  • Recently, the spread of intense social distancing and untact culture due to COVID-19 has increased the time spent indoors. In addition, according to the International Cancer Institute, fine dust was classified as a first-class carcinogen, a substance found to be carcinogenic, such as asbestos and benzene. As a result, interest in indoor air quality is increasing, and many studies are underway to reduce air pollutants. This study is a basic experiment of a board made to improve indoor air quality. The basic characteristics of the board, flexural strength and compressive strength, are analyzed and the results of the test are as follows. Experiments have shown that flexural strength and compressive strength tend to decrease as the replacement rate of hydrocarbons increases. It is believed that the strength of the sludge has decreased due to the increase in internal voids due to the increase in non-surface area, volume and diameter of microfiber as it undergoes the carbonation process. In addition, it is believed that the amount of moisture needed for curing during the mixing process was reduced due to the absorption of hydrocarbons.

  • PDF

무시멘트 기반 하이드로볼을 활용한 투수블록의 강도 특성 (Noncement-based Hydroball Evaluation of Permeable Block Strength Properties)

  • 황우준;이창우;이상수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2022년도 가을 학술논문 발표대회
    • /
    • pp.207-208
    • /
    • 2022
  • Since 1960, the green area has decreased due to rapid urbanization and the artificial surface has increased, and the repair and water function of the previous surface has decreased due to the decrease in rainwater absorption capacity. In addition, the risk of carbon dioxide and fine dust is emerging due to the use of fossil fuels due to urbanization. As a result, permeable blocks, an eco-friendly product, are in the spotlight. Therefore, this study was conducted to examine the strength properties of the permeable block using a hydroball. As a result of the experiment, the flexural strength and compressive strength tended to decrease as the hydroball replacement rate increased. It is judged that the hydroball absorbs a large amount of moisture during the mixing process and lacks moisture required for curing, resulting in a decrease in strength. According to KS F 4419, since the hydroball replacement rate is satisfied up to 20%, further research is needed to analyze the adsorption performance of air pollutants in the future and evaluate their utilization as a permeable block in the future.

  • PDF

제올라이트와 활성 황토를 혼입한 시멘트 모르타르의 광촉매(TiO2) 코팅에 따른 NOx 저감성능평가 (Evaluation of NOx Reduction Performance by Photocatalytic (TiO2) Coating of Cement Mortar Mixed with Zeolite and Activate Hwangtoh)

  • 박장현;김혁중
    • 한국건설순환자원학회논문집
    • /
    • 제8권4호
    • /
    • pp.483-489
    • /
    • 2020
  • 미세먼지는 머리카락 두께의 약 1/5 수준인 PM10(입자의 지름 10㎛이하)과 PM2.5(입자의 지름 2.5㎛이하)로 구분되며, 인체에 미치는 영향으로 폐질환, 혈관을 통한 동맥경화 및 심장 질환 등 각종 질병을 유발하는 발암물질로 알려져 있다. 이러한 미세먼지의 주요 원인은 도심지 도로변에서 발생되는 약 57.3%가 자동차에서 배출되는 이산화질소(NOx)로 알려져 있다. 이에 본 연구에서는 도로이동오염원에서 발생하는 NOx를 저감하기 위한 기능성 건설재료 개발의 일환으로 시멘트를 다공성 소재로 치환한 시멘트 모르타르의 치환율에 따른 NOx저감성능 비교 평가를 실시하였다. 또한 시멘트 모르타르의 광촉매 적용방법 및 도포 횟수에 따른 NOx저감성능을 비교 평가하였다. 실험결과 활성황토를 30% 치환하여 사용한 경우 약 32.7%의 저감효과를 나타내 가장 우수한 저감성능을 갖는 것으로 나타났다.

골재 중 0.08 mm 이하 미립분의 종류가 콘크리트의 특성에 미치는 영향 (The Influence of Fine Particles under 0.08 mm Contained in Aggregate on the Characteristics of Concrete)

  • 송진우;최재진
    • 콘크리트학회논문집
    • /
    • 제25권3호
    • /
    • pp.347-354
    • /
    • 2013
  • 최근 천연모래의 부족으로 부순 잔골재가 널리 사용되고 있다. 우리나라에서는 부순 잔골재 중의 0.08 mm 이하 미립분을 7% 이하로 제한하고 있으며 이는 ASTM의 규정과 유사한 것이나 그 외의 다른 나라의 규정과 비교할 때 상당히 엄격한 규정이다. 또한 부순 잔골재 중에는 파쇄 시에 발생하는 0.08 mm 이하 미립분을 20% 정도 포함하게 되며 물로 씻어내는 일도 용이하지 않을 뿐 아니라 자원이용의 극대화를 위해서도 잔입자량 한도의 상향 조정 가능 여부에 대한 검토가 필요하다. 그래서 이 연구에서는 0.08 mm 이하 미립분에 대한 특성 및 콘크리트 품질에 미치는 영향에 대한 실험을 실시하였으며, 비교를 위하여 실트 및 점성토 중의 미립분을 사용한 실험을 병행하였다. 미립분에 대해 실험한 결과 메틸렌블루 값은 부순 잔골재 중의 석분에 비하여 실트 및 점성토 중의 미립분에 대한 값이 보다 크게 나타났으며 또한 메틸렌블루 값은 packing density 및 액성한계, 소성한계와 높은 상관관계를 가지는 것으로 나타났다. 콘크리트 실험에서 동일한 슬럼프를 얻기 위한 고성능 감수제의 소요량은 미립분의 대체 사용량 증가에 따라 커지며, 메틸렌블루 값이 큰 미립분을 사용할 때 보다 크게 나타났다. 한편 부순 잔골재 중의 미립분을 20% 이내에서 대체 사용한 경우, 고성능감수제를 사용하여 반죽질기를 같게 한 콘크리트의 압축강도와 인장강도는 거의 변화가 없었으며 콘크리트의 건조수축량도 큰 차이를 보이지 않았다. 그러나 실트 및 점성토 중의 미립분을 대체 사용한 경우는 콘크리트의 강도가 현저히 저하하고 건조수축량도 크게 증가하는 것으로 나타났다.