Pressure Effects on the Dehydration Behavior of Natrolite (나트로라이트 탈수현상의 압력의존성에 관한 연구)

  • Hwang, Gil Chan;Jang, Young-Nam;Liu, Zhenxian;Lee, Yongjae
    • Journal of the Mineralogical Society of Korea
    • /
    • v.26 no.3
    • /
    • pp.175-187
    • /
    • 2013
  • In-situ Raman and X-ray diffraction experiments have been performed on mineral natrolite (Na-zeolite) to investigate the dehydration behavior under high temperature and high pressure-temperature conditions. XRD data show reversible dehydration up to $450^{\circ}C$ whereas Raman data show irreversible change when the material is heated up to $630^{\circ}C$. The existence of post-natrolite was newly identified to form from ${\beta}$-metanatrolite at $380^{\circ}C$ upon cooling. The formation of dehydrated metanatrolite under simultaneous high temperature-pressure (room temperature < T < $300^{\circ}C$, 0 GPa < P < 2.1 GPa) conditions was not observed.

The Pretreatment of Thiopental Sodium for Reducing Injection Pain of Propofol (Propofol 정주시 혈관통 감소를 위한 Thiopental Sodium 전처치)

  • Shin, Ok-Young;Lee, Dong-Kun;Kim, Keon-Sik;Kang, Wha-Ja;Lee, Doo-Ik;Kim, Dong-Soo
    • The Korean Journal of Pain
    • /
    • v.10 no.2
    • /
    • pp.220-224
    • /
    • 1997
  • Background: The incidence of pain on injection of propofol varies between 30 and 100%. A variety of pretreatments have been tried to alleviate this problem such as a local anesthetics, cooling and opioids. However, none of these pharmacological maneuvers were satisfactory yet. In a recent study, subhypnotic doses of both thiopental sodium and propofol decrease the acute pain. We report a comparison of thiopental sodium, lidocaine and placebo on the incidence and severity of pain on injection of propofol. Method: A controlled, double-blind study was performed to compare the prior administration of intravenous saline 2 ml(n=30, group S), lidocaine 20 mg(n=30, group L) and thiopental sodium 50 mg(n=30, group T) in alleviating the pain by propofol. Injection pain was assessed with the four-point verbal categorical scoring system. Result: The incidence of injection pain during induction was lower in group L(30%) and T(17%) than group S(77%). The incidence of injection pain was lower in group T(17%) than group L(30%), but not significant statistically. The pain scores for recall of pain in the recovery room was simlar to those pain during propofol induction. Conclusion: The pretreatment of thiopental sodium can be effective in reducing both incidence and severity of propofol injection pain and has similar effect to lidocaine to prevent propofol injection pain.

  • PDF

Growth Behavior of Thermally Grown Oxide Layer with Bond Coat Species in Thermal Barrier Coatings

  • Jung, Sung Hoon;Jeon, Soo Hyeok;Park, Hyeon-Myeong;Jung, Yeon Gil;Myoung, Sang Won;Yang, Byung Il
    • Journal of the Korean Ceramic Society
    • /
    • v.55 no.4
    • /
    • pp.344-351
    • /
    • 2018
  • The effects of bond coat species on the growth behavior of thermally grown oxide (TGO) layer in thermal barrier coatings (TBCs) was investigated through furnace cyclic test (FCT). Two types of feedstock powder with different particle sizes and distributions, AMDRY 962 and AMDRY 386-4, were used to prepare the bond coat, and were formed using air plasma spray (APS) process. The top coat was prepared by APS process using zirconia based powder containing 8 wt% yttria. The thicknesses of the top and bond coats were designed and controlled at 800 and $200{\mu}m$, respectively. Phase analysis was conducted for TBC specimens with and without heat treatment. FCTs were performed for TBC specimens at $1121^{\circ}C$ with a dwell time of 25 h, followed by natural air cooling for 1 h at room temperature. TBC specimens with and without heat treatment showed sound conditions for the AMDRY 962 bond coat and AMDRY 386-4 bond coat in FCTs, respectively. The growth behavior of TGO layer followed a parabolic mode as the time increased in FCTs, independent of bond coat species. The influences of bond coat species and heat treatment on the microstructural evolution, interfacial stability, and TGO growth behavior in TBCs are discussed.

