• 제목/요약/키워드: oxide particle

검색결과 725건 처리시간 0.028초

$TiO_2$ 두께에 따른 염료감응형 태양전지의 효율 변화 (The Effect of $TiO_2$ Thickness on the Performance of Dye-Sensitized Solar Cells)

  • 김대현;박미주;이성욱;최원석;홍병유
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.147-148
    • /
    • 2007
  • Dye-sensitized solar cell using conversion of solar energy to electrical energy appeared that which solves a environmental matter. The dye-sensitized solar cell uses nano-crystalline oxide semiconductor for absorbing dye. The $TiO_2$ is used most plentifully. The efficiency of the dye-sensitized solar cell changes consequently in the particle size, morphology, crystallization and surface state of the $TiO_2$. In this paper, we report The effect of titania$(TiO_2)$ thickness on the performance of dye-sensitized solar cells. Using doctor blade method, It produced the thickness of the $TiO_2$ with $7\;{\mu}m,\;10\;{\mu}m,\;13\;{\mu}m$. The efficiency was the best from $10{\mu}m$. It had relatively low efficiency on the thickness from $7\;{\mu}m\;to\;13\;{\mu}m$. The reason why it presents low efficiency on $7\;{\mu}m$ thickness is that excited electrons can not be delivered enough due to thin thickness of $7\;{\mu}m\;TiO_2$. And The reason why it presents low efficiency on $13\;{\mu}m$ thickness is that thick $13\;{\mu}m\;TiO_2$ can not penetrate the sunlight enough.

  • PDF

Modified Oxalate Method로 의해 합성한 LSCF Cathode의 전기적 특성 (Electrical Properties of Synthesis LSCF Cathode by Modified Oxalate Method)

  • 이미재;김세기;지미정;박상선;최영현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.30-31
    • /
    • 2006
  • The LSCF cathode for Solid Oxide Fuel Cell was investigated to develop high performance unit cell at intermediate temperature by modified oxalate method with different electrolyte. The LSCF precursors using oxalic acid, ethanol and $NH_4OH$ solution were prepared at $80^{\circ}C$, and pH was controlled as 2, 6, 7, 8, 9 and 10. The synthesis precursor powders were calcined at $800^{\circ}C$, $1000^{\circ}C$ and $1200^{\circ}C$ for 4hrs. Unit cells were prepared with the calcined LSCF cathode, buffer layer between cathode and each electrolyte that is the LSGM, YSZ, ScSZ and CeSZ. The synthesis LSCF powders by modified oxalate method were measured by scanning electron microscope and X-ray diffraction. The interfacial polarization resistance of cell was characterized by Solatron 1260 analyzer. The crystal of LSCF powders show single phase at pH 2, 6, 7, 8 and 9, and the average particle size was about $3{\mu}m$. The electric conductivity of synthesis LSCF cathode which was calcined at $1200^{\circ}C$ shows the highest value at pH 7. The cell consist of GDC had the lowest interfacial resistance (about 950 S/cm@650) of the cathode electrode. The polarization resistance of synthesis LSCF cathode by modified oxalate method has the value from 4.02 to 7.46ohm at $650^{\circ}C$. GDC among the electrolytes, shows the lowest polarization resistance.

  • PDF

필러의 입자크기가 고체전해질 연료전지용 밀봉유리의 열적 특성에 미치는 영향 (Effect of Particle Size of the Filler on the Thermal Properties of the Sealing Glass for Solid Oxide Fuel Cells)

  • 조민영;문지웅;이미재;최병현;박선민;황해진;최헌진
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.305-305
    • /
    • 2007
  • SOFC용 밀봉유리$({\sim}10.0{\times}10^{-7}/K)$의 열팽창 계수를 SUS430$({\sim}12.0{\times}10^{-7}/K)$ 인터커넥터에 매칭 시키기 위하여 모유리에 비하여 열팽창계수가 큰 $CaTiO_3\;({\sim}13.5{\times}10^{-7}/K)$ 입자를 필러로서 첨가하였다. 필러입자의 첨가량이 증가함에 따라 밀봉재의 열팽창 계수가 증가하고, 동일 함량의 필러를 첨가하는 경우 필러 입자의 크기가 작을 수록 밀봉재의 연화점 상승 폭이 커서 SUS430 기판과의 접합 상태가 불량해짐을 관찰하였다. 필 테스트, 접합시험, 미세구조 분석 등을 통하여 필러 입자 크기가 증가 할 수록 SUS430과의 접합이 가능한 범위 내에서 보다 많은 양의 필러를 첨가하는 것이 가능하기 때문에 열팽창 계수 제어가 용이하다는 것을 확인 할 수 있었다.

