A Study of Characteristics on the Dissimilar Metals (Alloy steel : A387 Gr. 91 - Carbon Steel : A516 Gr. 70) Welds Made with FCA Multiple Layer Welding: Part 2 (합금강(ASTM A387 Gr. 91) - 탄소강(ASTM A516 Gr.70) 이종금속의 FCA 다층 용접부 특성 평가 : Part. 2)

  • Shin, Tae Woo;Hyun, Jun Hyeok;Koh, Jin Hyun
    • Journal of Welding and Joining
    • /
    • v.35 no.3
    • /
    • pp.68-74
    • /
    • 2017
  • Characteristics of dissimilar metal welds between alloy steel ASTM A387 Gr. 91 and carbon steel ASTM A516 Gr.70 made with Flux cored arc welding(FCAW) have been evaluated in terms of microstructure, mechanical strength, chemical analysis by EDS as well as corrosion test. Three heat inputs of 15.0, 22.5, 30.0kJ/cm were employed to make joints of dissimilar metals with E71T-1C wire. Post-weld heat treatment was carried out at $750^{\circ}C$ for 2.5 h. Based on microstructural examination, Intragranular polygonal ferrite and grainboundary ferrite were formed only in first layer of weld metal. Another layers consisted of acicular ferrite and $Widmannst{\ddot{a}}tten$ ferrite. The amount of acicular ferrite was increased with decreasing heat input and layer. Heat affected zone of alloy steel showed the highest hardness due to the formation of tempered martensite and lower bainite. Lower and upper bainite were formed in heat affected zone of carbon steel. Tensile strengths of dissimilar metal welds decreased with increasing heat inputs. Dissimilar metal welds showed a good hot cracking resistance due to the low HCS index below 4. The salt spray test of dissimilar metals welds showed that the weight loss rate by corrosion below 170 hours was decreased with increasing heat inputs due to the increase of the amount of acicular ferrite.

Promotion of Plant Growth by Submergence and the Action Network of Hormones (침수에 의한 식물의 생장 촉진과 호르몬들의 작용 네트워크)

  • Cho Young Jun;Lee Young Na;Park Woong June
    • Journal of Life Science
    • /
    • v.15 no.1 s.68
    • /
    • pp.112-117
    • /
    • 2005
  • Plants living riverside show diverse resistance responses to submergence. The promoted petiole elongation of semi-aquaitc plants, e.g., such as Ranunculus sceleratus and Rumex palustris, is one of the adaptive responses mediated by the plant hormone ethylene. The gaseous hormone is trapped in submerged plant tissues and enhances the petiole growth by increasing sensitivity of the tissues to some plant hormones including auxin. Due to the stimulated growth of petioles, the leaves finally reach the water surface and can respirate again. At the water surface, the accumulated ethylene diffuses out from the tissues to the air. As a result, the increased hormone sensitivity decreases again, and thus the growth rate reduces to the basal level as before. The increased auxin sensitivities by ethylene observed in Ranunculus sceleratus, revealed by the changes in the auxin dose-response curves, indicate the increase of affinities of the receptors to auxin. However, the molecular mechanism of the affinity regulation remains still largely unknown, because the identity of the auxin receptor is still unclear.

The effect of various heat covering materials on the sprouting and occurrence of disease, insects during wintering of grape young tree (Shigyoku) (포도(자옥) 유목의 월동시 피복한 보온피복재 종류가 발아 및 병해 발생에 미치는 영향)

  • 남상영;김태수;김인재;김민자;이철희
    • Korean Journal of Plant Resources
    • /
    • v.13 no.3
    • /
    • pp.208-212
    • /
    • 2000
  • The effect of heat covering materials during cultivation of Shigyoku grape was examined on the effect of protection from freezing damage, labor reduction, and disease resistance during the wintering. This experimentwas accomplished using different combination of heat covering materials from the end of Nov as follows: straw and heat conservation cover B, kilding, color fabric A, and white needle punching fabric. Capacity of heat conservation was the least form white needle punching fabric, and the differences of other materials was slight. Early sprouting occurred by the treatment with heat conservation cover B, and the rate of sprouting was about 70.7% after 9 days of sprouting, showing 2.3-12.5% increase. Growth effect was not differ between heat conservation materials. Disease and insects occurred by the in dice 3.0-3.2 of crown gall from the heat conservation cover B treatment. Other damages were not observed or very little from other treatments. Demand of labor during steps of these treatments was more observed by 6% for kilding than heat conservation cover B, and those of color fabric A and white needle punching fabric were reduced by 6 and 15%, respectively.

