• Title/Summary/Keyword: pores structure

Search Result 516, Processing Time 0.031 seconds

Fabrication and Performance Investigation of Surface Temperature Sensor Using Fluorescent Nanoporous Thin Film I (형광 나노 포러스 박막을 이용한 표면 온도 센서의 제작 및 성능 연구 I)

  • Kim, Hyun Jung;Yoo, Jaisuk;Park, Jinil
    • Korean Journal of Air-Conditioning and Refrigeration Engineering
    • /
    • v.25 no.12
    • /
    • pp.668-673
    • /
    • 2013
  • In this study, specimens with nano-sized porous thin films were manufactured by injecting fluorescence solution into the pores. We intended to find out the difference of the fluorescence intensity in each region of the specimen through an experimental apparatus that makes a temperature field. Before conducting experiments, the optimized manufacturing conditions were determined by analysis of all parameters that influence the emission intensity, and the experiments were carried out with the specimens produced in the optimized conditions. Then, the calibration curves of the fluorescence intensity versus temperature were performed by taking the intensity distributions from the specimen in various temperature fields. The surfaces of specimens were coated with Rhodamine-B (Rh-B) fluorescent dye and measured based on the fluorescence intensity. Silica (SiO2) nanoporous structure with 1-um thickness was constructed on a cover glass, and fluorescence dye was absorbed into these porous thin films.

Resonance and Response of the Submerged Dual Buoy/Porous-Membrane Breakwaters in Oblique Seas

  • Kee, S.T.
    • Journal of Ocean Engineering and Technology
    • /
    • v.15 no.2
    • /
    • pp.22-32
    • /
    • 2001
  • The numerical investigation of obliquely incident wave interactions with fully submerged dual buoy/porous-membrane floating breakwaters placed in parallel with spacing is studied based on linear potential theory and Darcy's law. The numerical solutions are obtained by using a discrete-membrane dynamic model and second-kind modified Bessel function distribution over the entire boundaries of fluid regions. First, numerical solutions for an idealized dual submerged system without buoys are obtained. Second, a more practical dual submerged system with membrane tension provided by buoys at its tops is investigated by the multi-domain boundary element method particularly devised for dual buoy/porous-membrane problems with gaps. The velocity potentials of wave motion are coupled with porous-membrane deformation, and solved simultaneously since the boundary condition on porous-membrane is not known in advance. The effects of varying permeability on membranes and wave characteristics are discussed for the optimum design parameters of systems previously studied. The inclusion of permeability on membrane eliminates the resonances that aggravate the breakwater performance. The system is highly efficient when waves generated by the buoys and membranes were mutually canceled and its energy at resonance frequency dissipates through fine pores on membranes.

  • PDF

Development of Supercapacitors Using Porous Carbon Materials Synthesized from Plant Derived Precursors

  • Khairnar, Vilas;Jaybhaye, Sandesh;Hu, Chi-Chang;Afre, Rakesh;Soga, Tetsu;Sharon, Madhuri;Sharon, Maheshwar
    • Carbon letters
    • /
    • v.9 no.3
    • /
    • pp.188-194
    • /
    • 2008
  • Porous carbon materials synthesized from various plant derived precursors i.e. seeds of [Castor (Ricinus communis), Soap nut (Sapindus sp.), Cashew-nut (Semecarpus anacardium), Jack fruit (Artocarpus heterophyllus), Safflower (Carthamus tinctorius), Ambadi (Crotolaria juncea), Neem (Azadirachta indica), Bitter Almond (Prunus amygdalus), Sesamum (Sisamum indicum), Date-palm (Phoenix dactylifera),Canola (Brassica napus), Sunflower (Helianthus annulus)] and fibrous materials from [Corn stem- (Zea mays), Rice straw (Oryza sativa), Bamboo (Bombax bambusa) and Coconut fibers (Cocos nucifera)] were screened to make supercapacitor in 5M KOH solution. Carbon material obtained from Jack fruit seeds (92.0 F/g), Rice straw (83.0 F/g), Soap nut seeds (54.0 F/g), Castor seeds (44.34 F/g) and Bamboo (40.0 F/g) gave high capacitance value as compared to others. The magnitude of capacitance value was found to be inversely proportional to the scan rate of measurement. It is suggested that carbon material should possess large surface area and small pore size to get better value of capacitor. Moreover, the structure of carbon materials should be such that majority of pores are in the plane parallel to the plane of electrode and surface is fluffy like cotton ball.

