용접강관의 황화수소 응력부식균열에 관한 연구 (A Study of Sulfide Stress Corrosion Cracking in Welded Steel Pipe)

  • 박영록;김희진;강봉용
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2003년도 춘계학술발표대회 개요집
    • /
    • pp.257-259
    • /
    • 2003
  • Sulfide Stress Corrosion Cracking(SSCC) of welded Steel pipe has been investigated. A specimens are stressed into the synthetic sea water saturated with H$_2$S. Therefore SSCC occur at the hardnest point. we are discusses the test methods used for laboratory corrosion testing of welded steel pipe and the results of test.

  • PDF

GTAW-SMAW와 SAW를 이용한 고장력강관의 용접에 대한 연구 (A Study on the Welding Process of High Strength Steel Pipe in GTAW-SMAW and SAW)

  • 이철구;조선근
    • Journal of Welding and Joining
    • /
    • 제12권4호
    • /
    • pp.41-49
    • /
    • 1994
  • This study is to compare the welding quality of API 5L-X65 Steel- pipe's for natural gas transmission piping applied by SAW at shop and by GTAW-SMAW at site. The results can be summarized as follows; 1) Tensile strength of the welded zone by SAW(611.5 MPa) and by GTAW-SMAW(608.6 MPa) was maintained greater than that of the base metal(583.5 MPa). 2) Hardness of the welded zone and HAZ by SAW(Hv 194.8) & GTAW-SMAW (Hv 196.1) was slightly increased above that of the base metal (Hv 168.8), but less than the maximum allowable hardness(Hv 248). 3) Impact value of the welded zone by SAW(126.8 J) & GTAW-SMAW(88 J) became lower than that of the base metal(282.5 J), but was above the requirement of API 5L(68J). 4) Microscopic structure of the welded zone and HAZ by both SAW & GTAW-SMAW became fine-grained.

  • PDF

원전용 안전등급 밸브의 용접부 누설 클램핑 현장보수 기술 검토 (Preliminary Review of On-Site Clamping Repair Technology for Welding Part Leakage of Safety Related Valve in the Nuclear Power Plant)

  • 김기홍;김기수;정환석;장무경
    • 한국압력기기공학회 논문집
    • /
    • 제19권1호
    • /
    • pp.52-59
    • /
    • 2023
  • The welding part of the valve needs immediate action when leakage occurs due to cracks or damage. In order to repair leakage of the welding part, the valve must be separated from the pipe or replaced with a new valve. However, it is difficult to remove the valve while operating the power plant. This study presents a method to remove leakage by precisely processing the gap between the clamp and the incision part within 0.1mm while installed in the pipe system. If the external leakage is removed using a clamp on the welding part without removing the valve during operation, the time and cost required for maintenance can be reduced.

오비탈 용접법을 적용한 STS 316L 파이프 소재의 용접부 특성에 관한 연구 (A Study on the Welds Characteristics of Stainless Steel 316L Pipe using Orbital Welding Process)

  • 이병우;조상명
    • 동력기계공학회지
    • /
    • 제14권2호
    • /
    • pp.71-77
    • /
    • 2010
  • This paper was studied on microstructure, mechanical properties and corrosion characteristics of 316L stainless steel pipe welds was fabricated by orbital welding process. S-Ar specimen was fabricated by using Ar purge gas and S-$N_2$ specimen was fabricated by using $N_2$ purge gas. Ferrite was not detected in weld metal of S-$N_2$ specimen but the order of 0.13 Ferrite number(FN) was detected in weld metal of S-Ar specimen. Oxygen and Nitrogen concentration of S-$N_2$ specimen was higher than S-Ar specimen on HAZ and inner bead. The welds microstructural characteristics of S-Ar and S-$N_2$ specimens are similar. The microvickers hardness values of S-Ar and S-$N_2$ specimens welds were similar and average values of each regions were in the range of 174~194. The microstructures of S-Ar and S-$N_2$ weld metal were full austenite by primary austenite solidification. The Solidification structures of S-Ar and S-$N_2$ weld metal were formed directional dendrite toward bead center. The potentiodynamic polarization curve of STS 316L pipe welds exhibited typical active, passive, transpassive behaviour. Corrosion current density$(I_{corr.})$ and corrosion rate values of S-Ar specimen in 0.1M HCl solution were $0.95{\mu}A/cm^2$ and $0.31{\mu}A$/year respectively. The values of S-$N_2$ specimen were $1.4{\mu}A/cm^2$ and $0.45{\mu}m$/year.

GMA 용접공정을 이용한 오픈갭 수평고정관 초층 용접의 실험적 연구 (An Experimental Study on Root-pass Welding of Open Gap by GMA Welding Process in Pipeline)

  • 김지선;김일수;박창언;나현호;이지혜;정성명
    • Journal of Welding and Joining
    • /
    • 제29권3호
    • /
    • pp.64-69
    • /
    • 2011
  • Since welding process for most pipelines with large diameter has been carried out by the manual process, automation of the welding process is necessary for the sake of consistent weld quality and improvement in productivity. Therefore the development of the optimized algorithm to decide the welding condition is an effective technique to prove the feasibility of interface standards and intelligent control technology to increase productivity and reduce the cost of system integration. In this study, the pipe welding experiment has been carried out using plused GMA welding process to select optimal welding condition. And necessary information in root-pass welding has been obtained by applying in the pipeline using the selected welding conditions through the welding experiment.