Development of high-resolution atmosphere ocean coupled model and global warming projection with Earth Simulator -A whole research plan and result in FY2002-

  • Maruyama, Koki
    • 한국해안해양공학회:학술대회논문집
    • /
    • 한국해안해양공학회 2003년도 한국해안해양공학발표논문집
    • /
    • pp.18-27
    • /
    • 2003
  • The goal of the UN Framework Convention on Climate Change (UNFCCC) is to stabilize atmospheric CO2 concentration for preventing global warming in future. However, there are many unknown factors regarding stabilization of CO2 concentration. What level of concentration should be appropriate to prevent global warming? When should we stop the increase of CO2 concentration\ulcorner What kind of countermeasures of reducing CO2 emission will be available for CO2 stabilization?(omitted)

  • PDF

Synthesis of Titanium Diboride and Composites by Carbothermic Reduction of Titanium Oxide and Boric Oxide

  • Yoon, Su-Jong;Jha, Animesh
    • The Korean Journal of Ceramics
    • /
    • 제4권4호
    • /
    • pp.387-393
    • /
    • 1998
  • The formation of titanium diboride ($TiB_2$ ) via the reduction of $TiO_2$ with boric oxide and carbon was studied in a partially reducing atmosphere of argon mixed with 4 vol.%H2. The effect of reaction time, temperature, partial pressure of nitrogen and $TiO_2/B_2_O3$ stoichiometric ratio on the reducibility of oxides has been studied. The phases formed were analysed by using X-ray rowder diffraction and scanning sosctron microscopic techniques. In this paper, we also investigated the presence of $CaC_2$ as a reducing agent on the reducibility of oxide mixtures and on the Ti-B-C-Ca-O phase equilibria. The morphology of $TiB_2$ formed in the presence of $CaC_2$ is compared with the microstructure of $TiB_2$ formed as a consequence of carbothermic reduction. The observed variation in $TiB_2$ crystals formed is also explained.

  • PDF

Metabolic Characterization of Lactic Acid Bacterium Lactococcus garvieae sk11, Capable of Reducing Ferric Iron, Nitrate, and Fumarate

  • Yun, Su-Hee;Hwang, Tae-Sik;Park, Doo-Hyun
    • Journal of Microbiology and Biotechnology
    • /
    • 제17권2호
    • /
    • pp.218-225
    • /
    • 2007
  • A lactic acid bacterium capable of anaerobic respiration was isolated from soil with ferric iron-containing glucose basal medium and identified as L. garvieae by using 16S rDNA sequence homology. The isolate reduced ferric iron, nitrate, and fumarate to ferrous iron, nitrite, and succinate, respectively, under anaerobic $N_2$ atmosphere. Growth of the isolate was increased about 30-39% in glucose basal medium containing nitrate and fumarate, but not in the medium containing ferric iron. Specifically, metabolic reduction of nitrate and fumarate is thought to be controlled by the specific genes fnr, encoding FNR-like protein, and nir, regulating fumarate-nitrate reductase. Reduction activity of ferric iron by the isolate was estimated physiologically, enzymologically, and electrochemically. The results obtained led us to propose that the isolate metabolized nitrate and fumarate as an electron acceptor and has specific enzymes capable of reducing ferric iron in coupling with anaerobic respiration.

Optimized ultra-thin tunnel oxide layer characteristics by PECVD using N2O plasma growth for high efficiency n-type Si solar cell

