B2형 금속간화합물 NiTi 중에 L21형 Ni2AlTi상의 석출 (Precipitation of L21-type Ni2AlTi Phase in B2-type Intermetallic Compounds NiTi)

  • 한창석
    • 한국재료학회지
    • /
    • 제17권8호
    • /
    • pp.420-424
    • /
    • 2007
  • Precipitation behavior has been studied in NiTi-based ordered alloy using transmission electron microscopy. The hardness after solution treatment is high in NiTi alloy suggesting the large contribution of solid solution strengthening in this alloy system. However, the amount of age hardening is not large as compared to the large microstructural variations during aging. At the beginning of aging, the $L2_1-type$ $Ni_2AlTi$ precipitates keep a lattice coherency with the NiTi matrix. By longer periods of aging $Ni_2AlTi$ precipitates lose their coherency and change their morphology to the globular ones surrounded by misfit dislocations. Misfit dislocations, which are observed on {100} planes of H-precipitates have the Burgers vector of a <100> with a pure edge type. The lattice misfits of $NiTi-Ni_2AlTi$ system is estimated from the spacings of misfit dislocations to be 1.3% at 1273 K. The lattice misfits decrease with increasing aging temperature in this system.

Applicability of biocementation for organic soil and its effect on permeability

  • Sidik, Waleed S.;Canakci, Hanifi;Kilic, Ibrahim H.;Celik, Fatih
    • Geomechanics and Engineering
    • /
    • 제7권6호
    • /
    • pp.649-663
    • /
    • 2014
  • In past few years, the use of bacterial calcium carbonate precipitation (biocementation) has become popular as a ground improvement technique for sandy soil. However, this technique was not applied to organic soil. This study focused on bacterial calcium carbonate precipitation and its effect on permeability in organic soil. A special injection system was prepared for inducing bacterial solution to the samples. The bacterial solution supplied to the samples by gravity for 4 days in specific molds designed for this work. Calcite precipitation was observed by monitoring pH value and measuring amount of calcium carbonate. Change in the permeability was measured before and after biocementation. The test results showed that the pH values indicates that the treatment medium is appropriate for calcite precipitation, and amount of precipitated calcium carbonate in organic soil increased about 20% from untreated one. It was also found that the biocementation can be considered as an effective method for reducing permeability of organic soil. The results were supported by Scanning electron microscopy (SEM) analysis and energy-dispersive x-ray (EDX) analysis.

초음파 오일 스러지 처리 시스템 개발을 위한 기초 연구 (A Basic Study on the Development of Oily Sludge Treatment System by Ultrasonic Waves)

  • 이은방
    • 해양환경안전학회지
    • /
    • 제6권1호
    • /
    • pp.57-67
    • /
    • 2000
  • All crude oil carries a little of water, sand, and mineral sediment molecules tightly bounded with hydrocarbons. The result is the gradual precipitation of these heavier elements into thick, granular petroleum by products known as crude oil sludge. The oily sludges in ship tanks and in storage facilities have to be treated efficiently in order to keep the security and the capacity of storage facilities, to protect a serious environmental pollution, and to retrieve lost resource. The oily sludge treatment system should be designed to satisfy requirements mentioned in safe work condition. As a basic study, in this paper, an oily sludge treatment system by ultrasonic waves was proposed. Then, the features of ultrasonic energy and recovery of sludge with ultrasonic waves are investigated by experiments. As results, we found that ultrasonic waves are a new energy to flow oil sludge environment-friendly in safe work condition. In addition, it was shown that ultrasonic energy is more efficient than thermal energy in treating oil sludge, and that the volume of wastes for disposal is reduced remarkably.

  • PDF

Effects of pH, molar ratios and pre-treatment on phosphorus recovery through struvite crystallization from effluent of anaerobically digested swine wastewater

  • Kim, Daegi;Min, Kyung Jin;Lee, Kwanyong;Yu, Min Sung;Park, Ki Young
    • Environmental Engineering Research
    • /
    • 제22권1호
    • /
    • pp.12-18
    • /
    • 2017
  • Struvite precipitation has been proven to be an effective method in removing and recovering ammonia nitrogen (N) and phosphate phosphorus (P) from wastewater. In this study, effects of pH, molar ratios and pre-treatment of effluent of anaerobically digested swine wastewater were investigated to improve struvite crystallization. The magnesium : ammonium : phosphate ratio of 1.2 : 1.0 : 1.0 was found to be optimal, yet the molar ratio in the wastewater was 1 : 74.9 : 1.8. From the analysis, the optimum pH was between 8.0 and 9.0 for maximal phosphate P release and from 8.0 to 10.0 for maximal ammonia N and phosphate P removal from real wastewater. Analysis from Visual MINTEQ predicted the pH range of 7-11 for ammonia N and phosphate P removal and recovery as struvite. For pre-treatment, microwave pre-treatment was ineffective for phosphate P release but ultrasound pre-treatment showed up to 77.4% phosphate P release at 1,000 kJ/L of energy dose. Precipitates analysis showed that phosphorus and magnesium in the collected precipitate had almost same values as theoretical values, but the ammonia content was less than the theoretical value.

