Synthesis of Modified Silane Acrylic Resins and Their Physical Properties as Weather-Resistant Coatings

  • Yoo, Gyu-Yeol;Kim, Ji-Hyun;Park, Hong-Soo;Kim, Young-Geun;Kim, Seong-Kil
    • Journal of the Korean Applied Science and Technology
    • /
    • v.25 no.1
    • /
    • pp.1-14
    • /
    • 2008
  • To prepare weather-resistant modified silane acrylic resin coatings for an architectural purpose, tetrapolymers were synthesized by radical polymerization. 3-Methacryloxypropyltrimethoxysilane (MPTS) as a silicone monomer and n-butyl acrylate, methyl methacrylate, and n-butyl methacrylate as acrylic monomers were used. The composition of monomers was adjusted to fix the glass transition temperature of acrylic polymer for $20^{\circ}C$. The composition of MPTS in the synthesized polymer were varied from 10 wt% to 30 wt%. On the basis of synthesized resin amber paints were prepared and their physical properties and effects on weatherability were examined. The presence of MPTS in modified silane acrylic resins generally resulted in low molecular weight and broad molecular weight distribution, and also lowered the viscosity of the copolymers. The coated films prepared from these resins showed good and balanced properties in general. Adhesion to the substrate was outstanding in particular. Weatherability tests were carried out in three different types such as outdoor exposure, QUV, and SWO. The test results showed that the modified silane acrylic resins containing 30 wt% of MPTS had superior weathering properties.

The characters of lichens attached to the stonework cultural assets and removing methods of them (석조문화재에 부착하는 지의류의 특성과 그 제거방법)

  • Moon Kwang-Hee
    • 한국문화재보존과학회:학술대회논문집
    • /
    • 2005.11a
    • /
    • pp.100-103
    • /
    • 2005
  • Lichens play an important role in breaking down rocks physically and chemically. Physical weathering occurs mechanically through hyphae and rhizines growing into the rocks. Lichen substances such as oxalic acid, acidic polysaccharides and depsides may assist altering rocks chemically. These actions partly contribute to soil formation but prove harmful for the substratum. Some people do not like to keep lichens on stained glassof churches or on gravestones mainly because of its unglamorous appearance. A biocide, 'Koretrel', is very effective in removing lichens and blue-green algae from the surface of concrete. After spraying 'Koretrel' in the open air, lichens (Caloplaca sp., Endocarpon petrolepideum, Physciella melanchra, Phaeophyscia hispidula, etc.) growing on buildings died within three months and peeled off fromthe substratum. One year after treatment, concrete surfaces were almost lichen free for three or four years. The biocide makesuse of a kind of lichen substance and harmless both for substances and environment. Our recent experiments show that it is also useful for water grasses growing on the surface of an aqueduct of a hydroelectric power station.

  • PDF

암반공학적 측면에서본 신생대 암반비탈면의 공학적 문제 및 대책

  • Shin, Hee-Soon
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2005.10a
    • /
    • pp.285-289
    • /
    • 2005
  • The Cenozoic Era consists of two period , the Tertiary and the Quaternary Period. Weak rock types may include areas containing: 1) poorly cemented or uncemented sediments, 2) highly weathered rock, or 3) fault lines. Especially this paper deal with poorly cemented or uncemented sedimentary rocks in slope. Mechanical weathering is caused by physical processes such as absorption and release of water, and changes in temperature and stress at or near the exposed rock surface. It results in the opening of discontinuities, the formation of new discontinuities by rock fracture, the opening of grain boundaries, and the fracture or cleavage of individual mineral grains. Decomposition causes some silicate minerals such as feldspars to change to clay minerals. There was a strong negative correlation between water absorption and important engineering properties such as strength and durability.

  • PDF

Synthesis and Properties of Photocurable Dimethylol Propionic Acid modified Hyperbranched Acrylates (광경화형 Dimethylol Propionic Acid 변성 하이퍼브랜치 아크릴레이트의 합성과 물성)

  • Kim, Dong Kook;Lim, Jin Kyu;Kim, Woo Geun
    • Applied Chemistry for Engineering
    • /
    • v.16 no.3
    • /
    • pp.342-347
    • /
    • 2005
  • Photocurable hyperbranched acrylates were prepared from acrylic acid and hyperbranched polyol (HBP-16, 32, 64). Physical properties of three kinds of photocurable hyperbranched acrylated were investigated. Thermal stability of UV cured film measured by TGA shifted to higher temperature with increasing of functionality. Hardness, abrasion resistance, and tensile strength of UV cured film also increased with increasing functionality of acrylate. Weathering test for UV cured film showed the value of yellow index increased with increasing functionality of acrylate.

