• 제목/요약/키워드: ratio, Dyeing

Search Result 175, Processing Time 0.024 seconds

Supercritical Fluid Dyeing of Polyester Fiber with Two Different Dispersion Dyes (두 종류의 분산염료를 이용한 폴리에스테르 섬유의 초임계유체 염색)

  • Jung, In-Il;Lee, Sang-Yun;Lim, Gio-Bin;Ryu, Jong-Hoon
    • Clean Technology
    • /
    • v.17 no.2
    • /
    • pp.110-116
    • /
    • 2011
  • The dyeing of polyester fiber with two different disperse dyes (Disperse Red 60 and Disperse Yellow 54) was carried out using supercritical carbon dioxide ($SCCO_2$) as a dyeing medium at temperatures ranging from $50^{\circ}C$ to $90^{\circ}C$ and at pressures from 15 MPa to 30 MPa. The dye uptake of Disperse Red 60 on polyester fiber was found to increase with temperature at constant pressure and $SCCO_2$ density (700 kg/$m^3$). At $90^{\circ}C$ and 30 MPa, the dye uptake on polyester fiber increased with dyeing time and the saturation concentration of Red 60 was attained within 240 min, while a longer dyeing time was required for Yellow 54 to reach its saturation concentration. When dyestuff mixtures with mixing ratios of 0.01 to 9.0 (Red 60/Yellow 54) were used, the uptake ratio of the two dyes was found to be proportional to 0.26 power of their mixing ratio. Dyed fibers showed an orange color and the depth of the color depended upon the mixing ratio of the dyestuffs.

Study on Treatment Characteristic of Advanced Oxidation Process using Ozone Oxidation and Peroxone AOP Process for Waste Dyeing Water Effluent Treatment (오존접촉산화 공정과 Peroxone AOP 공정을 이용한 염색폐수방류수 고도산화 처리특성 연구)

  • Park, Jun-Hyung;Shin, Dong-Hoon;Ryu, Seong-Han;Jo, Seog-Jin;Lee, Sang-Hun
    • Textile Coloration and Finishing
    • /
    • v.23 no.4
    • /
    • pp.274-283
    • /
    • 2011
  • Effect of pH on ozone oxidation and peroxone AOP(Advanced Oxidation Process) process was analyzed and the optimal efficiency for both processes was obtained at pH 7.5. In case of ozone oxidation process, the efficiencies of color, $COD_{Mn}$ and $BOD_5$ removal were measured to 93%, 70% and 89% at a reaction time of 50 min(ozone dosage of 111.67mg/$\ell$). When reaction time increased to 90 min(ozone dosage of 201mg/$\ell$), the efficiencies of color, $COD_{Mn}$ and $BOD_5$ removal were increased by 3~5 %, indicating that the increment of removal efficiency was insignificant considering longer reaction time. Similarly, the ozone/$H_2O_2$ ratio was optimized to 0.5 for peroxone AOP process. Removal efficiencies of color, $COD_{Mn}$ and $BOD_5$ were measured 95%, 81% and 94% at a reaction time of 50 min(ozone dosage of 111.67mg/$\ell$). When reaction time increased to 90min(ozone dosage of 201mg/$\ell$), the removal efficiency of color, CODMn, and BOD5 increased slightly by 1~5%.

Study on the Dyeing Behavior of Palmatine, a Major Coloring Compound of Phellodendron Bark, on Cotton Fabric (황백 색소 팔마틴의 면직물에 대한 염색성 연구)

  • Li, Longchun;Narantuya, Lkhagva;Ahn, Cheunsoon
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.39 no.4
    • /
    • pp.601-612
    • /
    • 2015
  • This research investigated the dyeing behavior of palmatine (a major coloring compound of Phellodendron bark in addition to berberine) using mercerization (M), tannic acid (T), mercerization-tannic acid (MT), and tannic acid -mercerization (TM) pretreatments. Mercerization was conducted using $20^{\circ}C$ of 20% NaOH for 5 minutes. Tannic acid treatment was conducted using 15% o.w.f. solution of tannic acid at $60^{\circ}C$ for 30 minutes and fixed with potassium antimonyl tartrate trihydrate. Dyeing was conducted using 1% o.w.f. palmatine chloride hydrate with 1:100 liquor ratio at $10-95^{\circ}C$ for 10-60 minutes in a dyebath of pH 3-9. MT method resulted in the highest dye uptake and was two times higher than the average dye uptake of T method. MT method provided the best result when the dyeing temperature was $80^{\circ}C$ or $95^{\circ}C$ and the dyeing time was 60 minutes. The pH of the dyebath had less effect on the dye uptake but a pH higher than 5 provided better results. The study confirmed that palmatine is a major coloring compound of Phellodendron bark and that the MT method can be used as a successful cotton dyeing method.