The Analysis of the Energy Saving Performances of Building Materials using Phase Change Materials (상변화물질을 적용한 건축자재의 에너지절약 가능성 분석)

  • An, Sang-Min;Hwang, Suck-Ho;Kim, Tae-Yeon;Leigh, Seung-Bok
    • 한국태양에너지학회:학술대회논문집
    • /
    • 2011.04a
    • /
    • pp.162-167
    • /
    • 2011
  • Thermal storage plays an important role in building energy saving, which is greatly assisted by the incorporation of latent heat storage in building materials. A phase change material is a substance with a high heat of fusion which, melting and solidifying at a certain temperature, can be storing and releasing large amount of energy. Heat is stored or released when the material changes from solid to liquid. Integration of building materials incorporating PCMs into the building envelope can result in increased efficiency of the built environment. The aim of this research is to identify thermal performance of PCMs impregnated building materials which is applied to interior of building such as gypsum and red clay. In order to analyze thermal performance of phase change materials, test-cell experiments and simulation analysis were carried out. The results show that micro-encapsulated PCM has an effect to maintain a constant indoor temperature using latent heat through the test-cell experiments. PCM wallboard makes it possible to reduce the fluctuation of room temperature and heating and cooling load by using EnergyPlus simulation program. Phase change material can store solar energy directly in buildings. Increasing the heat capacity of a building is capable of improving human comfort by decreasing the frequency of indoor air temperature swings so that the interior air temperature is closer to the desired temperature for a long period of time.

  • PDF

Storage potential of low temperature adapted shiitake mushroom under freezing temperature (저온성 표고버섯의 빙점하 저장 잠재력)

  • Hwang, Yong Soo;Seo, Geon Sik
    • Korean Journal of Agricultural Science
    • /
    • v.40 no.3
    • /
    • pp.197-202
    • /
    • 2013
  • This study was aimed to find the storage potential of low temperature adapted shiitake mushroom under freezing temperature ($-3^{\circ}C$). Fresh shiitake mushroom was harvested at late Feb. and cooled to target temperature, $-3^{\circ}C$ in the cooling room for 24 hr. Cooled mushroom were then placed in plastic boxes, wrapped with plastic film ($30{\mu}m$), and stored at $-3^{\circ}C$ for 2 months. Weight loss of mushroom was ranged from 2.1 to 3.2%. Dry weight per unit fresh weight, however, was slightly increased because of moisture loss. Firmness of fruit body increased from $0.95kg/cm^{-2}$ (before storage) to $1.13kg/cm^{-2}$ (after 2 month storage). About half amount of starch was lost during 2 month storage. The amount of total and reducing sugars remained relatively constant. After storage, freshness of mushroom was recovered by thawing treatment. When recovered mushroom were packaged with styrofoam tray and PVC wrapping, and exposed to ambient and $10^{\circ}C$, respectively, brown spot on the gill of fruit body was found and slight decay symptom was also found at ambient temperature only but not at $10^{\circ}C$. Results indicated that low temperature adapted shiitake mushroom has a storage potential under freezing temperature ($-3^{\circ}C$). Freezing storage technology of fresh shiitake mushroom will contribute the increase of storability up to 2 months.

Evaluation For Mechanical Properties of High strength Concrete by Stressed Test and Tressed Residual Strength Test (설계하중 사전재하 및 잔존강도 시험방법에 따른 고강도콘크리트의 고온특성평가 -제 1보, 강도특성을 중심으로-)

  • Lee, Tae-Gyu;Kim, Young-Sun;Lee, Eui-Bae;Park, Chan-Gyu;Kim, Gyu-Yong;Kim, Moo-Han
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.04a
    • /
    • pp.869-872
    • /
    • 2008
  • Recently, the effects of high temperature on compressive strength, elastic modulus and strain at peak stress of high strength concrete were experimentally investigated. The present study is aimed to study the effect of elevated temperatures ranging from 20 to $700^{\circ}C$ on the material mechanical properties of high-strength concrete of 40, 60, 80MPa grade. In this study, the types of test were the stressed test and stressed residual test that the specimens are subjected to a 25% of ultimate compressive strength at room temperature and sustained during heating and when target temperature is reached, the specimens are loaded to failure. Or specimens are loaded to failure after 24hour cooling time. tests were conducted at various temperatures ($20{\sim}700^{\circ}C$) for concretes made with W/B ratios 46%, 32% and 25%. Test results showed that the relative values of compressive strength and elastic modulus decreased with increasing compressive strength grade of specimen.

  • PDF

Evaluation for mechanical properties of high strength concrete by stressed test and stressed residual strength test - part 2 strain properties - (설계하중 사전재하 및 잔존강도 시험방법에 따른 고강도콘크리트의 고온특성 평가 - 제2보 변형특성을 중심으로 -)

  • Kim, Young-Sun;Lee, Tae-Gyu;Lee, Dae-Hui;Lee, Seung-Hoon;Kim, Gyu-Yong;Kim, Moo-Han
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.04a
    • /
    • pp.761-764
    • /
    • 2008
  • The present study is aimed to study the effect of elevated temperatures ranging from 20 to $700^{\circ}C$ on the strain properties of high-strength concrete of 40, 60, 80MPa grade. In this study, the types of test were the stressed test and stressed residual test that the specimens are subjected to a 25% of ultimate compressive strength at room temperature and sustained during heating and when target temperature is reached, the specimens are loaded to failure. Or specimens are loaded to failure after 24hour cooling time. tests were conducted at various temperatures ($20{\sim}700^{\circ}C$) for concretes made with W/B ratios 46%, 32% and 25%. Test results showed that the relative values of elastic modulus decreased with increasing compressive strength grade of specimen and the axial strain at peak stress were influenced by the load before heating. thermal strain of concrete at high temperature was affected by the preload as well as the compressive strength.

