Indentation Damage of Porous Alumina Ceramice

  • Ha, Jang-Hoon;Lee, Chul-Seung;Kim, Jong-Ho;Kim, Do-Kyung
    • 한국세라믹학회지
    • /
    • 제41권1호
    • /
    • pp.19-23
    • /
    • 2004
  • The Hertzian indentation contact damage behavior of porous alumina with controlled pore shape was investigated by experiments. Porous alumina ceramics containing well-defined pore shape, size and distribution were prepared by incorporation of fugitive spherical starch. Porous alumina with isolated pore structure was prepared with porosity range up to 30%. The indentation stress-strain curves of porous alumina were constructed. Elastic modulus and yield stress can be obtained from the stress-strain relationship. Impulse excitation method for the measurement of elastic modulus was also conducted as well as Hertzian indentation and was confirmed as a useful tool to evaluate the elasticity of highly porous ceramics. Elastic modulus of the inter-connected pore structure is more sensitive to porosity than that of the isolated pore structure. When the specimen had isolated pore structure, higher yield point was obtained than it had inter-connected pore structure. This study proposed that the elastic modiulus of porous ceramics is strongly related to not only porosity, but also the structure of pore.

Si:C Ratio가 다공질 Self-Bonded SiC 세라믹스의 기공율과 곡강도에 미치는 영향 (Effect of Si:C Ratio on Porosity and Flexural Strength of Porous Self-Bonded Silicon Carbide Ceramics)

  • 임광영;김영욱;우상국;한인섭
    • 한국세라믹학회지
    • /
    • 제45권5호
    • /
    • pp.285-289
    • /
    • 2008
  • Porous self-bonded silicon carbide (SiC) ceramics were fabricated at temperatures ranging from 1750 to $1850^{\circ}C$ using SiC, silicon (Si), and carbon (C) powders as starting materials. The effect of the Si:C ratio on porosity and strength was investigated as a function of sintering temperature. It was possible to produce self-bonded SiC ceramics with porosities ranging from 36% to 43%. The porous ceramics showed a maximal porosity when the Si:C ratio was 2:1 regardless of the sintering temperature. In contrast, the maximum strength was obtained when the ratio was 5:1.

Effects of Carbon Fiber on Mechanical Behaviour of Al2O3 Porous Ceramics

  • Basnet, Bijay;Lim, Hyung Mi;Lee, Kee Sung;Kim, Ik Jin
    • 한국세라믹학회지
    • /
    • 제56권5호
    • /
    • pp.513-520
    • /
    • 2019
  • This study reports the improvement of mechanical properties of Al2O3 porous ceramics from colloidal suspension with the addition of carbon fiber by direct foaming. The initial colloidal suspension of Al2O3 was partially hydrophobized by surfactant to stabilize wet foam with the addition of carbon fiber from 2 to 8 wt% as stabilizer. The influence of carbon fiber on the air content, bubble size, pore size and pore distribution in terms of wet foam stability and physical properties of porous ceramics were discussed. The viscosity of the colloidal suspension was increased giving solid like properties with the increased in carbon fiber content. The mechanical properties of the sintered porous samples were investigated by Hertzian indentation test. The results show the wet foam stability of more than 90% corresponds to compressive loading of 156.48 N and elastic modulus of 57.44 MPa of sintered sample with 8 wt% of carbon fiber content.

프릿을 이용한 다공질 SiC 세라믹스의 저온 제조 공정 및 물성 (Low Temperature Processing and Properties of Porous Frit-Bonded SiC Ceramics)

  • 채수호;김영욱;송인혁;김해두;배지수;나상문;김승일
    • 한국세라믹학회지
    • /
    • 제46권5호
    • /
    • pp.488-492
    • /
    • 2009
  • Porous frit-bonded SiC ceramics were successfully prepared at a temperature as low as $800^{\circ}C$ from SiC, frit, and microbeads (glass or polymer). The effects of SiC starting particle size and microbead addition on microstructure, porosity, and flexural strength were investigated. The addition of hollow glass microbead improved the strength of frit-bonded SiC ceramics without the loss of porosity by acting additional binder phase between SiC grains. The 65 ${\mu}m$-sized SiC resulted in lower porosity and higher strength than 50 ${\mu}m$-sized SiC because of higher packing density. Typical flexural strengths of frit-bonded SiC were 23 MPa at 46% porosity and 19 MPa at 49% porosity.

초음파 변환기용 다공질 PZT 세라믹의 압전 및 음향 특성 (Piezoelecttic and Acoustic Properties of Porous PZT Ceramics for Ultrasonic Transducer Aplications)

  • 박정학;주용관;최헌일;사공건
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1995년도 춘계학술대회 논문집
    • /
    • pp.192-195
    • /
    • 1995
  • PZT powders were prepared by the molten salt synthesis method. The porous PZT was prepared from a mixture of PZT an polyvinylacohol(PVA) powders by BURPS(Burnout Plastic Sphere) technique. The piezolectirc and acoustic properties with various PVA wt% were studied, Piezoelectric coefficient d$\sub$33/ of porous PZT ceramics was almost same to that of single phase PZT ceramics, The thickness mode coupling factor k$\sub$t/ was 0.53~0.59 in comparable with the single phase PZT ceramics(k$\sub$t/=0.7)

