• 제목/요약/키워드: powder coating material

검색결과 185건 처리시간 0.024초

철강재료위 coating된 PTFE 막층의 미끄럼 마찰마모특성 연구 (A Study of Sliding Friction and Wear Properties for PTFE Layer coated on Steel)

  • 이한영
    • Tribology and Lubricants
    • /
    • 제24권2호
    • /
    • pp.96-103
    • /
    • 2008
  • PTFE is generally utilized as the form of composites with adding various fillers. The purpose of this paper lies on clarifying the friction and wear properties of the PTFE coating layer on steel. Especially, the effects of PTFE powder size for coating and surface roughness of the counter material on the properties are investigated. Sliding friction and wear tests are conducted at several sliding speeds by employing two types of PTFE coating layer using different powder sizes. One type of coating layer is composed of uniform fine powder, whereas the other type is made up of mixture powder of different sizes. As results, it is found that PTFE coating layer are effective to improve the wear resistance and to reduce the friction coefficient. It is clear that PTFE coating layers are abrasively removed by asperities of the counter material during sliding contact. However, PTFE coating layer with uniform fine powder shows somewhat better wear resistance than that with mixture powder of different sizes in low sliding speed region. It can be seen that the wear of the coating layer are drastically reduced because wear fragment from counter material are transferred to the coating layer. On the other hand, friction coefficient is shown not to be directly related with PTFE powder size in coating layer.

Kinetic spray 공정을 이용한 Cu repair 코팅 소재 제조 및 열처리에 따른 미세조직과 물성 변화 (Manufacturing of Cu Repair Coating Material Using the Kinetic Spray Process and Changes in the Microstructures and Properties by Heat Treatment)

  • 전민광;김형준;이기안
    • 한국분말재료학회지
    • /
    • 제21권5호
    • /
    • pp.349-354
    • /
    • 2014
  • This study is a basic research for repair material production which manufactured a Cu repair coating layer on the base material of a Cu plate using kinetic spray process. Furthermore, the manufactured material underwent an annealing heat treatment, and the changes of microstructure and macroscopic properties in the Cu repair coating layer and base material were examined. The powder feedstocks were sphere-shaped pure Cu powders with an average size of $27.7{\mu}m$. The produced repair coating material featured $600{\mu}m$ thickness and 0.8% porosity, and it had an identical ${\alpha}$-Cu single phase as the early powder. The produced Cu repair coating material and base material displayed extremely high adhesion characteristics that produced a boundary difficult to identify. Composition analysis confirmed that the impurities in the base material and repair coating material had no significant differences. Microstructure observation after a $500^{\circ}C/1hr$. heat treatment (vacuum condition) identified recovery, recrystallization and grain growth in the repair coating material and featured a more homogeneous microstructure. The hardness difference (${\Delta}H_v$) between the repair coating material and base material significantly reduced from 87 to 34 after undergoing heat treatment.

Kinetic Spray 공정을 이용한 벌크형 탄탈륨 소재의 제조 및 미세조직/물성 (Fabrication and Microstructure/Properties of Bulk-type Tantalum Material by a Kinetic Spray Process)

  • 이지혜;김지원;이기안
    • 한국분말재료학회지
    • /
    • 제23권1호
    • /
    • pp.8-14
    • /
    • 2016
  • A bulk-type Ta material is fabricated using the kinetic spray process and its microstructure and physical properties are investigated. Ta powder with an angular size in the range $9-37{\mu}m$ (purity 99.95%) is sprayed on a Cu plate to form a coating layer. As a result, ~7 mm-sized bulk-type high-density material capable of being used as a sputter material is fabricated. In order to assess the physical properties of the thick coating layer at different locations, the coating material is observed at three different locations (surface, center, and interface). Furthermore, a vacuum heat treatment is applied to the coating material to reduce the variation of physical properties at different locations of the coating material and improve the density. OM, Vickers hardness test, SEM, XRD, and EBSD are implemented for analyzing the microstructure and physical properties. The fabricated Ta coating material produces porosity of 0.11~0.12%, hardness of 311~327 Hv, and minor variations at different locations. In addition, a decrease in the porosity and hardness is observed at different locations upon heat treatment.

Ni계 합금분말 용사 코팅기술을 적용한 롤 제조기술 연구 (A Study on the Roll Manufacturing Technology Applying Powder Flame Spray Coating Technology of Ni-Based Alloy Powder)

  • 박지웅;김순국;반계범
    • 한국분말재료학회지
    • /
    • 제29권2호
    • /
    • pp.123-131
    • /
    • 2022
  • The purpose of this study is to improve the mechanical properties and develop manufacturing technology through self-soluble alloy powder flame spray coating on the surface of a run-out table roller for hot rolling. The roller surface of the run-out table should maintain high hardness at high temperatures and possess high wear, corrosion, and heat resistances. In addition, sufficient bonding strength between the thermal spray coating layer and base material, which would prevent the peel-off of the coating layer, is also an important factor. In this study, the most suitable powder and process for roll manufacturing technology are determined through the initial selection of commercial alloy powder for roll manufacturing, hardness, component analysis, and bond strength analysis of the powder and thermal spray coating layer according to the powder.

졸 코팅 법을 이용한 BaTiO3 분체의 첨가제 코팅 I - BaTiO3 졸 코팅 공정 연구 (Additive Coating of BaTiO3 Powder using Sol Coating Method I - Development of Coating Process by BaTiO3 Sol)

  • 신효순
    • 한국전기전자재료학회논문지
    • /
    • 제17권9호
    • /
    • pp.953-959
    • /
    • 2004
  • BaTiO$_3$ powder has been applied in so much electronic ceramics. Therefore, as recent, the method to add or coat additive will be needed BaTiO$_3$ powder. As a kind of the method, the coating of BaTiO$_3$ powder was considered. In this study, during BaTiO$_3$ powder was coated by BaTiO$_3$ sol, gelation path was experimented. Standard coating condition was set for homogeneous coating. The phase of the gel was deferent by gelation path. It was confirmed the amorphous gel was made in BaTiO$_3$ phase easily at low temperature. In the amorphous gel, particle growth was shown at 900$^{\circ}C$, because crystallization temperature was low. The optimal ratio of sol and powder was at 10 vol% for the homogeneous coating.