  • PDF

Ce$O_2$첨가 및 분말처리가 U$O_2$ 분말의 소결에 미치는 영향 (Effect of Ce$O_2$ Addition and Powder Treatment on the Sintering of U$O_2$ Powder)

  • 김형수;이영우;최창범;양명승;전풍일
    • 한국재료학회지
    • /
    • 제3권3호
    • /
    • pp.245-252
    • /
    • 1993
  • 순수 $UO_2$에 첨가량 변화 및 ball-milling 시간에 따른 (U, Ce)$O_2$ 분말의 특성과 각 조건별로 제조된 분말을 압분 및 소결하여 (U, Ce)$O_2$ 분말 특성에 따른 소결성을 비교 조사하였다. 실험 결과로 부터 ball-milling시간이 길어짐에 따라 입자들은 미세화되고, Ce$O_2$ 함량이 증가할수록 압분, 소결밀도는 저하 하였으며, $CeO_2$는 소결성을 저하시키는 산화물임을 확인하였다. 10wt%,$CeO_2$ 가 첨가된 (U, Ce)$O_2$ 분말의 경우, ball-milling 4시간 수행한 분말의 소결체가 기공의 수도 적고, 구형에 가까왔으며, 소결밀도가 가장 높았다. 이는 4시간 ball-milling한 (U, Ce)$O_2$분말이 비표면적이 크로 그의 packing ratio가 적절하였기 때문이다.

  • PDF

Cu 첨가된 Zr-Nb계 합금에서 열처리조건이 미세조직과 내식성에 미치는 영향 (Effects of Heat Treatment Conditions on Microstructure and Corrosion Resistance of Cu-contained Zr-Nb Alloy)

  • 최병권;백종혁;정용환
    • 열처리공학회지
    • /
    • 제17권4호
    • /
    • pp.223-229
    • /
    • 2004
  • The effects of the cooling and annealing conditions on the microstructures and corrosion properties were investigated for the Cu-contained Zr-Nb alloy (Zr-1.1Nb-0.07Cu). After annealing at $1050^{\circ}C$ for 15 min, the specimens were cooled by three methods of water quenching, air cooling, and furnace cooling. Widmanstatten structures were developed in both air- and furnace-cooled specimens, and the Widmanstatten plate width of the furnace-cooled specimens was wider than that of the air-cooled ones. The weight gain in the furnace-cooling case was higher than that in the air-cooling case. This could be the reason why the diffusion time was more enough during the furnace cooling than the air cooling. The oxide of the furnace-cooled specimen was nonunformly formed just beneath the Widmanstatten plate boundaries, where ${\beta}_{Zr}$ phases were exised concentrately. Compared with the $640^{\circ}C$ annealing after the water quenching, the $570^{\circ}C$ annealing could make the ${\beta}_{Nb}$ phases and a concomitant reduction of the Nb in the matrix, and then it could improve the corrosion resistance with the increase of the annealing time. It would be concluded that the corrosion resistance of the Zr-1.1Nb-0.07Cu was good when the Nb concentration in the matrix was reached at an equilibrium level and then the ${\beta}_{Nb}$ phase was formed.

잉크젯 프린팅을 이용한 초박막 투명 TiO2 코팅층 제조 (Preparation of Ultra-Thin Transparent TiO2 Coated Film by Ink-Jet Printing Method)

  • 윤초롱;오효진;이남희;;이원재;박경순;김선재
    • 한국표면공학회지
    • /
    • 제40권4호
    • /
    • pp.190-196
    • /
    • 2007
  • Dye sensitized solar cells(DSSC) are the most promising future energy resource due to their high energy efficiency, low production cost, and simple manufacturing process. But one problem in DSSC is short life time compared to silicon solar cells. This problem occurred from photocatalytic degradation of dye material by nanometer sized $TiO_2$ particles. To prevent dye degradation as well as to increase its life time, the transparent coating film is needed for UV blocking. In this study, we synthesized nanometer sized $TiO_2$ particles in sols by increasing its internal pressure up to 200 bar in autoclave at $120^{\circ}C$ for 10 hrs. The synthesized $TiO_2$ sols were all formed with brookite phase and their particle size was several nm to 30 nm. Synthesized $TiO_2$ sols were coated on the backside of fluorine doped tin oxide(FTO) glass by ink jet printing method. With increasing coating thickness by repeated ink jet coating, the absorbance of UV region (under 400 nm) also increases reasonably. Decomposition test of titania powders dispersed in 0.1 mM amaranth solution covered with $TiO_2$ coating glass shows more stable dye properties under UV irradiation, compared to that with as-received FTO glass.