  • PDF

Thermal and Mechanical Properties of a N2 Doped Porous 3C-SiC Thin Film (질소가 도핑된 다공질 3C-SiC 박막의 열적, 기계적 특성)

  • Kim, Kang-San;Chung, Gwiy-Sang
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.8
    • /
    • pp.651-654
    • /
    • 2010
  • This paper describes the thermal and mechanical properties of doped thin film 3C-SiC and porous 3C-SiC. In this work, the in-situ doped thin film 3C-SiC was deposited by using atmospheric pressure chemical vapor deposition (APCVD) method at $120^{\circ}C$ using single-precursor hexamethyildisilane: $Si_2(CH_3)_6$ (HMDS) as Si and C precursors. 0~40 sccm $N_2$ gas was used as doping source. After growing of doped thin film 3C-SiC, porous structure was achieved by anodization process with 380 nm UV-LED. Anodization time and current density were fixed at 60 sec and 7.1 mA/$cm^2$, respectively. The thermal and mechanical properties of the $N_2$ doped porous 3C-SiC was measured by temperature coefficient of resistance (TCR) and nano-indentation, respectively. In the case of 0 sccm, the variations of TCR of thin film and porous 3C-SiC are similar, but TCR conversely changed with increase of $N_2$ flow rate. Maximum young's modulus and hardness of porous 3C-SiC films were measured to be 276 GPa and 32 Gpa at 0 sccm $N_2$, respectively.

A Study of Characteristics on the Dissimilar Metals (Alloy Steel : A387 Gr. 91 - Carbon Steel : A516 Gr. 70) Welds Made with FCA Multiple Layer Welding : Part 1 (합금강(ASTM A387 Gr. 91) - 탄소강(ASTM A516 Gr.70) 이종금속의 FCA 다층 용접부 특성 평가 : Part. 1)

  • Shin, Tae Woo;Jang, Bok Su;Koh, Jin Hyun
    • Journal of Welding and Joining
    • /
    • v.34 no.3
    • /
    • pp.61-68
    • /
    • 2016
  • Characteristics of dissimilar metal welds between alloy steel ASTM A387 Gr. 91 and carbon steel ASTM A516 Gr.70 made with Flux cored arc welding(FCAW) have been evaluated in terms of microstructure, mechanical strength, chemical analysis by EDS as well as corrosion test. Three heat inputs of 15.0, 22.5, 30.0kJ/cm were employed to make joints of dissimilar metals with E91T1-B9C wire. Post-weld heat treatment was carried out at $750^{\circ}C$ for 2.5 h. Based on microstructural examination, tempered martensite and lower bainite were formed in first layer of weld metal. The amount of tempered martensite was decreased and the amount of lower bainite was increased with increasing heat input and layer. Heat affected zone of alloy steel showed the highest hardness due to the formation of tempered Martensite and lower Bainite. Tensile strengths of dissimilar welds decreased with increasing heat inputs. Dissimilar welds seemed to have a good hot cracking resistance due to the low HCS index below 4. The salt spray test of dissimilar metals showed that the corrosion rate increased with increasing heat inputs due to the increase of the amount of lower Bainite.

The Effect of Fatigue Fracture in shot peening Marine structural steel at stress ratio (쇼트피닝 가공된 해양구조용강의 피로파괴에 미치는 응력비의 영향)

