A Study on the Castability of Base Metal Alloys Which Sprue Shape and materials used in the Production of Dantal Prosdontics (치과 보철물 제작시 사용되는 Sprue의 재료 및 형태가 비귀금속 합금의 주조성에 미치는 영향에 관한 연구)

  • Choi, Un-Jae;Shin, Moo-Hak;Kim, Yeong-Soo
    • Journal of Technologic Dentistry
    • /
    • v.21 no.1
    • /
    • pp.87-96
    • /
    • 1999
  • In order to examine the influence of sprue(used to make crown supplements) on casting, 3 kinds of sprue materials(wax, wood, plastic) and 3 types of sprue(round, square, triangle) were made and buried and cast, then the comparison and analysis of casting characters among sprue materials and among sprue type show the following results : 1. The comparison of casting characters in accordance with sprue materials shows wax sprue of 83.3%, wood sprue 81.3%, and plastic sprue of 80.7%, Wax sprue was the bast materials for casting, However there was no statistically significant difference of casting characters among was, plastic and wood. 2. The comparison of casting in accordance with sprue types shows square sprue of 94.0%, round sprue of 86.9% and triangle sprue of 84.2%. square sprue had a best casting character. 3. When a ring cast using wood sprue was classified from burying materials. its cutting of casting body and sprue indicated much more than any other sprue material. It seems to be caused by the influence of wood residuals and carbon occurrence.

  • PDF

Effects of Pretreatment for Controlling Internal Water Transport Direction on Moisture Content Profile and Drying Defects in Large-Cross-Section Red Pine Round Timber during Kiln Drying

  • Bat-Uchral BATJARGAL;Taekyeong LEE;Myungsik CHO;Chang-Jin LEE;Hwanmyeong YEO
    • Journal of the Korean Wood Science and Technology
    • /
    • v.51 no.6
    • /
    • pp.493-508
    • /
    • 2023
  • Round timber materials of 600 mm length, cut from large-cross-section round timber of red pine (Pinus densiflora S. et Z.) of 450 mm width and 4.2 m length, were prepared as the target of kiln drying in this study. After treating the target materials through end sealing (ES), end sealing - kerfing (ES-K), lateral sealing - end sealing - boring (LS-ES-B), or lateral sealing - partial end sealing (LS-PES), the effects of the treatment on the incidence of drying defects were determined. The target materials with exposed lateral surface and sealed cross surface were steamed at the initial temperature of 65℃ above the official pest control temperature of 56℃, followed by kiln drying toward the final temperature of 75℃. The target materials with sealed lateral surfaces, on the other hand, were dried at the initial temperature of 90℃ at almost the maximum temperature of conventional kiln drying, as there is no risk of early check formation caused by surface moisture evaporation. The final temperature was set at approximately 100℃. The drying time, taken for the target materials with initial moisture content of 70%-80% to reach the target moisture content of 19%, varied across treatment conditions. The measured drying time was 1,146 hours (approximately 48 days) for the timber with sealed cross surface and 745 hours (approximately 31 days) for the timber with sealed lateral surface, until the moisture content reached the target level. The formation of surface checks could not be prevented in the control and ES groups, but a definite preventive effect was obtained for the LS-ES-B and LS-PES groups.

Deterioration and Preservation Technique of Wooden Cultural Properties (Part I) -Biodeterioration of Wooden Round Columns, Janggeongpanjeon, Built in 15 century- (목조문화재 열화 및 보존기술에 관한 연구(제1보) -장경각 구조부재중 큰기둥의 생물적 열화 특성 -)

  • Kim, Yeong-Suk;Yoon, Jeong-Hee;Kang, Ho-Yang;Park, Sang-Jin
    • Journal of the Korean Wood Science and Technology
    • /
    • v.35 no.1
    • /
    • pp.51-63
    • /
    • 2007
  • The biodeterioration behaviors of wooden parts in the Janggeongpanjeon built in 15 century were investigated according to the types of wood species, positions and parts of wooden column, and environmental conditions. It was found that a high differences of deterioration in the progressing levels of wood decay, according to the types of wood species, positions and parts of wooden column, and environmental conditions. The decay levels were high in the contacted areas with stone foundation which are about up to 8~40 cm above it, although it was shown the many of wooden parts of the round columns are still good condition. In the case of decay type, it was shown the brown-rot in many of the columns at outside of building which made of hardwoods. The decay in position of the columns was most serious in the directions of east-north, west-north and north. It was also indicated that the durability of Zelkova serrata was higher than other wood species of the round columns, while it was in inferior anti-insects.