Laser Cladding 공정으로 제조된 Tribaloy T-800 코팅 소재의 미세조직 및 용융 Al 침식 특성 (Microstructure and Liquid Al Erosion Property of Tribaloy T-800 Coating Material Manufactured by Laser Cladding Process)

  • 김경욱;함기수;박순홍;이기안
    • 한국분말재료학회지
    • /
    • 제27권3호
    • /
    • pp.210-218
    • /
    • 2020
  • A T-800 (Co-Mo-Cr) coating material is fabricated using Co-Mo-Cr powder feedstock and laser cladding. The microstructure and melted Al erosion properties of the laser-cladded T-800 coating material are investigated. The Al erosion properties of the HVOF-sprayed MoB-CoCr and bulk T-800 material are also examined and compared with the laser-cladded T-800 coating material. Co and lave phases (Co2MoCr and Co3Mo2Si) are detected in both the laser-cladded T-800 coating and the bulk T-800 materials. However, the sizes of the lave phases are measured as 7.9 ㎛ and 60.6 ㎛ for the laser-cladded and bulk T-800 materials, respectively. After the Al erosion tests, the erosion layer thicknesses of the three materials are measured as 91.50 ㎛ (HVOF MoB-CoCr coating), 204.83 ㎛ (laser cladded T-800), and 226.33 ㎛ (bulk T-800). In the HVOF MoB-CoCr coating material, coarse cracks and delamination of the coating layer are observed. On the other hand, no cracks or local delamination of the coating layer are detected in the laser T-800 material even after the Al erosion test. Based on the above results, the authors discuss the appropriate material and process that could replace conventional bulk T-800 materials used as molten Al pots.

METALLIC COATING PROTECTION ON DIELECTROMAGNETS PREPARED FROM MIXTURE OF HARD MAGNETIC POWDERS

  • Slusarek, Barbara;Wasenczuk, Andrzej
    • 한국자기학회지
    • /
    • 제5권5호
    • /
    • pp.687-689
    • /
    • 1995
  • Our team works on mixture of hard magnetic materials. As hard magnetic material we used mixture of powders: melt-spun ribbon Nd-Fe-B, ferrite and Alnico. Their different mixtures are basic material for dielectromagnets under our investigation. Main disadvantage of dielectromagnets with Nd-Fe-B alloy powder as a component is a low corrosion resistance. Protection against corrosion is covering dielectromagnets with metallic or organic coating film. The coating film protects dielectromagnets from free particles on the surface and low resistance for mechanical stresses too. The surface of dielectromagnets prepared from mixture of powders if formed by metallic particles - powder of Nd-Fe-B and Alnico, particles of oxide - powder of ferrite and particles of resin - bonding materials. Team work on technology of laying the metallic coating on dielectromagnets prepared from mixture of mentioned powders. Papers show the results of initial investigation on metallic coating technology. It shows influence of type and used technology of the metallic coating film on magnetic properties of dielectromagnets.

  • PDF

환경친화형 에폭시계 분체도료의 조성구축 연구 (Study on the Compositional Construction of Epoxy Based Powder Paint)

  • 임홍준;정경호
    • 청정기술
    • /
    • 제12권1호
    • /
    • pp.27-35
    • /
    • 2006
  • 본 실험은 에폭시계 분체도료의 물성에 영향을 미치는 에폭시 수지, 경화제, 충전제 및 안료 의 최적 조성 결정에 대한 연구이다. 본 연구에서 사용된 에폭시계 수지의 경화 시스템은 Diglycidyl ether of bisphenol-A (DGEBA)와 경화제로 dicyan diamide (DICY)를 사용하였다. 코팅 재료의 경화거동과 유변물성은 DSC와 레오메터를 사용하여 조사되었다. 또한 코팅재료의 스틸에 대한 접착력은 lap shear 실험을 이용하여 조사되었다. 연구 결과에 따르면 에폭시계 분체도료의 최적 조성은 에폭시계 수지 기준으로 DICY 6 phr, $CaCO_3$ 20 phr 및 $TiO_2$ 10 phr 이었다.

  • PDF

Ni Coating Characteristics of High K Capacitor Ceramic Powders

  • Park, Jung-Min;Lee, Hee-Young;Kim, Jeong-Joo
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.339-339
    • /
    • 2007
  • Metal coating on ceramic powder has long been attracting interest for various applications such as superconductor where the brittle nature of high temperature ceramic superconductor was complemented by silver coating and metalloceramics where mechanical property improvement was achieved via electroless plating. More recently it has become of great interest in embedded passive device applications since metal coating on ceramic particles may result in the enhancement of the dielectric properties of ceramic-polymer composite capacitors. In our study, nickel ion-containing solution was used for coating commercial capacitor-grade $BaTiO_3$ powder. After filtering process, the powder was dried and heat-treated in 5% forming gas at $900^{\circ}C$. XRD and TEM were utilized for the observation of crystallization behavior and morphology of the particles. It was found that the nickel coating characteristics were strongly dependent on the several parameters and processing variables, such as starting $BaTiO_3$ particle size, nickel source, solution chemistry, coating temperature and time. In this paper, the effects of these variables on the coating characteristics will be presented in some detail.

  • PDF