• 제목/요약/키워드: non-beryllium Ni-Cr alloy

검색결과 7건 처리시간 0.02초

베릴륨 불포함 치과 주조용 니켈-크롬 합금 중 금속의치상용 합금과 금속소부도재관용 합금의 부식에 관한연구 (Corrosion of the non-beryllium dental casting Ni-Cr alloys for the denture base framework metal and the porcelain-fused-to-metal crown)

  • 김홍식;송재상;박수철
    • 대한치과기공학회지
    • /
    • 제34권4호
    • /
    • pp.337-344
    • /
    • 2012
  • Purpose: This study examined the corrosion level by alloy type and pH, and used the corrosion levels as the dental health data. The study utilized one Ni-Cr alloy for the full and removable partial denture metal frameworks and two Ni-Cr alloys for porcelain-fused-to-metal crown, among the non-beryllium dental casting non-precious Ni-Cr alloys. Methods: The alloy specimens were manufactured in $10cm^2$ and stored in the corrosive solution(pH 2.2-4.4) in the electrical water bath($37^{\circ}C$) for seven days. Afterwards, the metal ions were quantitatively analyzed using the ICP. Results: Of the three metal alloys, Bellabond-Plus$^{(R)}$alloy and SOLIBOND N$^{(R)}$alloy, with 22% or higher chrome chemical contents, had higher corrosion resistance than Jdium-100$^{(R)}$alloy with 20% chrome chemical content. In all three alloys, the corrosion of Ni was highest, and metal ion corrosion was higher in the pH 2.2 corrosive solution. Conclusion: Although Ni-Cr alloy was not very corrosive, a Ni-allergic patient should not have Ni-Cr alloy prosthesis. The Ni-Cr alloy for porcelain-fused-to-metal crown should be designed for the dental porcelain to cover the whole crown.

베릴륨이 함유되지 않은 니켈-크롬 합금 코어와 코발트-크롬 합금 코어의 적합도 비교평가 (Comparison of the marginal and internal fit of cores fabricated by Ni-Cr alloy(non-beryllium) and Co-Cr alloy)

  • 김기백;김재홍;김웅철;김지환
    • 대한치과기공학회지
    • /
    • 제34권4호
    • /
    • pp.353-359
    • /
    • 2012
  • Purpose: The aim of this study measured and compared the marginal and internal fit of metal cores with two base metal alloy (Ni-Cr alloy(non-beryllium), Co-Cr alloy). Methods: Maxillary right first molar abutment fabricated by titanium was prepared for this study. Impressions(10ea) were made from titanium model, and study models were poured with improved dental stone. Wax cores of twenty were prepared for burn-out and casting. Ten wax cores cast Ni-Cr alloy(non-Be), and finally ten cast Co-Cr alloy. Marginal and internal fit of cores was evaluated using silicone replica technique and digital microscope(x160). The data were statistically analyzed with the independent samples t-test (${\alpha}$ <.05). Results: Mean(standard deviation, SD) marginal and internal fit total size of Ni-Cr alloy(non-Be) group was $73.3(14.4){\mu}m$ and of Co-Cr alloy group $65.6(17.4){\mu}m$. The marginal and internal fit total size of Ni-Cr alloy group(non-Be) was statistically significantly greater than that of Co-Cr alloy group (P=.004). Conclusion: Co-Cr alloy cores in this study had a better marginal fit than Ni-Cr alloy(non-Be) cores.

베릴륨이 포함되지 않은 도재용착주조관용 비 귀금속 합금의 재사용에 따른 금속과 도재간의 전단결합강도에 관한 연구 (The study of Shear Bond Strength on recasting of non-beryllium non-precious alloy for Porcelain between Metal)

  • 김소리;김웅철;김혜영;김지환
    • 대한치과기공학회지
    • /
    • 제35권1호
    • /
    • pp.43-48
    • /
    • 2013
  • Purpose: This study aimed to investigate the shear bond strength for non-precious alloy castings without beryllium, which has been used repeatedly for economical reason. Methods: The Schmitz-Schulmeyer test method was used to evaluate the shear bond strength between the non-beryllium Ni-Cr alloy Vera Bond 2V(AlbaDent, Inc. USA) and the Ceramco 3(Dentstply, York, PA, USA) porcelain powder. The maximum loading and shear bond strength were measured. The average shear strength(MPa) was analyzed with the one-way ANOVA and the Tukey's test( =.05). The fracture specimens were examined using Microscope to determine the failure pattern. Results: The mean shear bond strengths(SD) in MPa were group A(100% new metal) control 28.72(3.31); group B(50% new + 50% reused) 27.28(1.13); group C(all reused) 26.61(5.47). Microscope examination showed that group A and B specimens presented mixed failure, and group C specimens showed adhesive failure. Conclusion: In conclusion, forward this non-precious alloy dose not contain beryllium for how should use a more systematic study and for future advanced research is performed giving effect to be considered desirable.