Formation of YSZ Coatings Deposited by Suspension Vacuum Plasma Spraying (서스펜션 진공 플라즈마 용사법을 통한 YSZ 코팅의 형성)

  • Yoo, Yeon Woo;Byon, Eungsun
    • Journal of the Korean institute of surface engineering
    • /
    • v.50 no.6
    • /
    • pp.460-464
    • /
    • 2017
  • As increasing thermal efficiency of the gas turbine, the performance improvement of thermal barrier coatings is also becoming important. Ytrria stabilized zirconia(YSZ) is the most popular materials for ceramic top coating because of its low thermal conductivity. In order to enhance the performance of thermal barrier coatings for hot sections in the gas turbine, suspension plasma spraying was developed in order to feed nano-sized powders. YSZ coatings formed by suspension plasma spraying showed better performance than YSZ coatings due to its exclusive microstructure. In this research, two YSZ coatings were deposited by suspension vacuum plasma spraying at 400 mbar and 250 mbar. Microstructures of YSZ coatings were analyzed by scanning electron image(SEM) on each spraying conditions, respectively. Crystalline structure transformation was not detected by X-ray diffraction. Thermal conductivity of suspension vacuum plasma sprayed YSZ coatings were measured by laser flash analysis. Thermal conductivity of suspension vacuum plasma sprayed YSZ coatings containing horizontally oriented nano-sized pores and vertical cracks showed $0.6-1.0W/m{\cdot}K$, similar to thermal conductivity of YSZ coatings formed by atmospheric plasma spraying.

Plasma-Sprayed $Al_{2}O_{3}-SiO_{2}$ Multi-Oxide Films on Stainless Steel Substrate

  • Korobova, N.;Soh, Deawha
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.11a
    • /
    • pp.116-119
    • /
    • 2000
  • The advantage of plasma-sprayed coating is their good resistance against thermal shock due to the porous state of the coated layer with a consequently low Youngs modules. However, the existence of many pores with a bimodal distribution and a laminar structure in the coating reduces coating strength and oxidation protection of the base metals. In order to counteract these problems, there have been many efforts to obtain dense coatings by spraying under low pressure or vacuum and by controlling particle size and morphology of the spraying materials. The aim of the present study is to survey the effects of the HIP treatment between 1100 and 130$0^{\circ}C$ on plasma-sprayed oxide coating of A1$_2$O$_3$, A1$_2$O$_3$-SiO$_2$ on the metal substrate (type C18N10T stainless steel). These effects were characterized by phase identification, Vickers hardness measurement, and tensile test before and after HIPing, These results show that high-pressure treatment has an advantage for improving adhesive strength and Vickers hardness of plasma- sprayed coatings.

  • PDF

Synthesis and Characteristics of W-Ni-Fe Nanocomposite Powder by Hydrogen Reduction of Oxides (산화물 수소환원에 의한 W-Ni-Fe 나노복합분말의 합성과 특성)

  • 이창우;윤의식;이재성
    • Journal of Powder Materials
    • /
    • v.8 no.1
    • /
    • pp.49-54
    • /
    • 2001
  • The synthesis and characteristics of W-Ni-Fe nanocomposite powder by hydrogen reduction of ball milled W-Ni-Fe oxide mixture were investigated. The ball milled oxide mixture was prepared by high energy attrition milling of W blue powder, NiO and $Fe_2O_3$ for 1 h. The structure of the oxide mixture was characteristic of nano porous agglomerate composite powder consisting of nanoscale particles and pores which act as effective removal path of water vapor during hydrogen reduction process. The reduction experiment showed that the reduction reaction starts from NiO, followed by $Fe_2O_3$ and finally W oxide. It was also found that during the reduction process rapid alloying of Ni-Fe yielded the formation of $\gamma$-Ni-Fe. After reduction at 80$0^{\circ}C$ for 1 h, the nano-composite powder of W-4.57Ni-2.34Fe comprising W and $\gamma$-Ni-Fe phases was produced, of which grain size was35nm for W and 87 nm for $\gamma$-Ni-Fe, respectively. Sinterability of the W heavy alloy nanopowder showing full density and sound microstructure under the condition of 147$0^{\circ}C$/20 min is thought to be suitable for raw material for powder injection molding of tungsten heavy alloy.