The Dyeability of Silk Fabrics with Sweet Potato Stem·Leaf Extract (고구마 줄기·잎 추출액을 이용한 견직물의 염색성)

  • Hong, Bo Geun;Lee, Jeong Sook
    • Textile Coloration and Finishing
    • /
    • v.28 no.3
    • /
    • pp.219-229
    • /
    • 2016
  • The purpose of this study was to investigate the dyeability of silk fabrics with sweet potato stem leaf extract. To obtain the optimal dyeing conditions it was examined at various dyeing conditions(temperature, pH, time and bath ratio). The dyeability and the depths of shade which were evaluated in terms of K/S and CIELAB color difference values of the dyed and mordanted fabrics were also investigated. After dyeing, various color fastness(wash fastness, dry cleaning fastness, light fastness, rub fastness, and perspiration fastness) was measured and reviewed for UV protective, deodorant and antimicrobial functionality. The optimun output, as a result, was shown at 100% of dye concentration, $90^{\circ}C$ of dyeing temperature and 80 minutes of dyeing time while in terms of dye uptake depending on the kind of mordants and mordanting, it was found that among four mordants of $Alk(SO_4)_2$, $CuSO_4$, $SnCl_2$, and $FeSO_4$, post-mordanting with $SnCl_2$ showed the best results. Color fastness to dry cleaning, washing and rubbing was found strong at grade 4-5 and the grade to perspiration was as good as 3 while to light fastness was good at 4 as well. In aspects of functional properties, it showed excellent results of 98.3% UV protection rate and 88% deodorization rate. Antibacterial activity was 99.9% against staphylococcus aureus and 73.3% against klebisella pneumoniae. In conclusion, we validated that the dyestuffs from the disused sweet potato stem leaf extract would be useful as a natural dye material using the optimized conditions and dyeability for silk dyeing.

The Dyeing Properties and Functionality of Water Lily(Nymphaea tetragona) Leaves Extract as a New Natural Dye Resource(2): Dyeing of Silk and Wool Fibers (새로운 천연염료로서 수련 잎 추출색소의 염색성과 기능성(2): 견·모섬유를 중심으로)

  • Yeo, Youngmi;Shin, Younsook
    • Textile Coloration and Finishing
    • /
    • v.29 no.3
    • /
    • pp.171-179
    • /
    • 2017
  • This study was to investigate the practicality and functionality of water lily(Nymphaea tetragona) leaves as a natural dye resource while searching for various dyeing methods to utilize them. Effect of dyeing condition including methanol ratio of dyebath, dyeing temperature and time, mordanting method, etc were investigated. Colorants were prepared by extraction in methanol and followed drying process. When composing 30% of methanol in the dyebath, better dyeuptake and uniform dyeing were resulted. Pre-mordanting method gave better results in terms of dye uptake than post-mordanting method on the wool fabrics. Fe and Ti were effective for increasing the dye uptake on the silk fabrics. Depending on mordant type and mordanting method, the dyed fabrics got various color showing green, khaki, brownish yellow, dark brown, dark gray and so on. As for color fastness, the silk fabrics dyed with water lily extract showed relatively high rating in light fastness(3~4, 4~5 rating), washing fastness(4~5, 5 rating), and rubbing fastness(4, 4~5 rating). The silk and wool fabrics dyed with water lily leaves extract showed excellent antimicrobial activity over 98% of bacterial reduction rate against Staphylococcus aureus and Klebsiella pneumoniae. It was confirmed that water lily leaves can be used as a natural dye resource for dyeing wool and silk fabrics because its colorants showed excellent affinity and antimicrobial functionality as well as good colorfastness.

Dyeing and Deodorizing Properties of Cotton, Silk, and Wool Fabrics Dyed with Various Natural Colorants (여러 가지 천연 염재를 이용한 면, 견, 모직물의 염색 및 소취 특성)

  • Hwang, Eun-Kyung;Lee, Young-Hee;Kim, Han-Do
    • Textile Coloration and Finishing
    • /
    • v.19 no.6
    • /
    • pp.12-20
    • /
    • 2007
  • Four kinds of natural dying solutions (natural colorant extracts)were obtained by extraction from sappan wood, black tea, peony, and clove using water as extracting solvent at $90^{\circ}C$ for 90 min with liquor ratio (solid natural colorant material/solvent water, weight ratio) of 1/10. The dyeing, colour fastness and deodorizing properties of fabrics (cotton, silk, and wool fabrics) dyed with natural colorant extracts were compared. It was found that these properties were significantly dependent on the concentration of extracts, the structure of colorant, and the kind of fabrics. The K/S value of dyed cotton fabric increased in the order of peony < sappan wood < clove < black tea, however, the values of dyed silk and wool fabrics were in the order of peony < sappan wood < black tea < clove. Colour fastness (light, water, and perspiration fastness) was in the range of 3 - 5 grade except for sappan wood. The deodorizing performance of fabrics dyed with various natural colorants extracts was in the range of 56 - 99%. The deodorizing performance increased in the order of peony < black tea < sappan wood < clove. Especially, the deodorizing performance of all fabrics dyed with clove was found to be the highest at 98-99%.