  • PDF

Effect of Metastable Tetragonal $ZrO_2$ Phase on the Mechanicmal Properties in $Al_2O_3-ZrO_2$ System ($Al_2O_3-ZrO_2$계에서 기계적 성질에 미치는 준안정 저앙 $ZrO_2$상의 효과)

  • Kim, Jin-Young;Hwang, Kyu-Hong;Kim, Hwan
    • Journal of the Korean Ceramic Society
    • /
    • v.21 no.2
    • /
    • pp.149-155
    • /
    • 1984
  • The effect of $ZrO_2$ dispersed phase on the mechanical properties in $Al_2O_3$-$ZrO_2$system has been studied. There are both metastable tetragonal phase and stable monoclinic phase of $ZrO_2$particles diespersed in Al2O3 matrix at room temperature. Metastable tetragonal $ZrO_2$ changes to the stable monoclinic structure within the stress field of the crack. And microcracks are formed by the expansion of $ZrO_2$during the tetragonal-monoclinic transformation on cooling. Therefore stress-induced phase transformation and inclusion-induced microcracking contribute to the mec-hanical properties of $Al_2O_3$-$ZrO_2$system. Sintered composites containing 10m/o $ZrO_2$ yield KiC values of 6.5MN/$m^{3/2}$ much greater than that of pure $Al_2O_3$ This increase results from microcrack extension and stress-induced phase transformation absor-bing energy by crack propagation. Flexural strength of composites is decreased considerably in comparison with pure $Al_2O_3$ This decrease results from microcrack as a crack former and higher porosity than pure $Al_2O_3$.

  • PDF

Crystallographic Analysis of Ar Encapsulate within Cs3-A Zeolite

  • Lim, Woo Taik;Kim, Bok Jo;Park, Jong Sam;Chang, Chang Hwan;Jung, Sung Wook;Heo, Nam Ho
    • Analytical Science and Technology
    • /
    • v.15 no.6
    • /
    • pp.540-549
    • /
    • 2002
  • The arrangement of encapsulated Ar atoms in the molecular-dimensioned cavities of fully dehydrated zeolite A of unit-cell composition $Cs_3Na_8HSi_{12}Al_{12}O_{48}$ ($Cs_3$-A) has been studied crystallographically to probe the confinement effect of guest species in microporous environment. Atoms of Ar were encapsulated in the cavities of $Cs_3$-A by treatment with 410 atm of Ar at $400^{\circ}C$ for two days, followed by cooling at room temperature. The crystal structure of $Cs_3Na_8H$-A(4Ar) ($P_e$ = 410 atm, $a=12.245(2){\AA}$, $R_1=0.0543$, and $R_2=0.0552$) has been determined by single crystal X-ray diffraction technique in the cubic space group $Pm\bar{3}m$ at 21 (1) $^{\circ}C$ and 1 atm. Encapsulated Ar atoms are distributed in three crystallographic distinct positions: 1.5 Ar atoms per unit cell opposite 6-rings, 1.5 opposite four-rings in the large cavity, and finally 1.0 in the sodalite-unit. The possible structures of argon clusters, such as $Ar_2$, $Ar_3$, and $Ar_4$, are proposed.

Comparative Evaluation of the Characteristics of High Si-High Mo Ductile Cast Iron, High Si-High Mo C. V. Cast Iron and Ni-resist Cast Iron (고규소 고몰리브덴 구상흑연주철, 고규소 고몰리브덴 C. V. 주철 및 Ni-resist 주철 특성의 비교 평가)

  • Ju, Young-Kyu;Choe, Kyeong-Hwan;Lee, Sang-Mok;Kim, Myung-Ho;Yun, Sang-Weon;Lee, Kyong-Whoan
    • Journal of Korea Foundry Society
    • /
    • v.29 no.3
    • /
    • pp.120-127
    • /
    • 2009
  • The characterestics of high Si-high Mo ductile cast iron, high Si-high Mo C.V. cast iron and Ni-resist cast iron were compared and evaluated. The nodule count of the last one was lower and the nodularity was higher than those for the first one, respectively. The first two had ferritic matrices with small amounts of molybdenum carbides. The first one had the highest tensile strength and the last one the lowest elongation. This had the highest high temperature strength and that of the second one was greatly increased from the room temperature strength. The volumes of the first two were decreased during cooling and that of the last one changed little. The thermal expansion coefficient of the last one was the highest and the first one the lowest. During high temperature oxidation, even though the volume of the first one was increased, the weight was decreased and the volume and weight of the second one were increased. The change of the increased weight of the last one was more than that of thickness.