Many researches have recently discussed about the film thickness as a good substitute or supplement for VMA or other volumetric criteria in the design procedure. Some researchers have not only proposed the specific number for the recommended film thickness, but also introduced the new calculation procedures or concepts. Each model (index model and the virtual model) has its own advantages and disadvantages in terms of the ability to account for the volumetric properties of the mixture. In this paper, the modified virtual model was proposed to combine advantages from both models. However, it cannot be disregarded the way to determine the appropriate particle shape factors for different sources and sizes of aggregates. In order to evaluate the different calculation methods, mixtures with two aggregate sources and eight gradations were designed based on the dominant aggregate size range (DASR) porosity concept. Superpave indirect tensile test (IDT) and asphalt pavement analyzer (AEA) test were used to describe the performance of mixtures. Test results indicated that the virtual model, which is the same to the modified virtual model for sphere 1:1 case, is better than the conventional standard model to define the range of the film thickness to have better performance of asphalt mixtures.
Journal of the Korea Academia-Industrial cooperation Society
/
v.19
no.5
/
pp.146-152
/
2018
In this study, to improve the performance of asphalt mixtures for plastic deformation occurring mainly in Korea, complex modifiers were prepared by mixing powders and liquid type modifiers. The main constituents were powdery diatomaceous earth, mica and carbon black, and liquid type solid 70% SBR latex. The tensile strength ratios for the two asphalt mixtures used in the test were above 0.80 for the Ministry of Land Transportation (2017) asphalt mixture production and construction guidelines. The effects of increasing the tensile strength in the dry state was more than 14% when the composite modifier was added. The deformation rate per minute by the wheel tracking test load was an average of 0.07 to 0.147 for each mixture. The strain rate per minute was improved by the modifier, and the dynamic stability was improved by almost 100% from 295 to 590. In addition, the final settling was reduced from 11.38 mm to 9.57 mm. A plastic deformation test using the triaxial compression test showed that the amount of deformation entering the plastic deformation failure zone at the end of the second stage section and in the third stage plastic deformation section was 1.76 mm for the conventional mixture and 1.50 mm for the complex modifier mixture. The average slope of the complex modifier asphalt mixture mixed with the multi-functional modifier was 0.005 mm/sec. The plastic deformation rate is relatively small in the section where the road pavement exhibits stable common performance, i.e. the traffic load.
Journal of the Korea Academia-Industrial cooperation Society
/
v.19
no.5
/
pp.54-63
/
2018
In this study, the stability and economic feasibility of a MSE (Mechanically stability earth) wall with a pre-cast concrete pacing panel was investigated for a standard section of highway. Based on the design criteria, the MSE walls of the panel type were designed considering the load conditions of the highway, such as the dead load of the concrete pavement, traffic load, and impact load of the barrier. The length of the ribbed metal strip was arranged at 0.9H according to the height of the MSE walls. Because the length of the reinforcement was set to 0.9H according to the height of the MSE wall, the external stability governed by the shape of the reinforced soil was not affected by the height increase. The factor of safety (FOS) for the bearing capacity was decreased drastically due to the increase in self-weight according to the height of the MSE wall. As a result of examining the internal stability according to the cohesive gravity method, the FOS of pullout was increased and the FOS of fracture was decreased. As the height of the MSEW wall increases, the horizontal earth pressure acting as an active force and the vertical earth pressure acting as a resistance force are increased together, so that the FOS of the pullout is increased. Because the long-term allowable tensile force of the ribbed metal strip is constant, the FOS of the fracture is decreased by only an increase in the horizontal earth pressure according to the height. The panel type MSE wall was more economical than the block type at all heights. Compared to the concrete retaining wall, it has excellent economic efficiency at a height of 5.0 m or more.