열처리가 Elgiloy 선재의 기계적 성질에 미치는 영향 (THE EFFECTS OF HEAT TREATMENT ON THE MECHANICAL PROPERTIES OF THE ELGILOY WIRE)

  • 허택;이병태;최석규;김형일
    • 대한치과교정학회지
    • /
    • 제22권3호
    • /
    • pp.557-578
    • /
    • 1992
  • Heat treatment which removes internal stress enhances the mechanical properties of the orthodontic arch wire. The main purpose of this experiment was to investigate the effects of the heat treatment on the mechanical properties of the Elgiloy wire. The Elfiloy wire, 0.016' X 0.022' and 0.018' X 0.025', were heat treated in an electric oven for 5, 10 and 15 minutes at selected temperatures between 300 and $900^{\circ}C$. Tensile strength and load deflection rate were measured to reveal the changes of mechanical property at various conditions, and each specimen was observed under metallurgic microscope. Also to trace the precipitation material due to overheat treatment, a qualitative analysis was carried out with EDS system. It was found that heat treatment at a low temperature caused an increase in the tensile strength and bending resistance, and a maintenance in the fibrous in the tensile strength and bending resistance, and a maintenance in the fibrous structure of both sizes of wire. The changes observed in properties and appearance were probably due to the relief of internal stresses incurred in the metal during cold working. In both sizes of wire the tensile strength and the bending resistance continued to decrease at high temperature, and the fibrous structure continued to disappear then was not observed at $900^{\circ}C$. The carbide precipitation founded in grain boundary at $750^{\circ}C$ probably was other elements carbide (Ni, Co) except Cr. The grain growth was observed at $1100^{\circ}C$. Optimum heat treatment for the 0.016' X 0.022' Elgiloy wire was 10 minutes at $500^{\circ}C$, and for the 0.018' X 0.025' Elgiloy wire it was 5 to 15 minutes at $500^{\circ}C$.

  • PDF

진공 정밀주조한 Inconel 713C 합금의 조직과 기계적 성질에 미치는 열처리의 영향 (The Effect of Heat Treatment on the Microstructures and Mechanical Properties of Inconel 713C Alloy Vacuum Investment Castings)

  • 유병기;최학규;박흥일;정해용
    • 한국주조공학회지
    • /
    • 제40권2호
    • /
    • pp.16-24
    • /
    • 2020
  • The effect of a heat treatment on the microstructure and mechanical properties of Inconel 713C alloy vacuum investment castings were investigated. The microstructure of the as-cast state was observed, showing well-developed dendrite structures and distributed carbide particles and solidified massive precipitates in the grain or grain boundary during solidification, in this case the γ′ phase and MC particles. During a heat treatment, the γ phase matrix was reinforced by solid solution elements, carbide particles from the film morphology precipitated along the grain boundary, and many micro-precipitates of second γ′ phases 0.2 ㎛~2 ㎛ in size were newly formed in the γ phase matrix according to SEM-EDS analysis results. The tensile strength at a high temperature (850℃) decreased slightly becoming comparable with the room-temperature result, while the hardness value of the specimen after the vacuum heat treatment increased by approximately 19%, becoming similar to that of the as-cast condition. However, the impact values at room temperature and low temperature (-196℃) were approximated; this alloy was mostly not affected by an impact at a low temperature. In the observations of the fracture surface morphologies of the specimens after the tensile tests, the fractures at room temperature were a mix of brittle and ductile fractures, and an intergranular fracture in the inter-dendrite structure and some dimples in the matrix were observed, whereas the fractures at high temperatures were ductile fractures, with many dimples arising due to precipitation. It was found that a reinforced matrix and precipitates of carbide and the γ′ phase due to the heat treatment had significant effects, contributing greatly to the excellent mechanical properties.