  • PDF

Ball Milling and Sintering Behavior of High Speed Steel Powders Containing VC and Co (VC 및 Co함유 고속도공구강 분말의 볼밀링 및 소결거동)

  • 김용진
    • Journal of Powder Materials
    • /
    • v.3 no.3
    • /
    • pp.181-187
    • /
    • 1996
  • Cobalt and VC powders were ball milled with M2 grade high speed steel powders under various ball to powder ratios. The powders milled under higher ball to powder ratio become finer, more irregular and have a broader size distribution, and thus possess a lower compressibility and a better sinterability regarding densification. Increasing the ball to powder ratio lowered the sintering temperature to obtain the density level necessary to isolate all the pores. Lowering the sintering temperature is very critical to maintain fine microstructure since grain and carbide coarsening are accelerated by higher sintering temperature due to more liquid phase formation. The powders obtained by ball milling at 20 to 1 ratio has the lowest compressibility but has the best sinterability, almost compatible to unmilled pure M2 powders. A sintered body over 97% theoretical density with fine microstructures having average grain size of ~10 microns was obtained from the powder by sintering at 1260 $^{\circ}C$ for 1 hour in vacuum. XRD results indicate that two types of carbides are mainly present in the sintered structure, MC and $M_{6}C$ type. The MC type carbides are more or less round shaped and mainly located at the grain boundaries whereas the $M_{6}C$ type are angular shaped and mainly located inside the grains.

  • PDF

Structural and Dielectric Properties of BST-MgO with $B_2O_3-Li_2CO_3$ Thick Films ($B_2O_3-Li_2CO_3$가 첨가된 BST-MgO 후막의 구조 및 유전 특성)

  • Kang, Won-Seok;Kim, Jae-Sik;Koh, Jung-Hyuk;Lee, Young-Hie
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.19-20
    • /
    • 2007
  • At first the $Ba_{0.5}Sr_{0.5}TiO_3$-MgO powder with $B_2O_3-Li_2CO_3$ were made by the Sol-Gel method. The thick films of BST-MgO with $B_2O_3-Li_2CO_3$ were fabricated on the $Al_2O_3$ substrates coated with Pt by the screen printing method. The structural and dielectric properties of the BST-MgO thick film with $B_2O_3-Li_2CO_3$, addition were investigated. The structure of the BST-MgO with $B_2O_3-Li_2CO_3$ thick films were dense and homogeneous with no pores. The dielectric constant was increased and dielectric loss was decreased with increasing the sintering temperature.

  • PDF

Structural and Dielectirc Properties of BST-MgO with $B_{2}O_{3}-Li_{2}CO_{3}$ Thick Films ($B_{2}O_{3}-Li_{2}CO_{3}$의 첨가량에 따른 BST-MgO 후막의 구조 및 유전 특성)

  • Kang, Won-Seok;Koh, Jung-Hyuk;Nam, Song-Min;Lee, Young-Hie
    • Proceedings of the KIEE Conference
    • /
    • 2007.07a
    • /
    • pp.1261-1262
    • /
    • 2007
  • At first the $Ba_{0.5}Sr_{0.5}TiO_{3}$-MgO powder with $B_{2}O_{3}-Li_{2}CO_{3}$ were made by the Sol-Gel method. And then the thick films of BST-MgO with $B_{2}O_{3}-Li_{2}CO_{3}$ were fabricated on the $Al_{2}O_{3}$ substrates coated with Pt by the screen printing method. The structural and dielectric properties of the BST-MgO thick film with $B_{2}O_{3}-Li_{2}CO_{3}$ addition were investigated. The structure of the BST-MgO with $B_{2}O_{3}-Li_{2}CO_{3}$ thick films were dense and homogeneous with no pores. The dielectric constant and dielectric loss were increased with decreasing the $B_{2}O_{3}-Li_{2}CO_{3}$ addition ratio.

  • PDF

Surface Treatments of Titanium Biomaterials by Anodization (양극산화법에 의한 생체적합형 티타늄 표면 개질)

  • Mun, Kyu-Shik;Kim, Jae-Yeon;Kim, Dong-Hyun;Cheon, Se-Jun;Kim, Hyo-Eun;Lee, Myoung-Hoon;Choi, Won-Youl
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.11a
    • /
    • pp.306-306
    • /
    • 2007
  • The surface was transformed to porous titanium oxide by the anodization of pure titanium. Titanium was anodized in non-aqueous and aqueous electrolytes at different potentials between 5 V and 150 V. Various electrolytes were compose of ethylene glycerol, $H_2SO_4,\;NH_4F\;and\;H_2O$. We obtained titania nanotube arrays on the micro pore of titanium. Micro pores and nano tubes were obtained by anodization at high potentials and low potentials, respectively. Morphologies of nanotubes and micro pore were characterized by FE-SEM. The unique surface structure is very attractive to electrical and medical applications such as gas sensor, biosensor, dental implant and stent.