Dyeability and Antimicrobiality of the Silk Fabric Dyed with Inula Britannica (금불초로 염색한 견직물의 염색성 및 항균성)

  • 김병희;송화순
    • Journal of the Korean Home Economics Association
    • /
    • v.40 no.8
    • /
    • pp.99-105
    • /
    • 2002
  • This study was to investigate the natural dyeing materials in domestic, trials to detect new Inula Britannica. An appropriate dyeing condition ;was bath ratio 1:20, 50% (o.w.f.)conc., $80^{\circ}C$, 50min. The K/S values of silk fabric was the most efficient for the pre-mordanting method. The value of dyed fabric was mostly dark, for the mordanting, the chroma was best clear when using the Cr-mordant, color difference was distinct when using the Fe-mordant. The antimicrobiality of Inula Britannica itself appeared as a 6mm halo zone, dyed fabric was excellent with result of over 90% in mordant. In the case of dye fastness, the drycleaning and wet cleaning fastness was excellent, rubbing and perspiration fastness was improved, and light fastness was over level 2.

Syntheses and Characteristics of Intermolecular Charge-Transfer Complex Dyes (분자간 전하이동형 기능성 색소의 합성과 물성)

  • Kim, Sung Hoon;Lee, Soon Nam;Lim, Yong Jin
    • Textile Coloration and Finishing
    • /
    • v.4 no.1
    • /
    • pp.21-25
    • /
    • 1992
  • The charge-transfer(CT) complexes derived from various donors and acceptors were evaluated as coloring matter. Dyes absorbing light in the region from the visible to the near-infrared wavelengths were synthesized. In order to determine the molar ratio of the donor to the acceptor in the CT complex in the solution, the continuous variational method was applied to each system. A 1:1 correspondence between the donor and the acceptor molecules in the CT complex in the solution is established. Color development properties in paper were examined. The longer the exposure time at constant temperature, the deeper the strength of color in paper. The strength of color at high temperature was decreased, because sublimed CT dyes in paper were migrated out side of paper.

  • PDF

The Physical Properties and Dyeability of Poly(trimethylene terephthalate) Fibers (Poly(trimethylene terephthalate) 섬유의 물성과 염색성)

  • 윤석한;김태경;임용진;조규민
    • Textile Coloration and Finishing
    • /
    • v.13 no.3
    • /
    • pp.197-202
    • /
    • 2001
  • The mechanical properties and dyeability of Poly(trimethylene terephthalate)(PTT) were investigated and compared to PET. Glass transition temperature of PTT was lower than that of PET, because amorphous region of PTT is mote flexible. n has smaller molecular and specific stress and larger strain than those of PET, due to the difference of molecular structure. Dyeing transition temperature of PTT was lower by $20^\circ{C}$ than that of PET. Because PTT has flexible chain and zigzag structure, dyeing Fate of PTT is faster than PET and dyeing of PTT is begun at lower temperature. As the hydrophobicity of disperse dyes increased, the ratio of equilibrium dye uptake on PTT to that on PET was increased.

  • PDF

Effect of Heat Treatment on Dyeing and Physical Properties of Nylon 6 Ultramicrofiber (초극세 나일론 6 섬유의 염색성 및 물성에 미치는 열처리의 영향)

  • 정동석;이두환;이문철
    • Textile Coloration and Finishing
    • /
    • v.14 no.6
    • /
    • pp.328-334
    • /
    • 2002
  • Nylon 6 staple ultramicrofiber(UMF, 0.074) and regular staple fiber (Regular, 2.0d) were annealed at In, 130, 160 and $180^\circ{C}$ under tension free for 10 min and U min. The treated fibers were dyed with Acid Red 18 and Blue n3. They were adjusted at PH 5.0 of dye bath in buffer solution of $CH_3COOH/CH_3/COONa(0.1mo1/1)$. Liquor ratio was kept at 1000:1. Dyeing rate of UMF annealed at $100^\circ{C}$ was decreased, but was increased for regular nylon. Also dye equilibrium of UMF at $100^\circ{C}$ was increased for Acid Red 18, but was decreased for Acid Blue 83. The intensities of X-ray diffraction peaks of UMF increased with increasing annealing temperature. Also the crystallinity of heat-sotted fibers by DSC thermogram was well agreed with the tendency of density Amino end group, moisture regain and water absorbency were decreased with increasing annealing temperature.