  • Jeon, Minhan;Kang, Jiyoon;Oh, Donghyun;Shim, Gyeongbae;Kim, Shangho;Balaji, Nagarajan;Park, Cheolmin;Song, Jinsoo;Yi, Junsin
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2016년도 제50회 동계 정기학술대회 초록집
    • /
    • pp.308-309
    • /
    • 2016
  • Reducing surface recombination is a critical factor for high efficiency silicon solar cells. The passivation process is for reducing dangling bonds which are carrier. Tunnel oxide layer is one of main issues to achieve a good passivation between silicon wafer and emitter layer. Many research use wet-chemical oxidation or thermally grown which the highest conversion efficiencies have been reported so far. In this study, we deposit ultra-thin tunnel oxide layer by PECVD (Plasma Enhanced Chemical Vapor Deposition) using $N_2O$ plasma. Both side deposit tunnel oxide layer in different RF-power and phosphorus doped a-Si:H layer. After deposit, samples are annealed at $850^{\circ}C$ for 1 hour in $N_2$ gas atmosphere. After annealing, samples are measured lifetime and implied Voc (iVoc) by QSSPC (Quasi-Steady-State Photo Conductance). After measure, samples are annealed at $400^{\circ}C$ for 30 minute in $Ar/H_2$ gas atmosphere and then measure again lifetime and implied VOC. The lifetime is increase after all process also implied VOC. The highest results are lifetime $762{\mu}s$, implied Voc 733 mV at RF-power 200 W. The results of C-V measurement shows that Dit is increase when RF-power increase. Using this optimized tunnel oxide layer is attributed to increase iVoc. As a consequence, the cell efficiency is increased such as tunnel mechanism based solar cell application.

  • PDF

ZrTiO4계 Gray 안료 합성과 형성기구 (Synthesis and Formation Mechanism of ZrTiO4 Gray Pigment)

  • 황동하;이병하
    • 한국세라믹학회지
    • /
    • 제49권1호
    • /
    • pp.84-89
    • /
    • 2012
  • Attempts were made to develop a stable gray pigment at reducing atmosphere, substituting Ti in $ZrTiO_4$ with Mn, Fe, Co and Cu The pigment synthesized at $1300~1500^{\circ}C$ by solid state method with the composition of $ZrTi_{1-x-y}A_xB_yO_4$ (x = y = 0.005, 0.015, 0.035, 0.055, 0.075, 0.095, 0.115, 0.135, 0.155, 0.175 and 0.195 mole, A = Mn(III), Fe(III), Co(II, III) and Cu(II) (chromophores), B = Sb (counterion). The pigments were fired at $1400^{\circ}C$ for 3 h with substitute amount changes of Mn, Fe, Co and Cu to $ZrTiO_4$ crystals, and analyzed by Raman spectroscopy to figure out substitute limits. Results indicated 0.035 mole for Mn, 0.115 mole for Fe, 0.015 mole for Co and 0.015 mole for Cu as substitute limits, respectively. Figs. 1, 2, 3, and 4 represent each substitute pigments of Mn, Fe, Co and Cu. Synthesized pigment was applied to a lime and a lime-magnesia glaze at 7 wt% each, and fired at reducing atmosphere of $1240^{\circ}C$, soaking time 1h. Gray color was obtained with CIE-$L^*a^*b^*$ values at 44.55, -0.65, 1.19(Mn), 40.36, -0.90, 0.30(Fe), 42.63, -0.03, -1.49(Cu) and -40.79, -0.28, -0.91(Co), respectively.

${Er_2}{O_3}$첨가가 $BaTiO_3$계 내환원성 X7R 재질의 유전특성에 미치는 효과 (Effects of ${Er_2}{O_3}$ Addition on the Dielectric Properties of Non-reducible $BaTiO_3$-based X7R Dielectrics)

  • 박재성;황진현;한영호
    • 한국재료학회지
    • /
    • 제11권1호
    • /
    • pp.44-47
    • /
    • 2001
  • Ni 전극을 사용하는 $BaTiO_3$계 내환원성 X7R 조성에서 $Er_2$$O_3$ 첨가가 유전특성에 미치는 영향에 대하여 환원성 분위기에서 연구하였다. $MnO_2-MgO$가 첨가된 내환원조성에서 첨가량이 조절된 $Er_2O_3$의 복합첨가로 유전율의 온도안정성이 향상되어 X7R 규격을 만족시켰으며 2,970 이상의 상온 유전상수와 1.0% 이하의 유전손실율이 관찰되었다. $Er_2O_3$가 3.0 mol% 이상으로 과량 첨가되었을 경우 유전체의 온도특성은 향상되었으나 상온 유전상수가 현저히 감소하였다. 다른 첨가조성(1.5 mol% $Er_2O_3$2.0 mol% MgO)이 고정될 때 TCC곡선은 $MnO_2$첨가량이 증가함에 따라 시계방향으로 회전하였으며, 온도안정성을 향상시켰다.

