticorrosion coatings were prepared by layer by layer (lbl) addition of chitosan (Ch) and polyvinyl butyral (PVB) on mild carbon steel substrate. Chitosan coatings exhibited enhanced coating stability and corrosion resistance in aggressive environments by the application of a PVB top layer. Chitosan layer in the lbl coatings have been modified by using glutaraldehyde (Glu) and silica ($SiO_2$). Performance of different coatings was tested using electrochemical impedance spectroscopy and immersion test. The best anticorrosion performance was observed in case of 10 % Ch_$SiO_2$_PVB coatings, which withstand immersion test over 25 days in 0.5 M salt solution without visible corrosion. 10 % Ch_$SiO_2$ coatings without the PVB top layer didn't last more than 3days. Application of PVB top layer sealed the defects in the chitosan pre-layer and improved its hydrophobic nature as well. Raman spectra and SEM of steel surfaces after corrosion study and removal of PVB_Ch/Glu_PVB coatings showed a passive layer of iron oxide, attributing to the self-healing nature of these coatings. Conducting particle like graphene reinforcement of chitosan in the lbl coatings enhanced corrosion resistance of chitosan coatings.

Apatite Formation of NaOH-treated Porous PCL Scaffolds in Simulated Body Fluid (NaOH 처리에 따른 다공성 PCL 지지체의 의사체액 환경에서의 아파타이트 형성)

  • Lee, Hyang-Mi;Jin, Hyeong-Ho;Hyun, Yong-Taek;Park, Hong-Chae;Yoon, Seog-Young
    • Korean Journal of Materials Research
    • /
    • v.17 no.11
    • /
    • pp.622-627
    • /
    • 2007
  • Porous poly(e-caprolactone) (PCL) scaffolds were fabricated by salt leaching method. The PCL scaffolds were treated with aqueous NaOH for 0h, 2h, 4h, 8h, and 12h at $40^{\circ}C$. The NaOH-treated PCL scaffolds were dipped in $CaCl_2$ and $K_2HPO_4{\cdot}_3H_2O$ solution alternately three times to induce apatite nuclei onto the surface of the scaffolds. The NaOH-treated PCL scaffolds were immersed into SBF solution for 1day to grow the apatite. The apatite formation were investigated as a fuction of NaOH treatment time. The hydrophilicty and surface area of the PCL scaffolds were increased with NaOH-treatment time. The NaOH-treated PCL scaffolds were successfully formed a dense and uniform bone-like apatite layer after immersion for 1 day in SBF solution.

The effect of attack of chloride and sulphate on ground granulated blast furnace slag concrete

  • Ashish, Deepankar K.;Singh, Bhupinder;Verma, Surender K.
    • Advances in concrete construction
    • /
    • v.4 no.2
    • /
    • pp.107-121
    • /
    • 2016
  • This concrete is one of the most versatile construction material widely used for almost a century now. It was considered to be very durable material and required a little or no maintenance since long time. The assumption is very true, except when it is subjected to highly aggressive environments. The deterioration of concrete structures day by day due to aggressive environment is compelling engineers to assess the loss in advance so that proper preventive measure can be taken to achieve required durability to concrete structures. The compounds present in cement concrete are attacked by many salt solutions and acids. These chemicals are encountered by almost all concrete structures. The present study has been undertaken to investigate the effect of attack of chlorides and sulphates with varying severity on compressive strength of ground granulated blast furnace slag (GGBFS) concrete after immersion in salt solution for 28 days. The results indicate that the durability of GGBFS concrete increases with the increase in percentage replacement of cement by GGBFS for 20% and then gradually decreases with increases in percentage of GGBFS with cement (as in the study for 40% and 60%). Also there is increase in strength of GGBFS concrete with increase in age. Thus the durability of concrete improves when GGBFS is added as partial replacement of cement. In this study the strength of GGBFS concrete is less affected by chemicals as compared to conventional concrete when exposed to aggressive environment.

A Study on the Vulcanization System and Two-Step Foaming Properties for Natural Rubber Foam (천연고무의 가황시스템 및 성형공정에 따른 2단 발포 특성 연구)

  • Sunhee Lee;Ye-Eun Park;Dikshita Chowdhury
    • Textile Coloration and Finishing
    • /
    • v.35 no.4
    • /
    • pp.246-255
    • /
    • 2023
  • In this study, we investigated for natural rubber foam to replace petrochemical-based neoprene foam. Experiments were conducted on vulcanization system and 2-step foaming process of natural rubber. The vulcanization system were EV(Efficient Vulcanization Cure), Semi-EV(Semi-Efficient Vulcanization Cure) and CV(Conventional Vulcanization Cure). In the 2-step foaming process, first molding temperature was 140℃, times were 15, 20, 25, and 30minutes, and the second molding temperature was 160℃, the times 5, 10, 15, and 20minutes. The cure and viscosity characterization were evaluated by oscillating disc rheometer (ODR) and mooney viscosmeter. Various mechanical characteristics, including hardness, tensile strength, elongation at the point of rupture, and tear strength, were quantified. Subsequently, an assessment of alterations in these mechanical attributes was conducted post-immersion in a NaCl solution. In addition degree of volume change was measured after immersing the NR foam in NaCl solution and the low-temperature permanent compression set was evaluated at 4℃. And expansion ratio and shrinkage ratio of NR foam were evaluated for 28 days. As a result the EV vulcanization system showed the least change in physical properties before and after salt water immersion, and the lowest shrinkage ratio for 28 days. In addition it was confirmed that the 2-step foaming optimum condition differed depending on the appropriate vulcanization condition.

