A study on the Synthesis end Properties of Polyurethane Resin Based on PPG as a Glycol (폴리프로필렌글리콜을 글리콜 성분으로 하는 폴리우레탄 수지의 합성 및 물성에 관한 연구)

  • Yoo, Kil-Sang;Choi, Sang-Goo
    • Elastomers and Composites
    • /
    • v.35 no.3
    • /
    • pp.205-214
    • /
    • 2000
  • The polyurethane resin was prepared by the reaction of tolylenediisocyanate(TDI) and polypropyleneglycol(PPG). Physical properties of the resin were investigated experimentally. Charging catalyst before TDI-dropping induced the rapid increase of viscosity. On the other hand, charging catalyst after TDI-dropping resulted in mild stability without immoderate generation of heat on reaction. The use of phosphoric acid as catalyst led to low viscosity by restraining side-reaction such as forming of branch-chain, buret reaction and allopanate reaction, but it showed low cross-link density and slow drying. The curing speed was more influenced by structures of molecules rather than NCO/OH ratio. Including PPG 400 over 30 wt % showed excellent adhesive strength due to increase of crosslink density.

  • PDF

Analysis of Properties of Water-Dispersed Bio-Polyurethane Based on Caster Oil for Lamb Leather Surface (Lamb Leather용 Caster Oil 기반 수분산 바이오 폴리우레탄필름의 제조)

  • Lee, Joo-Youb
    • Journal of the Korean Applied Science and Technology
    • /
    • v.39 no.2
    • /
    • pp.161-168
    • /
    • 2022
  • Unmodified castor oil (CO) was used to obtain a castor-based aqueous polyurethane (CPUD) and isophorone diisocyanate (IPDI) was used to obtain a transparent film. The mixing effect of polypropyleneglycole (PPG) was analyzed to increase flexibility. In addition, ethylenediamine (EDA) was used as a chain extender. Tensile strength, elongation, and abrasion resistance were measured according to the change according to the castor oil content and the change in the chain extender, respectively. The tensile strength of the sample containing a lot of castor oil was 1.112 kgf/㎟, and the elongation was 88%. The tensile strength of the sample containing a lot of chain extender was 3.33kgf/㎟, and the elongation was 99%. The surface strength was visually confirmed through SEM. The surface strength was visually confirmed through SEM.