  • PDF

무가압 분말 충전 성형법을 이용한 알루미나 세라믹스의 제조 (II) 무가압 분말 충전 성형법에 의해 제조된 소결체 특성 관찰 (Preparation of Alumina Ceramics by Pressureless Powder Packing Forming Method (II) Characterization of Sintered Body Fabricated by Pressureless Powder Packing Forming Method)

  • 박정형;성재석
    • 한국세라믹학회지
    • /
    • 제32권1호
    • /
    • pp.113-119
    • /
    • 1995
  • The green body was fabricated by a new forming method, pressureless powder packaing forming method, and the characteristics of sintered specimen were investigated. It was found that alumina ceramics prepared by the present method showed porous structure with narrow pore size distribution, and in case of abrasive powder sintered body, compared with dry-pressed specimen, had the nearly same density. Especially, the specimen prepared with spray-dried granules showed the characteristic that granules were not either deformed or fractured during forming and sintering process. Therefore, it was found that this new forming method was effective method in fabrication of porous ceramics on account of easy control of porosity and pore size and its high thermal stability.

  • PDF

고Alumina질 다공성 세라믹스의 내열충격성 및 내Slag성 (기공크기에 따른) (Thermal Spalling and Resistance to Slag Attack in Porous High Alumina Ceramic (According to Pore Size))

  • 김병훈;나용한
    • 한국세라믹학회지
    • /
    • 제30권9호
    • /
    • pp.747-753
    • /
    • 1993
  • The investigation was carried out to study the behaviors of the pore size and porosity, the mechanical strength, the resistance to thermal spallings and slag attacks according to particle sizes of starting raw materials in porous high Alumina ceramics. This porous ceramics have been used in processing of the clean steel by the blowing of the inert gas. The required properties in the practice are the suitable pores size, the sharp pores distribution for a uniform blowing of the gas, the strong corrosion resistance to slags and molten metals and the resistance to thermal spalling. The optimized properties in porous high alumina ceramics of the specimen No. 3 was found to be the very low slag intrusion and the superior resistance to thermal spalling because of the suitable pore size of 2.5${\mu}{\textrm}{m}$, the porosity of 30% and the high sinterability.

  • PDF

Fabrication of Porous RBSN Ceramics with Aligned Channels by an Ice-Templating Method

  • 김동석;고재웅;김도경
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2012년도 춘계학술발표대회
    • /
    • pp.97.1-97.1
    • /
    • 2012
  • Porous ceramics are widely used for applications such as catalysis supports, gas distributors and filters such as DPF. For these purpose, it is important to have proper porosity controlling pore structure while maintaining mechanical and thermal properties. In this work, we have prepared the porous ceramic structures made of reaction bonded silicon nitride with hierarchical pore structures. Uni-directionally aligned pore channels, which are mostly filled with ${\beta}$-Si3N4 whiskers, were achieved by an ice-templating method. The structures of the pore channels and the walls are controllable by the processing conditions, such as solid concentration, freezing rate of the slurry, and additives. We have investigated and characterized the influences of the conditions on the microstructures and the properties, such as porosity, pore size distribution, lamellar thickness, wavelength, and orientations. The compressive strength test and flow test was performed to determine the structural integrity and air permeability.

  • PDF

SiC Fiber 강화 다공질 반응 소결 탄화규소 Composite의 제조 및 기계적 특성 (Fabrication of SiC Fiber Reinforced Porous Reaction Bonded SiC Composite and Its Mechanical Properties)

  • 한재호;박상환
    • 한국세라믹학회지
    • /
    • 제43권8호
    • /
    • pp.509-514
    • /
    • 2006
  • In this study, chopped Hi-Nicalon SiC fiber Reinforced Porous Reaction Bonded SiC (RBSC) composites and it fabrication process were developed by using Si melt infiltration process. The porosity and average pore size in fabricated chopped SiC fiber reinforced porous RBSC composites were in the range of $30{\sim}40%$ and $40-90{\mu}m$, which mainly determined by the SiC powder size used as starting material and amount of residual Si in porous composites. The maximum flexural strength of chopped SiC fiber reinforced porous RBSC composite was as high as 80 MPa. The delayed fracture behavior was observed in chopped SiC fiber reinforced porous RBSC composites upon 3-point bending strength test.

고분자 복제 템플릿 방법을 이용하여 제조된 다공성 탄화규소의 미세구조 특성 (Characterization of Microstructure on Porous Silicon Carbide Prepared by Polymer Replica Template Method)

  • 이윤주;김수룡;김영희;신동근;원지연;권우택
    • 한국세라믹학회지
    • /
    • 제51권6호
    • /
    • pp.539-543
    • /
    • 2014
  • Foam type porous silicon carbide ceramics were fabricated by a polymer replica method using polyurethane foam, carbon black, phenol resin, and silicon powder as raw materials. The influence of the C/Si mole ratio of the ceramic slurry and heat treatment temperature on the porous silicon carbide microstructure was investigated. To characterize the microstructure of porous silicon carbide ceramics, BET, bulk density, X-ray Powder Diffraction (XRD), and Scanning Electron Microscope (SEM) analyses were employed. The results revealed that the surface area of the porous silicon carbide ceramics decreases with increased heat treatment temperature and carbon content at the $2^{nd}$ heat treatment stage. The addition of carbon to the ceramic slurry, which was composed of phenol resin and silicon powder, enhanced the direct carbonization reaction of silicon. This is ascribed to a consequent decrease of the wetting angles of carbon to silicon with increasing heat treatment temperature.