  • Park, Kyoung-Dong;Han, Kun-Mo;Jin, Young-Beom
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2003.10a
    • /
    • pp.138-144
    • /
    • 2003
  • Rencentely, the request for the light weight is more incresed in the area of industrial environment and machinery and consistent effort is needed to accomplish high strength of material for the direction of light weight. we got the following characteristic from crack growth test carried out in the range of stress ration of 0.1, 0.3 and 0.6 by means of opening mode displacement. At the content stress ratio, the threshold stress intensity factor crack range ${\Delta}K_{th}$in the early stage of fatigue crack growth (Region I) and dtress intensity factor range ${\Delta}K$ in the stable of fatigue crack growth (Region II) with an increase in ${\Delta}K$. Fatigue life shows more improvement in the Shot-peened material than in the Un-peening material. And compressive residual stress of surface on the Shot peening processed operate resistance force of fatigue. So we can obtain fallowings. (1) The fatigue crack growth rate on stage II is conspicuous with the size of compressive residual stress and is depend on Paris equation. (2) Although the maxium compressive residual stress is deeply and widely formed from surface, fatigue life does not improve than when maxium compressive residual stress is formed in surface. (3) The threshold stress intensity factor range is increased with increasing compressive residual stress.

  • PDF

Arsenic Trioxide Promotes Paclitaxel Cytotoxicity in Resistant Breast Cancer Cells

  • Bakhshaiesh, Tayebeh Oghabi;Armat, Marzie;Shanehbandi, Dariush;Sharifi, Simin;Baradaran, Behzad;Hejazi, Mohammad Saeed;Samadi, Nasser
    • Asian Pacific Journal of Cancer Prevention
    • /
    • v.16 no.13
    • /
    • pp.5191-5197
    • /
    • 2015
  • A partial response or resistance to chemotherapeutic agents is considered as a main obstacle in treatment of patients with cancer, including breast cancer. Refining taxane-based treatment procedures using adjuvant or combination treatment is a novel strategy to increase the efficiency of chemotherapy. PPM1D is a molecule activated by reactive oxygen species. whose expression is reported to modulate the recruitment of DNA repair molecules. In this study we examined the impact of arsenic trioxide on efficacy of paclitaxel-induced apoptosis in paclitaxel-resistant MCF-7 cells. We also investigated the expression of PPM1D and TP53 genes in response to this combination treatment. Resistant cells were developed from the parent MCF-7 cell line by applying increasing concentrations of paclitaxel. MTT assays were applied to determine the rate of cell survival. DAPI staining using fluorescent microscopy was employed to study apoptotic bodies. Real-time RT-PCR analysis was also applied to determine PPM1D mRNA levels. Our results revealed that combination of arsenic trioxide and paclitaxel elevates the efficacy of the latter in induction of apoptosis in MCF-7/PAC resistant cells. Applying arsenic trioxide also caused significant decreases in PPM1D mRNA levels (p<0.05). Our findings suggest that arsenic trioxide increases paclitaxel-induced apoptosis by down regulation of PPM1D expression. PPM1D dependent signaling can be considered as a novel target to improve the efficacy of chemotherapeutic agents in resistant breast cancer cells.

Treatment of Intraoperative Thrombosis and Spasm in Free Tissue Transfers Using the Fogarty Catheter (포가티 카테터를 이용한 유리조직 전이술 시 수술 중 혈전 및 연축의 치료)

  • Lee, Seung Ryul;Yun, Young Mook;Oh, Sang-Ha
    • Archives of Plastic Surgery
    • /
    • v.35 no.2
    • /
    • pp.159-164
    • /
    • 2008
  • Purpose: Microvascular free tissue transfer has become a reliable technique for the reconstruction of complex wounds. Occasionally, unexpected intraoperative thrombosis and/or spasm of recipient artery might be annoying problems even for the technically competent microvascular surgeons. If such problems are not treated properly, they will inevitably cause to flap failure. Methods: From January 2006 to February 2007, soft tissue reconstructions by free tissue transfers were performed on 21 patients having complex defects in the lower extremity. Although segmental revision and various pharmacologic agents were repeatedly applied, arterial occlusions were not managed in 6 cases. For removal of thrombi and release of spasm, Fogarty No. 2 or No. 3 catheters were inserted into the lumen to the proximal recipient artery. Its balloon was then inflated after passing through a resistant area. Next, the catheter was gently withdrawn backward. Results: After the Fogarty catheter was inserted two or three times, the pulsatile arterial flow was restored. When the catheter was inserted into the lumen, a feeling of resistance existed in a 5-10cm more proximal portion that could not be easily accessed from the vascular end. After the reestablishment of blood flow, successful anastomoses were achieved and immediate rethrombosis or spasm did not occur. No long-term sequelae associated with balloon trauma to the arterial wall were observed. Conclusion: The use of the Fogarty catheter can be an effective method in treating pedicle thrombosis and spasm. This is a very simple and rapid technique that offers microvascular surgeons another option to increase the success rate of microvascular anastomosis in free tissue transfers.

