Eutectic Nanocomposites for Thermophotovoltaic Application

  • Han, Young-Hwan;Lee, Jae-Hyung;Kakegawa, Kazuyuki
    • Transactions on Electrical and Electronic Materials
    • /
    • v.11 no.6
    • /
    • pp.249-252
    • /
    • 2010
  • The ground amorphous powder was consolidated into a dense sintered body with a typical ultrafine $Al_2O_3-GdAlO_3$ eutectic structure by spark plasma sintering (SPS). Sintered material with ultrafine and dense eutectic structure was obtained by an appropriate combination of rapid quenching and SPS at lower temperature and more quickly than by conventional sintering. The $Al_2O_3$-based rare earth eutectic ceramics for solar cell emitters are believed to have a higher efficiency and the $Al_2O_3$ based eutectic ceramics with ultrafine grains will be one of the promising materials showing excellent selective emitter characteristics.

Rapid Sintering Process of Ultra Fine WC-Co Hard Materials by High-Frequency Induction Heating

  • Kim, H.C;Oh, D.Y.;Jeong, J.W.;Shon, I.J.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2003.10a
    • /
    • pp.39-40
    • /
    • 2003
  • 1) Using a developed high-frequency induction heated sintering method, the rapid densification of WC-Co hard materials was accomplished using ultra fine powders with 260 nm size within 1 minute. 2) The relative density of the composite was 99.5% for the applide pressure of 60MPa and the induced current for 90% output of total capacity. 3) The grain size of WC-Co hard materials is about 260nm and the average thickness of the binder phase determined is about 11nm. The fracture toughness and the hardness of this work 12 $MPa{\cdot}nm^2$, respectively. 4) Using pressureless sintering, we produced dense WC-Co hard materials with a relative density of 97% without applying pressure.

  • PDF

The Effect of La-silicon Oxynitride on the Densification of ${Si_3}{N_4}$ Ceramics by Spark Plasma Sintering

  • Cho, Kyeong-Sik;Kim, Sungjin;Beak, Sung-Ho;Park, Heon-Jin;Lee, June-Gunn
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.8
    • /
    • pp.687-692
    • /
    • 2001
  • Silicon nitride-La-silicon oxynitride ceramics were fabricated by Spark Plasma Sintering (SPS). The density, crystalline phase and microstructure were compared with those obtained by Hot Pressing (HP). The full density was achieved within 40 min by spark plasma sintering at 1$650^{\circ}C$, whereas the same result was required by hot pressing with a dwell time of 500 min at higher temperature. There were some differences in the microstructure and second phases in the sintered ceramics, which are attributed to the rapid densification in the spark plasma sintering. The fine and acicular grain microstructure appeared in spark plasma sintering.

  • PDF

Thermoelectric Properties of Rapid Solidified p-type Bi2Te3 Alloy Fabricated by Spark Plasma Sintering(SPS) Process (방전 플라즈마 소결법(SPS)으로 제조된 급속응고 p-type Bi2Te3 합금의 소결 특성)

  • Moon, Chul-Dong;Hong, Soon-Jik;Kim, Do-Hyang;Kim, Taek-Soo
    • Journal of Powder Materials
    • /
    • v.17 no.6
    • /
    • pp.494-498
    • /
    • 2010
  • The p-type thermoelectric compounds of $Bi_2Te_3$ based doped with 3wt% Te were fabricated by a combination of rapid solidification and spark plasma sintering (SPS) process. The effect of holding time during spark plasma sintering (SPS) on the microstructure and thermoelectric properties were investigated using scanning electron microscope (SEM), X-ray diffraction (XRD) and thermoelectric properties. The powders as solidified consisted of homogeneous thermoelectric phases. The thermoelectric figure of merit measured to be maximum ($3.41{\times}10^{-3}/K$) at the SPS temperature of $430^{\circ}C$.

Rapid Sintering of Nanostuctured Tungsten Carbide by High-Frequency Induction Heating and its Mechanical Properties (고주파유도 가열에 의한 나노구조의 텅스텐 카바이드 급속소결과 기계적 성질)

  • Kang, Hyun-Su;Doh, Jung-Mann;Hong, Kyung-Tae;Ko, In-Yong;Shon, In-Jin
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.11
    • /
    • pp.1009-1013
    • /
    • 2010
  • Extremely dense WC with a relative density of up to 99% was obtained within five minutes under a pressure of 80 MPa using the High-Frequency Induction Heated Sintering method. The average grain size of the WC was about 71 nm. The advantage of this process is not only rapid densification to obtain a neartheoretical density but also the prohibition of grain growth in nano-structured materials. The hardness and fracture toughness of the dense WC produced by HFIHS were $2660kg{\cdot}mm^{-2}$ and $7.2MPa{\cdot}m^{1/2}$, respectively.

A Study on the Manufacturing Rapid Prototype Using Bronze (Bronze를 이용한 쾌속조형제조에 대한 연구)

  • 전병철;김재도
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1995.10a
    • /
    • pp.204-209
    • /
    • 1995
  • The implementation of rapid prototyping technologies has been developed for automotive engineering by utilizing concurrent engineering principes integrated with slective laser sintering. The Selective Laser Sintering, in which a part is generated in layers form powder using a computer-controlled laser scanning apparatus and power feed system. An over view of the basic principles of SLS Machine operation is given. Binding mechanisms are described for power which becomes thermally activated bye the scanning laser beam; viscous flow and melting of a low-melting-point phase in powder. The production of parts from metal is described, including post processing to improve structural integrity and induce a transformation.

  • PDF

Process developments for direct manufacturing of metallic prototypes (금속시제품의 신속제작을 위한 공정기술개발)

  • 송용억
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1996.04a
    • /
    • pp.605-609
    • /
    • 1996
  • In order to ensure that the prototype corresponds as closely as possible to the serial part subsequently to be manufactured, the materials used for the prototye should, wherever possible, be identical to those used in production. In case of metallic parts, however, this demand is still not completely fulfilled by the available Rapid Prototyping techniques. Since only conventional manufacturing processes caan currentlybe used to produce metallic prototypes directly, these are extremely cost and labor intensive. For this reason, work is being undertaken worldwide to develop Selective Laser Sintering (referred to SLS) and Laser Generating for direct manufacture of metallic parts. In this paper the results of both process developments are reported. As the present results show, they have great application potentials in prototyping tools, especially molds and dies.

  • PDF

A Study on Manufacturing Resin-based Blow Mold using SLS Parts and Forming Prototype-car Parts (SLS 조형품을 이용한 수지형 블로우 몰드 제작 및 시작차 부품성형에 관한 연구)

  • 양화준;황보중;이석희
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.17 no.7
    • /
    • pp.124-131
    • /
    • 2000
  • Rapid Prototyping(RP) models are no longer used only for design verification. Currently, parts built utilizing layer manufacturing technology can be employed as functional prototypes and as patterns or tools for different manufacturing processes such as vacuum casting, investment casting, injection molding, precise casting and sand casting. This trend of Rapid Prototyping application meets the requirement of concurrent engineering and its range covers a more spreaded area. The aim of this paper is saving the manufacturing lead time and cost of plastic parts having hollow space shapes used by prototype-car. Using rapid prototype patterns, made by the Selective Laser Sintering(SLS) technique, a new approach of manufacturing resin-based blow mold is discussed. It has a great potential fur making prototype-car parts with the batch size of under 200 parts, in case of rapid modification due to a subsequent design changes in developing stage. So, the process proposed in this research shows reduction of process time and manufacturing cost when compared with the conventional process such as a Zinc Alloy fur Stamping(ZAS) mold.

  • PDF