Geotechnical characteristics of the collapsed $\bigcirc\bigcirc$tunnel slope in Yeosu-Suncheon area (여수-순천 도로확장공사 구간 $\bigcirc\bigcirc$터널 붕괴사면 지반특성)

  • Kim, Seung-Hyun;Koo, Ho-Bon;Lee, Jeong-Yup;Rhee, Jong-Hyun;Kim, Seung-Hee
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2008.03a
    • /
    • pp.848-857
    • /
    • 2008
  • In September 2007, the collapses of slopes and landslides are happened at Jeonlanamdo due to heavy rains accompanied with Typoon "Nari". The study area is the tunnel portal slope in new road construction site. This slope consists of pyroclastic rocks and has lots of faults. Particularly, the residual soils of the slope is deteriorated with yellowish mudstone layer as a results of chemical and physical weathering. This has a variety of swelling clay minerals and might be moved easily down at the gentle terrain. The inner factor of $\bigcirc\bigcirc$tunnel portal slope's collapse is the geological weak zone, the convergent topography, the inferiority of drainage and the heavy rain act on the failure as direct trigger.

  • PDF

The Case Study of Cut-Slope Stability in Pyroclastic-Rock Area (화산쇄설암 분포지역 내 절토사면 안정성 사례연구)

  • Lee, Jeong-Yeob;Koo, Ho-Bon;Kim, Seung-Hyun
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2008.03a
    • /
    • pp.884-893
    • /
    • 2008
  • The purpose of this case study is cut-slope stability in pyroclastic-rock area. Pyroclastic-rock is very vulerable by Chemical and physical weathering. And risk increase of Pyroclastic-rock proportional to exposure time. This case of cut-slope located in Jeollabuk-do Jinan-gun and reserch order is topography character research, geological character research, field survey, measure method presentation.

  • PDF

Influence of the Soluble Salt on the Exfoliation of the Stone Monument (수용성염이 석조문화재 표면 박리현상에 미치는 영향)

  • Do, Jin-Young;Lim, Kwon-Woong
    • Journal of Conservation Science
    • /
    • v.22
    • /
    • pp.121-134
    • /
    • 2008
  • The mechanism of stone exfoliation and its cause in relation to chemical weathering by soluble salt were studied. Chemical, mineralogical and physical analysis was performed in exfoliation samples from stone monuments. The representative salt is gypsum in the exfoliation samples. In order to understand the salt reaction, stone samples(tuff and granite) were treated with two type of the salt, gypsum and sodium sulfate, which have different solubility. The capillary water uptakes are slight increased in impregnated with Na2SO4 and weathering simulation of two rock types. It means that the rock is deteriorated in the near of the surface by $Na_2SO_4$. $CaSO_4{\cdot}2H_2O$ bring out the thicker exfoliation than $Na_2SO_4$ because it is penetrated into the deeper zone and amount of accumulated salt is more abundant in the inner part than in the near of the surface. The exfoliation was formed in the tuff by salt treatment and 30cycle of weathering simulation, but there are not significant symptoms of exfoliation in the granite by same condition. This result was caused by the different capillary water uptakes and porosity of the rocks. In the tuff, salt solutions are penetrated into the inner part due to its high capillary water uptakes and porosity but the granite, which has low value relatively, can be formed thinner exfoliation.

  • PDF

Petrological Characteristics and Deterioration State of Standing Buddha Statue in the Gwanchoksa Temple, Nonsan, Korea (논산 관촉사 석조미륵보살입상의 암석학적 특성과 풍화훼손도)