The Variation of Microstructures and Mechanical Properties by Thermomechanical Treatment in Al-Li Based Alloys (AI-Li제 합금의 가공열처리에 따른 조직과 기계적성질의 변화)

  • Kim, Ki Won;Woo, Kee Do;Lee, Kwang Ro;Lee, Min Sang;Lee, Min Ho;Hwang, Ho Eul
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.4 no.3
    • /
    • pp.13-20
    • /
    • 1991
  • The present work was aimed to examine the variation of precipitations and mechanical properties by thermomechanical treatments (TMT) in Al-2.19 wt%Li and Al-2.0 wt%Li-0.11 wt%Zr alloys. This study was performed by TEM, SEM observation, DSC, electrical resistance measurement, hardness and tensile strength measurement. First peak of resistivity aged at $90^{\circ}C$ was caused by precipitation of ${\delta}^{\prime}$-precursor phase, and second peak was caused by precipitation of ${\delta}^{\prime}$ phase. According to this result, the precipitation process of Al-2.19 wt%Li alloy was as follow : $SSSS{\rightarrow}{\delta}^{\prime}$-precursor phase ${\rightarrow}{\delta}^{\prime}$ (Coherent ${\rightarrow}$ Semi-coherent) ${\rightarrow}{\delta}$. In a Al-2.0 wt%Li-0.11 wt%Zr ternary alloy, the first peak of resistivity was appeared at initial aging heat-treatment. It is result from exsistant of ${\delta}^{\prime}$-precursor phase. The effect acceleration in a binary alloy was not appeared and the over-aging ternary alloy was accelerated with increase of the reduction rate. It is caused by combination effect of ${\delta}^{\prime}$ and composite phase.

  • PDF

The Isoflurane Concentration of Precision Vaporizer Goldman Vaporizer According to Room Temperature and Carrier Gas Flow Rate (온도 및 유량에 따른 흡입 마취제 전용 기화기와 Goldman 기화기의 isoflurane 농도 변화)

  • 김성미;장화석;이정선;최치봉;임희란;최준철;김휘율
    • Journal of Veterinary Clinics
    • /
    • v.21 no.3
    • /
    • pp.270-275
    • /
    • 2004
  • Anesthetic machines may be equipped with either a precision or nonprecision vaporizer. A precision vaporizer is designed to deliver an exact concentration of anesthetic agent. Goldman vaporizer is a low-flow, closed-circle circuit with a low resistance vaporizer, in circuit. Vaporizers used within circle system(VIC) are not usually temperature compensated and this is generally thought to be a disadvantage. As the volatile agent is vaporized, heat is extracted from the liquid and temperature decreases. This cooling of the liquid leads to a decrease in concentration of the anaesthetic agent delivered by the vaporizer. The purpose of this study is to examine the mechanical consistency of the delivery of isoflurane from Goldman vaporizer and precision vaporizer at various gas flow rates and temperatures. And we first studied isoflurane concentration according to room temperature changes delivered by a Goldman vaporizer and precision vaporizer using different gas flow. The room temperature of $15^{\circ}C,$ $20^{\circ}C,$ $28^{\circ}C$ and fresh gas flow rates of 0.5, 1.0, 1.5, 2.0, 3.0 l/min were used. The inspired agent concentration was measured using a Datex-Ohmeda multigas analyzer. As rose in room temperature, the isoflurane concentration of precision vaporizer approximated the dial setting. On the other hand, at a dial setting concentration of 5.0 percent the delivered isoflurane concentration of precision vaporizer was more than the dial setting in high temperature. The isoflurane concentration of precision vaporizer remained constant despite the increase in temperature. The isoflurane concentration of Goldman vaporizer was increased with rise in room temperature and decreased with rise in gas flow.