베릴륨함유 치과 주조용 비귀금속 합금의 젖산용액에 의한 금속 노출수준 평가 (Evaluation of a metal level in non-precious metal alloys dental casting having beryllium by lactic acid Solution)

  • 박수철;장은진;한석윤
    • 대한치과기공학회지
    • /
    • 제33권2호
    • /
    • pp.121-128
    • /
    • 2011
  • Purpose: The purpose of this study is to investigate the level of each metal in non-precious metal alloys dental casting, still used even banned for use and trade by the law, for oral health. Methods: Two kinds of metal alloys were analyzed. One was Ticonium 100 for removable prosthesis and the other was Rexillium V for dental porcelain. Two samples of each metal alloy were made in 0.5g, 1.0g, and 1.5g. Total number of samples were 12. Two kinds of lactic acid Solution, pH7 and pH4.6, were injected into each samples. After injection, each samples had been for 21days ${\pm}$ 1 hour in the water tank of which temperature was $37^{\circ}C$. The level of metal was measured in each sample by inductively couplled plasma-atomic emission spectrometer. Results: In both metal alloys, metals, chrome, nickel, beryllium, and molybdenum, were founded. In Ticonium 1000, the highest level of nickel was 2.531ppm in 1.5g pH4.6 sample while the highest level of nickel was 4.062ppm in 1.5g pH4.6 sample of Rexillium V. In chemical composition of these methal alloys, chrome(14~17%) was much more than beryllium(1.95~1.99%) and molybdenum(5.0~9.0%) but berllium and molybdenum were founded more than chrome in samples. Therefore, chrome showed better anti-corrosion than other metal alloys. In both metal alloys, more metals were founded in higher pH level and more mass. Levels of chrome was significantly different in samples of both metal alloys in each pH level(p<0.05). Levels of nickels was significantly different in samples of both metal alloys in each pH level(p<0.05). Conclusion: For oral health, further studies are needed in nickel-chrome metal alloy and cobalt metal alloy of non-beryllium in addittion to beryllium metal alloy and also long-term studies needed in various period and other non-percious metal alloys for dental casting.

도재용착주조관용 Co-Cr계 비귀금속 합금의 전단결합강도 비교평가에 관한 연구 (The study on Comparison Evaluation of Shear Bond Strength of Co-Cr Based Alloy using for Porcelain Fused Metal)

  • 김희진;김부섭
    • 대한치과기공학회지
    • /
    • 제32권3호
    • /
    • pp.195-207
    • /
    • 2010
  • Purpose: The purpose of this study was to observe the microstructural changes of surface in the specimens, performing the shear bond strength testing. The currently most used non-precious alloys are nickel-chromium based alloys with or without beryllium. However, their biocompatibility has been questioned concerning possible damages to the health of the patient and professionals involved in the fabrication of prosthesis caused by long exposure to Ni and Be. An option to nickel-chromium alloys is the cobalt-chromium alloy, an alternative that does not sacrifice the physical properties of the metal porcelain systems. Studies in the animals substantially show that the cobalt-chromium alloys are relatively well tolerated, being therefore more biocompatible than the nickel-chromium alloys. Methods: Non-addition Be to nickel-chromium based alloy(Bellabond plus) and cobalt-chromium alloy which has been widely used(Wirobond C) fused with ZEO light porcelain classified control group and cobalt-chromium alloy which is developing alloy of Alphadent company in Korea(Alphadent alloy) fused with ZEO light porcelain classified experimental group. The specimens of $4mm{\times}4mm{\times}0.5mm$ were prepared as-cast and as-opaque to cast body to analyze the mechanical characteristic change, the microstructure of alloy surface. The phase change was used to observe through XRD analysis and OM/SEM was used to observe the surface of specimens as-cast and as-opaque to cast body. Chemical formation of their elements was measured with EDS. Then hardness was measured with Micro Vicker's hardness tester. Shear bond strength test thirty specimens of $10mm{\times}10mm{\times}2mm$ was prepared, veneered, 3mm high and 3mm in diameter, over the alloy specimens. The shear bond strength test was performed in a universal testing machine(UTM) with a cross head speed of 0.5mm/min. Ultimate shear bond strength data were analyzed with one-way ANOVA and the Scheffe's test (P<0.05). Within the limits of this study, the following conclusions were drawn: The X-ray diffraction analysis results for the as-cast and as-opaque specimens showed that the major relative intensity of Bellabond plus alloy were changed smaller than Wirobond C and Alphadent Co-Cr based alloys. Results: Microstructural analysis results for the opaque specimens showed all the alloys increased carbides and precipitation(PPT). Alphadent Co-Cr based alloy showed the carbides of lamellar type. The Vickers hardness results for the opaque specimens showed Wirobond C and Alphadent Co-Cr based alloys were increaser than before ascast, but Bellabond plus alloy relatively decreased. The mean shear bond strengths (MPa) were: 33.11 for Wirobond C/ZEO light; 25.00 for Alphadent Co-Cr alloy/ZEO light; 18.02 for Bellabond plus/ZEO light. Conclusion: The mean shear bond strengths for Co-Cr and Ni-Cr based alloy were significantly different. But the all groups showed metal-metal oxide modes in shear bond strengths test at the interface.