  • Yun, Seok-Bong;Kaug, Yean-Chun;Park, Sung-Mi;Yi, Jeong-Eun;Lee, Chan-Hee;Choi, Seok-Won
    • Economic and Environmental Geology
    • /
    • v.39 no.6 s.181
    • /
    • pp.629-641
    • /
    • 2006
  • The Standing Buddha Statue in the Gwanchoksa temple consists of medium to coarse grained biotite granodiorite with dark grey color, and it has a week gneissosity along the pegmatite veins. The results of magnetic susceptibility and geochemical patterns of the host rock of Standing Buddha Statue and the basement rock suggest that both values are formed from the co-genetic magma with the same differentiation process. The CIAs of the basement rock and the Standing Buddha Statue are calculated to 51.43 and 50.86, and the WPIs are estimated 4.52 and 8.95, respectively. So the weathering potential from the host rock of Standing Buddha Statue and basement rock prove to be high. The Standing Buddha Statue is terribly damaged with physical weathering from deterioration and exfoliation, and are scattered with secondary pollutant and precipitate. Basement rock is also in danger of ground collapse because of irregularly developed discontinuity system. Most surface of Standing Buddha Statue is seriously discolored into yellowish brown and dark gray, or black precipitates are also formed. Moreover, it is heavily covered with crustose lichen, fungi and algae, or moss are also found. In order to control the influential factors with the complex deterioration of Standing Buddha Statue, it is needed to rearrange a site environments, and conservation scientific management is required to protect it from covering lichens, exfoliations and fractures.

Species Identification and Weathering of Wooden Striker on the Divine Bell of King Songdok (성덕대왕신종(聖德大王神鍾) 당목(撞木)의 수종(樹種)과 열화(劣化))

  • Kang, Aekyung
    • Conservation Science in Museum
    • /
    • v.4
    • /
    • pp.71-78
    • /
    • 2003
  • The wooden striker on the Divine Bell of King Seongdeok was examined to identify the species of the wood and the outdoor wood weathering caused by solar light, moisture, temperature and air. The species of the wooden striker was identified to Zelkova serrata. When observed the striker with naked eyes, the results were surface discoloration (graying), cracking and roughness. In order to examine the morphological changes according to deterioration type, the specimen were separated to three part(I, II,III-spot). The I-spot was discolored to gray and at the same time entirely covered with dust. So the observation was impossible. The II-spot was also discolored but its texture could be observed. On it could observe numerous fungal hypae and dirts like dust flown into the cell lumens. The cell wall has been so weakened by weathering that it lost the physical intensity. This have made microchecks and splits on the cell wall. Although fungal hypae covered the cell, they did not result in wood decay. The III-spot, located just 0.5 mm below the surface, was maintaining the natural red-brown color of the wood. Its cell wall was similar to that of sound wood. These changes are different from wood decay, and limited only to the surface of the striker-less than or equal to 0.5 mm below.

Deterioration Characteristic Analysis for Stone Properties in the Taereung Royal Tomb of the Joseon Dynasty using Nondestructive Analysis (비파괴 분석을 활용한 조선왕릉 태릉 석조물의 손상특성 분석)

  • Lee, Myeonseong;Choie, Myoungju;Lee, Taejong;Chun, Yungun
    • Korean Journal of Heritage: History & Science
    • /
    • v.53 no.2
    • /
    • pp.222-241
    • /
    • 2020
  • The Taereung Royal Tomb from the Joseon Dynasty is the tomb of Empress Munjeong, the second queen of King Jungjong, and it contains various types of stone artifacts. All of these stone artifacts were constructed using coarse- to medium-grained biotite granite. The major types of deterioration of the stone artifacts are identified as surface weathering and biological contaminants. Exfoliation (145 sculptures), granular decomposition (138 sculptures), and repair materials (156 sculptures), along with biological contaminant algae (154 sculptures), lichen (165 sculptures) and moss (97 sculptures), have a high occurrence frequency. In particular, it is deemed that immediate conservation treatment is required, as biological deterioration (algae) represents the most serious condition (grade 3 or higher in 94% of all stones), and it is thought that exfoliation and granulation decomposition are required for long-term conservation management. As a result of equo -tip hardness and ultrasonic measurement, more than 70% of stones were found to have very weak physical properties. Through hyperspectral analysis, organisms were shown to inhabit more than 80% of the surface of burial mound stone artifacts, and P (phosphorus), S (sulfur), Cl (chlorine), and Ca (calcium) were detected in this area. This is because Taereung Royal Tomb has been exposed to the outdoors for hundreds of years and has been weathered by physical, chemical, and biological factors. Therefore, among the stone artifacts in the Taereung Royal Tomb, those with high physical weathering grades are considered to require consolidation to reinforce them physically. Since organisms are highly likely to cause stone damage, they must be removed via dry and wet cleaning. In addition, in order to delay the reoccurrence of organisms following conservation treatment, it is necessary to regularly clean up the soil that has flowed into the burial mound, and to monitor conservation conditions over the long term.