Jo, Shin Haeng;Kim, Nak Seok;Kim, Young Jin;Kim, Wan Sang;Lee, Suck Hong
한국방재학회:학술대회논문집
/
2011.02a
/
pp.178-178
/
2011
도로소음은 다양한 소음원에 의해 발생하며, 도로를 이용하는 사람과 도로 주변사람에게 큰 불편을 초래한다. 보다 쾌적한 환경을 원하는 현대인에게 있어 도로 소음의 경감은 중요한 환경 공해로 작용한다. 도로 소음을 줄이기 위해서는 여러 가지 방법이 있을 수 있으며, 이 중 도로 포장의 개선을 통해 도로 소음을 경감할 수 있으며, 이와 같은 포장을 저소음 포장이라고 한다. 저소음 포장은 주행하는 차량의 타이어와 노면이 마찰하면서 발생하는 소음을 최소화하기 위한 것으로 소음 발생의 메커니즘을 바탕으로 하고 있다. 저소음 포장중 가장 널리 사용되고 있는 방법은 공극을 늘리는 것이다. 약 20%의 공극은 타이어와 노면 사이의 에어펌핑음을 최소화 하며, 소리를 흡수하는 역할로 약 3dB의 소음 가소 효과가 있는 것으로 알려져 있다. 소음을 감소시키는 또 하나의 방법은 노면의 표면 조직을 매끈하게 하여 타이어와 노면의 충격음을 줄이는 방법이다. 노면의 평탄성을 개선하기 위해 포장에 사용되는 골재의 최대크기를 줄이는 소입경 포장을 소음 가소의 목적으로 유럽 등지에서 많이 사용되고 있다. 본 연구에서는 이와 같은 저소음 기능을 위해 공극률을 크게 하고 소입경 골재를 사용하는 소입경 저소음 포장의 현장 적용을 위한 배합 설계를 수행하였다. 소입경 저소음 포장의 최대 골재 크기는 현장 적용성과 경제성을 고려하여 10mm 골재를 사용하였으며, 수도권에서 입수한 4곳의 산지 골재를 분석하여 골재 합성 입도를 산정하였다. 10mm 저소음 포장의 골재 입도 범위는 공극률 15~18%를 목표로 하며, 이를 만족하기 위하여 배합 설계를 수행한 결과 5mm 통과 중량 백분율이 약 30%로 하는 개립도가 적당한 것으로 나타났다. 공극이 증가함에 따라 포장의 내구성 향상을 위해 사용된 고점도 바인더는 아스팔트 혼합물의 생산 및 시공온도를 증가시키게 된다. 또한 굵은골재의 비율이 높은 개립도 아스팔트 혼합물의 경우 운반과정과 포설 과정에서 온도가 빨리 떨어지는 단점이 있다. 이를 극복하기 위하여 중온 첨가제의 사용을 통해 생산 및 다짐온도를 낮추고자 하였다. 소입경 저소음 포장의 배합설계 과정은 배수성 포장의 배합설계 과정과 유사하나, 칸타브로 손실률과 흐름실험의 변곡점을 기준으로 할 경우, 칸타브로 손실률과 흐름 손실률이 매우 작아 변곡점을 판단하기 어렵기 때문에 칸타브로 손실률과 흐름 손실률의 기준 만족 여부로 판별하고, 최적 아스팔트 함량은 공극률을 기준으로 산정하는 것이 바람직할 것으로 판단된다. 중온 첨가제를 사용할 경우는 중온 첨가제로 인한 점도의 변화를 감안하여 혼합 및 다짐 온도를 결정하고 배합 설계를 수행하며, 중온 첨가제의 특성과 양에 따라 최적 아스팔트 함량이 변화하게 된다.
The effect of modified asphalts is evaluated by simple comparison of a single parameter (i.e., tensile strength, stiffness, etc.) between modified asphalt mixture and unmodified mixture. The use of a single parameter to evaluate the effect of modified asphalt must be questioned. Rather, a single unified framework that accounts for changes in key mixture properties is needed to effectively evaluate the modified asphalt mixtures. This study used a new performance-based fracture parameter as a single unified framework, the Energy Ratio (ER), for quantifying the effect of modified asphalts oil the fracture resistance of mixtures. The Energy Ratio was then used as a performance criterion for calculating the construction cost of two modified asphalt pavements (SBS and Crumb Rubber) and unmodified asphalt pavement. The results showed that the Energy Ratio of SBS modified asphalt was higher than those of crumb rubber and unmodified asphalt. Cost analyses indicated that the construction cost of the AC layer would be reduced by up to 24% by SBS modification. Based on the results, the Energy Ratio is capable of evaluating the effect of modified mixtures, and may form the basis of a promising fracture criterion for performance-based thickness design in asphalt pavements.
The field plate load test has a good potential for determining modulus since it measures both plate pressure and settlement. Conventionally the modulus has been assumed to be a constant secant value defined from the settlement of the plate at a given load intensity. A constant modulus (modulus of subgrade reaction, k), however, may not be a representative value of subgrade soil under working load. Field strain(o. stress)-dependent modulus characteristics of subgrade soils, at relatively low to intermediate strains, are important in the pavement design. In this study, the field strain dependent moduli of subgrade soils were obtained using cyclic plate load test. Testing procedure and data reduction method are proposed. The field crosshole and laboratory resonant column tests were also performed to determine field nonlinear modulus at $0.001\%\;to\;0.1\%$ strains, and the modulus values and nonlinear trends are compared to those obtained by cyclic plate load tests. Both modulus values match relatively well when the different state of stress between two tests was considered, and the applicability of field cyclic plate load test for determining nonlinear modulus values of subgrade soils is verified.