Effects of Post Individualities on Treatability of Small Diameter Japanese Larch (Larix Leptolepis) with ACQ and CCA (낙엽송 원주상 소경목의 원목성상과 방부 처리성)

  • Kim, Yeong-Suk;Hong, Soon-Il;Yun, Jeong-Hee
    • Journal of the Korean Wood Science and Technology
    • /
    • v.34 no.1
    • /
    • pp.52-60
    • /
    • 2006
  • This study investigated how wood properties (i.e., annual rings, sapwood, heartwood, and cracks) might affect preservative treatment in Japanese larch (Larix leptolepis) round-wood product. We specially focused on small-diameter (~10 cm diameter) wood that is commercially sold in market. Among 100 wood samples, the groups of sample with 13~16, 17~20 annual rings represented 33 and 27 in each frequency, while 2~3 and 4~5 mm annual ring width accounted for 72 and 68 in frequency. More than a half (54%) of wood samples contained a mix of heartwood and sapwood in its surface. The rest (46%) had only heartwood exposed in the wood surface. A wide range of checks were showed in the wood samples, but the highest frequency was observed in samples with 1~6 surface (1~14 mm in size) checks and 1~4 end-grain (8~14 mm in size) checks in each round-wood sample. Pressure treatment resulted in a wide range of penetration of ACQ (Alkaline Copper Quat) into the wood, showing $4.3{\pm}4.19mm$ penetration in the wood samples contained a mix of heartwood and sapwood in its surface. However preservative treatment was much less effective for the heartwood only wood samples, ranging average 1.3 mm with ACQ and 1.1 mm with CCA (Chromated Copper Arsenate). These penetration results shown in heartwood samples did not meet the penetration standard that is required for H3 by the Korean Forest Service in relation to wood preservation treatment. These low penetration results were not significantly improved even if we incised wood samples to improve treatment effect, showing only small increase of 0.7 mm with ACQ and 0.6 mm with CCA. When preservative treatment was tested with heartwood, penetration of preservatives decrease with increase of annual rings per a cross-section area (r=0.5345). We also found that the length and number of check had no effect on preservative treatment, showing r=0.1301 and r=0.1802, respectively.

Surface Checking Reduction Effect of Preservative-treated Korean Larch Round-woods with Various Physical Treatments (물리적 처리에 따른 낙엽송 방부원주목의 표면할렬 방지효과)

  • Pang, Sung-Jun;Oh, Jung-Kwon;Lee, Sang-Joon;Park, Jun-Ho;Jang, Sung-Il;Lee, Jun-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • v.45 no.1
    • /
    • pp.107-115
    • /
    • 2017
  • In this study, the surface check reduction effect of preservative-treated Korean larch round-wood was investigated by applying three physical treatments, such as incising, kerfing, and kiln-drying. Moreover, the possibility of long-term service life was also checked by comparing the depth of surface check and the penetration depth of preservative. A rapid gradient of wood moisture content between surface and center causes a surface check. Thus, the effect of reducing surface check was carried out at the lowest equilibrium moisture content (EMC) condition, temperature ($2^{\circ}C$), humidity (44.6%), in outdoor locations in Korea until the test specimens reach to the 8.6% EMC. As a result, the preservative-treated specimens without incising, kerfing, kiln-drying (Type C) could not ensure the long-term service life due to a large surface check. Because the surface check depth of all specimens was deeper than the penetration depth of preservative. In case of the incising treated specimens (Type I), 80% of them, the depth of surface check was not deeper than the penetration depth of preservative. However, when a kerfing was additionally treated (Type B), a possibility of happening deeper surface check than penetration depth of preservative was increased rather than Type I.

Effect of End-coating Around Pith of Heavy Timbers of Red Pine and Korean Pine on High-temperature and Low-humidity Drying Characteristics (중심부분 엔드코팅처리가 국산 소나무와 잣나무 중목구조부재의 고온저습건조 특성에 미치는 영향)

  • Lee, Chang-Jin;Lee, Nam-Ho;Eom, Chang-Deuk;Shin, Ik-Hyun;Park, Moon-Jae;Park, Joo-Saeng
    • Journal of the Korean Wood Science and Technology
    • /
    • v.41 no.3
    • /
    • pp.221-233
    • /
    • 2013
  • This study was performed to identify the effect of end-coating around pith of heavy timbers of Red pine and Korean pine on high temperature and low humidity drying characteristics. Total drying times were 268 hours, and ranges of final moisture content was investigated that Red Pine 9.2% to 10.8% MC for square and round timber, in case of Korean Pine 15.0% to 22.0% MC for square timber, 12.8% to 20.4% MC for round timber. Moisture content distribution of Red Pine was a uniform, but part of high moisture content was found in Korean Pine. In case of Korean pine, the surface checks were occurred more severe than in case of Red pine, and end-coating treatment were investigated to be ineffective on surface check. The internal checks were only formed on the two timbers. The value of the case hardenings was investigated that the ranges 3.7% to 9.1% for Red pine. In case of Korean pine, on the other hand, the case hardenings presence a few as 20.9% to 35.8%.