졸겔법으로 제작된 Al-doped ZnO 박막의 Aluminum Chloride 농도에 따른 구조적 및 광학적 특성 (Effects of Aluminum Chloride Concentrations on Structural and Optical Properties of Al-doped ZnO Thin Films Prepared by the Sol-Gel Method)

  • 조관식;김민수;임광국;이재용;임재영
    • 대한금속재료학회지
    • /
    • 제50권11호
    • /
    • pp.847-854
    • /
    • 2012
  • Al-doped ZnO (AZO) thin films were grown on quartz substrates by the sol-gel method. The effects of the Al mole fraction on the structural and optical properties of the AZO thin films were investigated by scanning electron microscopy (SEM), X-ray diffraction (XRD), and UV-VIS spectroscopy. The particle size of the AZO thin films decreased with an increase in Al concentrations. The optical parameters, the optical band gap, absorption coefficient, refractive index, dispersion parameter, and optical conductivity, were studied in order to investigate the effects of Al concentration on the optical properties of AZO thin films. The dispersion energy, single-oscillator energy, average oscillator wavelength, average oscillator strength, and refractive index at an infinite wavelength of the AZO thin films were affected by the Al incorporation. The optical conductivity of the AZO thin films also increased with increasing photon energy.

산화철계 가중응집제가 활성슬러지의 침전성 및 탈수성에 미치는 영향 (The effect of iron oxide ballasted flocculant on the activated sludge settleability and dewaterability)

  • 양혜지;김용범;최영균
    • 상하수도학회지
    • /
    • 제35권4호
    • /
    • pp.277-284
    • /
    • 2021
  • The ballasted flocculation effects of the mill scale and magnetite on activated sludge were investigated. Both ballasted flocculants (BF) could remarkably improve the sludge settleability in terms of zone settling velocity (ZSV) and sludge volume index (SVI). With the BF dosage of 0.2 to 2.0 g-BF/g-SS, the magnetite particles showed better efficiency on improving settling behavior of activated sludge than the mill scale due to higher surface area and hydrophobic property. The efficiency of SVI30 with magnetite injection was 2.5 to 11.3% higher than mill scale injection and that of the ZSV appreciated from 23.7% to 44.4% for magnetite injection. Averaged floc size of the BF sludge with magnetite dosage (0.5 g-BF/g-SS) was 2.3 times higher than that of the control sludge. Dewaterability of the sludge was also greatly improved by addition of the BF. The specific resistance to filtration (SRF) was reduced exponentially with increasing the dosage of BF. However, the BF's particle size effect on the SRF looks to be marginal. Consequently, for improving the dewaterability, the BF played a physical role to remove the pore water of the biological flocs by intrusive attachment and a chemical role to induce aggregation of the flocs by charge neutralization.

이온결합 형성에 따른 이액형 폴리우레탄 접착제의 기계적 특성 향상 (Enhancement of Mechanical Properties of 2K Polyurethane Adhesives via Forming Ionic Bonds)

  • 권하은;김두헌;김구니
    • 접착 및 계면
    • /
    • 제22권4호
    • /
    • pp.128-135
    • /
    • 2021
  • 본 연구에서는 acid group을 포함하는 acid 폴리올을 합성하였고, acid 폴리올을 함량별로 도입하여 신규 폴리우레탄 접착제를 개발하였다. Acid 폴리올 도입하였을 때 acid content가 0.1~0.3 wt%일 때 기계적 물성이 최댓값을 나타냈으며, 0.5 wt% 이상의 함량에서는 기계적 물성 및 접착 강도가 감소하는 것을 확인하였다. Acid group으로는 carboxylic acid와 sulfuric acid를 도입하여 특성을 비교하였으며, carboxylic acid가 sulfuric acid보다 강한 수소 결합력을 보이며 기계적 물성을 향상시켰다. 또한, ZnO와 CaCO3를 도입하여 입자의 크기와 물성의 상관관계를 확인하였다. ZnO와 CaCO3를 도입한 경우 acid group과 이온결합이 형성되어 기계적 물성이 증가하는 것을 확인하였다.

반연속주조된 대형 블룸에서 발생하는 거시편석 및 석출물 거동 (Behavior of Macrosegregation and Precipitation Developed in Semi-continuously Cast Large Bloom)

  • 김혜주;이형록;김경아;이주동;오경식;권상흠;김동규
    • 한국주조공학회지
    • /
    • 제39권1호
    • /
    • pp.7-13
    • /
    • 2019
  • Few studies of large blooms over 700 mm thick among those used for the forging of raw materials have been reported. The cooling rate difference between the surface and the center of a large bloom is large, and the degradation of the mechanical properties is likely in cases involving excessively coarse precipitates resulted from the slow cooling rate of a large bloom after casting. Therefore, a schematic investigation of the growth behaviors of precipitates while varying their locations in blooms is necessary. The dissolution behaviors of precipitates were investigated by simulating a reheating process during which the bloom is heated to a high temperature. The segregation behavior of the as-cast large bloom was also investigated. Reheating specimens were obtained after an isothermal heat treatment at $1150^{\circ}C$ with various holding times to simulate the reheating process, with the samples undergoing a subsequent water quenching step. The precipitates were extracted using an electrolytic extractor and a particle size analysis was conducted with the aid of SEM, EDS, and TEM. In the present work, Al oxide, MnS and Nb carbide were mainly observed.