Asphalt pavements have to perform under the conditions of heavily-loaded vehicles due to the industrialization and large temperature variance between the summer and the winter. Due to these factors, a characteristics change of early permanent deformation becomes a big issue, and to remedy this problem many research to use modified asphalt are being widely conducted. However, most of the modified asphalt is being paved after milling the surface course and applying tackcoating, and it is being used mostly for the repair and maintenance purpose rather than pavement of new national road. The purpose of this investigation is to obtain some fundamental data for the evaluation of the performance and long-term performance of the construction material mixtures by the laboratory test and field experiments. For the field experiment, 200m of two-lanes national road, that is being paved for the new national road under the direction of Pusan Regional Construction Management Office, was paved with SBS PMA and PSMA asphalt mixtures, which are an modified asphalt mixtures used for the surface course, on top of the base course paved with other modified asphalt mixtures. The remaining section of the new national road was paved with dense grade mixture. The laboratory tests assessed and analyzed the mixture characteristics by Marshall's stability test, strength tests and wheel-tracking test. On the basis of the evaluation result of the temperature control and roughness of the newly constructed road at the field experiment site, it is desired to evaluate and identify the most economic modified asphalt mixtures by long-term performance evaluation and LCC(Life Cycle Cost) analysis in order to apply the test result to the design of new road construction in the future.
Kim, Jong-Min;Kim, Jang-Wook;Noh, Kwan-Sub;Kim, Kyung-Tae
International Journal of Highway Engineering
/
v.14
no.1
/
pp.35-43
/
2012
The Government is implementing the safety measures for pedestrian in living zone to decrease the traffic accident casualties in half. It is urgently to study the guideline because it contains to make the guideline of a median strip in City to prevent the violation of central line and jaywalking on the main contents. So, this study analyzed the pedestrian accidents and the violation of central line, and studied the type of a median strip, the installation guideline through studying the minimum crossing. Consequently, this study found out that a median strip which revised the attention inducement stick to decrease jaywalking could not have the strong prevention function of a crash barrier, so if it happens separation after the collision between vehicles, it induced the secondary accidents, and could take negative effects on traffic safety. In consideration of driving safety, this study analyzed that if it installs a median stirp, it has to ensure one meter, and such a thing could prevent the separation of lane or damage of facilities. However, if it is hard to ensure the space because of narrow road width, it could install a median strip in case of installing the road surface mark 0.5m. And the installation of the attention inducement stick or a median strip on the central line could be possible to induce the violation of central line, thus it is desirable not to install only anythings but also raised pavement markers.
Recently, a top record of hourly-based rainfall has been changed annually and flood damages of road have increased. To solve this problem, pavements for drainage were developed and practically constructed but there was no considerations on sub-base. In this research, we proposed standard for distribution of particle size of sub-base to consider strength characteristic and drainage property. We focused to compare coefficients strength and permeability by laboratory tests. Prior to tests, 4 samples were selected under the consideration on the international or domestic design guideline. In the tests, strength characteristics were compared with resilient modulus. Also, permeability characteristics were compared with coefficient of upward and downward permeability. Resilient modulus was determined with MR test using cyclic triaxial testing system. Two permeability tests were carried out. One is variable head permeability test for downward drainage and the other is Rowe Cell test for upward drainage. In the case of Rowe Cell test, middle-sized sampler with 150mm diameter was used for this study. Consequentially, we tried to find the optimum distribution of particle size to satisfy both of strength and permeability characteristics for sub-base.
KSCE Journal of Civil and Environmental Engineering Research
/
v.31
no.3D
/
pp.433-439
/
2011
The frost depth(frost penetration) is used to install anti-frost heave layers in pavement designs. The freezing index is calculated by an annual accumulated value of multiplying the period of time with temperatures below zero, and the corresponding temperature. Therefore, the DAAT(daily average air temperature) calculation method may play an effect on the FI(freezing index). The Weather Observatory used to supply 4 average air temperatures per day, but currently supplies 8 per day. With this study, we divided the southern part(below FI=$350^{\circ}C{\cdot}day$) of the Korean peninsula into 6 areas according to site conditions(low embankment, embankment-cutting slope, and the cutting slope) and established a field measurement system for 15 positions to check the effects on the result of FI according to differing DAAT calculation methods. The air temperatures obtained by the field measurement system was used to calculate and compare the FI. As a result, the freezing index calculated based on the $DAAT_4(T_4)$ is normally greater by 3% than the one on $DAAT_8(T_8)$. In addition, the calibration equation for the freezing index using air temperatures was proposed through the research.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.