베릴륨이 포함되지 않은 도재용착용 비귀금속 합금과 세라믹간의 전단결합강도와 계면특성 (Shear Bond Strength and Interfacial Characterization of Ceramic to Beryllium Free Nonprecious Alloys for Porcelain Fused to Metal Crown)

  • 정인성;김치영
    • 한국콘텐츠학회논문지
    • /
    • 제10권11호
    • /
    • pp.228-234
    • /
    • 2010
  • 치과도재용 합금으로 사용되는 합금 중 베릴륨이 함유된 비귀금속 Ni-Cr합금과 베릴륨이 함유되지 않은 비귀금속 Ni-Cr합금 그리고 베릴륨이 함유되지 않은 비귀금속 Co-Cr 합금과 세라믹간의 결합강도와 파절양상 그리고 계면특성을 분석하고자 하였다. 결합강도는 만능시험기를 이용하여 전단력시험을 통하여 전단결합력을 측정하였으며, 전단시험에 의한 파단면을 이용하여 파절양상을 관찰하였다. 그리고 합금-도재간의 계면을 관찰하였다. 전단결합강도 측정 결과, 베릴륨이 포함된 T-3가 41.13(${\pm}5.11$)MPa로 가장 높게 나타났으며, 베릴륨이 포함된 VeraBond(40.72(${\pm}5.98$)MPa), Co-Cr 합금인 Wirobond(38.40(${\pm}9.66$)MPa), 베릴륨이 포함되지 않은 Verabond 2V(32.77(${\pm}4.31$)MPa), Bellabond N(28.63(${\pm}6.39$)MPa), Bellabond plus(24.97(${\pm}6.13$)MPa), Argeloy N.P. Star(22.69(${\pm}3.41$)MPa) 순으로 나타났다. 비귀금속 합금들과 세라믹간의 파절양상은 모든 시편에서 금속표면에 세라믹이 일부 부착된 복합파절(mixed failure) 양상을 보였다.

도재용착용 Non beryllium 합금의 degassing과 opaque의 소성술식에 따른 결합강도 분석 (Shear bond strength analysis of non beryllium PFM metal with degassing and opaque firing techniques)

  • 임중재;이상혁
    • 한국산학기술학회논문지
    • /
    • 제16권7호
    • /
    • pp.4357-4363
    • /
    • 2015
  • 본 연구는 베릴륨 함유하지 않은 Ni-Cr계 도재용 금속에 전용도재를 도포, 소성된 시편을 3점 굴곡 시험으로 결합강도를 측정하고, SAM/EDS로 표면성분관찰 실험한 AVOVA와 Tukey HSAD 사후검정을 실시한 결과는 다음과 같은 결론을 얻었다. 첫째. 모든 군에서 ISO 9693의 치과용 금속-도재 시편의 최소 결합강도의 최소치인 25 MPa의 전단결합강도를 상위하며 안정적인 결과값을 나타냈다. 둘째. 결합 강도는 대조군 V1은 $32.37{\pm}1.91MPa$으로 나타났고, 실험군 V2 $38.25{\pm}1.38MPa$, 실험군 V3 $46.43{\pm}2.14MPa$, 그리고 실험군 V4 $47.21{\pm}1.72MPa$, 순으로 나타났으며 통계적으로 유의한 차이를 보였다. 사후 검정 (Tukey's HSD test) 결과, 결합강도 실험결과 실험군 V4는, 대조군 V1보다 높게 나타났다. 셋째. 금속-도재의 결합에서 산화처리를 시행한 군보다 시행하지 않고 불투명 도재를 도포하고 소성한 군이 높게 나타났으며, paste불투명 도재보다 분말 불투명도재의 사용에 따른 결합강도가 더 높게 나타났다. 넷째. 실험군 V4는 금속과 도재의 결합강도 비교에서 가장 높게 나타났다.