Corrosion Characterestic of Rolling Stock Structural Steel by Environmental Degradation (환경열화에 의한 철도차량 구조용강의 부식 특성)

  • Kim Yong-Ki;Chang Se-Ky;Oh Chang-Rok;Goo Byeong-Chun
    • Proceedings of the KSR Conference
    • /
    • 2004.10a
    • /
    • pp.680-685
    • /
    • 2004
  • The effects of acid rain and salt content on corrosion behavior were investigated with rolling stock structural steels be caused by environmental. Since these materials are exposed to the corrosive environments like polluted air, acid rain and sea water, it is important to investigate corrosion behaviour in various corrosive environments. The aqueous corrosion of the characteristic materials in aerated acid rain and neutral solution were studied by using immersion tests, electrochemical measurements and analytical techniques. In order to examine corrosion characteristic, structural steels were electrochemically evaluated with respect to the dissolved oxygen content, pH, chloride ion concentration.

  • PDF

A Study for Improving Properties of Antiwashout Underwater Concrete Mixed with Mineral Admixtures (광물질 혼화재를 혼합한 수중불분리성 콘크리트의 물성 향상을 위한 연구)

  • 문한영;신국재;이창수
    • Journal of the Korea Concrete Institute
    • /
    • v.14 no.3
    • /
    • pp.409-419
    • /
    • 2002
  • Nowadays, antiwashout underwater concrete is widely used for constructing underwater concrete structures but they, especially placed in marine environment, can be easily attacked by chemical ions such as SO$\^$2-/$\_$4/ Cl$\^$-/ and Mg$\^$2+/, so the quality and capability of concrete structures go down. In this paper, to solve and improve those matters, flyash and GGBFS(ground granulated blast furnace slag) were used as partial replacements for ordinary portland cement. As results of experiments for fundamental properties of antiwashout underwater concrete containing 10, 20, 30% of flyash and 40, 50, 60 % of GGBFS respectively, setting time, air contents, suspended solids and pH value were satisfied with the "Standard Specification of Antiwashout Admixtures for Concrete" prescribed by KSCE, and also slump flow, efflux time and elevation of head were more improved than that of control concrete. From the compressive strength test, it was revealed that the antiwashout underwater concrete containing mineral admixtures(flyash and GGBFS) is more effective for long term compressive strength than control concrete. An attempt to know how durable when they are under chemical attack has also been done by immersing in chemical solutions that were x2 artificial seawater, 5 % sulphuric acid solution, 10%, sodium sulfate solution and 10% calcium chloride solution. After immersion test for 91days, XRD analysis was carried out to investigate the reactants between cement hydrates and chemical ions and some crystalline such as gypsum ettringite and Fridel′s salt were confirmed.

Preparation of highly hydrophobic PVDF hollow fiber composite membrane with lotus leaf-like surface and its desalination properties

  • Li, Hongbin;Zi, Xingchen;Shi, Wenying;Qin, Longwei;Zhang, Haixia;Qin, Xiaohong
    • Membrane and Water Treatment
    • /
    • v.10 no.4
    • /
    • pp.287-298
    • /
    • 2019
  • Lotus leaf has a special dual micro and nano surface structure which gives its highly hydrophobic surface characteristics and so-called self cleaning effect. In order to endow PVDF hollow fiber membrane with this special structure and improve the hydrophobicity of membrane surface, PVDF hollow fiber composite membranes was obtained through the immersion coating of poly(vinylidene fluoride-co-hexafluoropropylene) (PVDF-HFP) dilute solution on the outside surface of PVDF support membrane. The prepared PVDF composite membranes were used in the vacuum membrane distillation (VMD) for the desalination. The effects of PVDF-HFP dilute solution concentration in the dope solution and coating time on VMD separation performance was studied. Membranes were characterized by SEM, WCA measurement, porosity, and liquid entry pressure of water. VMD test was carried out using $35g{\cdot}L^{-1}$ NaCl aqueous solution as the feed solution at feed temperature of $30^{\circ}C$ and the permeate pressure of 31.3 kPa. The vapour flux reached a maximum when PVDF-HFP concentration in the dilute solution was 5 wt% and the coating time was kept in the range of 10-60 s. This was attributed to the well configuration of micro-nano rods which was similar with the dual micro-nano structure on the lotus leaf. Compared with the original PVDF membrane, the salt rejection can be well maintained which was greater than 99.99 % meanwhile permeation water conductivity was kept at a low value of $7-9{\mu}S{\cdot}cm^{-1}$ during the continuous testing for 360 h.