Anatomical Comparison of Compression, Opposite, and Lateral Woods in a Branch of Pinus parviflora S. et Z. (섬잣나무(Pinus parviflora S. et Z.) 지재의 압축이상재, 측면재, 대응재에 관한 해부학적 특성 비교)

  • Xu, Guang Zhu;Eom, Young Geun
    • Journal of the Korean Wood Science and Technology
    • /
    • v.33 no.1 s.129
    • /
    • pp.38-47
    • /
    • 2005
  • Compression, lateral, and opposite woods in a branch of Pinus parviflora S. et Z. were described and compared in the qualitative anatomical aspects through light and scanning electron microscopy. Tracheid transition from earlywood to latewood in the compression wood appeared to be relatively more gradual than in the opposite or lateral wood. Growth ring width and proportion of latewood were thought to be greater in the compression wood than in the lateral or opposite wood. The latewood tracheids of compression wood in transverse surface were mostly round, differently from those of lateral and opposite woods with square to angular shapes. Also, intercellular spaces, helical cavities and checks, and slit-like pit apertures were observed only in the compression wood tracheids. Cross-field pitting in the compression wood appeared not to be used as diagnostic guide because of their severe alteration from normal fenestriform or window-like type to cupressoid to taxodioid types. In tangential surface, fusiform rays in the compression wood were wider but lower than those in the lateral wood or opposite wood. In conclusion, compression wood was different from lateral and opposite woods but lateral and opposite woods were almost identical in qualitative anatomical features.

Study on Methods for Determining Half-Life of Domestic Wooden Panel among Harvested Wood Products (국산 목질판상재의 반감기 결정방법에 관한 연구)

  • Chang, Yoon-Seong;Han, Yeonjung;Park, Jun-Ho;Son, Whi-Lim;Park, Joo-Saeng;Park, Moon-Jae;Yeo, Hwanmyeong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.42 no.3
    • /
    • pp.309-317
    • /
    • 2014
  • Harvested wood products (HWP) are known as products from the tree such as sawn wood, plywood, particle board, structural lumber, wooden interior material, wooden furniture, and paper products. Because carbon is locked up in the HWP until eventual end-use of HWP, HWP played a role as the carbon storage which has the effect of stabilizing the concentration of carbon dioxide in the atmosphere. For these reasons, the suggestion that it must admit the carbon storage effect of HWP has been constantly raised. In 2011, the 17th session of the Conference of the Parties (COP) to the United Nations Framework Convention on Climate Change (UNFCCC) which was held in Durban, South Africa, assigned "Production Approach" which targets only the HWP producted by using round wood of domestic forestry as a official method for carbon accounting. Therefore, it is necessary that each country has to determine the half-life of wood in order to correspond to the discussions and negotiations between countries in the future and to develop an inventory of product-specific domestic wood. In this study, some countries' examples of the methods and conditions for determining half-life of HWP were investigated, and it was tried to derive the factor and methodology to determine half-life span of domestic HWP appropriately.

Effects of Polyethylene Glycol Treatment for Improvement of Preservative Penetration and Prevention of Drying Check of Preservative Treated Round Post (방부처리 원주가공재의 방부제 침윤도 향상 및 건조 할렬 방지를 위한 폴리에틸렌 글리콜 처리 효과)

  • Lee, Jong-Shin;Yoon, Sun-Mi
    • Journal of the Korean Wood Science and Technology
    • /
    • v.30 no.4
    • /
    • pp.27-32
    • /
    • 2002
  • We investigated the effect of polyethylene glycol(PEG) treatment of preservative treated green japanese cedar(Cryptomeria japonica) round posts on their preservative penetration and check formation during the air drying. The round rods were dip-treated in 10% preservative solution of Basilit CFK for 1 day, followed by application(3, 5, and 10 times) with 50% PEG-400 solution, and then dried for 30 days under natural conditions. The rate of preservative penetration into sapwood was a low by 23.2% without PEG treatment, whereas that was a high by about 51.2~64.5% with PEG treatment. From these results, it was assumed that PEG played an affirmative role in the penetration of preservative components loaded onto the surface of round rods by dipping. During the air drying, the formation of drying checks decreased significantly with increasing application times of PEG. Even though some drying checks in PEG treated rods were developed, the number and size of checks was reduced remarkably by PEG treatment. After 2 months of outdoor exposure, PEG treatment failed to reduce checking in preservative-treated rods whereas finishing of polyurethane resin lacquer after PEG treatment was significantly effective in preventing check development.

Notes on Poria from Korea (한국산 Poria국에 대한 소고)

  • 홍순우
    • Journal of Plant Biology
    • /
    • v.19 no.3
    • /
    • pp.65-68
    • /
    • 1976
  • The present genus, once applied as an all-round taxon on resupinate polypores, was considered on account of its common occurrence throughout the world and outstanding wood-rotting nature. In Korea two species, P. vaporaria(but even this seems misjudged) and P. cocos have been known. The authors used to examine tentatively the materials formerly preserved in dried state. Among about 40 collections half of them was recognized as P. cocos and 4 unrecorded species, P. versipora, P. subacida, P. medulla-panis, and P. eupora, which are newly registered to Korea in this article.

  • PDF