  • PDF

석탄회를 이용한 저밀도 세라믹 담체의 제조 기구 (Formation Mechanism of Low Density Ceramic Supporter with Fly Ash)

  • 황연;이효숙;이우철;정용대;이원권
    • 자원리싸이클링
    • /
    • 제9권2호
    • /
    • pp.33-39
    • /
    • 2000
  • 생물여과법에 의한 유해성 유기물 제거용 저밀도 담체로 사용하기 위하여 석탄회를 출발물질로 이용하여 세라믹 담체를 제조하였다. 석탄회에 기공 조절용 및 탄소함량 조절용으로 밀가루를 첨가하여 약환원성 분위기를 유지하여 $1200^{\circ}C$에서 소결한 결과 1.6~1.8 g/$\textrm{cm}^3$의 겉보기 밀도를 얻을 수 있었다. 소결 시 공기를 차단하고 급속히 승온하여 시편 조성의 일부를 환원시킴으로써 액상을 형성할 수 있었으며, 이렇게 형성된 액상은 시편의 표면부근에 폐기공을 형성하여 밀도를 낮추었다.

  • PDF

ZnO-Fe2O3계 Spinel안료에 대한 연구 (Synthesis of Spinel Pigment on ZnO-Fe2O3 System)

  • 이진성;이응상
    • 한국세라믹학회지
    • /
    • 제26권2호
    • /
    • pp.187-194
    • /
    • 1989
  • Synthesis of spinel pigment on ZnO-Fe2O3 system. The object of this research is the synthesis of new spinel pigments on the basic of ZnO-Fe2O3 system which was substituted by ZnO-Fe2O3 by MgO-Al2O3. This research was progressed by measuring the X-ray diffraction and the reflectances of the substitued ZnO-Fe2O3 group. Which was obtained by sintering at the temperature of 1,00$0^{\circ}C$, 1,10$0^{\circ}C$, 1,20$0^{\circ}C$ and 1,25$0^{\circ}C$ and them by regrinding. In order to coloring test, here basic compositions of Barium glaze, Zinc glaze, Lime glaze, Lead glaze and Talc glaze used in this experiment are obtained from the ceramic work. Adding synthetic stains in these basic glazes with 3%, mixing and glazing on the specimen. The specimens was fired at 1,28$0^{\circ}C$ in reducing and oxidizing atmosphere in the gas kiln. The results of the research as follow. 1. Many kinds of spinel pigment was produced on ZnO-Fe2O3 system that is to say, not always only spinel. 2. Spinel peak was observed strongly on the ZnO-Fe2O3 system withsubstituting by MgO-Fe2O3 and MgO-Al2O3 group(the ratio of MgO, Al2O3 being increased, observed more strongly). 3. The most effective temperature ranges was 1,20$0^{\circ}C$~1,25$0^{\circ}C$. 4. The color of spinel pigments on this system was observed by "stable YR". 5. It was yellow red in oxidizing and green in reducing atmosphere on the coloring test.ring test.

  • PDF

고체산화물연료전지 연결재용 La0.7Ca0.3Cr0.9Co0.1O3-δ 조성계에 Ca Source 변화에 따른 소결 및 전기적 특성에 관한 연구 (Effects of Ca-Source on the Sintering and Electrical Properties of La0.7Ca0.3Cr0.9Co0.1O3-δ for Solid Oxide Fuel Cell Interconnects)

  • 박성태;최병현;지미정;안용태;최헌진
    • 한국세라믹학회지
    • /
    • 제48권3호
    • /
    • pp.246-250
    • /
    • 2011
  • Effects on sintering and electrical properties of $La_{0.7}Ca_{0.3}Cr_{0.9}Co_{0.1}O_{3-{\delta}}$ system, a interconnect material for cylindrical and flat tubular solid oxide fuel cells (SOFC), have been investigated by Ca-source when using $CaCO_3$ and $CaF_2$. When using $CaCO_3$ and $CaF_2$ was mixing as Ca-source, single phased perovskite solid solution was observed for each sample. The sintering temperature was decreased by $CaF_2$ contents was increased. When using 0.1 mole $CaF_2$ was densely sintered at $1400^{\circ}C$ and relative density was 93.8%. Also, electrical conductivity in oxidation and reducing atmosphere was 47, 4.3 S/cm, respectively, due to $F^-$ ion enhance the electrical conductivity in reducing atmosphere.