Weathering Characteristics according to Seawater Immersion of the Magai Wareiishi Jizo (Buddhist Statue Carved on Rock Surface) in Hiroshima, Japan (일본 히로시마현 마애화령석지장(磨崖和靈石地藏)의 해수 침수에 의한 풍화특성)

  • Lee, Sun Myung;Lee, Myeong Seong;Chun, Yu Gun;Lee, Jae Man;Morii, Masayuki
    • Journal of Conservation Science
    • /
    • v.28 no.4
    • /
    • pp.329-341
    • /
    • 2012
  • Magai Wareiishi Jizo (Buddhist statue carved on rock surface) is close to shoreline and a part of rock block is periodically immersed by seawater. Rock material of the Wareiishi-jizo statue is composed mainly of medium or coarse-grained biotite granite and very durable. However, physical properties of the rock have been changed according to the complex interactions of the salt solution and surrounding environment. Exfoliation of the rock surface is a serious condition by salt crystallization. Exfoliation (14.6%) is concentrated on the upper part of the rock block with mainly boundary of seawater as the center. On the other hand, lower part of the rock block show black layers by contaminants deposition. In addition, brown discoloration and biological contaminants is overlapped. Rock surface show high discoloration rate of 50.5% (black discoloration, 29.2% > yellow discoloration, 14.1% > brown discoloration, 4.4% > green discoloration, 2.9%). Upper part of the rock block had a lot of change in the physical properties than lower part that is immersed by seawater. In particular, surface properties of the rock block was very weak state at the boundary surface of seawater permeation.

Determining the Proportions of Bone and Cartilage Growth in the Crucian Carp (carassius auratus) Using the Modified Simultaneous Differential Staining Technique

  • Lee, Jin-Heon
    • Journal of Environmental Health Sciences
    • /
    • v.36 no.4
    • /
    • pp.337-341
    • /
    • 2010
  • The modified simultaneous differential staining technique, which enables double staining of cartilage and bones, needs to be improved to prevent soft tissues from being damaged during the staining process. Key factors influencing the extent to which soft tissues are damaged include the fixative used, macerating time, potassium hydroxide concentration, incubation temperature and the removal of skin from specimens. Here we describe a protocol that enables the hardening of tissues during bleaching and maceration. We also describe a method for objectively measuring rates of cartilage and bone growth. The use of formalin as a fixative rendered soft tissues more rigid due to the resulting chemical bonds formed between proteins. Blotted specimens were immersed in 1% potassium hydroxide (KOH) and incubated at $37^{\circ}C$ for 1 day (smaller specimens) or 2-3 days (larger specimens). The 1% KOH solution was also used as the diluent solution for the subsequent immersion in a graded series of 30%, 50%, 70%, 90%, 100% glycerol solutions, a procedure that made soft tissues even more transparent and hardened. It was not necessary to remove the skin of specimens shorter than 2 cm, since the macerating solution could easily penetrate their thin skin layer and continuously remove those pigments hindering visibility. Since excessive osmosis is another factor that can damage soft tissues in the macerating process by causing the rupture of those cells not able to withstand the osmotic pressure, here it was minimized by balancing the salt concentration between the interior and exterior of cells with the addition of 0.9% sodium chloride (NaCl) in the macerating solution. Finally, to determine the proportions of cartilage and bone growth, photographs of the stained specimens were taken with a dissecting microscope and sections corresponding to the cartilage and bones were cut out from the printed pictures and weighed. Our results show that this method is suitable for the objective evaluation of bone and cartilage growth.

Enhanced performance of thin-film nanocomposite RO/NWF membrane by adding ZnO nanospheres in aqueous phase during interfacial polymerization process

  • Li, Hongbin;Shi, Wenying;Su, Yuheng;Hou, Hongxiang;Du, Qiyun;Zhang, Haixia;Qin, Xiaohong
    • Membrane and Water Treatment
    • /
    • v.8 no.3
    • /
    • pp.225-244
    • /
    • 2017
  • A novel thin-film nanocomposite (TFN) reverse osmosis (RO)/non-woven fabric (NWF) membrane was prepared by adding zinc oxide (ZnO) nanospheres ($30{\pm}10nm$) during the interfacial polymerization process of m-phenylenediamine (MPD) and trimesoyl chloride (TMC) on self-made polysulfone (PSF) membrane/polyester (PET) non-woven fabric support. The improved performance of TFN RO membrane was verified in terms of water contact angle (WCA), water flux, salt rejection, antifouling properties and chlorine resistance. The results showed that the WCA value of TFN RO surface had a continuous decrease with the increasing of ZnO content in MPD aqueous solution. The water flux of composite TFN RO membranes acquired a remarkable increase with a stable high solute rejection (94.5 %) in $1g{\cdot}L^{-1}$ NaCl aqueous solution under the optimized addition amount of ZnO (1 wt%). The continuous testing of membrane separation performance after the immersion in sodium hypochlorite solution indicated that the introduction of ZnO nanospheres also dramatically enhanced the antifouling properties and the chlorine resistance of composite RO membranes.