CO-기 합금의 열처리에 의한 미세조직 및 기계적 특성변화에 관한 연구 (The Effect of Heat Treatment on the Microstructural Evolution and Mechanical Properties of Co-base Materials)

  • 김기엽;정병호;안용식
    • 동력기계공학회지
    • /
    • 제5권2호
    • /
    • pp.63-70
    • /
    • 2001
  • To obtain the optimal condition of heat treatment of wear-resistant alloy, hardness and Charpy V-notch test have been performed with Co-based Stellite No.4, No.6 and Tribaloy 800 alloys, following by heat treatment at the various conditions. Heat treatment at $1250^{\circ}C$ for 1 hours caused the as-casted Tribaloy 800 with FCC crystal structure to transform to HCP structure and lamellar eutectic structure was disappeared, which did not influence on the hardness. Aging at $800^{\circ}C$ for 20 hours, following by $1250^{\circ}C$ for 2 hours heat treatment has enhanced hardness significantly, which is due to the precipitation of large amounts of Laves-phase. The hardness of Stellite alloys was increased by the aging at $800^{\circ}C$ to 5 hours, and was nearly constant by the aging over 5 hours. The toughness of Stellite alloys was a few influenced by the aging treatment.

  • PDF

금속-세라믹용 Pd-Au-Ag-Sn계 합금의 모의소성 후 계류에 따른 석출경화 (Precipitation Hardening by Holding After Simulated Complete Firing in a Metal-Ceramic Alloy of Pd-Au-Ag-Sn System)

  • 김민정;신혜정;권용훈;김형일;설효정
    • 대한치과재료학회지
    • /
    • 제43권4호
    • /
    • pp.343-349
    • /
    • 2016
  • This experiment was carried out to examine whether the post-firing heat treatment is effective in increasing the hardness of metal-ceramic alloy of the Pd-Au-Ag-Sn system. Precipitation hardening by holding at $600^{\circ}C$ after simulated complete porcelain firing in a metal-ceramic alloy of the Pd-Au-Ag-Sn system was examined by observing the change in hardness, crystal structure, and microstructure using a hardness test, X-ray diffraction (XRD), and field emission scanning electron microscopy (FE-SEM). The hardness of the alloy increased apparently by holding the specimen at $600^{\circ}C$ for 30 min after simulated complete porcelain firing. The formation of fine grain interior precipitates during holding at $600^{\circ}C$ caused the formation of lattice strain in the grain interior, resulting in apparent hardening. The faster cooling rate (stage 0) during simulated complete porcelain firing resulted in more effective precipitation hardening during holding at $600^{\circ}C$. From the above results, an appropriate post-firing heat treatment, such as holding at $600^{\circ}C$ for 30 min after complete porcelain firing may increase the durability of metal-ceramic prostheses composed of Pd-Au-Ag-Sn alloy.

Removal of sulfate ion from semiconductor wastewater by ettringite precipitation

  • Chung, Chong-Min
    • Membrane and Water Treatment
    • /
    • 제13권4호
    • /
    • pp.183-189
    • /
    • 2022
  • This study seeks towards an optimal way to control sulfate ions in semiconductor wastewater effluent with potential eco-toxicity. We developed a system based on ettringite (Ca6Al2(SO4)3(OH)12·26H2O). The basic idea is that the pH of the water is raised to approximately 12 with Ca(OH)2. After, aluminium salt is added, leading to the precipitation of ettringite. Lab-scale batch and continuous experiment results with real semiconductor wastewater demonstrated that 1.5 and 1 of stoichiometric quantities for Ca2+ and A3+ with pH above 12.7 could be considered as the optimal operation condition with 15% of sludge recycle to the influent. A mixed AlCl3 + Fe reagent was selected as the beneficial Al3+ source in ettringite process, which resulted in 80% of sludge volume reduction and improved sludge dewaterability. The results of continuous experiment showed that with precipitation as ettringite, sulfate concentration can be stably reduced to less than 50 mg/L in effluent from the influent 2,050 ± 175 mg/L on average (1,705 ~ 2,633 mg/L).

METHANOGENIC FERMENTATION OF FAT-CONTAINING WASTEWATER MEDIATED BY IRON

  • Zubair, A.;Ivanov, V.;Kim, In-S.
    • 한국생물공학회:학술대회논문집
    • /
    • 한국생물공학회 2000년도 춘계학술발표대회
    • /
    • pp.109-112
    • /
    • 2000
  • Long chain fatty acids (LCFA) are potential inhibitors of bacteria involved in anaerobic digestion because of their surface activity. Precipitation of long-chain fatty acids with iron can improve the anaerobic degradation due to their precipitation and reducing surface properties. Degradation of stearic acid was improved in the presence of iron (II). The methane production was increased 1.6 times as compared to control. Iron-containing soil was applied for degradation of vegetable oil as model case. The methane production was increased 1.5 times as compared to control. Yield of methane production was 0.09 and 0.06L/g COD in experiment and control respectively. Optimum COD/Fe ratio was found 20 mg/mg. Iron (II) can be produced in the treatment system from iron (III) hydroxide or iron containing minerals.